메뉴 건너뛰기




Volumn 22, Issue 1, 1999, Pages 1-12

Iron and nickel Aluminide composites

Author keywords

Composite; Intermetallics; Iron aluminides; Mechanical preperties; Nickel aluminides

Indexed keywords

ALUMINA; BENDING STRENGTH; CORROSION RESISTANCE; INFILTRATION; INTERMETALLICS; IRON ALLOYS; NICKEL ALLOYS; SILICON CARBIDE; SINTERING; TITANIUM CARBIDE; TUNGSTEN CARBIDE; VOLUME FRACTION;

EID: 0032785951     PISSN: 02533839     EISSN: 21587299     Source Type: Journal    
DOI: 10.1080/02533839.1999.9670437     Document Type: Article
Times cited : (21)

References (45)
  • 1
    • 0027112368 scopus 로고
    • Mechanical Properties of Advanced Nickel Aluminides
    • Alexander, D. J., and Sikka, V. K., 1992. “Mechanical Properties of Advanced Nickel Aluminides,”. Mater. Sci. Eng., A152:114–119.
    • (1992) Mater. Sci. Eng. , vol.A152 , pp. 114-119
    • Alexander, D.J.1    Sikka, V.K.2
  • 3
    • 0026256168 scopus 로고
    • The Deformation and Fracture of Constrained Metal Sheets
    • Bannister, M., and Ashby, M. F., 1991. “The Deformation and Fracture of Constrained Metal Sheets,”. Acta Metall. Mater., 39 (11):2575–82.
    • (1991) Acta Metall. Mater. , vol.39 , Issue.11 , pp. 2575-2582
    • Bannister, M.1    Ashby, M.F.2
  • 6
    • 0000111559 scopus 로고
    • Effects of Deviations from Stoichiometry on the Strength Anomaly and Fracture Behavior of B-Doped FeAl
    • Carleton, R., George, E. P., and Zee, R. H., 1995. “Effects of Deviations from Stoichiometry on the Strength Anomaly and Fracture Behavior of B-Doped FeAl,”. Intermetallics, 3:433–441.
    • (1995) Intermetallics , vol.3 , pp. 433-441
    • Carleton, R.1    George, E.P.2    Zee, R.H.3
  • 7
    • 0024665190 scopus 로고
    • Thermodynamic Properties of the Co-W-C System
    • Guillermet, A. F., 1989. “Thermodynamic Properties of the Co-W-C System,”. Metall. Trans. A, 20A:935–56.
    • (1989) Metall. Trans. A , vol.20A , pp. 935-956
    • Guillermet, A.F.1
  • 8
    • 0030144914 scopus 로고    scopus 로고
    • Electrochemical Behavior of Tungsten-Carbide Hardmetals
    • Human, M. A., and Exner, H. E., 1996. “Electrochemical Behavior of Tungsten-Carbide Hardmetals,”. Mater. Sci. Eng., A209:180–191.
    • (1996) Mater. Sci. Eng. , vol.A209 , pp. 180-191
    • Human, M.A.1    Exner, H.E.2
  • 13
    • 0040283606 scopus 로고
    • Moisture-induced Environmental Embrittlement of Ordered Intermetallic Alloys at Ambient Temperatures
    • Liu C.T., Cahn R.W., Sauthoff G., (eds), Kluwer
    • Liu, C. T., 1992. “Moisture-induced Environmental Embrittlement of Ordered Intermetallic Alloys at Ambient Temperatures,”. In Ordered Intermetallics - Physical. Metallurgy and Mechanical Behaviour, Edited by:Liu, C. T., Cahn, R. W., and Sauthoff, G., 321–334. Kluwer.
    • (1992) Ordered Intermetallics - Physical. Metallurgy and Mechanical Behaviour , pp. 321-334
    • Liu, C.T.1
  • 14
    • 0039730305 scopus 로고
    • Nickel Aluminides for Structural Use
    • Liu, C. T., and Sikka, V. K., 1986. “Nickel Aluminides for Structural Use,”. JOM, 38 (5):19–21.
    • (1986) JOM , vol.38 , Issue.5 , pp. 19-21
    • Liu, C.T.1    Sikka, V.K.2
  • 16
