1
-
-
84879140928
-
Surface deformation of steels in impact-abrasion: the effect of sample angle and test duration
-
Ratia V., Miettunen I., Kuokkala V.T. Surface deformation of steels in impact-abrasion: the effect of sample angle and test duration. Wear 2013, 301:94-101.
-
(2013)
Wear
, vol.301
, pp. 94-101
-
-
Ratia, V.1
Miettunen, I.2
Kuokkala, V.T.3
-
2
-
-
84963680460
-
Effect of different strengthening methods on rolling/sliding wear of ferrite-pearlite steel
-
Zeng D., Lu L., Zhang N., Gong Y., Zhang J. Effect of different strengthening methods on rolling/sliding wear of ferrite-pearlite steel. Wear 2016, 358-359:62-71.
-
(2016)
Wear
, pp. 62-71
-
-
Zeng, D.1
Lu, L.2
Zhang, N.3
Gong, Y.4
Zhang, J.5
-
3
-
-
10644294506
-
On the influence of retained austenite in the abrasive wear behavior of a laser surface melted tool steel
-
Colaco R., Vilar R. On the influence of retained austenite in the abrasive wear behavior of a laser surface melted tool steel. Wear 2005, 258:225-231.
-
(2005)
Wear
, vol.258
, pp. 225-231
-
-
Colaco, R.1
Vilar, R.2
-
4
-
-
84957604857
-
Wear mapping and transitions in wheel and rail materials under different contact pressure and sliding velocity conditions
-
Ding H.H., He C.G., Ma L., Guo J., Liu Q.Y., Wang W.J. Wear mapping and transitions in wheel and rail materials under different contact pressure and sliding velocity conditions. Wear 2016, 352-353:1-8.
-
(2016)
Wear
, pp. 1-8
-
-
Ding, H.H.1
He, C.G.2
Ma, L.3
Guo, J.4
Liu, Q.Y.5
Wang, W.J.6
-
5
-
-
84884199286
-
Impact-abrasion wear characteristics of in-situ VC-reinforced austenitic steel matrix composite
-
Moghaddam E.G., Karimzadeh N., Varahram N., Davami P. Impact-abrasion wear characteristics of in-situ VC-reinforced austenitic steel matrix composite. Mater. Sci. Eng. A 2013, 585:422-429.
-
(2013)
Mater. Sci. Eng. A
, vol.585
, pp. 422-429
-
-
Moghaddam, E.G.1
Karimzadeh, N.2
Varahram, N.3
Davami, P.4
-
6
-
-
84957580392
-
Comparisons of the two-body abrasive wear behaviour of four different ferrous microstructures with similar hardness levels
-
Narayanaswamy B., Hodgson P., Beladi H. Comparisons of the two-body abrasive wear behaviour of four different ferrous microstructures with similar hardness levels. Wear 2016, 350-351:155-165.
-
(2016)
Wear
, pp. 155-165
-
-
Narayanaswamy, B.1
Hodgson, P.2
Beladi, H.3
-
7
-
-
0028416299
-
The design of an impact abrasion testing machine
-
Zhang D., Beeley P.R., Baker A.J. The design of an impact abrasion testing machine. Wear 1994, 173:59-64.
-
(1994)
Wear
, vol.173
, pp. 59-64
-
-
Zhang, D.1
Beeley, P.R.2
Baker, A.J.3
-
8
-
-
84910674385
-
Wear behavior and work hardening of high strength steels in high stress abrasion
-
Lindroos M., Valtonen K., Kemppainen A., Laukkanen A., Holmberg K., Kuokkala V. Wear behavior and work hardening of high strength steels in high stress abrasion. Wear 2015, 322-323:32-40.
-
(2015)
Wear
, pp. 32-40
-
-
Lindroos, M.1
Valtonen, K.2
Kemppainen, A.3
Laukkanen, A.4
Holmberg, K.5
Kuokkala, V.6
-
9
-
-
84880024554
-
Friction behavior evaluation of an EBT zinc-coated trip 700 steel sheet through flat friction tests
-
Coello J., Miguel V., Martinez A., Avellaneda F.J., Calatayud A. Friction behavior evaluation of an EBT zinc-coated trip 700 steel sheet through flat friction tests. Wear 2013, 305:129-139.
-
(2013)
Wear
, vol.305
, pp. 129-139
-
-
Coello, J.1
Miguel, V.2
Martinez, A.3
Avellaneda, F.J.4
Calatayud, A.5
-
11
-
-
83855164368
-
Effect of precipitation hardening on hardness and microstructure of austenitic manganese steel
-
Aribo S., Alaneme K.K., Folorunso D.O., Aramide F.O. Effect of precipitation hardening on hardness and microstructure of austenitic manganese steel. J. Miner. Mater. Charact. Eng. 2010, 9:157-164.
-
(2010)
J. Miner. Mater. Charact. Eng.
, vol.9
, pp. 157-164
-
-
Aribo, S.1
Alaneme, K.K.2
Folorunso, D.O.3
Aramide, F.O.4
-
12
-
-
84926480604
-
Nano/ultrafine grained austenitic stainless steel through the formation and reversion of deformation-induced martensite: mechanisms, microstructures, mechanical properties, and TRIP effect
-
Shirdel M., Mirzadeh H., Parsa M.H. Nano/ultrafine grained austenitic stainless steel through the formation and reversion of deformation-induced martensite: mechanisms, microstructures, mechanical properties, and TRIP effect. Mater. Charact. 2015, 103:150-161.
-
(2015)
Mater. Charact.
