메뉴 건너뛰기




Volumn 79, Issue 7, 1996, Pages 1907-1914

Contact damage in plasma-sprayed alumina-based coatings

Author keywords

[No Author keywords available]

Indexed keywords

CRACKING (CHEMICAL); DELAMINATION; LOADING; MICROCRACKS; PLASTIC DEFORMATION; STEEL; STRAIN; STRESSES; SUBSTRATES;

EID: 0030194221     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.1996.tb08012.x     Document Type: Article
Times cited : (54)

References (29)
  • 1
    • 0000032884 scopus 로고
    • Plasma-Sprayed Coatings
    • H. Herman, "Plasma-Sprayed Coatings," Sci. Am., 256 [9] 113-88 (1988).
    • (1988) Sci. Am. , vol.256 , Issue.9 , pp. 113-188
    • Herman, H.1
  • 2
    • 84974201221 scopus 로고
    • Plasma Spray Deposition Processes
    • H. Herman, "Plasma Spray Deposition Processes," MRS Bull., 13, 60-67 (1988).
    • (1988) MRS Bull. , vol.13 , pp. 60-67
    • Herman, H.1
  • 3
    • 0001118172 scopus 로고
    • Plasma-Sprayed Ceramic Coatings
    • Edited by J. B. Wachtman and R. A. Haber. Noyes, Park Ridge, NJ
    • H. Herman, C. C. Berndt, and H. Wang, "Plasma-Sprayed Ceramic Coatings"; pp. 131-88 in Ceramic Films and Coatings. Edited by J. B. Wachtman and R. A. Haber. Noyes, Park Ridge, NJ, 1993.
    • (1993) Ceramic Films and Coatings , pp. 131-188
    • Herman, H.1    Berndt, C.C.2    Wang, H.3
  • 7
    • 0000332208 scopus 로고
    • On the Theory of Hertzian Fracture
    • F. C. Frank and B. R. Lawn, "On the Theory of Hertzian Fracture," Proc. R. Soc. London, A. 299 [1458] 291-306 (1967).
    • (1967) Proc. R. Soc. London, A , vol.299 , Issue.1458 , pp. 291-306
    • Frank, F.C.1    Lawn, B.R.2
  • 8
    • 0016521376 scopus 로고
    • Indentation Fracture: Principles and Applications
    • B. R. Lawn and T. R. Wilshaw, "Indentation Fracture: Principles and Applications," J. Mater. Sci., 10 [6] 1049-81 (1975).
    • (1975) J. Mater. Sci. , vol.10 , Issue.6 , pp. 1049-1081
    • Lawn, B.R.1    Wilshaw, T.R.2
  • 9
    • 84884280887 scopus 로고
    • Indentation Fatigue: A Simple Cyclic Hertzian Test for Measuring Damage Accumulation in Polycrystalline Ceramics
    • F. Guiberteau, N. P. Padture, H. Cai, and B. R. Lawn, "Indentation Fatigue: A Simple Cyclic Hertzian Test for Measuring Damage Accumulation in Polycrystalline Ceramics," Philos. Mag. A, 68 [5] 1003-16 (1993).
    • (1993) Philos. Mag. A , vol.68 , Issue.5 , pp. 1003-1016
    • Guiberteau, F.1    Padture, N.P.2    Cai, H.3    Lawn, B.R.4
  • 11
    • 0028479433 scopus 로고
    • Effect of Grain Size on Hertzian Contact in Alumina
    • F. Guiberteau, N. P. Padture, and B. R, Lawn, "Effect of Grain Size on Hertzian Contact in Alumina," J. Am. Ceram. Soc., 77 [7] 1825-31 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.7 , pp. 1825-1831
    • Guiberteau, F.1    Padture, N.P.2    Lawn, B.R.3
  • 12
    • 0028392231 scopus 로고
    • Deformation and Fracture of Mica-Containing Glass-Ceramics in Hertzian Contacts
    • H. Cai, M. A. Stevens Kalceff, and B. R. Lawn, "Deformation and Fracture of Mica-Containing Glass-Ceramics in Hertzian Contacts," J. Mater. Res., 9 [3] 762-70 (1994).
    • (1994) J. Mater. Res. , vol.9 , Issue.3 , pp. 762-770
    • Cai, H.1    Stevens Kalceff, M.A.2    Lawn, B.R.3
  • 13
