Volumn 99, Issue 1, 2000, Pages 231-245

Some considerations on the mitigation of fretting damage by the application of surface-modification technologies

Author keywords

[No Author keywords available]

Indexed keywords

CORROSION RESISTANCE; DEGRADATION; FRETTING CORROSION; FRICTION; HARDNESS; PROTECTIVE COATINGS; SURFACE CHEMISTRY; SURFACE ROUGHNESS; WEAR RESISTANCE;

EID: 0033908536     PISSN: 09240136     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0924-0136(99)00429-X     Document Type: Article
Times cited : (157)

References (92)
  • 2
  • 3
    • 0024053604 scopus 로고
    • Fretting wear mechanisms and their effects on fretting fatigue
    • Berthier Y., Colombie Ch., Vinvent L., Godet M. Fretting wear mechanisms and their effects on fretting fatigue. J. Tribol. 110:1988;517-524.
    • (1988) J. Tribol. , vol.110 , pp. 517-524
    • Berthier, Y.1    Colombie, C.2    Vinvent, L.3    Godet, M.4
  • 4
    • 0037740488 scopus 로고
    • Occurrence of fretting fatigue failures in practice
    • in: R.B. Waterhouse (Ed.), Elsevier Applied Science, London
    • P.J.E. Forsyth, Occurrence of fretting fatigue failures in practice, in: R.B. Waterhouse (Ed.), Fretting Fatigue, Elsevier Applied Science, London, 1981, pp. 121-125.
    • (1981) Fretting Fatigue , pp. 121-125
    • Forsyth, P.J.E.1
  • 5
    • 0041561515 scopus 로고
    • Wear, fretting and fretting fatigue
    • in: R.B. Waterhouse, D. Kirk (Eds.), Gournay-sur-Marne IITT-International
    • D.E. Taylor, R.B. Waterhouse, Wear, fretting and fretting fatigue, in: R.B. Waterhouse, D. Kirk (Eds.), Metal Behavior and Surface Engineering, Gournay-sur-Marne IITT-International 1989, pp. 13-35.
    • (1989) Metal Behavior and Surface Engineering , pp. 13-35
    • Taylor, D.E.1    Waterhouse, R.B.2
  • 6
    • 0022232759 scopus 로고
    • Recent trend in studies of fretting wear
    • Sato J. Recent trend in studies of fretting wear. Trans. JSLE. 30:1995;853-858.
    • (1995) Trans. JSLE , vol.30 , pp. 853-858
    • Sato, J.1
  • 7
    • 0024863765 scopus 로고
    • Fretting maps and fretting behavior of some FCC metal alloys
    • Vingsbo O., Odfalk M., Shen N.E. Fretting maps and fretting behavior of some FCC metal alloys. Wear. 133:1989;275-282.
    • (1989) Wear , vol.133 , pp. 275-282
    • Vingsbo, O.1    Odfalk, M.2    Shen, N.E.3
  • 9
  • 10
    • 0014804711 scopus 로고
    • The mechanism of fretting
    • Hurricks P.L. The mechanism of fretting. Wear. 15:1970;389-409.
    • (1970) Wear , vol.15 , pp. 389-409
    • Hurricks, P.L.1
  • 11
    • 85122007569 scopus 로고
    • Variables of fretting process: are they 50 of them?
    • in: M.H. Attia, R.B. Waterhouse (Eds.), ASTM, Philadelphia
    • J.M. Dobromirski, Variables of fretting process: are they 50 of them? in: M.H. Attia, R.B. Waterhouse (Eds.), Standardization of Fretting Fatigue Test Methods and Equipment, ASTM STP 1159, ASTM, Philadelphia, 1992, pp. 60-66.
    • (1992) Standardization of Fretting Fatigue Test Methods and Equipment, ASTM STP , vol.1159 , pp. 60-66
    • Dobromirski, J.M.1
  • 12
    • 0001665645 scopus 로고
    • Palliatives for fretting fatigue
    • in: R.B. Waterhouse, T.C. Lind1ey (Eds.), Mechanical Engineering Publications, London
    • J. Beard, Palliatives for fretting fatigue, in: R.B. Waterhouse, T.C. Lind1ey (Eds.), Fretting Fatigue, ESIS 18, Mechanical Engineering Publications, London, 1994, pp. 419-436.
    • (1994) Fretting Fatigue, ESIS , vol.18 , pp. 419-436
    • Beard, J.1
  • 13
    • 0031103852 scopus 로고    scopus 로고
    • Direct observations of fretting of steel
    • Baker R.F., Olver A.V. Direct observations of fretting of steel. Wear. 203/204:1997;425-433.
