메뉴 건너뛰기




Volumn 124, Issue 3, 2002, Pages 271-276

Evaluation and improvement of the adhesive fracture toughness of CVD diamond on silicon substrate

Author keywords

[No Author keywords available]

Indexed keywords


EID: 0041369600     PISSN: 10437398     EISSN: None     Source Type: Journal    
DOI: 10.1115/1.1481374     Document Type: Article
Times cited : (1)

References (19)
  • 1
    • 0024610549 scopus 로고
    • Diamond-ceramic coating of the future
    • Spear, K. E., 1989, "Diamond-Ceramic Coating of the Future," J. Am. Ceram. Soc., 72(2), pp. 171-191.
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.2 , pp. 171-191
    • Spear, K.E.1
  • 2
    • 0000143835 scopus 로고
    • Temperature dependence and effect of series resistance on the electrical characteristics of a polycrystalline diamond metal-insulator-semiconductor diode
    • Rang, W. P., Davidson, J. L., Gurhuz, Y., and Kerns, D. V., 1995, "Temperature Dependence and Effect of Series Resistance on the Electrical Characteristics of a Polycrystalline Diamond Metal-Insulator-Semiconductor Diode," J. Appl. Phys., 78(2), pp. 1101-1107.
    • (1995) J. Appl. Phys. , vol.78 , Issue.2 , pp. 1101-1107
    • Rang, W.P.1    Davidson, J.L.2    Gurhuz, Y.3    Kerns, D.V.4
  • 3
    • 0021873854 scopus 로고
    • Techniques for evaluating mechanical properties of hard coatings
    • Mehrotra, P. K., and Quinto, D. T., 1985, "Techniques for Evaluating Mechanical Properties of Hard Coatings," J. Vac. Sci. Technol., 3(6), pp. 2401-2405.
    • (1985) J. Vac. Sci. Technol. , vol.3 , Issue.6 , pp. 2401-2405
    • Mehrotra, P.K.1    Quinto, D.T.2
  • 4
    • 0001060228 scopus 로고
    • Microindentation adhesion tester and its application to thin films
    • Tsukamoto, Y., Kuroda, H., Sato, A., and Yamaguchi, H., 1992, "Microindentation Adhesion Tester and its Application to Thin Films," Thin Solid Films, 213(2), pp. 220-225.
    • (1992) Thin Solid Films , vol.213 , Issue.2 , pp. 220-225
    • Tsukamoto, Y.1    Kuroda, H.2    Sato, A.3    Yamaguchi, H.4
  • 5
    • 0031245672 scopus 로고    scopus 로고
    • Application of heat treatment and dispersive strengthening concept in interlayer deposition to enhance diamond film adherence
    • Lin, C. R., Kuo, C. T. and Chang, R. M., 1997. "Application of Heat Treatment and Dispersive Strengthening Concept in Interlayer Deposition to Enhance Diamond Film Adherence," Thin Solid Films, 308-309(1-2). pp. 273-278.
    • (1997) Thin Solid Films , vol.308-309 , Issue.1-2 , pp. 273-278
    • Lin, C.R.1    Kuo, C.T.2    Chang, R.M.3
  • 6
    • 0000580728 scopus 로고    scopus 로고
    • A multilayer approach to high adhesion diamond-like carbon coatings on titanium
    • Dumkum, C., Grant, D. M., and McColl, I. R., 1997, "A Multilayer Approach to High Adhesion Diamond-Like Carbon Coatings on Titanium," Diamond Relat. Mater., 6(7), pp. 802-806.
    • (1997) Diamond Relat. Mater. , vol.6 , Issue.7 , pp. 802-806
    • Dumkum, C.1    Grant, D.M.2    McColl, I.R.3
  • 7
    • 0025517018 scopus 로고
    • Adhesion and tribological properties of diamond films on various substrates
    • Kuo, C.-T., Yen, T.-Y., Huang, T. H., and Hsu, S. E., 1990. "Adhesion and Tribological Properties of Diamond Films on Various Substrates," J. Mater. Res., 5(11), pp. 2515-2523.
    • (1990) J. Mater. Res. , vol.5 , Issue.11 , pp. 2515-2523
    • Kuo, C.-T.1    Yen, T.-Y.2    Huang, T.H.3    Hsu, S.E.4
  • 8
    • 0028374969 scopus 로고
    • Morphologies and adhesion strength of diamond films deposited on WC-6% Co cemented carbides with different surface characteristics
    • Peng, X.-L., and Gan, Z.-P., 1994. "Morphologies and Adhesion Strength of Diamond Films Deposited on WC-6% Co Cemented Carbides with Different Surface Characteristics," Thin Solid Films, 239(1), pp. 47-50.
    • (1994) Thin Solid Films , vol.239 , Issue.1 , pp. 47-50
    • Peng, X.-L.1    Gan, Z.-P.2
  • 9
    • 0031246618 scopus 로고    scopus 로고
    • Effect of sandblasting on adhesion strength of diamond coatings