    • 51249177892 scopus 로고
    • Identification of Thermodynamically Stable Ceramic Reinforcement Materials for Iron Aluminides
    • Misra, A. K., 1990. “Identification of Thermodynamically Stable Ceramic Reinforcement Materials for Iron Aluminides,”. Metall. Trans. A, 21A:441
    • (1990) Metall. Trans. A , vol.21A , pp. 441
    • Misra, A.K.1
  • 18
    • 0030894518 scopus 로고    scopus 로고
    • In-situ SEM Observation of the Fracture Behaviour of Titanium Carbide/Nickel Aluminide Composites
    • Plucknett, K. P., Becher, P. F., and Alexander, K. B., 1997. “In-situ SEM Observation of the Fracture Behaviour of Titanium Carbide/Nickel Aluminide Composites,”. J. of Microscopy, 185:206–216.
    • (1997) J. of Microscopy , vol.185 , pp. 206-216
    • Plucknett, K.P.1    Becher, P.F.2    Alexander, K.B.3
  • 26
    • 0001862414 scopus 로고
    • Selected Properties of Iron Aluminides
    • Schneibel J.H., Crimp M.A., (eds), Warrendale, PA: TMS
    • Schneibel, J. H., 1994. “Selected Properties of Iron Aluminides,”. In Processing, Properties, and Applications of Iron Aluminides, Edited by:Schneibel, J. H., and Crimp, M. A., Warrendale, PA:TMS.
    • (1994) Processing, Properties, and Applications of Iron Aluminides
    • Schneibel, J.H.1
  • 27
    • 85023937574 scopus 로고    scopus 로고
    • 1996 World Congress on Powder Metallurgy & Particulate Materials, Metal Powder Industries Federation
    • Schneibel, J. H., and Subramanian, R., “Bonding of WC with an Iron Aluminide (FeAl) Intermetallic,”. 1996 World Congress on Powder Metallurgy & Particulate Materials. Vol. 5, pp. 16–167–16–175. Metal Powder Industries Federation.
    • Bonding of WC with an Iron Aluminide (FeAl) Intermetallic , vol.5 , pp. 16-167
    • Schneibel, J.H.1    Subramanian, R.2
  • 29
    • 0005244298 scopus 로고    scopus 로고
    • Liquid-Phase Sintering of Iron Aluminide-Bonded Ceramics
    • German R.M., Messing G.L., Cornwall R.G., (eds), New York: Marcel Dekker
    • Schneibel, J. H., and Carmichael, C. A., 1996. “Liquid-Phase Sintering of Iron Aluminide-Bonded Ceramics,”. In Sintering Technology, Edited by:German, R. M., Messing, G. L., and Cornwall, R. G., 253–60. New York:Marcel Dekker.
    • (1996) Sintering Technology , pp. 253-260
    • Schneibel, J.H.1    Carmichael, C.A.2
  • 32
    • 0028570292 scopus 로고    scopus 로고
    • 3Al Composites
    • Graves J.A., Bowman R.R., Lewandowski J.J., (eds), MRS Symposium Proceedings, Pittsburgh, PA: MRS
    • 3Al Composites,”. MRS Symposium Proceedings. Intermetallic Matrix Composites III, Edited by:Graves, J. A., Bowman, R. R., and Lewandowski, J. J., Vol. 350, Pittsburgh, PA:MRS.
    • Intermetallic Matrix Composites III , vol.350
    • Schneibel, J.H.1    Alexander, K.B.2
  • 33
    • 0031711270 scopus 로고    scopus 로고
    • Pond R.C., Clark W.A.T., King A.H., Williams D.B., (eds), Boundaries and Interfaces in Materials: The David A. Smith Symposium, Warrendale, PA: TMS
    • 2 Composites,”. Boundaries and Interfaces in Materials:The David A. Smith Symposium. Edited by:Pond, R. C., Clark, W. A. T., King, A. H., and Williams, D. B., pp. 315–321. Warrendale, PA:TMS.