    • (1997) Wear , vol.203 , Issue.204 , pp. 425-433
    • Baker, R.F.1    Olver, A.V.2
  • 14
    • 0028255786 scopus 로고
    • In situ observation of the unlubricated wear process
    • Wang W., Wen S. In situ observation of the unlubricated wear process. Wear. 171:1994;19-23.
    • (1994) Wear , vol.171 , pp. 19-23
    • Wang, W.1    Wen, S.2
  • 15
    • 0032124576 scopus 로고    scopus 로고
    • Study on fretting wear behavior of laser treated coatings by X-ray imaging
    • Fu Y.Q., Batchelor A.W. Study on fretting wear behavior of laser treated coatings by X-ray imaging. Wear. 218:1998;250-260.
    • (1998) Wear , vol.218 , pp. 250-260
    • Fu, Y.Q.1    Batchelor, A.W.2
  • 16
    • 0032155459 scopus 로고    scopus 로고
    • Revealing the hidden world of fretting wear processes of advanced surface coatings by X-ray imaging
    • Fu Y.Q., Batchelor A.W., Loh N.L. Revealing the hidden world of fretting wear processes of advanced surface coatings by X-ray imaging. Surf. Coat. Technol. 107:1998;133-141.
    • (1998) Surf. Coat. Technol. , vol.107 , pp. 133-141
    • Fu, Y.Q.1    Batchelor, A.W.2    Loh, N.L.3
  • 17
    • 0018517808 scopus 로고
    • A literature review of palliatives for fretting fatigue
    • Gordelier S.C., Chiver T.C. A literature review of palliatives for fretting fatigue. Wear. 56:1967;177-190.
    • (1967) Wear , vol.56 , pp. 177-190
    • Gordelier, S.C.1    Chiver, T.C.2
  • 18
    • 0024045073 scopus 로고
    • Effect of lubricants on fretting wear of steel
    • Sato J., Shima M., Sugawara T. Effect of lubricants on fretting wear of steel. Wear. 110:1988;83-95.
    • (1988) Wear , vol.110 , pp. 83-95
    • Sato, J.1    Shima, M.2    Sugawara, T.3
  • 19
    • 0026798725 scopus 로고
    • The effect of lubricant additives on fretting wear
    • Qiu Y., Roylance B.J. The effect of lubricant additives on fretting wear. Lubrication Eng. 48:1992;801-808.
    • (1992) Lubrication Eng. , vol.48 , pp. 801-808
    • Qiu, Y.1    Roylance, B.J.2
  • 20
    • 0005314213 scopus 로고
    • The effect of surface treatment on the fatigue and fretting-fatigue of metallic materials
    • Pergamon Press, Oxford
    • R.B. Waterhouse, The effect of surface treatment on the fatigue and fretting-fatigue of metallic materials, in: Metal Treatments against Wear, Corrosion, Fretting and Fatigue, Pergamon Press, Oxford, 1988, pp. 31-40.
    • (1988) In: Metal Treatments Against Wear, Corrosion, Fretting and Fatigue , pp. 31-40
    • Waterhouse, R.B.1
  • 22
    • 0022153079 scopus 로고
    • The use of coatings to control fretting wear at ambient and elevated temperatures
    • Harris S.J., Overs M.P., Gould A.J. The use of coatings to control fretting wear at ambient and elevated temperatures. Wear. 106:1985;35.
    • (1985) Wear , vol.106 , pp. 35
    • Harris, S.J.1    Overs, M.P.2    Gould, A.J.3
  • 23
    • 0017994017 scopus 로고
    • Fretting of AISI 93100 steel and selected fretting resistance surface treatments
    • Bill R.C. Fretting of AISI 93100 steel and selected fretting resistance surface treatments. ALSE Trans. 21:1978;236-242.
    • (1978) ALSE Trans. , vol.21 , pp. 236-242
    • Bill, R.C.1
  • 24
    • 0343801279 scopus 로고
    • Engineering the surface to combat wear
    • Elsevier, Amsterdam
    • T. Bell, Engineering the surface to combat wear, Thin Films in Tribology, Elsevier, Amsterdam, 1993, pp. 54-59.
    • (1993) Thin Films in Tribology , pp. 54-59
    • Bell, T.1
  • 26
    • 0016356144 scopus 로고
    • Prevention of fretting by ion plated film
    • Ohmae N., Nakai T., Tsukizoe T. Prevention of fretting by ion plated film. Wear. 30:1974;299-309.
