Volumn 84, Issue 5, 2001, Pages 1066-1072

Contact-induced Damage in Ceramic Coatings on Compliant Substrates: Fracture Mechanics and Design

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; CRACK INITIATION; ELASTIC MODULI; FRACTURE MECHANICS; FRICTION; HARDNESS; PLASTICITY; POLYCARBONATES; PRODUCT DESIGN; STRENGTH OF MATERIALS; TOUGHNESS; ZIRCONIA;

EID: 0035353997     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.2001.tb00791.x     Document Type: Article
Times cited : (108)

References (38)
  • 2
    • 0032137856 scopus 로고    scopus 로고
    • Indentation of Ceramics with Spheres: A Century after Hertz
    • B. R. Lawn, "Indentation of Ceramics With Spheres: A Century After Hertz," J. Am. Ceram. Soc., 81 [8] 1977-94 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.8 , pp. 1977-1994
    • Lawn, B.R.1
  • 3
    • 0030691360 scopus 로고    scopus 로고
    • Ceramics in Restorative and Prosthetic Dentistry
    • J. R. Kelly, "Ceramics in Restorative and Prosthetic Dentistry," Ann. Rev. Mater. Sci., 27 443-68 (1997).
    • (1997) Ann. Rev. Mater. Sci. , vol.27 , pp. 443-468
    • Kelly, J.R.1
  • 4
    • 0032223649 scopus 로고    scopus 로고
    • Mechanical Characterization of Dental Ceramics Using Hertzian Contacts
    • I. M. Peterson, A. Pajares, B. R. Lawn, V. P. Thompson, and E. D. Rekow, "Mechanical Characterization of Dental Ceramics Using Hertzian Contacts," J. Dent. Res., 77 [4] 589-602 (1998).
    • (1998) J. Dent. Res. , vol.77 , Issue.4 , pp. 589-602
    • Peterson, I.M.1    Pajares, A.2    Lawn, B.R.3    Thompson, V.P.4    Rekow, E.D.5
  • 5
    • 0033146116 scopus 로고    scopus 로고
    • Clinically Relevant Approach to Failure Testing of All-Ceramic Restorations
    • J. R. Kelly, "Clinically Relevant Approach to Failure Testing of All-Ceramic Restorations," J. Prosthet. Dent., 81 [6] 652-61 (1999).
    • (1999) J. Prosthet. Dent. , vol.81 , Issue.6 , pp. 652-661
    • Kelly, J.R.1
  • 6
    • 84884280887 scopus 로고
    • Indentation Fatigue: A Simple Cyclic Hertzian Test for Measuring Damage Accumulation in Polycrystalline Ceramics
    • F. Guiberteau, N. P. Padture, H. Cai, and B. R. Lawn, "Indentation Fatigue: A Simple Cyclic Hertzian Test for Measuring Damage Accumulation in Polycrystalline Ceramics," Philos. Mag. A, 68 [5] 1003-16 (1993).
    • (1993) Philos. Mag. A , vol.68 , Issue.5 , pp. 1003-1016
    • Guiberteau, F.1    Padture, N.P.2    Cai, H.3    Lawn, B.R.4
  • 7
    • 0028479433 scopus 로고
    • Effect of Grain Size on Hertzian Contact in Alumina
    • F. Guiberteau, N. P. Padture, and B. R. Lawn, "Effect of Grain Size on Hertzian Contact in Alumina," J. Am. Ceram. Soc., 77 [7] 1825-31 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.7 , pp. 1825-1831
    • Guiberteau, F.1    Padture, N.P.2    Lawn, B.R.3
  • 8
    • 0028392231 scopus 로고
    • Deformation and Fracture of Mica-Containing Glass-Ceramics in Hertzian Contacts
    • H. Cai, M. A. Stevens Kalceff, and B. R. Lawn, "Deformation and Fracture of Mica-Containing Glass-Ceramics In Hertzian Contacts," J. Mater. Res., 9 [3] 762-70 (1994).
    • (1994) J. Mater. Res. , vol.9 , Issue.3 , pp. 762-770
    • Cai, H.1    Stevens Kalceff, M.A.2    Lawn, B.R.3
  • 9
    • 0035297360 scopus 로고    scopus 로고
    • Brittle Fracture Versus Quasi Plasticity in Ceramics: A Simple Predictive Index
    • Y.-W. Rhee, H.-W. Kim, Y. Deng, and B. R. Lawn, "Brittle Fracture Versus Quasi Plasticity in Ceramics: A Simple Predictive Index," J. Am. Ceram. Soc., 84 [3] 561-65 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.3 , pp. 561-565
    • Rhee, Y.-W.1    Kim, H.-W.2    Deng, Y.3    Lawn, B.R.4
  • 10
    • 0027655860 scopus 로고
    • The Fracture Resistance of All-Ceramic Crowns on Supporting Structures with Different Elastic Moduli
    • S. S. Scherrer and W. G. d. Rijk, "The Fracture Resistance of All-Ceramic Crowns on Supporting Structures With Different Elastic Moduli," Int. J. Prosthodontics, 6 [5] 462-67 (1993).
