Volumn 11, Issue 4, 2004, Pages 225-230

Hygrothermal aging effect on the interlaminar fracture of woven fabric fibre/ PEI composite material

Author keywords

Carbon fabric; Delamination modes; Glass fabric; Hygrothermal aging; PEI

Indexed keywords

DELAMINATION MODES; DELAMINATION RESISTANCE; HYGROTHERMAL AGING; OSMOTIC SWELLING;

EID: 9244231127     PISSN: 0334181X     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (6)

References (15)
  • 1
    • 0036675453 scopus 로고    scopus 로고
    • Dynamic fracture toughness measurements in composites by instrumental Charpy testing: Influence of aging
    • A. Fernández-Canteli, A. Argüelles, J. Viña, M. Ramulu and A.S. Kobayashi, Dynamic fracture toughness measurements in composites by instrumental Charpy testing: influence of aging, Comp. Sci & Tech. 62, 1315-1325 (2002).
    • (2002) Comp. Sci & Tech. , vol.62 , pp. 1315-1325
    • Fernández-Canteli, A.1    Argüelles, A.2    Viña, J.3    Ramulu, M.4    Kobayashi, A.S.5
  • 2
    • 0036500013 scopus 로고    scopus 로고
    • The effect of aging on the damage events in woven-fibre composite materials under different loading conditions
    • D. Scida, Z. Aboura and M.L. Benzeggagh, The effect of aging on the damage events in woven-fibre composite materials under different loading conditions, Comp. Sci. & Tech. 62, 551-557 (2002).
    • (2002) Comp. Sci. & Tech. , vol.62 , pp. 551-557
    • Scida, D.1    Aboura, Z.2    Benzeggagh, M.L.3
  • 3
    • 0242290488 scopus 로고    scopus 로고
    • The effect of moisture on the tensile and interlaminar shear strengths of glass or carbon fiber reinforced PEI
    • J. Viña, E.A. García, A. Argüelles and I. Viña, The effect of moisture on the tensile and interlaminar shear strengths of glass or carbon fiber reinforced PEI, J. Mat. Sci. Let. 19, 579-581 (2000).
    • (2000) J. Mat. Sci. Let. , vol.19 , pp. 579-581
    • Viña, J.1    García, E.A.2    Argüelles, A.3    Viña, I.4
  • 4
    • 2442701667 scopus 로고    scopus 로고
    • Long-term durability of fiber reinforced polymer-matrix composite materials for infrastructure applications: A review
    • K. Liao, C.R. Schultheisz, D.L. Hunston and L.C. Brinson, "Long-term durability of fiber reinforced polymer-matrix composite materials for infrastructure applications: A review", J. Adv. Mat., 30 (4), 3-40 (1998).
    • (1998) J. Adv. Mat. , vol.30 , Issue.4 , pp. 3-40
    • Liao, K.1    Schultheisz, C.R.2    Hunston, D.L.3    Brinson, L.C.4
  • 5
    • 0030649467 scopus 로고    scopus 로고
    • Mechanical properties and failure behaviour of carbon fibre reinforced polymer composites under the influence of moisture
    • R. Selzer and K. Friedrich, "Mechanical properties and failure behaviour of carbon fibre reinforced polymer composites under the influence of moisture", Composites, 28A, 595-604 (1997).
    • (1997) Composites , vol.28 A , pp. 595-604
    • Selzer, R.1    Friedrich, K.2
  • 6
    • 0032027793 scopus 로고    scopus 로고
    • Moisture-effects on the toughness, mode I and mode II of particles filled quasi-isotropic grass-fibre reinforced polyester resin composites
    • V.K. Srivastava and P.J. Hogg, "Moisture-effects on the toughness, mode I and mode II of particles filled quasi-isotropic grass-fibre reinforced polyester resin composites", J Mat. Sci., 33, 1129-1136 (1998).
    • (1998) J Mat. Sci. , vol.33 , pp. 1129-1136
    • Srivastava, V.K.1    Hogg, P.J.2
  • 7
    • 0030361417 scopus 로고    scopus 로고
    • Moisture effects on mode II delamination behavior of carbon/epoxy composites
    • S. Zhao and M. Gedke, "Moisture effects on Mode II delamination behavior of carbon/epoxy composites", Adv. Comp. Mater., 5 (4), 291-307 (1996).
    • (1996) Adv. Comp. Mater. , vol.5 , Issue.4 , pp. 291-307
    • Zhao, S.1    Gedke, M.2
  • 8
    • 0007430925 scopus 로고    scopus 로고
    • Standard test method for mode I interlaminar fracture toughness of unidirectional fibre-reinforced polymer matrix composite
    • ASTM D 5528, 14.02
    • 8. ASTM D 5528, Standard Test Method for Mode I Interlaminar Fracture Toughness of Unidirectional Fibre-Reinforced Polymer Matrix Composite, Annual Book of ASTM Standards, 14.02, 272-281.
    • Annual Book of ASTM Standards , vol.8 , pp. 272-281
  • 9
    • 0032760776 scopus 로고    scopus 로고
    • Mode I and Mode II fracture toughness of high-performance 3000 g mole-1 reactive poly(etherimide)/carbon fiber composites
    • T.A. Bullions, R.H. Mehta, B. Taan, E. McGrath and A.C. Kranbuehl, "Mode I and Mode II fracture toughness of high-performance 3000 g mole-1 reactive poly(etherimide)/carbon fiber composites", Composites, 30A, 153-162 (1999).
    • (1999) Composites , vol.30 A , pp. 153-162
    • Bullions, T.A.1    Mehta, R.H.2    Taan, B.3    McGrath, E.4    Kranbuehl, A.C.5
  • 11
    • 0027845087 scopus 로고
    • Round robin testing for mode I interlaminar fracture toughness of composite materials
    • T.K. O'Brien and R.H. Martin, "Round robin testing for Mode I interlaminar fracture toughness of composite materials", J. Comp. Tech. & Res., 15 (4), 269-281 (1993).
    • (1993) J. Comp. Tech. & Res. , vol.15 , Issue.4 , pp. 269-281
    • O'Brien, T.K.1    Martin, R.H.2
  • 13
    • 9244247986 scopus 로고    scopus 로고
    • Standard test method for mode II interlaminar fracture toughness of unidirectional fibre-reinforced polymer matrix composite
    • ASTM D 790, 14.02
    • ASTM D 790, Standard Test Method for Mode II Interlaminar Fracture Toughness of Unidirectional Fibre-Reinforced Polymer Matrix Composite, Annual Book of ASTM Standards, 14.02.
    • Annual Book of ASTM Standards
  • 15
    • 0001014069 scopus 로고
    • The analysis of interlaminar fracture in unidirectional fibre-polymer composites
    • S. Hashemi, A.J. Kinloch and J.G. Williams, "The analysis of interlaminar fracture in unidirectional fibre-polymer composites", Proc. R. Soc. Lond., A427, 173-190 (1990)
    • (1990) Proc. R. Soc. Lond. , vol.A427 , pp. 173-190
    • Hashemi, S.1    Kinloch, A.J.2    Williams, J.G.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.