    • (1974) Wear , vol.30 , pp. 299-309
    • Ohmae, N.1    Nakai, T.2    Tsukizoe, T.3
  • 27
    • 0017894951 scopus 로고
    • Ion-plated thin films for anti-wear applications
    • Ohmae N., Tsukizoe T., Nakai T. Ion-plated thin films for anti-wear applications. J. Lub. Technol. 100:1978;129-135.
    • (1978) J. Lub. Technol. , vol.100 , pp. 129-135
    • Ohmae, N.1    Tsukizoe, T.2    Nakai, T.3
  • 28
    • 84992236640 scopus 로고
    • The fretting wear of certain hard coatings including TiN applied to a 0.4 C steel
    • Mechanical Engineering Publications, London, UK, 1-3 July
    • R.B. Waterhouse, R.C. Cobb, The fretting wear of certain hard coatings including TiN applied to a 0.4 C steel. Fifth Years on Tribology - Friction, Lubrication and Wear, Vol. 2, Mechanical Engineering Publications, London, UK, 1-3 July 1987, pp. 629-636.
    • (1987) Fifth Years on Tribology - Friction, Lubrication and Wear , vol.2 , pp. 629-636
    • Waterhouse, R.B.1    Cobb, R.C.2
  • 30
    • 0032523649 scopus 로고    scopus 로고
    • The tribochemical behavior of TiN-coatings during fretting wear
    • de Wit E., Blanpain B., Froyen L., Celis J.P. The tribochemical behavior of TiN-coatings during fretting wear. Wear. 217:1998;215-224.
    • (1998) Wear , vol.217 , pp. 215-224
    • De Wit, E.1    Blanpain, B.2    Froyen, L.3    Celis, J.P.4
  • 31
    • 0029361018 scopus 로고
    • Oxidational wear of TiN coatings on tool steel and nitrided tool steel in unlubricated fretting
    • Mohrbacher H., Blanpain B., Celis J.P., Roos J.R., Stals L., Van Stappen M. Oxidational wear of TiN coatings on tool steel and nitrided tool steel in unlubricated fretting. Wear. 188:1995;130-137.
    • (1995) Wear , vol.188 , pp. 130-137
    • Mohrbacher, H.1    Blanpain, B.2    Celis, J.P.3    Roos, J.R.4    Stals, L.5    Van Stappen, M.6
  • 33
    • 0028992234 scopus 로고
    • The influence of humidity on the fretting behavior of PVD TiN coatings
    • Mohrbacher H., Blanpain B., Cellis J.P., Roos J.R. The influence of humidity on the fretting behavior of PVD TiN coatings. Wear. 180:1995;43-52.
    • (1995) Wear , vol.180 , pp. 43-52
    • Mohrbacher, H.1    Blanpain, B.2    Cellis, J.P.3    Roos, J.R.4
  • 34
    • 0030483976 scopus 로고    scopus 로고
    • The fretting behavior of PVD TiN coatings in aqueous solutions
    • Wu P.Q., Mohrbacher H., Celis J.P. The fretting behavior of PVD TiN coatings in aqueous solutions. Wear. 201:1996;171-177.
    • (1996) Wear , vol.201 , pp. 171-177
    • Wu, P.Q.1    Mohrbacher, H.2    Celis, J.P.3
  • 36
    • 0029253161 scopus 로고
    • Fretting of titanium nitride and diamond-like carbon coatings at high frequencies and low amplitude
    • Schouterden K., Blanpain B., Celis J.P., Vingsbo O. Fretting of titanium nitride and diamond-like carbon coatings at high frequencies and low amplitude. Wear. 181-183:1995;86-93.
    • (1995) Wear , vol.181 , Issue.183 , pp. 86-93
    • Schouterden, K.1    Blanpain, B.2    Celis, J.P.3    Vingsbo, O.4
  • 40
    • 0009401312 scopus 로고
    • Low amplitude oscillating sliding wear on chemical wear on the chemical vapor deposited diamond coatings
    • Mohrbacher H., Blampain B., Celis J.P., Roos J.R. Low amplitude oscillating sliding wear on chemical wear on the chemical vapor deposited diamond coatings. Diamond Related Mater. 2:1993;879.
    • (1993) Diamond Related Mater. , vol.2 , pp. 879
    • Mohrbacher, H.1    Blampain, B.2    Celis, J.P.3    Roos, J.R.4
  • 41
    • 0028671110 scopus 로고
    • Fretting behavior of hard coating under high normal load
    • Fouvry S., Kapsa Ph., Vincent L. Fretting behavior of hard coating under high normal load. Surf. Coat. Technol. 68/69:1994;494-499.
