Volumn 106, Issue 2-3, 1998, Pages 193-197

Improvement in fretting wear and fatigue resistance of Ti-6Al-4V by application of several surface treatments and coatings

Author keywords

CrN film; CuNiIn film; Duplex treatment; Fretting fatigue; Fretting wear; Ion beam enhanced deposition; Shot peening; Ti 6Al 4V

Indexed keywords

CORROSION FATIGUE; DEPOSITION; FATIGUE OF MATERIALS; FRICTION; HARDNESS; ION BEAMS; RESIDUAL STRESSES; SURFACE ROUGHNESS; SURFACE TREATMENT; WEAR RESISTANCE;

EID: 0032482917     PISSN: 02578972     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0257-8972(98)00528-3     Document Type: Article
Times cited : (123)

References (22)
  • 2
  • 3
    • 0005314213 scopus 로고
    • The effect of surface treatment on the fatigue and fretting-fatigue of metallic materials
    • Pergamon, Oxford
    • R.B. Waterhouse, The effect of surface treatment on the fatigue and fretting-fatigue of metallic materials, in: Metal Treatments Against Wear, Corrosion, Fretting and Fatigue, Pergamon, Oxford, 1988, pp. 31-40.
    • (1988) In: Metal Treatments Against Wear, Corrosion, Fretting and Fatigue , pp. 31-40
    • Waterhouse, R.B.1
  • 4
    • 0029310775 scopus 로고
    • Basis of a coating choice methodology in fretting
    • Carton J.F., Vannes A.B., Vincent L. Basis of a coating choice methodology in fretting. Wear. 185:1995;47.
    • (1995) Wear , vol.185 , pp. 47
    • Carton, J.F.1    Vannes, A.B.2    Vincent, L.3
  • 5
    • 0025556802 scopus 로고
    • Use of ion beam assisted deposition to modify the microstructure and properties of thin films
    • Smidt F.A. Use of ion beam assisted deposition to modify the microstructure and properties of thin films. Int. Mater. Rev. 35:1990;61.
    • (1990) Int. Mater. Rev. , vol.35 , pp. 61
    • Smidt, F.A.1
  • 6
    • 0026188192 scopus 로고
    • Ion beam assisted thin film deposition
    • Hirvonen J.K. Ion beam assisted thin film deposition. Mater. Sci. Rep. 6:1991;215.
    • (1991) Mater. Sci. Rep. , vol.6 , pp. 215
    • Hirvonen, J.K.1
  • 7
    • 0032523661 scopus 로고    scopus 로고
    • Development and characterization of CrN films by ion-beam-enhanced-deposition for improved wear resistance
    • Fu Y.Q., Zhu X.D., Tang B., Hu X., He J., Xu K., Batchelor A.W. Development and characterization of CrN films by ion-beam-enhanced-deposition for improved wear resistance. Wear. 217:1998;159-166.
    • (1998) Wear , vol.217 , pp. 159-166
    • Fu, Y.Q.1    Zhu, X.D.2    Tang, B.3    Hu, X.4    He, J.5    Xu, K.6    Batchelor, A.W.7
  • 8
    • 0003066447 scopus 로고    scopus 로고
    • Laser nitriding of pure titanium with Ni, Cr for improved wear performance
    • Fu Y.Q., Batchelor A.W. Laser nitriding of pure titanium with Ni, Cr for improved wear performance. Wear. 214:1998;135-142.
    • (1998) Wear , vol.214 , pp. 135-142
    • Fu, Y.Q.1    Batchelor, A.W.2
  • 9
    • 0026117901 scopus 로고
    • Sliding wear and fretting fatigue resistance of amorphous Ni-P coatings
    • Gao H., Gu H., Zhou H. Sliding wear and fretting fatigue resistance of amorphous Ni-P coatings. Wear. 142:1991;291-301.
    • (1991) Wear , vol.142 , pp. 291-301
    • Gao, H.1    Gu, H.2    Zhou, H.3
  • 10
    • 0030131453 scopus 로고    scopus 로고
    • Effect of ion energy on the mechanical properties of ion beam assisted deposition (IBAD) wear resistant coatings
    • Cotell C.M., Hirvonen J.K. Effect of ion energy on the mechanical properties of ion beam assisted deposition (IBAD) wear resistant coatings. Surf. Coat. Technol. 81:1996;118-125.
    • (1996) Surf. Coat. Technol. , vol.81 , pp. 118-125
    • Cotell, C.M.1    Hirvonen, J.K.2
  • 11
    • 0024715808 scopus 로고
    • Fundamental of ion-beam-assisted deposition: Techniques and film properties
    • Hubler G.K. Fundamental of ion-beam-assisted deposition: techniques and film properties. Mater. Sci. Eng. A. 115:1989;181.