    • 0028529919 scopus 로고
    • Toughness Properties of a Silicon Carbide with an In-Situ-Induced Heterogeneous Grain Structure
    • N. P. Padture and B. R. Lawn, "Toughness Properties of a Silicon Carbide with an In-Situ-Induced Heterogeneous Grain Structure," J. Am. Ceram. Soc., 77 [10] 2518-22 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.10 , pp. 2518-2522
    • Padture, N.P.1    Lawn, B.R.2
  • 14
    • 0029252557 scopus 로고
    • Effect of Microstructural Coarsening on Hertzian Contact Damage in Silicon Nitride
    • H. H. K. Xu, L. Wei, N. P. Padture, B. R. Lawn, and R. L. Yeckley, "Effect of Microstructural Coarsening on Hertzian Contact Damage in Silicon Nitride," J. Mater. Sci., 30, 869-78 (1995).
    • (1995) J. Mater. Sci. , vol.30 , pp. 869-878
    • Xu, H.H.K.1    Wei, L.2    Padture, N.P.3    Lawn, B.R.4    Yeckley, R.L.5
  • 15
    • 0029291635 scopus 로고
    • Hertzian Contact Damage in Magnesia-Partially-Stabilized Zirconia
    • A. Pajares, F. Guiberteau, B. R. Lawn, and S. Lathabai, "Hertzian Contact Damage in Magnesia-Partially-Stabilized Zirconia," J. Am. Ceram. Soc., 78 [4] 1083-86 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.4 , pp. 1083-1086
    • Pajares, A.1    Guiberteau, F.2    Lawn, B.R.3    Lathabai, S.4
  • 16
    • 0029756440 scopus 로고    scopus 로고
    • Damage-Resistant Alumina-Based Layer Composites
    • L. An, H. M. Chan, N. P. Padture, and B. R. Lawn, "Damage-Resistant Alumina-Based Layer Composites," J. Mater. Res., 11 [1] 204-10 (1996).
    • (1996) J. Mater. Res. , vol.11 , Issue.1 , pp. 204-210
    • An, L.1    Chan, H.M.2    Padture, N.P.3    Lawn, B.R.4
  • 17
    • 0030107011 scopus 로고    scopus 로고
    • Crack Suppression in Strongly Bonded Homogeneous/Heterogeneous Laminates: A Study on Glass/Glass-Ceramic Bilayers
    • S. Wuttiphan, B. R. Lawn, and N. P. Padture, "Crack Suppression in Strongly Bonded Homogeneous/Heterogeneous Laminates: A Study on Glass/Glass-Ceramic Bilayers," J. Am. Ceram. Soc., 79 [3] 634-40 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.3 , pp. 634-640
    • Wuttiphan, S.1    Lawn, B.R.2    Padture, N.P.3
  • 18
    • 0000042704 scopus 로고    scopus 로고
    • Mechanical Characterization of Plasma-Sprayed Ceramic Coatings on Metal Substrates by Contact Testing
    • A. Pajares, L. Wei, B. R. Lawn, N. P. Padture, and C. C. Berndt, "Mechanical Characterization of Plasma-Sprayed Ceramic Coatings on Metal Substrates by Contact Testing," Mater. Sci. Eng., A, 208 [2] 158-65 (1996).
    • (1996) Mater. Sci. Eng., A , vol.208 , Issue.2 , pp. 158-165
    • Pajares, A.1    Wei, L.2    Lawn, B.R.3    Padture, N.P.4    Berndt, C.C.5
  • 19
    • 0040601955 scopus 로고
    • Ph.D. Thesis. State University of New York at Stony Brook, Stony Brook, NY
    • J. Ilavsky, "Studies of Plasma Sprayed Alumina"; Ph.D. Thesis. State University of New York at Stony Brook, Stony Brook, NY, 1994.
    • (1994) Studies of Plasma Sprayed Alumina
    • Ilavsky, J.1
  • 21
    • 35248834654 scopus 로고
    • The Deformation of Metals by Vickers-Type Pyramidal Indenters
    • T. O. Mulheam, "The Deformation of Metals by Vickers-Type Pyramidal Indenters," J. Mech. Phys. Solids, 7, 85-96 (1959).
