Volumn 19, Issue 6, 2003, Pages 542-551

Stress distribution and failure mode of dental ceramic structures under Hertzian indentation

Author keywords

Ceramic strength; Dental materials; Hertzian indentation; Stress distribution

Indexed keywords

DENTAL MATERIALS; FAILURE (MECHANICAL); INDENTATION; STRESS CONCENTRATION; SUBSTRATES; SURFACE PROPERTIES; TENSILE STRENGTH;

EID: 0041491460     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0109-5641(02)00103-3     Document Type: Article
Times cited : (49)

References (43)
  • 1
    • 0025492382 scopus 로고
    • Fracture-surface analysis of dental ceramic: Clinically failed restorations
    • Kelly J.R., Giordano R., Pober R., Cima M.J. Fracture-surface analysis of dental ceramic: clinically failed restorations. Int J Prosthodont. 3:(5):1990;430-440.
    • (1990) Int J Prosthodont , vol.3 , Issue.5 , pp. 430-440
    • Kelly, J.R.1    Giordano, R.2    Pober, R.3    Cima, M.J.4
  • 2
    • 0027655860 scopus 로고
    • The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli
    • Scherrer S.S., de Rijk W.G. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. Int J Prosthodont. 6:(5):1993;462-467.
    • (1993) Int J Prosthodont , vol.6 , Issue.5 , pp. 462-467
    • Scherrer, S.S.1    De Rijk, W.G.2
  • 3
    • 0028511896 scopus 로고
    • In vitro fracture behaviour of ceramic and metal-ceramic restorations
    • Smith T.B., Kelly J.R., Tesk J.A. In vitro fracture behaviour of ceramic and metal-ceramic restorations. J Prosthodont. 3:1994;138-144.
    • (1994) J Prosthodont , vol.3 , pp. 138-144
    • Smith, T.B.1    Kelly, J.R.2    Tesk, J.A.3
  • 4
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • Thompson J.Y., Anusavice K.J., Naman A., Morris H.F. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res. 73:(12):1994;1824-1832.
    • (1994) J Dent Res , vol.73 , Issue.12 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Naman, A.3    Morris, H.F.4
  • 5
    • 0028476223 scopus 로고
    • Fracture strength of all-cerarnic crowns
    • Yoshinari M., Dérand T. Fracture strength of all-cerarnic crowns. Int J Prosthodont. 7:(4):1994;329-338.
    • (1994) Int J Prosthodont , vol.7 , Issue.4 , pp. 329-338
    • Yoshinari, M.1    Dérand, T.2
  • 6
    • 0029444234 scopus 로고
    • In-ceram failure behavior and core-veneer interface quality as influenced by residual infiltration glass
    • Carrier D.D., Kelly J.R. In-Ceram failure behavior and core-veneer interface quality as influenced by residual infiltration glass. J Prosthodont. 4:(4):1995;237-242.
    • (1995) J Prosthodont , vol.4 , Issue.4 , pp. 237-242
    • Carrier, D.D.1    Kelly, J.R.2
  • 7
    • 0029318343 scopus 로고
    • Failure of all-ceramic crown fixed partial dentures in vivo and in vitro: Analysis and modeling
    • Kelly J.R., Tesk J.A., Sorensen J.A. Failure of all-ceramic crown fixed partial dentures in vivo and in vitro: analysis and modeling. J Dent Res. 74:(6):1995;1253-1258.
    • (1995) J Dent Res , vol.74 , Issue.6 , pp. 1253-1258
    • Kelly, J.R.1    Tesk, J.A.2    Sorensen, J.A.3
  • 8
    • 0033146116 scopus 로고    scopus 로고
    • Clinically relevant approach to failure testing of all-ceramic restorations
    • Kelly J.R. Clinically relevant approach to failure testing of all-ceramic restorations. J Prosthet Dent. 81:1999;652-661.
    • (1999) J Prosthet Dent , vol.81 , pp. 652-661
    • Kelly, J.R.1
  • 9
  • 10
    • 0025224747 scopus 로고
    • Three-dimensional finite element analysis of glass-ceramic crown
    • Hojjatie B., Anusavice K.J. Three-dimensional finite element analysis of glass-ceramic crown. J Biomech. 23:(11):1990;1157-1166.
    • (1990) J Biomech , vol.23 , Issue.11 , pp. 1157-1166
    • Hojjatie, B.1    Anusavice, K.J.2
  • 11