    • (1994) Surf. Coat. Technol. , vol.6869 , pp. 494-499
    • Fouvry, S.1    Kapsa, P.2    Vincent, L.3
  • 42
    • 0029170643 scopus 로고
    • A system approach to the tribological testing of coated materials
    • Cellis J.P. A system approach to the tribological testing of coated materials. Surf. Coat. Technol. 74/75:1995;15-22.
    • (1995) Surf. Coat. Technol. , vol.7475 , pp. 15-22
    • Cellis, J.P.1
  • 44
    • 0005886906 scopus 로고
    • Effect of TiN coating by the CVD and OVD processes on fretting fatigue characteristics in steel
    • in: R.B. Waterhouse, T.C. Lindley (Eds.), Mechanical Engineering Publications, London
    • K. Sato, S. Kodama, Effect of TiN coating by the CVD and OVD processes on fretting fatigue characteristics in steel, in: R.B. Waterhouse, T.C. Lindley (Eds.), Fretting Fatigue, ESIS 18, Mechanical Engineering Publications, London, 1994, pp. 513-526.
    • (1994) Fretting Fatigue, ESIS , vol.18 , pp. 513-526
    • Sato, K.1    Kodama, S.2
  • 45
    • 0024144994 scopus 로고
    • Optimizing ion implantation conditions for improving wear, fatigue and fretting fatigue of Ti-6Al-4V
    • Elder J.E., Thamburraj R., Patnaik P.C. Optimizing ion implantation conditions for improving wear, fatigue and fretting fatigue of Ti-6Al-4V. Int. Mater. Rev. 33:1988;289-313.
    • (1988) Int. Mater. Rev. , vol.33 , pp. 289-313
    • Elder, J.E.1    Thamburraj, R.2    Patnaik, P.C.3
  • 46
    • 0026156017 scopus 로고
    • Fretting wear of carbon-ion implanted physical-vapor-deposited TiN coatings
    • Ross J.S., Celis J.P., Frank M. Fretting wear of carbon-ion implanted physical-vapor-deposited TiN coatings. Surf. Coat. Technol. 45:1991;89-98.
    • (1991) Surf. Coat. Technol. , vol.45 , pp. 89-98
    • Ross, J.S.1    Celis, J.P.2    Frank, M.3
  • 47
    • 0024716260 scopus 로고
    • Effect of ion implantation on fatigue, fretting and fretting-corrosion of Ti-6Al-4V
    • Saritas S., Proctor R.P.M., Grant W.A. Effect of ion implantation on fatigue, fretting and fretting-corrosion of Ti-6Al-4V. Mater. Sci. Eng. A. 115:1989;307-314.
    • (1989) Mater. Sci. Eng. A , vol.115 , pp. 307-314
    • Saritas, S.1    Proctor, R.P.M.2    Grant, W.A.3
  • 48
    • 0023128623 scopus 로고
    • Ion implantation of alloys for biomaterials and other applications
    • Perry A.J. Ion implantation of alloys for biomaterials and other applications. Surf. Eng. 3:1987;154-160.
    • (1987) Surf. Eng. , vol.3 , pp. 154-160
    • Perry, A.J.1
  • 49
    • 0028133919 scopus 로고
    • Corrosion and mechanical behavior of ion implanted bearing steels for improved fretting behavior
    • Was G.S., Demaree J.D. Corrosion and mechanical behavior of ion implanted bearing steels for improved fretting behavior. Surf. Coat. Technol. 66:1994;446-452.
    • (1994) Surf. Coat. Technol. , vol.66 , pp. 446-452
    • Was, G.S.1    Demaree, J.D.2
  • 50
    • 0030238353 scopus 로고    scopus 로고
    • Wear and fretting wear behavior of ion implanted zircalloy-4
    • Han J.G., Lee J.S., Choi B.H., Kin W., Tang G. Wear and fretting wear behavior of ion implanted zircalloy-4. Surf. Coat. Technol. 83:1996;307-312.
    • (1996) Surf. Coat. Technol. , vol.83 , pp. 307-312
    • Han, J.G.1    Lee, J.S.2    Choi, B.H.3    Kin, W.4    Tang, G.5
  • 52
    • 0027626636 scopus 로고
    • A machine for fretting wear testing of plasma surface modified materials
    • Stanstorm W., Sirdharan Z., Conrod J.R. A machine for fretting wear testing of plasma surface modified materials. Wear. 166:1993;163-168.