    • 2 Composites , pp. 315-321
    • Schneibel, J.H.1    Subramanian, R.2
  • 35
    • 0023385812 scopus 로고
    • Experimental Study of the Mechanics of Fracture in WC-Co Alloys
    • July
    • Sigl, L. S., and Exner, H. E., 1987. “Experimental Study of the Mechanics of Fracture in WC-Co Alloys,”. Metall. Trans. A, 18A July:1299–1308.
    • (1987) Metall. Trans. A , vol.18A , pp. 1299-1308
    • Sigl, L.S.1    Exner, H.E.2
  • 38
    • 0038270218 scopus 로고    scopus 로고
    • FeAl-TiC Cermets - Melt Infiltration Processing and Mechanical Properties
    • Subramanian, R., and Schneibel, J. H., 1997. “FeAl-TiC Cermets - Melt Infiltration Processing and Mechanical Properties,”. Mater. Sci. Eng., A239–240:633–9.
    • (1997) Mater. Sci. Eng. , vol.A239–240 , pp. 633-639
    • Subramanian, R.1    Schneibel, J.H.2
  • 39
    • 0032021519 scopus 로고    scopus 로고
    • FeAl-TiC and FeAl-WC Composites - Melt Infiltration Processing, Microstructure and Mechanical Properties
    • Subramanian, R., and Schneibel, J. H., 1998. “FeAl-TiC and FeAl-WC Composites - Melt Infiltration Processing, Microstructure and Mechanical Properties,”. Mater. Sci. Eng., A244:103–112.
    • (1998) Mater. Sci. Eng. , vol.A244 , pp. 103-112
    • Subramanian, R.1    Schneibel, J.H.2
  • 40
    • 0031207005 scopus 로고    scopus 로고
    • Intermetallic Bonded WC-based Cermets by Pressureless Melt Infiltration
    • June
    • Subramanian, R., and Schneibel, J. H., 1997. “Intermetallic Bonded WC-based Cermets by Pressureless Melt Infiltration,”. Intermetallics, 5 (4) June:401–408.
    • (1997) Intermetallics , vol.5 , Issue.4 , pp. 401-408
    • Subramanian, R.1    Schneibel, J.H.2
  • 41
    • 0031207373 scopus 로고    scopus 로고
    • Processing Iron-Aluminide Composites Containing Carbides and Borides
    • Subramanian, R., and Schneibel, J. H., 1997. “Processing Iron-Aluminide Composites Containing Carbides and Borides,”. JOM, 49 (8):50–54. 68
    • (1997) JOM , vol.49 , Issue.8 , pp. 68-54
    • Subramanian, R.1    Schneibel, J.H.2
  • 42
    • 0032132140 scopus 로고    scopus 로고
    • The Ductile-Brittle Size Transition of Iron Aluminide Ligaments in an FeAl/TiC Composite
    • Subramanian, R., and Schneibel, J. H., 1998. “The Ductile-Brittle Size Transition of Iron Aluminide Ligaments in an FeAl/TiC Composite,”. Acta Mater., 46 (13):4733–4741.
    • (1998) Acta Mater. , vol.46 , Issue.13 , pp. 4733-4741
    • Subramanian, R.1    Schneibel, J.H.2
  • 43
    • 85023950124 scopus 로고    scopus 로고
    • Iron Aluminide-Titanium Carbide Composites - Microstructure and Mechanical Properties, in 1996 World Congress on Powder Metallurgy & Particulate Materials, 6 vols
    • Subramanian, R., Schneibel, J. H., and Alexander, K. B., 1996. Iron Aluminide-Titanium Carbide Composites - Microstructure and Mechanical Properties, in 1996 World Congress on Powder Metallurgy & Particulate Materials, 6 vols. Metal Powder Industries Federation, 5:16–159–16–165.
    • (1996) Metal Powder Industries Federation , vol.5 , pp. 16-159
    • Subramanian, R.1    Schneibel, J.H.2    Alexander, K.B.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.