    • 0026891764 scopus 로고
    • Tensile stress in glass-ceramic crowns: Effect of flaws and cement voids
    • Anusavice K.J., Hojjatie B. Tensile stress in glass-ceramic crowns: effect of flaws and cement voids. Int J Prosthodont. 5:(4):1992;351-358.
    • (1992) Int J Prosthodont , vol.5 , Issue.4 , pp. 351-358
    • Anusavice, K.J.1    Hojjatie, B.2
  • 12
    • 0030154926 scopus 로고    scopus 로고
    • Contact damage as a failure mode during in vitro testing
    • Harvey C.K., Kelly J.R. Contact damage as a failure mode during in vitro testing. J Prosthodont. 5:(2):1996;95-100.
    • (1996) J Prosthodont , vol.5 , Issue.2 , pp. 95-100
    • Harvey, C.K.1    Kelly, J.R.2
  • 13
    • 0032223649 scopus 로고    scopus 로고
    • Mechanical characterization of dental ceramics by Hertzian contacts
    • Peterson I.M., Pajares A., Lawn B.R., Thompson V.P., Rekow E.D. Mechanical characterization of dental ceramics by Hertzian contacts. J Dent Res. 77:(4):1998;589-602.
    • (1998) J Dent Res , vol.77 , Issue.4 , pp. 589-602
    • Peterson, I.M.1    Pajares, A.2    Lawn, B.R.3    Thompson, V.P.4    Rekow, E.D.5
  • 14
    • 0031598699 scopus 로고    scopus 로고
    • Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics
    • Peterson I.M., Wuttiphan S., Lawn B.R., Chyung K. Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics. Dent Mater. 14:(1):1998;80-89.
    • (1998) Dent Mater , vol.14 , Issue.1 , pp. 80-89
    • Peterson, I.M.1    Wuttiphan, S.2    Lawn, B.R.3    Chyung, K.4
  • 15
    • 0031619605 scopus 로고    scopus 로고
    • Influence of glass-ceramic thickness on Hertzian and bulk fracture mechanisms
    • Tsai Y.L., Petsche P.E., Anusavice K.J., Yang M.C. Influence of glass-ceramic thickness on Hertzian and bulk fracture mechanisms. Int J Prosthodont. 11:(1):1998;27-32.
    • (1998) Int J Prosthodont , vol.11 , Issue.1 , pp. 27-32
    • Tsai, Y.L.1    Petsche, P.E.2    Anusavice, K.J.3    Yang, M.C.4
  • 16
    • 0033278008 scopus 로고    scopus 로고
    • Contact damage resistance and strength degradation of glass-infiltrated alumina and spinel ceramics
    • Jung Y.G., Peterson I.M., Pajares A., Lawn B.R. Contact damage resistance and strength degradation of glass-infiltrated alumina and spinel ceramics. J Dent Res. 78:(3):1999;804-818.
    • (1999) J Dent Res , vol.78 , Issue.3 , pp. 804-818
    • Jung, Y.G.1    Peterson, I.M.2    Pajares, A.3    Lawn, B.R.4
  • 18
    • 0035353997 scopus 로고    scopus 로고
    • Contact-induced damage in ceramic coatings on compliant substrates: Fracture mechanics and design
    • Rhee Y.W., Kim H.W., Deng Y., Lawn B.R. Contact-induced damage in ceramic coatings on compliant substrates: Fracture mechanics and design. J Am Ceram Soc. 84:(5):2001;1066-1072.
    • (2001) J Am Ceram Soc , vol.84 , Issue.5 , pp. 1066-1072
    • Rhee, Y.W.1    Kim, H.W.2    Deng, Y.3    Lawn, B.R.4
  • 19
    • 0035512807 scopus 로고    scopus 로고
    • Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: A review
    • Lawn B.R., Deng Y., Thompson V.P. Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: a review. J Prosthet Dent. 86:(5):2001;495-510.
    • (2001) J Prosthet Dent , vol.86 , Issue.5 , pp. 495-510
    • Lawn, B.R.1    Deng, Y.2    Thompson, V.P.3
  • 20
    • 0036565362 scopus 로고    scopus 로고
    • Cracking in ceramic/metal/polymer trilayer systems
    • Zhao H., Miranda P., Lawn B.R., Hu X.Z. Cracking in ceramic/metal/polymer trilayer systems. J Mater Res. 17:(5):2002;1102-1111.
    • (2002) J Mater Res , vol.17 , Issue.5 , pp. 1102-1111
    • Zhao, H.1    Miranda, P.2    Lawn, B.R.3    Hu, X.Z.4
  • 21
    • 0036206982 scopus 로고    scopus 로고
    • Characterization of damage modes in dental ceramic bilayer structures