    • (1993) Wear , vol.166 , pp. 163-168
    • Stanstorm, W.1    Sirdharan, Z.2    Conrod, J.R.3
  • 53
    • 0029394275 scopus 로고
    • A fretting wear study of a nitrogen implanted titanium alloy
    • Horswill N.C., Sridharan K., Conrad J.R. A fretting wear study of a nitrogen implanted titanium alloy. J. Mater. Sci. Lett. 14:1995;1349-1351.
    • (1995) J. Mater. Sci. Lett. , vol.14 , pp. 1349-1351
    • Horswill, N.C.1    Sridharan, K.2    Conrad, J.R.3
  • 54
    • 0032523661 scopus 로고    scopus 로고
    • Development and characterization of CrN films by ion-beam-enhanced-deposition for improved wear resistance
    • Fu Y.Q., Zhu X.D., Tang B., Hu X.F., He J.W., Xu K.W., Batchelor A.W. Development and characterization of CrN films by ion-beam-enhanced-deposition for improved wear resistance. Wear. 217:1998;159-166.
    • (1998) Wear , vol.217 , pp. 159-166
    • Fu, Y.Q.1    Zhu, X.D.2    Tang, B.3    Hu, X.F.4    He, J.W.5    Xu, K.W.6    Batchelor, A.W.7
  • 55
    • 0032210073 scopus 로고    scopus 로고
    • Mechanical and tribological properties of ion-beam-enhanced deposition TiN thin films
    • Fu Y.Q., Zhu X.D., Xu K.W., He J.W. Mechanical and tribological properties of ion-beam-enhanced deposition TiN thin films. J. Mater. Process. Technol. 83:1998;209-216.
    • (1998) J. Mater. Process. Technol. , vol.83 , pp. 209-216
    • Fu, Y.Q.1    Zhu, X.D.2    Xu, K.W.3    He, J.W.4
  • 56
    • 84992256261 scopus 로고    scopus 로고
    • Ph.D. Thesis, Nanyang Technological University
    • Y.Q. Fu, Ph.D. Thesis, Nanyang Technological University, 1998.
    • (1998)
    • Fu, Y.Q.1
  • 57
    • 0030423641 scopus 로고    scopus 로고
    • Quantification of fretting damage
    • Fouvry S., Kapsa P., Vincent L. Quantification of fretting damage. Wear. 200:1996;186-205.
    • (1996) Wear , vol.200 , pp. 186-205
    • Fouvry, S.1    Kapsa, P.2    Vincent, L.3
  • 58
    • 4243612176 scopus 로고    scopus 로고
    • Wear analysis in fretting of hard coatings through a dissipated energy concept
    • Fouvry S., Kapsa P., Zahouani H., Vincent L. Wear analysis in fretting of hard coatings through a dissipated energy concept. Wear. 203/204:1997;393-403.
    • (1997) Wear , vol.203 , Issue.204 , pp. 393-403
    • Fouvry, S.1    Kapsa, P.2    Zahouani, H.3    Vincent, L.4
  • 59
    • 0001038441 scopus 로고
    • Laser surface treatments: microstructural aspects
    • in: W. Gissler, H.A. Jehn (Eds.), Kluwer Academic Publishers, Dordrecht
    • A. Frenk, W. Kurz, Laser surface treatments: microstructural aspects, in: W. Gissler, H.A. Jehn (Eds.), Advanced Techniques for Surface Engineering, Kluwer Academic Publishers, Dordrecht, 1992, pp. 235-252.
    • (1992) Advanced Techniques for Surface Engineering , pp. 235-252
    • Frenk, A.1    Kurz, W.2
  • 60
    • 0028207819 scopus 로고
    • Fretting wear behavior of 2Cr13 stainless steel before and after laser treatment
    • Yang D.H., Zhang X.S., Xue Q.J. Fretting wear behavior of 2Cr13 stainless steel before and after laser treatment. Wear. 171:1994;13-18.
    • (1994) Wear , vol.171 , pp. 13-18
    • Yang, D.H.1    Zhang, X.S.2    Xue, Q.J.3
  • 61
    • 0027111974 scopus 로고
    • Control of fretting wear of roping wire by laser surface alloying and physical vapor deposition coatings
    • Batchelor A.W., Stachowiak G.W., Stachowiak G.B. Control of fretting wear of roping wire by laser surface alloying and physical vapor deposition coatings. Wear. 152:1992;127-150.
