1
-
-
0020098385
-
-
Nagarajan, R.; Kalpacki, B. Polym. Prepr. Am. Chem. Soc., Div. Polym. Chem. 1982, 23, 41.
-
(1982)
Polym. Prepr. Am. Chem. Soc., Div. Polym. Chem.
, vol.23
, pp. 41
-
-
Nagarajan, R.1
Kalpacki, B.2
-
2
-
-
0000778643
-
-
Francois, J.; Dayantis, J.; Sabbadin, J. Eur. Polym. J. 1985, 21, 165.
-
(1985)
Eur. Polym. J.
, vol.21
, pp. 165
-
-
Francois, J.1
Dayantis, J.2
Sabbadin, J.3
-
4
-
-
36449007358
-
-
Chari, K.; Antalek, B.; Lin, M. Y.; Sinha, S. K. J. Chem. Phys. 1994, 100, 5294.
-
(1994)
J. Chem. Phys.
, vol.100
, pp. 5294
-
-
Chari, K.1
Antalek, B.2
Lin, M.Y.3
Sinha, S.K.4
-
6
-
-
0034227594
-
-
Mya, K. Y.; Jamieson, A. M.; Sirivat, A. Langmuir 2000, 16, 6131.
-
(2000)
Langmuir
, vol.16
, pp. 6131
-
-
Mya, K.Y.1
Jamieson, A.M.2
Sirivat, A.3
-
7
-
-
0035870358
-
-
Smitter, L.; Guedez, A. J.; Muller, A. J.; Saez, A. E. J. Colloid Interface Sci. 2001, 236, 343.
-
(2001)
J. Colloid Interface Sci.
, vol.236
, pp. 343
-
-
Smitter, L.1
Guedez, A.J.2
Muller, A.J.3
Saez, A.E.4
-
8
-
-
1542274850
-
-
note
-
In the absence of added electrolyte, one observes a peak in viscosity at saturation. The reason for the peak is explained in the earlier references.
-
-
-
-
9
-
-
0000552707
-
-
Chari, K.; Antalek, B.; Minter, J. Phys. Rev. Lett. 1995, 74, 3624.
-
(1995)
Phys. Rev. Lett.
, vol.74
, pp. 3624
-
-
Chari, K.1
Antalek, B.2
Minter, J.3
-
13
-
-
85089110602
-
-
note
-
w = 8000). In our case, the polymer coil is much larger.
-
-
-
-
15
-
-
0642303347
-
-
Thiyagarajan, P.; Epperson, J. E.; Crawford, R. K.; Carpenter, J. M.; Klippert, T. E.; Wozniak, D. G. J. Appl. Crystallogr. 1997, 30, 280.
-
(1997)
J. Appl. Crystallogr.
, vol.30
, pp. 280
-
-
Thiyagarajan, P.1
Epperson, J.E.2
Crawford, R.K.3
Carpenter, J.M.4
Klippert, T.E.5
Wozniak, D.G.6
-
20
-
-
0000928475
-
-
Dobrynin, A. V.; Colby, R. H.; Rubinstein, M. Macromolecules 1995, 28, 1859 and references therein.
-
(1995)
Macromolecules
, vol.28
, pp. 1859
-
-
Dobrynin, A.V.1
Colby, R.H.2
Rubinstein, M.3
-
22
-
-
1542274851
-
-
note
-
The scattering peak corresponds to a spacing d = 2π/Q of 44 Å. For a milcelle radius of 20 Å this is equivalent to a surface-to-surface distance of 4 Å that is of the order of the electrical double layer thickness at this salt concentration.
-
-
-
-
26
-
-
0025414291
-
-
The results are reminiscent of those obtained by Winnik, F. M.; Ringsdorf, H.; Venzmer, J. Macromolecules 1990, 23, 2415
-
(1990)
Macromolecules
, vol.23
, pp. 2415
-
-
Winnik, F.M.1
Ringsdorf, H.2
Venzmer, J.3
-
27
-
-
0026106531
-
-
and by Schild, H. G.; Muthukumar, M.; Tirrell, D. A. Macromolecules 1991, 24, 948 on addition of methanol to a solution of poly(N-isopropylacrylamide) in water.
-
(1991)
Macromolecules
, vol.24
, pp. 948
-
-
Schild, H.G.1
Muthukumar, M.2
Tirrell, D.A.3
-
31
-
-
0021412230
-
-
Pincus, P. A.; Sandroff, C. J.; Witten, T. A. J. Phys. (Paris) 1984, 45, 725.
-
(1984)
J. Phys. (Paris)
, vol.45
, pp. 725
-
-
Pincus, P.A.1
Sandroff, C.J.2
Witten, T.A.3
-
33
-
-
4243212324
-
-
Bekiranov, S.; Bruinsma, R.; Pincus, P. Phys. Rev. E 1997, 55, 577 and references therein.
-
(1997)
Phys. Rev. E
, vol.55
, pp. 577
-
-
Bekiranov, S.1
Bruinsma, R.2
Pincus, P.3
-
34
-
-
36749108182
-
-
Cotton, J. P.; Nierlich, M.; Boue, F.; Daoud, M.; Farnoux, B.; Jannik, G.; Dupplessix, R.; Picot, C. J. Chem. Phys. 1978, 65, 1101.
-
(1978)
J. Chem. Phys.
, vol.65
, pp. 1101
-
-
Cotton, J.P.1
Nierlich, M.2
Boue, F.3
Daoud, M.4
Farnoux, B.5
Jannik, G.6
Dupplessix, R.7
Picot, C.8
-
36
-
-
0001072702
-
-
Colby, R. H.; Rubinstein, M.; Daoud, M. J. Phys. II France 1994, 4, 1299.
-
(1994)
J. Phys. II France
, vol.4
, pp. 1299
-
-
Colby, R.H.1
Rubinstein, M.2
Daoud, M.3
-
38
-
-
0011883913
-
-
Karlstrom, G.; Carlsson, A.; Lindman, B. J. Phys. Chem. 1990, 94, 5005.
-
(1990)
J. Phys. Chem.
, vol.94
, pp. 5005
-
-
Karlstrom, G.1
Carlsson, A.2
Lindman, B.3
|