    • Deng Y., Lawn B.R., Lloyd I.K. Characterization of damage modes in dental ceramic bilayer structures. J Biomed Mater Res. 63:(2):2002;137-145.
    • (2002) J Biomed Mater Res , vol.63 , Issue.2 , pp. 137-145
    • Deng, Y.1    Lawn, B.R.2    Lloyd, I.K.3
  • 22
    • 0032137856 scopus 로고    scopus 로고
    • Indentation of ceramics with spheres: A century after Hertz
    • Lawn B.R. Indentation of ceramics with spheres: a century after Hertz. J Am Ceram Soc. 81:(8):1998;1977-1994.
    • (1998) J Am Ceram Soc , vol.81 , Issue.8 , pp. 1977-1994
    • Lawn, B.R.1
  • 23
    • 0028437167 scopus 로고
    • Fracture resistance of teeth restored with dentine-bonded crown
    • Burke F.J., Watts D.C. Fracture resistance of teeth restored with dentine-bonded crown. Quint Int. 25:1994;335-340.
    • (1994) Quint Int , vol.25 , pp. 335-340
    • Burke, F.J.1    Watts, D.C.2
  • 24
    • 0034441675 scopus 로고    scopus 로고
    • Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness
    • Wakabayashi N., Anusavice K.J. Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness. J Dent Res. 79:(6):2000;1398-1404.
    • (2000) J Dent Res , vol.79 , Issue.6 , pp. 1398-1404
    • Wakabayashi, N.1    Anusavice, K.J.2
  • 27
    • 0032595445 scopus 로고    scopus 로고
    • Fracture modes in brittle coatings with large interlayer modulus mismatch
    • Chai H., Lawn B.R., Wuttiphan S. Fracture modes in brittle coatings with large interlayer modulus mismatch. J Mater Res. 14:(9):1999;3805-3817.
    • (1999) J Mater Res , vol.14 , Issue.9 , pp. 3805-3817
    • Chai, H.1    Lawn, B.R.2    Wuttiphan, S.3
  • 28
    • 0034256180 scopus 로고    scopus 로고
    • Cracking of bilayer coatings adhesively bonded to substrate of unlike modulus
    • Lee K.S., Rhee Y.-W., Blackburn D.H., Lawn B.R. Cracking of bilayer coatings adhesively bonded to substrate of unlike modulus. J Mater Res. 15:(8):2000;1653-1656.
    • (2000) J Mater Res , vol.15 , Issue.8 , pp. 1653-1656
    • Lee, K.S.1    Rhee, Y.-W.2    Blackburn, D.H.3    Lawn, B.R.4
  • 29
    • 0016826367 scopus 로고
    • Experimental determination of the rigidity modulus, Poisson's ratio and elastic limit in shear of human dentine
    • Renson C.E., Braden M. Experimental determination of the rigidity modulus, Poisson's ratio and elastic limit in shear of human dentine. Arch Oral Biol. 20:1975;43-47.
    • (1975) Arch Oral Biol , vol.20 , pp. 43-47
    • Renson, C.E.1    Braden, M.2
  • 30
    • 0027682681 scopus 로고
    • Assessment by nano-indentation of the hardness and elasticity of the resin-dentine bonding area
    • Meerbeek B.V., Willems G., Celis J.P., Roos J.R., Braem M., Lambrechts P., Vanherle G. Assessment by nano-indentation of the hardness and elasticity of the resin-dentine bonding area. J Dent Res. 72:(10):1993;1434-1442.
    • (1993) J Dent Res , vol.72 , Issue.10 , pp. 1434-1442
    • Meerbeek, B.V.1    Willems, G.2    Celis, J.P.3    Roos, J.R.4    Braem, M.5    Lambrechts, P.6    Vanherle, G.7
  • 31
    • 0030276099 scopus 로고    scopus 로고
    • Fracture resistance of human enamel and three all-ceramic crown systems: On extracted teeth
    • Scherrer S.S., de Rijk W.G., Belser U.C. Fracture resistance of human enamel and three all-ceramic crown systems: on extracted teeth. Int J Prosthodont. 9:1996;580-585.
    • (1996) Int J Prosthodont , vol.9 , pp. 580-585
    • Scherrer, S.S.1    De Rijk, W.G.2    Belser, U.C.3
  • 32
    • 0035468475 scopus 로고    scopus 로고
    • Determination of elastic modulus of dentin by small spherical diamond indenters
    • Poolthong S., Mori T., Swain M. Determination of elastic modulus of dentin by small spherical diamond indenters. Dent Mater J. 20:(3):2001;227-236.
    • (2001) Dent Mater J , vol.20 , Issue.3 , pp. 227-236