    • (1992) Wear , vol.152 , pp. 127-150
    • Batchelor, A.W.1    Stachowiak, G.W.2    Stachowiak, G.B.3
  • 62
    • 0001551634 scopus 로고    scopus 로고
    • Investigation on laser alloying of aluminum alloy AA6061 with Ni, Cr. part II. Effects of laser alloying on fretting wear resistance
    • Fu Y.Q., Batchelor A.W. Investigation on laser alloying of aluminum alloy AA6061 with Ni, Cr. part II. Effects of laser alloying on fretting wear resistance. Surf. Coat. Technol. 102:1998;119-126.
    • (1998) Surf. Coat. Technol. , vol.102 , pp. 119-126
    • Fu, Y.Q.1    Batchelor, A.W.2
  • 63
    • 0003066447 scopus 로고    scopus 로고
    • Laser nitriding of pure titanium with Ni, Cr for improved wear performance
    • Fu Y.Q., Batchelor A.W. Laser nitriding of pure titanium with Ni, Cr for improved wear performance. Wear. 214:1998;82-90.
    • (1998) Wear , vol.214 , pp. 82-90
    • Fu, Y.Q.1    Batchelor, A.W.2
  • 64
    • 0028534414 scopus 로고
    • Suspension of fretting wear between roping wires by coatings and laser-alloyed layers of molybdenum
    • Stachowiak G.W., Stachowiak G.B., Batchelor A.W. Suspension of fretting wear between roping wires by coatings and laser-alloyed layers of molybdenum. Wear. 178:1994;69-77.
    • (1994) Wear , vol.178 , pp. 69-77
    • Stachowiak, G.W.1    Stachowiak, G.B.2    Batchelor, A.W.3
  • 66
    • 0007484269 scopus 로고
    • Plasma spraying - A versatile coating technique
    • in: W. Gissler, H.A. Jenn (Eds.), Kluwer Academic Publishers, Dordrecht
    • F. Brossa, E. Lang, Plasma spraying - a versatile coating technique, in: W. Gissler, H.A. Jenn (Eds.), Advanced Techniques for Surface Engineering, Kluwer Academic Publishers, Dordrecht, 1992, pp. 199-234.
    • (1992) Advanced Techniques for Surface Engineering , pp. 199-234
    • Brossa, F.1    Lang, E.2
  • 67
    • 0022153079 scopus 로고
    • The use of coatings to control fretting wear at ambient and elevated temperatures
    • Harris S.J., Overs M.P., Gould A.J. The use of coatings to control fretting wear at ambient and elevated temperatures. Wear. 106:1985;33-52.
    • (1985) Wear , vol.106 , pp. 33-52
    • Harris, S.J.1    Overs, M.P.2    Gould, A.J.3
  • 68
    • 0011104137 scopus 로고
    • Sprayed molybdenum coatings as a protection against fretting fatigue
    • Taylor D.E., Waterhouse R.B. Sprayed molybdenum coatings as a protection against fretting fatigue. Wear. 20:1972;401-407.
    • (1972) Wear , vol.20 , pp. 401-407
    • Taylor, D.E.1    Waterhouse, R.B.2
  • 69
    • 0019441584 scopus 로고
    • Development of coatings based on Fe-Cr-Ni-Al for resisting fretting wear in the temperature range 20-700°C
    • Overs M.P., Harris S.J., Waterhouse R.B. Development of coatings based on Fe-Cr-Ni-Al for resisting fretting wear in the temperature range 20-700°C. Wear. 75:1980;251-258.
    • (1980) Wear , vol.75 , pp. 251-258
    • Overs, M.P.1    Harris, S.J.2    Waterhouse, R.B.3
  • 70
    • 0022153082 scopus 로고
    • The use of coatings to control fretting wear of sprayed cermet coatings
    • Chivers T.C., Overs M.P., Gould A.J. The use of coatings to control fretting wear of sprayed cermet coatings. Wear. 106:1985;63-76.
    • (1985) Wear , vol.106 , pp. 63-76
    • Chivers, T.C.1    Overs, M.P.2    Gould, A.J.3
  • 73
    • 0028419756 scopus 로고
    • Fretting in orthopedic implants: A review
    • Hoppner D.W., Chandrasekaran V. Fretting in orthopedic implants: a review. Wear. 173:1994;189-197.