    • (1993) Int. J. Prosthodontics , vol.6 , Issue.5 , pp. 462-467
    • Scherrer, S.S.1    Rijk, W.G.D.2
  • 11
    • 0030107011 scopus 로고    scopus 로고
    • Crack Suppression in Strongly-Bonded Homogeneous/Heterogeneous Laminates: A Study on Glass/Glass-Ceramic Bilayers
    • S. Wuttiphan, B. R. Lawn, and N. P. Padture, "Crack Suppression in Strongly-Bonded Homogeneous/Heterogeneous Laminates: A Study on Glass/Glass-Ceramic Bilayers," J. Am. Ceram. Soc., 79 [3] 634-40 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.3 , pp. 634-640
    • Wuttiphan, S.1    Lawn, B.R.2    Padture, N.P.3
  • 12
    • 0029756440 scopus 로고    scopus 로고
    • Damage-Resistant Alumina-Based Layer Composites
    • L. An, H. M. Chan, N. P. Padture, and B. R. Lawn, "Damage-Resistant Alumina-Based Layer Composites," J. Mater. Res., 11 [1] 204-10 (1996).
    • (1996) J. Mater. Res. , vol.11 , Issue.1 , pp. 204-210
    • An, L.1    Chan, H.M.2    Padture, N.P.3    Lawn, B.R.4
  • 13
    • 0030126078 scopus 로고    scopus 로고
    • Hertzian Contact Response of Tailored Silicon Nitride Multilayers
    • H. Liu, B. R. Lawn, and S. M. Hsu, "Hertzian Contact Response of Tailored Silicon Nitride Multilayers," J. Am. Ceram. Soc., 79 [4] 1009-14 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.4 , pp. 1009-1014
    • Liu, H.1    Lawn, B.R.2    Hsu, S.M.3
  • 14
    • 0031189559 scopus 로고    scopus 로고
    • Spherical Indentation and Fracture of Glass Plates
    • T. J. Lardner, J. E. Ritter, and G.-Q. Zhu, "Spherical Indentation and Fracture of Glass Plates," J. Am. Ceram. Soc., 80 [7] 1851-62 (1997).
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.7 , pp. 1851-1862
    • Lardner, T.J.1    Ritter, J.E.2    Zhu, G.-Q.3
  • 15
    • 0032028115 scopus 로고    scopus 로고
    • Contact-Induced Transverse Fractures in Brittle Layers on Soft Substrates: A Study on Silicon Nitride Bilayers
    • K. S. Lee, S. Wuttiphan, X. Z. Hu, S. K. Lee, and B. R. Lawn, "Contact-Induced Transverse Fractures in Brittle Layers on Soft Substrates: A Study on Silicon Nitride Bilayers," J. Am. Ceram. Soc., 81 [3] 571-80 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.3 , pp. 571-580
    • Lee, K.S.1    Wuttiphan, S.2    Hu, X.Z.3    Lee, S.K.4    Lawn, B.R.5
  • 16
    • 0032595445 scopus 로고    scopus 로고
    • Fracture Modes in Brittle Coatings with Large Interlayer Modulus Mismatch
    • H. Chai, B. R. Lawn, and S. Wuttiphan, "Fracture Modes in Brittle Coatings with Large Interlayer Modulus Mismatch," J. Mater. Res., 14 [9] 3805-17 (1999).
    • (1999) J. Mater. Res. , vol.14 , Issue.9 , pp. 3805-3817
    • Chai, H.1    Lawn, B.R.2    Wuttiphan, S.3
  • 17
    • 0034174580 scopus 로고    scopus 로고
    • Role of Adhesive Interlayer in Transverse Fracture of Brittle Layer Structures
    • H. Chai and B. R. Lawn, "Role of Adhesive Interlayer in Transverse Fracture of Brittle Layer Structures," J. Mater. Res., 15 [4] 1017-24 (2000).