    • Zhang, B., and Zhou, L., 1997. "Effect of Sandblasting on Adhesion Strength of Diamond Coatings," Thin Solid Films, 307(1-2), pp. 21-28.
    • (1997) Thin Solid Films , vol.307 , Issue.1-2 , pp. 21-28
    • Zhang, B.1    Zhou, L.2
  • 10
    • 36149056611 scopus 로고
    • The adhesion and surface energy of elastic solids
    • Kendall, K., 1971, "The Adhesion and Surface Energy of Elastic Solids," J. Phys. D, 4(2), pp. 1186-1195.
    • (1971) J. Phys. D , vol.4 , Issue.2 , pp. 1186-1195
    • Kendall, K.1
  • 11
    • 0021517474 scopus 로고
    • Measurements of adherence of residually stressed thin films by indentation. II. Experiments with ZnO/Si
    • Rossington, C., Evans, A. G., Marshall, D. B., and Khuri-Yakub, B. T., 1984, "Measurements of Adherence of Residually Stressed Thin Films by Indentation. II. Experiments with ZnO/Si," J. Appl. Phys., 56(10), pp. 2639-2644.
    • (1984) J. Appl. Phys. , vol.56 , Issue.10 , pp. 2639-2644
    • Rossington, C.1    Evans, A.G.2    Marshall, D.B.3    Khuri-Yakub, B.T.4
  • 12
    • 0021522097 scopus 로고
    • Measurement of adherence of residually stressed thin films by indentation. I. Mechanics of interface delamination
    • Marshall, D. B., and Evans, A. G., 1984, "Measurement of Adherence of Residually Stressed Thin Films by Indentation. I. Mechanics of Interface Delamination," J. Appl. Phys., 56(10), pp. 2632-2638.
    • (1984) J. Appl. Phys. , vol.56 , Issue.10 , pp. 2632-2638
    • Marshall, D.B.1    Evans, A.G.2
  • 13
    • 0032292237 scopus 로고    scopus 로고
    • Direct measurement of the adhesive fracture resistance of CVD diamond particles
    • Kamiya, S., Takahashi, H., Saka, M., and Abé, H., 1998, "Direct Measurement of the Adhesive Fracture Resistance of CVD Diamond Particles," ASME J. Electron, Packag., 120(4), pp. 367-371.
    • (1998) ASME J. Electron, Packag. , vol.120 , Issue.4 , pp. 367-371
    • Kamiya, S.1    Takahashi, H.2    Saka, M.3    Abé, H.4
  • 14
    • 4243597147 scopus 로고
    • Analysis of the composite structures in diamond thin films by Raman spectroscopy
    • Shroder, R. E., Nemanich, R. J., and Glass, J. T., 1990, "Analysis of the Composite Structures in Diamond Thin Films by Raman Spectroscopy," Phys. Rev. B, 41(6), pp. 3738-3745.
    • (1990) Phys. Rev. B , vol.41 , Issue.6 , pp. 3738-3745
    • Shroder, R.E.1    Nemanich, R.J.2    Glass, J.T.3
  • 15
    • 0025517150 scopus 로고
    • Chemical structure and physical properties of diamond-like amorphous carbon films prepared by magnetron sputtering
    • Cho, N.-H., Krishnan, K. M., Veirs, D. K., Rubin, M. D., Hopper, C. B., Bhushan, B., and Bogy, D. B., 1990, "Chemical Structure and Physical Properties of Diamond-Like Amorphous Carbon Films Prepared by Magnetron Sputtering," J. Mater. Res., 5(11), pp. 2543-2554.
    • (1990) J. Mater. Res. , vol.5 , Issue.11 , pp. 2543-2554
    • Cho, N.-H.1    Krishnan, K.M.2    Veirs, D.K.3    Rubin, M.D.4    Hopper, C.B.5    Bhushan, B.6    Bogy, D.B.7
  • 16
    • 0030396045 scopus 로고    scopus 로고
    • Origins of the residual stress in CVD diamond films
    • Kuo, C. T., Lin, C. R., and Lien, H. M., 1996. "Origins of the Residual Stress in CVD Diamond Films," Thin Solid Films, 290-291, pp. 254-259.
    • (1996) Thin Solid Films , vol.290-291 , pp. 254-259
    • Kuo, C.T.1    Lin, C.R.2    Lien, H.M.3
  • 17
    • 0029487654 scopus 로고
    • Residual stress, Young's modulus and fracture stress of hot flame deposited diamond
    • Hollman, P., Alahelisten, A., Olsson, S., and Hogmark, S., 1995, "Residual stress, Young's Modulus and Fracture Stress of Hot Flame Deposited Diamond." Thin Solid Films, 270, pp. 137-142.
    • (1995) Thin Solid Films , vol.270 , pp. 137-142
    • Hollman, P.1    Alahelisten, A.2    Olsson, S.3    Hogmark, S.4
  • 18
    • 0019009450 scopus 로고
    • Fracture toughness of silicon
    • Chen, C. P., and Leipold, M. N., 1980, "Fracture Toughness of Silicon," Am. Ceram. Soc. Bull., 59(4), pp. 469-472.
    • (1980) Am. Ceram. Soc. Bull. , vol.59 , Issue.4 , pp. 469-472
    • Chen, C.P.1    Leipold, M.N.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.