1
-
-
0003250495
-
Combined Advanced Finishing and UV-Laser Conditioning for Producing UV-Damage-Resistant Fused Silica Optics
-
presented at (SPIE, Bellingham, WA)
-
J. A. Menapace, B. Penetrante, D. Golini, A. Slomba, P. E. Miller, T. Parham, M. Nichols, and J. Peterson, “Combined Advanced Finishing and UV-Laser Conditioning for Producing UV-Damage-Resistant Fused Silica Optics”, presented at the Boulder Damage Symposium, 10/1/01, and to be published in Laser-Induced Damage in Optical Materials (SPIE, Bellingham, WA, 2001).
-
(2001)
the Boulder Damage Symposium, 10/1/01, and to be published in Laser-Induced Damage in Optical Materials
-
-
Menapace, J. A.1
Penetrante, B.2
Golini, D.3
Slomba, A.4
Miller, P. E.5
Parham, T.6
Nichols, M.7
Peterson, J.8
-
2
-
-
0032402531
-
Magnetorheological suspension-based finishing technology (MRF)
-
J. M. Sater, ed., Proc. SPIE
-
W. Kordonski, D. Golini, P. Dumas, S. Hogan, and S. Jacobs, “Magnetorheological suspension-based finishing technology (MRF)”, in Fifth Annual International Symposium on Smart Structures and Materials, J. M. Sater, ed., Proc. SPIE 3326, 527-535 (1998).
-
(1998)
Fifth Annual International Symposium on Smart Structures and Materials
, vol.3326
, pp. 527-535
-
-
Kordonski, W.1
Golini, D.2
Dumas, P.3
Hogan, S.4
Jacobs, S.5
-
3
-
-
0010753438
-
-
Ph.D. dissertation (University of Rochester, Rochester, N.Y), chap. 3
-
A. B. Shorey, “Mechanisms of material removal in magnetorheological finishing (MRF) of glass”, Ph.D. dissertation (University of Rochester, Rochester, N.Y., 2000), chap. 3.
-
(2000)
Mechanisms of material removal in magnetorheological finishing (MRF) of glass
-
-
Shorey, A. B.1
-
5
-
-
85166709137
-
Magnetorheological Fluid Composition and Enhanced Material Removal Rates with Nanodiamonds
-
S. D. Jacobs, E. Fess, B. E. Gillman, H. Edwards, D. Golini, W. I. Kordonski, V. W. Kordonski, I. Prokhorov, and F. Yang, “Magnetorheological Fluid Composition and Enhanced Material Removal Rates with Nanodiamonds”, OSA Topical Meeting on Optical Fabrication and Testing, Technical Digest 7, pp. 48-51 (1996).
-
(1996)
OSA Topical Meeting on Optical Fabrication and Testing, Technical Digest
, vol.7
, pp. 48-51
-
-
Jacobs, S. D.1
Fess, E.2
Gillman, B. E.3
Edwards, H.4
Golini, D.5
Kordonski, W. I.6
Kordonski, V. W.7
Prokhorov, I.8
Yang, F.9
-
7
-
-
0033353718
-
Details of the polishing spot in magnetorheological finishing (MRF)
-
edited by H. Stahl (SPIE, Bellingham, WA)
-
S. R. Arrasmith, I. A. Kozhinova, L. L. Gregg, A. B. Shorey, H. J. Romanofsky, S. D. Jacobs, D. Golini, W. I. Kordonski, S. Hogan, and P. Dumas, “Details of the polishing spot in magnetorheological finishing (MRF)”, in Optical Manufacturing and Testing III, edited by H. Stahl (SPIE, Bellingham, WA, 1999), Vol.3782, pp. 92-100.
-
(1999)
Optical Manufacturing and Testing III
, vol.3782
, pp. 92-100
-
-
Arrasmith, S. R.1
Kozhinova, I. A.2
Gregg, L. L.3
Shorey, A. B.4
Romanofsky, H. J.5
Jacobs, S. D.6
Golini, D.7
Kordonski, W. I.8
Hogan, S.9
Dumas, P.10
-
9
-
-
84893183888
-
-
Coupons were provided by Mr. 408 St. Paul Street, Rochester, NY 14605
-
Coupons were provided by Mr. William S. Beich, G-S Plastic Optics, 408 St. Paul Street, Rochester, NY 14605.
-
G-S Plastic Optics
-
-
Beich, William S.1
-
10
-
-
0010364371
-
Nanodiamonds Enhance Removal in Magnetorheological Finishing
-
S. D. Jacobs, “Nanodiamonds Enhance Removal in Magnetorheological Finishing”, Finer Points 7, 47-54 (1995).
-
(1995)
Finer Points
, vol.7
, pp. 47-54
-
-
Jacobs, S. D.1
-
11
-
-
85166705150
-
-
Taylor Hobsen, Inc., 2100 Golf Road, Suite 350, Rolling Meadows, IL 60008
-
Taylor Hobsen Series 2 Form Talysurf PGI System, Taylor Hobsen, Inc., 2100 Golf Road, Suite 350, Rolling Meadows, IL 60008.
-
Taylor Hobsen Series 2 Form Talysurf PGI System
-
-
-
12
-
-
85166709119
-
-
Zygo NewView® 5000, 20x Mirau, min/mod (%) = 5, FDA res = Hi, unfiltered, areal over 250m x 350µm, averaged over 3 sites.
-
Zygo NewView® 5000, 20x Mirau, min/mod (%) = 5, FDA res = Hi, unfiltered, areal over 250m x 350µm, averaged over 3 sites
-
-
|