    • (2000) J. Mater. Res. , vol.15 , Issue.4 , pp. 1017-1024
    • Chai, H.1    Lawn, B.R.2
  • 19
    • 0030194221 scopus 로고    scopus 로고
    • Contact Damage in Plasma-Sprayed Alumina-Based Coatings
    • A. Pajares, L. Wei, B. R. Lawn, and C. C. Berndt, "Contact Damage in Plasma-Sprayed Alumina-Based Coatings," J. Am. Ceram. Soc., 79 [7] 1907-14 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.7 , pp. 1907-1914
    • Pajares, A.1    Wei, L.2    Lawn, B.R.3    Berndt, C.C.4
  • 21
    • 0028440877 scopus 로고
    • Effect of Cement Film Thickness on the Fracture Resistance of a Machinable Glass-Ceramic
    • S. S. Scherrer, W. G. D. Rijk, U. C. Belser, and J.-M. Meyer, "Effect of Cement Film Thickness on the Fracture Resistance of a Machinable Glass-Ceramic," Dent. Mater., 10 172-77 (1994).
    • (1994) Dent. Mater. , vol.10 , pp. 172-177
    • Scherrer, S.S.1    Rijk, W.G.D.2    Belser, U.C.3    Meyer, J.-M.4
  • 23
    • 0000332208 scopus 로고
    • On the Theory of Hertzian Fracture
    • F. C. Frank and B. R. Lawn, "On the Theory of Hertzian Fracture," Proc. R. Soc. London, A, 299 [1458] 291-306 (1967).
    • (1967) Proc. R. Soc. London, A , vol.299 , Issue.1458 , pp. 291-306
    • Frank, F.C.1    Lawn, B.R.2
  • 24
    • 0003749418 scopus 로고
    • Cambridge University Press, Cambridge, U.K.
    • B. R. Lawn, Fracture of Brittle Solids; Cambridge University Press, Cambridge, U.K., 1993.
    • (1993) Fracture of Brittle Solids
    • Lawn, B.R.1
  • 25
    • 0014568867 scopus 로고
    • Hertzian Fracture Experiments on Abraded Glass Surfaces as Definitive Evidence for an Energy Balance Explanation of Auerbach's Law
    • F. B. Langitan and B. R. Lawn, "Hertzian Fracture Experiments on Abraded Glass Surfaces as Definitive Evidence for an Energy Balance Explanation of Auerbach's Law," J. Appl. Phys., 40 [10] 4009-17 (1969).
    • (1969) J. Appl. Phys. , vol.40 , Issue.10 , pp. 4009-4017
    • Langitan, F.B.1    Lawn, B.R.2
  • 26
    • 0031234167 scopus 로고    scopus 로고
    • Role of Microstructure in Hertzian Contact Damage in Silicon Nitride: I. Mechanical Characterization
    • S. K. Lee, S. Wuttiphan, and B. R. Lawn, "Role of Microstructure in Hertzian Contact Damage in Silicon Nitride: I. Mechanical Characterization," J. Am. Ceram. Soc., 80 [9] 2367-81 (1997).
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.9 , pp. 2367-2381
    • Lee, S.K.1    Wuttiphan, S.2    Lawn, B.R.3
  • 27
    • 0031598699 scopus 로고    scopus 로고
    • Role of Microstructure on Contact Damage and Strength Degradation of Micaceous Glass-Ceramics
    • I. M. Peterson, S. Wuttiphan, B. R. Lawn, and K. Chyung, "Role of Microstructure on Contact Damage and Strength Degradation of Micaceous Glass-Ceramics," Dent. Mater., 14, 80-89 (1998).
    • (1998) Dent. Mater. , vol.14 , pp. 80-89
    • Peterson, I.M.1    Wuttiphan, S.2    Lawn, B.R.3    Chyung, K.4
  • 28
    • 85040875608 scopus 로고
    • Cambridge University Press, London, U.K.
    • K. L. Johnson, Contact Mechanics; Cambridge University Press, London, U.K., 1985.
    • (1985) Contact Mechanics
    • Johnson, K.L.1
  • 29
    • 0013129083 scopus 로고
    • Indentation Fracture: Applications in the Assessment of Strength of Ceramics
    • B. R. Lawn, D. B. Marshall, P. Chantikul, and G. R. Anstis, "Indentation Fracture: Applications in the Assessment of Strength of Ceramics," J. Aust. Ceram. Soc., 16 [1] 4-9 (1980).
    • (1980) J. Aust. Ceram. Soc. , vol.16 , Issue.1 , pp. 4-9
    • Lawn, B.R.1    Marshall, D.B.2    Chantikul, P.3    Anstis, G.R.4
  • 30
    • 0034439683 scopus 로고    scopus 로고
    • Lifetime-Limiting Strength Degradation from Contact Fatigue in Dental Ceramics
    • Y.-G. Jung, I. M. Peterson, D. K. Kim, and B. R. Lawn, "Lifetime-Limiting Strength Degradation from Contact Fatigue in Dental Ceramics," J. Dent. Res., 79 [2] 722-31 (2000).