    • Poolthong, S.1    Mori, T.2    Swain, M.3
  • 33
    • 0028432232 scopus 로고
    • Structure-property relations and crack resistance at the bovine dentine-enamel junction
    • Lin C.P., Douglas W.H. Structure-property relations and crack resistance at the bovine dentine-enamel junction. J Dent Res. 73:(5):1994;1072-1078.
    • (1994) J Dent Res , vol.73 , Issue.5 , pp. 1072-1078
    • Lin, C.P.1    Douglas, W.H.2
  • 35
    • 0032044383 scopus 로고    scopus 로고
    • Microscopic and energy dispersive X-ray analysis of surface adaptation of dental cements to dental ceramic surfaces
    • Thompson J.Y., Rapp M.M., Parker A.J. Microscopic and energy dispersive X-ray analysis of surface adaptation of dental cements to dental ceramic surfaces. J Prosthet Dent. 79:(4):1998;378-383.
    • (1998) J Prosthet Dent , vol.79 , Issue.4 , pp. 378-383
    • Thompson, J.Y.1    Rapp, M.M.2    Parker, A.J.3
  • 36
    • 0034174580 scopus 로고    scopus 로고
    • Role of adhesive interlayer in transverse fracture of brittle layer structures
    • Chai H., Lawn B.R. Role of adhesive interlayer in transverse fracture of brittle layer structures. J Mater Res. 15:(4):2000;1017-1023.
    • (2000) J Mater Res , vol.15 , Issue.4 , pp. 1017-1023
    • Chai, H.1    Lawn, B.R.2
  • 37
    • 0028435856 scopus 로고
    • Finite element analysis estimates of cement microfracture under complete veneer crowns
    • Kamposiora P., Papavasilious G., Bayne S.C., Felton D.A. Finite element analysis estimates of cement microfracture under complete veneer crowns. J Prosthet Dent. 71:1994;435-441.
    • (1994) J Prosthet Dent , vol.71 , pp. 435-441
    • Kamposiora, P.1    Papavasilious, G.2    Bayne, S.C.3    Felton, D.A.4
  • 38
    • 0042778611 scopus 로고
    • The VITA hi-ceram crown system: A clinical and laboratory investigation
    • Abstr. No. 811
    • Scherrer S.S., Mojon P., Belser U.G., Meyer J.M. The VITA hi-ceram crown system: A clinical and laboratory investigation. J Dent Res. 67:1988;214. Abstr. No. 811.
    • (1988) J Dent Res , vol.67 , pp. 214
    • Scherrer, S.S.1    Mojon, P.2    Belser, U.G.3    Meyer, J.M.4
  • 39
    • 0023672023 scopus 로고
    • Comparison of fit of two types of all-ceramic crowns
    • Davis D.R. Comparison of fit of two types of all-ceramic crowns. J Prosthet Dent. 59:1988;12-16.
    • (1988) J Prosthet Dent , vol.59 , pp. 12-16
    • Davis, D.R.1
  • 40
    • 0029242639 scopus 로고
    • The effect of cement thickness on the fracture strength of all-ceramic crowns
    • Tuntiprawon M., Wilson P.R. The effect of cement thickness on the fracture strength of all-ceramic crowns. Aust Dent J. 40:(1):1995;17-21.
    • (1995) Aust Dent J , vol.40 , Issue.1 , pp. 17-21
    • Tuntiprawon, M.1    Wilson, P.R.2
  • 41
    • 0028440877 scopus 로고
    • Effect of cement film thickness on the fracture resistance of a machinable glass-ceramic
    • Scherrer S.S., de Rijk W.G., Belser U.G., Meyer J.M. Effect of cement film thickness on the fracture resistance of a machinable glass-ceramic. Dent Mater. 10:(5):1994;172-177.
    • (1994) Dent Mater , vol.10 , Issue.5 , pp. 172-177
    • Scherrer, S.S.1    De Rijk, W.G.2    Belser, U.G.3    Meyer, J.M.4
  • 42
    • 0033146045 scopus 로고    scopus 로고
    • Survival of Dicor glass-ceramic dental restorations over 14 years. Part II: Effect of thickness of Dicor materials and design of tooth preparation
    • Malament K.A., Socransky S.S. Survival of Dicor glass-ceramic dental restorations over 14 years. Part II: Effect of thickness of Dicor materials and design of tooth preparation. J Prosthet Dent. 81:(6):1999;662-667.
    • (1999) J Prosthet Dent , vol.81 , Issue.6 , pp. 662-667
    • Malament, K.A.1    Socransky, S.S.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.