Volumn 83, Issue 18, 2003, Pages 3800-3802

Fabrication and electrical characterization of polyaniline-based nanofibers with diameter below 30 nm

Author keywords

[No Author keywords available]

Indexed keywords

ATOMIC FORCE MICROSCOPY; CONDUCTIVE PLASTICS; CURRENT VOLTAGE CHARACTERISTICS; ELECTRIC CONDUCTIVITY; ELECTRONIC PROPERTIES; GRAIN SIZE AND SHAPE; MOLECULAR WEIGHT; NATURAL FIBERS; POLYETHYLENE OXIDES; POLYMER BLENDS; SCANNING ELECTRON MICROSCOPY;

EID: 0345359878     PISSN: 00036951     EISSN: None     Source Type: Journal    
DOI: 10.1063/1.1622108     Document Type: Article
Times cited : (199)

References (13)
  • 6
    • 0344861305 scopus 로고    scopus 로고
    • note
    • Semiconducting SWNTs are doped by exposure to atmosphere and have a one-dimensional conductivity well above the SCM detection limit.
  • 7
    • 0345724249 scopus 로고    scopus 로고
    • note
    • PEO nanofibers were electrospun from a solution of 50 mg PEO (mol. wt. 900 000) dissolved in 10 ml chloroform and collected on an oxidized silicon wafer. SCM of insulating and conducting fibers will be discussed in detail elsewhere [C. Staii, N. Pinto, and A. T. Johnson (unpublished)].
  • 8
    • 0344861304 scopus 로고    scopus 로고
    • note
    • Fibers are dedoped when placed in water, with a color change from green to deep blue. Nanofibers show an age-dependent conductivity if left in air that is minimized if they are stored in a water-free atmosphere [J. Goldsmith, A.G. MacDiarmid, and A.T. Johnson (unpublished)].