    • (1959) J. Mech. Phys. Solids , vol.7 , pp. 85-96
    • Mulheam, T.O.1
  • 22
    • 0004274342 scopus 로고
    • Cambridge University Press, Cambridge, U.K.
    • S. Suresh, Fatigue of Materials. Cambridge University Press, Cambridge, U.K., 1991.
    • (1991) Fatigue of Materials
    • Suresh, S.1
  • 23
    • 0028517781 scopus 로고
    • Cyclic Fatigue of a Mica-Containing Glass-Ceramic at Hertzian Contacts
    • H. Cai, M. A. S. Kalceff, B. M. Hooks, B. R. Lawn, and K. Chyung, "Cyclic Fatigue of a Mica-Containing Glass-Ceramic at Hertzian Contacts," J. Mater. Res., 9 [10] 2654-61 (1994).
    • (1994) J. Mater. Res. , vol.9 , Issue.10 , pp. 2654-2661
    • Cai, H.1    Kalceff, M.A.S.2    Hooks, B.M.3    Lawn, B.R.4    Chyung, K.5
  • 24
    • 0029326204 scopus 로고
    • Contact Fatigue of a Silicon Carbide with a Heterogeneous Grain Structure
    • N. P. Padture and B. R. Lawn, "Contact Fatigue of a Silicon Carbide with a Heterogeneous Grain Structure," J. Am. Ceram. Soc., 78 [6] 1431-38 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.6 , pp. 1431-1438
    • Padture, N.P.1    Lawn, B.R.2
  • 25
    • 0001764222 scopus 로고
    • Fatigue in Ceramics with Interconnecting Weak Interfaces: A Study Using Cyclic Hertzian Contacts
    • N. P. Padture and B. R. Lawn, "Fatigue in Ceramics with Interconnecting Weak Interfaces: A Study Using Cyclic Hertzian Contacts," Acta Metall., 43 [4] 1609-17 (1995).
    • (1995) Acta Metall. , vol.43 , Issue.4 , pp. 1609-1617
    • Padture, N.P.1    Lawn, B.R.2
  • 26
    • 0029392234 scopus 로고
    • Damage Accumulation and Cyclic Fatigue in Mg-PSZ at Hertzian Contacts
    • A. Pajares, L. Wei, B. R. Lawn, and D. B. Marshall, "Damage Accumulation and Cyclic Fatigue in Mg-PSZ at Hertzian Contacts," J. Mater. Res., 10 [10] 2613-25 (1995).
    • (1995) J. Mater. Res. , vol.10 , Issue.10 , pp. 2613-2625
    • Pajares, A.1    Wei, L.2    Lawn, B.R.3    Marshall, D.B.4
  • 27
    • 0018503878 scopus 로고
    • Residual Stress Effects in Sharp-Contact Cracking: I. Indentation Fracture Mechanics
    • D. B. Marshall and B. R. Lawn, "Residual Stress Effects in Sharp-Contact Cracking: I. Indentation Fracture Mechanics," J. Mater. Sci., 14 [8] 2001-12 (1979).
    • (1979) J. Mater. Sci. , vol.14 , Issue.8 , pp. 2001-2012
    • Marshall, D.B.1    Lawn, B.R.2
  • 28
    • 0019058952 scopus 로고
    • Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack System
    • B. R. Lawn, A. G. Evans, and D. B. Marshall, "Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack System," J. Am. Ceram. Soc., 63 [9-10] 574-81 (1980).
    • (1980) J. Am. Ceram. Soc. , vol.63 , Issue.9-10 , pp. 574-581
    • Lawn, B.R.1    Evans, A.G.2    Marshall, D.B.3
  • 29
    • 0028433966 scopus 로고
    • A Model for Microcrack Initiation and Propagation Beneath Hertzian Contacts in Polycrystalline Ceramics
    • B. R. Lawn, N. P. Padture, F. Guiberteau, and H. Cai, "A Model for Microcrack Initiation and Propagation Beneath Hertzian Contacts in Polycrystalline Ceramics," Acta Metall., 42 [5] 1683-93 (1994).
    • (1994) Acta Metall. , vol.42 , Issue.5 , pp. 1683-1693
    • Lawn, B.R.1    Padture, N.P.2    Guiberteau, F.3    Cai, H.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.