, vol.103
, pp. 150-161
-
-
Shirdel, M.1
Mirzadeh, H.2
Parsa, M.H.3
-
13
-
-
84904250073
-
The influence of the austempering temperature on the transformation behavior and properties of ultra-high-trength TRIP-aided bainitic-ferritic sheet steel
-
Zhao Z.Z., Yin H.X., Zhao A.M., Gong Z.Q., He J.G., Tong T.T., Hu H.J. The influence of the austempering temperature on the transformation behavior and properties of ultra-high-trength TRIP-aided bainitic-ferritic sheet steel. Mater. Sci. Eng. A 2014, 613:8-16.
-
(2014)
Mater. Sci. Eng. A
, vol.613
, pp. 8-16
-
-
Zhao, Z.Z.1
Yin, H.X.2
Zhao, A.M.3
Gong, Z.Q.4
He, J.G.5
Tong, T.T.6
Hu, H.J.7
-
14
-
-
84961153947
-
In situ synchrotron X-ray diffraction studies of the effect of microstructure on tensile behavior and retained austenite stability of thermo-mechanically processed transformation induced plasticity steel
-
Yab J., Liss K.D., Timokhina I.B., Pereloma E.V. In situ synchrotron X-ray diffraction studies of the effect of microstructure on tensile behavior and retained austenite stability of thermo-mechanically processed transformation induced plasticity steel. Mater. Sci. Eng. A 2016, 662:185-197.
-
(2016)
Mater. Sci. Eng. A
, vol.662
, pp. 185-197
-
-
Yab, J.1
Liss, K.D.2
Timokhina, I.B.3
Pereloma, E.V.4
-
17
-
-
0038753827
-
Carbon partitioning into austenite after martensite transformation
-
Speer J.G., Matlock D.K., De Cooman B.C., Schroth J.G. Carbon partitioning into austenite after martensite transformation. Acta Mater. 2003, 51:2611-2622.
-
(2003)
Acta Mater.
, vol.51
, pp. 2611-2622
-
-
Speer, J.G.1
Matlock, D.K.2
De Cooman, B.C.3
Schroth, J.G.4
-
18
-
-
38549127197
-
Design of structure, composition and heat treatment process for high strength steel
-
Xu Z.Y. Design of structure, composition and heat treatment process for high strength steel. Mater. Sci. Forum 2007, 561-565:2283-2286.
-
(2007)
Mater. Sci. Forum
, pp. 2283-2286
-
-
Xu, Z.Y.1
-
19
-
-
53849128833
-
Effect of retained austenite stabilized via quench and partitioning on the strain hardening of martensitic steels
-
De Moor E., Lacroix S., Clarke A.J., Penning J., Speer J.G. Effect of retained austenite stabilized via quench and partitioning on the strain hardening of martensitic steels. Metall. Mater. Trans. A 2008, 39:2586-2595.
-
(2008)
Metall. Mater. Trans. A
, vol.39
, pp. 2586-2595
-
-
De Moor, E.1
Lacroix, S.2
Clarke, A.J.3
Penning, J.4
Speer, J.G.5
-
20
-
-
84880020416
-
Impact-abrasive-corrosion wear of Fe-based alloys: Influence of microstructure and chemical composition upon wear resistance
-
Efremenko V.G., Shimizu K., Noguchi T., Efremenko A.V., Chabak Yu.G. Impact-abrasive-corrosion wear of Fe-based alloys: Influence of microstructure and chemical composition upon wear resistance. Wear 2013, 305:155-165.
-
(2013)
Wear
, vol.305
, pp. 155-165
-
-
Efremenko, V.G.1
Shimizu, K.2
Noguchi, T.3
Efremenko, A.V.4
Chabak, Y.G.5
-
21
-
-
84925249959
-
Characterization of transition carbides in quench and partitioned steel microstructures by Mössbauer spectroscopy and complementary techniques
-
Pierce D.T., Coughlin D.R., Willianson D.L., Clarke K.D., Clarke A.J., Speer J.G., De Moor E. Characterization of transition carbides in quench and partitioned steel microstructures by Mössbauer spectroscopy and complementary techniques. Acta Mater. 2015, 90:417-430.
-
(2015)
Acta Mater.
, vol.90
, pp. 417-430
-
-
Pierce, D.T.1
Coughlin, D.R.2
Willianson, D.L.3
Clarke, K.D.4
Clarke, A.J.5
Speer, J.G.6
De Moor, E.7
-
22
-
-
84964317148
-
The scratch and abrasive wear behaviour of a tempered martensitic construction steel and its dual phase variants
-
Xu X., van der Zwaag S., Xu W. The scratch and abrasive wear behaviour of a tempered martensitic construction steel and its dual phase variants. Wear 2016, 358-359:80-88.
-
(2016)
Wear
, pp. 80-88
-
-
Xu, X.1
van der Zwaag, S.2
Xu, W.3
-
24
-
-
33746237693
-
A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steel
-
Koistinen D.P., Marburger R.E. A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steel. Acta Metall. 1959, 7:59-60.
-
(1959)
Acta Metall.
, vol.7
, pp. 59-60
-
-
Koistinen, D.P.1
Marburger, R.E.2
-
25
-
-
84886848434
-
Three-body abrasive wear of fine pearlite, nanostructured bainite and martensite
-
Das Bakshi S., Shipway P.H., Bhadeshia H.K.D.H. Three-body abrasive wear of fine pearlite, nanostructured bainite and martensite. Wear 2013, 308:46-53.
-
(2013)
Wear
, vol.308
, pp. 46-53
-
-
Das Bakshi, S.1
Shipway, P.H.2
Bhadeshia, H.K.D.H.3
|