    • (2000) J. Dent. Res. , vol.79 , Issue.2 , pp. 722-731
    • Jung, Y.-G.1    Peterson, I.M.2    Kim, D.K.3    Lawn, B.R.4
  • 31
    • 0030259864 scopus 로고    scopus 로고
    • Stress Analysis of Contact Deformation in Quasi-Plastic Ceramics
    • A. C. Fischer-Cripps and B. R. Lawn, "Stress Analysis of Contact Deformation in Quasi-Plastic Ceramics," J. Am. Ceram. Soc., 79 [10] 2609-18 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.10 , pp. 2609-2618
    • Fischer-Cripps, A.C.1    Lawn, B.R.2
  • 32
  • 33
    • 0343081542 scopus 로고    scopus 로고
    • Cyclic Fatigue of Intrinsically Brittle Ceramics in Contact with Spheres
    • D. K. Kim, Y.-G. Jung, I. M. Peterson, and B. R. Lawn, "Cyclic Fatigue of Intrinsically Brittle Ceramics in Contact With Spheres," Acta Mater., 47 [18] 4711-25 (1999).
    • (1999) Acta Mater. , vol.47 , Issue.18 , pp. 4711-4725
    • Kim, D.K.1    Jung, Y.-G.2    Peterson, I.M.3    Lawn, B.R.4
  • 34
    • 0034274757 scopus 로고    scopus 로고
    • Model for Cyclic Fatigue of Quasi-Plastic Ceramics in Contact with Spheres
    • K. S. Lee, Y.-G. Jung, I. M. Peterson, B. R. Lawn, D. K. Kim, and S. K. Lee, "Model for Cyclic Fatigue of Quasi-Plastic Ceramics in Contact with Spheres," J. Am. Ceram. Soc., 83 [9] 2255-62 (2000).
    • (2000) J. Am. Ceram. Soc. , vol.83 , Issue.9 , pp. 2255-2262
    • Lee, K.S.1    Jung, Y.-G.2    Peterson, I.M.3    Lawn, B.R.4    Kim, D.K.5    Lee, S.K.6
  • 35
    • 0034256180 scopus 로고    scopus 로고
    • Cracking of Brittle Coatings Adhesively Bonded to Substrates of Unlike Modulus
    • K. S. Lee, Y.-W. Rhee, D. H. Blackburn, B. R. Lawn, and H. Chai, "Cracking of Brittle Coatings Adhesively Bonded to Substrates of Unlike Modulus," J. Mater. Res., 15 [8] 1653-56 (2000).
    • (2000) J. Mater. Res. , vol.15 , Issue.8 , pp. 1653-1656
    • Lee, K.S.1    Rhee, Y.-W.2    Blackburn, D.H.3    Lawn, B.R.4    Chai, H.5
  • 36
    • 0024884622 scopus 로고
    • Crack Deflection at an Interface between Dissimilar Elastic Materials
    • M.-W. He and J. W. Hutchinson, "Crack Deflection at an Interface between Dissimilar Elastic Materials," Int. J. Solids Struct., 25 [9] 1053-67 (1989).
    • (1989) Int. J. Solids Struct. , vol.25 , Issue.9 , pp. 1053-1067
    • He, M.-W.1    Hutchinson, J.W.2
  • 37
    • 0027697669 scopus 로고
    • Cracking and Damage Mechanisms in Ceramic/Metal Multilayers
    • M. C. Shaw, D. B. Marshall, M. S. Dadkhah, and A. G. Evans, "Cracking and Damage Mechanisms in Ceramic/Metal Multilayers," Acta Metall. Mater., 41 [11] 3311-22 (1993).
    • (1993) Acta Metall. Mater. , vol.41 , Issue.11 , pp. 3311-3322
    • Shaw, M.C.1    Marshall, D.B.2    Dadkhah, M.S.3    Evans, A.G.4
  • 38
    • 0016521376 scopus 로고
    • Indentation Fracture: Principles and Applications
    • B. R. Lawn and T. R. Wilshaw, "Indentation Fracture: Principles and Applications," J. Mater. Sci., 10 [6] 1049-81 (1975).
    • (1975) J. Mater. Sci. , vol.10 , Issue.6 , pp. 1049-1081
    • Lawn, B.R.1    Wilshaw, T.R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.