    • (1994) Wear , vol.173 , pp. 189-197
    • Hoppner, D.W.1    Chandrasekaran, V.2
  • 74
    • 0032522052 scopus 로고    scopus 로고
    • Fretting wear behaviors of thermal sprayed hydroxyapatite (HA) bioceramic coating under unlubricated condition
    • Fu Y.Q., Batchelor A.W., Wang Y., Khor K.A. Fretting wear behaviors of thermal sprayed hydroxyapatite (HA) bioceramic coating under unlubricated condition. Wear. 217:1998;132-139.
    • (1998) Wear , vol.217 , pp. 132-139
    • Fu, Y.Q.1    Batchelor, A.W.2    Wang, Y.3    Khor, K.A.4
  • 75
    • 0032766416 scopus 로고    scopus 로고
    • Fretting wear behaviors of thermal sprayed hydroxyapatite (HA) bioceramic coating lubricated with bovine albumin
    • Fu Y.Q., Batchelor A.W., Khor K.A. Fretting wear behaviors of thermal sprayed hydroxyapatite (HA) bioceramic coating lubricated with bovine albumin. Wear. 230:1999;98-102.
    • (1999) Wear , vol.230 , pp. 98-102
    • Fu, Y.Q.1    Batchelor, A.W.2    Khor, K.A.3
  • 76
    • 0242522489 scopus 로고    scopus 로고
    • Hot isostatic pressing of hydroxyapatite coating for improved fretting wear resistance
    • Fu Y.Q., Batchelor A.W., Khor K.A. Hot isostatic pressing of hydroxyapatite coating for improved fretting wear resistance. J. Mater. Sci. Lett. 17:1998;1695-1696.
    • (1998) J. Mater. Sci. Lett. , vol.17 , pp. 1695-1696
    • Fu, Y.Q.1    Batchelor, A.W.2    Khor, K.A.3
  • 77
    • 0029407657 scopus 로고
    • Hot isostatic pressing of plasma sprayed thermal barrier coating systems
    • Khor K.A., Loh N.L. Hot isostatic pressing of plasma sprayed thermal barrier coating systems. J. Mater. Manuf. Process. 10:1995;1241-1256.
    • (1995) J. Mater. Manuf. Process , vol.10 , pp. 1241-1256
    • Khor, K.A.1    Loh, N.L.2
  • 78
    • 0040285977 scopus 로고
    • The effect of surface treatments on the fretting wear of an aluminum alloy/steel couple
    • Waterhouse R.B. The effect of surface treatments on the fretting wear of an aluminum alloy/steel couple. Wear. 68:1982;310-334.
    • (1982) Wear , vol.68 , pp. 310-334
    • Waterhouse, R.B.1
  • 79
    • 0342496000 scopus 로고
    • The effect of shot-peening on the fretting fatigue behavior of an austenite stainless steel and a mild steel
    • Waterhouse R.B., Saunders D.A. The effect of shot-peening on the fretting fatigue behavior of an austenite stainless steel and a mild steel. Wear. 53:1979;381-386.
    • (1979) Wear , vol.53 , pp. 381-386
    • Waterhouse, R.B.1    Saunders, D.A.2
  • 80
    • 0006970792 scopus 로고    scopus 로고
    • Realising the potential of duplex surface engineering
    • in: I.M. Hutchings (Ed.), Mechanical Engineering Publications, UK
    • T. Bell, Realising the potential of duplex surface engineering, in: I.M. Hutchings (Ed.), New Directions in Tribology, Mechanical Engineering Publications, UK, 1997, pp. 121-133.
    • (1997) New Directions in Tribology , pp. 121-133
    • Bell, T.1
  • 81
    • 0032482917 scopus 로고    scopus 로고
    • Comparison of different surface engineering methods on improvement of fretting wear and fretting fatigue resistance of Ti-6Al-4V
    • Fu Y.Q., Loh N.L., Batchelor A.W., Liu D.X., Zhu X.D., He J.W., Xu K.W. Comparison of different surface engineering methods on improvement of fretting wear and fretting fatigue resistance of Ti-6Al-4V. Surf. Coat. Technol. 106:1998;193-197.
    • (1998) Surf. Coat. Technol. , vol.106 , pp. 193-197
    • Fu, Y.Q.1    Loh, N.L.2    Batchelor, A.W.3    Liu, D.X.4    Zhu, X.D.5    He, J.W.6    Xu, K.W.7
  • 82
    • 0026622450 scopus 로고
    • Residual stress and surface roughness in fretting fatigue
    • Waterhouse R.B., Trowsdale A.J. Residual stress and surface roughness in fretting fatigue. J. Phys. D. 25:1992;A236-A239.