    • (1989) Mater. Sci. Eng. a , vol.115 , pp. 181
    • Hubler, G.K.1
  • 12
    • 0024045071 scopus 로고
    • Contact conditions and surface degradation mechanisms in low amplitude fretting
    • Bryggman U., Soderberg S. Contact conditions and surface degradation mechanisms in low amplitude fretting. Wear. 125:1988;39-52.
    • (1988) Wear , vol.125 , pp. 39-52
    • Bryggman, U.1    Soderberg, S.2
  • 13
    • 0028133919 scopus 로고
    • Corrosion and mechanical behavior of ion implanted bearing steels for improved fretting behavior
    • Was G.S., Demaree J.D., Rotberg V., Kim K. Corrosion and mechanical behavior of ion implanted bearing steels for improved fretting behavior. Surf. Coat. Technol. 66:1994;446-452.
    • (1994) Surf. Coat. Technol. , vol.66 , pp. 446-452
    • Was, G.S.1    Demaree, J.D.2    Rotberg, V.3    Kim, K.4
  • 14
    • 0342642842 scopus 로고
    • The stability of compressive stresses induced by shot-peening under conditions of fatigue and fretting fatigue
    • Pergamon, Oxford
    • G. Fair, B. Noble, R.B. Waterhouse, The stability of compressive stresses induced by shot-peening under conditions of fatigue and fretting fatigue, in: Advances in Surface Treatments, Pergamon, Oxford, 1993, pp. 1-8.
    • (1993) In: Advances in Surface Treatments , pp. 1-8
    • Fair, G.1    Noble, B.2    Waterhouse, R.B.3
  • 15
    • 0039694232 scopus 로고
    • Metallurgical observation on the fretting of shot-peened aluminum surfaces
    • in: R.B. Waterhouse, A. Nikulari (Eds.) Pergamon, Oxford
    • G. Leadbeater, B. Noble, R.B. Waterhouse, Metallurgical observation on the fretting of shot-peened aluminum surfaces, in: R.B. Waterhouse, A. Nikulari (Eds.), Metal Treatments against Wear, Corrosion, Fretting and Fatigue, Pergamon, Oxford, 1988, pp. 67-86.
    • (1988) Metal Treatments Against Wear, Corrosion, Fretting and Fatigue , pp. 67-86
    • Leadbeater, G.1    Noble, B.2    Waterhouse, R.B.3
  • 16
    • 85122007569 scopus 로고
    • Variables of fretting process: are there 50 of them?
    • in: M.H. Attia, R.B. Waterhouse (Eds.) ASTP STP 1159
    • J.M. Dobromirski, Variables of fretting process: are there 50 of them?, in: M.H. Attia, R.B. Waterhouse (Eds.), Standardization of Fretting Fatigue Test Methods and Equipment, ASTP STP 1159, 1992, pp. 60-66.
    • (1992) Standardization of Fretting Fatigue Test Methods and Equipment , pp. 60-66
    • Dobromirski, J.M.1
  • 17
  • 18
    • 0029394275 scopus 로고
    • A fretting wear study of a nitrogen implanted titanium alloy
    • Horswill N.C., Sridharan K., Corad J.R. A fretting wear study of a nitrogen implanted titanium alloy. J. Mater. Sci. Lett. 14:1995;1349-1351.
    • (1995) J. Mater. Sci. Lett. , vol.14 , pp. 1349-1351
    • Horswill, N.C.1    Sridharan, K.2    Corad, J.R.3
  • 19
    • 0040285977 scopus 로고
    • The effect of surface treatments on the fretting wear of an aluminum alloy/steel couple
    • Waterhouse R.B. The effect of surface treatments on the fretting wear of an aluminum alloy/steel couple. Wear. 68:1982;310-334.
    • (1982) Wear , vol.68 , pp. 310-334
    • Waterhouse, R.B.1
  • 20
    • 0002839856 scopus 로고
    • The fretting wear of electrodeposited contact coatings
    • Souter J.W., Staunton W. The fretting wear of electrodeposited contact coatings. Inst. Met. Finish. 66:1988;8-14.
    • (1988) Inst. Met. Finish. , vol.66 , pp. 8-14
    • Souter, J.W.1    Staunton, W.2
  • 21
    • 0027111974 scopus 로고
    • Control of fretting wear of roping wire by laser surface alloying and physical vapor deposition coatings
    • Batchelor A.W., Stachowiak G.W., Stachowiak G.B. Control of fretting wear of roping wire by laser surface alloying and physical vapor deposition coatings. Wear. 152:1992;127-150.
    • (1992) Wear , vol.152 , pp. 127-150
    • Batchelor, A.W.1    Stachowiak, G.W.2    Stachowiak, G.B.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.