    • (1992) J. Phys. D , vol.25 , pp. 236-A239
    • Waterhouse, R.B.1    Trowsdale, A.J.2
  • 83
    • 0021656482 scopus 로고
    • The fatigue of an aluminum alloy produced by fretting on a shot-peened surface, advances in fracture research
    • Pergamon Press, Oxford
    • G. Leadbeater, B. Noble, R.B. Waterhouse, The fatigue of an aluminum alloy produced by fretting on a shot-peened surface, advances in fracture research, Proceedings of the Sixth International Conference on Fracture, Pergamon Press, Oxford, 1984, pp. 2125-2132.
    • (1984) Proceedings of the Sixth International Conference on Fracture , pp. 2125-2132
    • Leadbeater, G.1    Noble, B.2    Waterhouse, R.B.3
  • 84
    • 0020815622 scopus 로고
    • Fretting wear and fretting fatigue properties of electroless nickel-phosphorus coatings
    • Gould A.J., Boden P.J., Harris S.J. Fretting wear and fretting fatigue properties of electroless nickel-phosphorus coatings. Trans. Inst. Met. Finish. 61:1983;97.
    • (1983) Trans. Inst. Met. Finish. , vol.61 , pp. 97
    • Gould, A.J.1    Boden, P.J.2    Harris, S.J.3
  • 85
    • 0026117901 scopus 로고
    • Sliding wear and fatigue resistance of amorphous Ni-P coatings
    • Gao H.S., Gu H.C., Zhou H.J. Sliding wear and fatigue resistance of amorphous Ni-P coatings. Wear. 142:1991;291-301.
    • (1991) Wear , vol.142 , pp. 291-301
    • Gao, H.S.1    Gu, H.C.2    Zhou, H.J.3
  • 86
    • 0032482870 scopus 로고    scopus 로고
    • Analysis chemical valence of the elements of the oxidized surface layer of a thermally sprayed Ni-Cr coating under fretting
    • He Q., Guo S., Liu W. Analysis chemical valence of the elements of the oxidized surface layer of a thermally sprayed Ni-Cr coating under fretting. Surf. Coat. Technol. 106:1998;91-93.
    • (1998) Surf. Coat. Technol. , vol.106 , pp. 91-93
    • He, Q.1    Guo, S.2    Liu, W.3
  • 87
    • 0024045071 scopus 로고
    • Contact conditions and surface degradation mechanisms in low amplitude fretting
    • Bryggman U., Soderberg S. Contact conditions and surface degradation mechanisms in low amplitude fretting. Wear. 125:1988;39-52.
    • (1988) Wear , vol.125 , pp. 39-52
    • Bryggman, U.1    Soderberg, S.2
  • 89
    • 0001985425 scopus 로고
    • Materials and fretting
    • in: R.B. Waterhouse, T.C. Lindley (Eds.), Mechanical Engineering Publications, London
    • L. Vincent, Materials and fretting, in: R.B. Waterhouse, T.C. Lindley (Eds.), Fretting Fatigue, ESIS 18, Mechanical Engineering Publications, London, 1994, pp. 323-337.
    • (1994) Fretting Fatigue, ESIS , vol.18 , pp. 323-337
    • Vincent, L.1
  • 90
    • 0003102988 scopus 로고
    • A methodology for coating selection
    • in: D. Dowson (Ed.), Elsevier, Amsterdam
    • A. Matthews, K. Holmberg, S. Franklin, A methodology for coating selection, in: D. Dowson (Ed.), Thin Films in Tribology, Elsevier, Amsterdam, 1993, pp. 422-439.
    • (1993) Thin Films in Tribology , pp. 422-439
    • Matthews, A.1    Holmberg, K.2    Franklin, S.3
  • 91
    • 0029310775 scopus 로고
    • Basis of a coating choice methodology in fretting
    • Carton J.F., Vannes A.B., Vincent L. Basis of a coating choice methodology in fretting. Wear. 185:1995;47.
    • (1995) Wear , vol.185 , pp. 47
    • Carton, J.F.1    Vannes, A.B.2    Vincent, L.3
  • 92
    • 0029256821 scopus 로고
    • Analysis of a tube-grid oscillatory contact: Methodology for the selection of superficial treatments
    • Voisin J.M., Vannes A.B., Vincent L., Daviot J., Giraud B. Analysis of a tube-grid oscillatory contact: methodology for the selection of superficial treatments. Wear. 181-183:1995;826-832.
    • (1995) Wear , vol.181 , Issue.183 , pp. 826-832
    • Voisin, J.M.1    Vannes, A.B.2    Vincent, L.3    Daviot, J.4    Giraud, B.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.