메뉴 건너뛰기




Volumn 266, Issue , 2014, Pages 106-112

Synthesis of carbon nanotubes on FexOy doped Al2O3-ZrO2 nanopowder

Author keywords

Carbon nanotubes; Ceramics; Nanopowder; Oxides

Indexed keywords

ALUMINA; ALUMINUM OXIDE; FLAME SPRAYING; IRON OXIDES; MOLYBDENUM METALLOGRAPHY; MORPHOLOGY; ORGANOMETALLICS; OXIDES; ZIRCONIA;

EID: 84903756145     PISSN: 00325910     EISSN: 1873328X     Source Type: Journal    
DOI: 10.1016/j.powtec.2014.06.020     Document Type: Article
Times cited : (8)

References (44)
  • 1
    • 0037008487 scopus 로고    scopus 로고
    • Carbon nanotubes-the route toward applications
    • Baughman R.H., Zakhidov A.A., de Heer W.A. Carbon nanotubes-the route toward applications. Science 2002, 297:787-792.
    • (2002) Science , vol.297 , pp. 787-792
    • Baughman, R.H.1    Zakhidov, A.A.2    de Heer, W.A.3
  • 2
    • 0036603751 scopus 로고    scopus 로고
    • The revolutionary creation of new advanced materials-carbon nanotube composites
    • Lau K.T., Hui D. The revolutionary creation of new advanced materials-carbon nanotube composites. Compos. Part B 2002, 33:263-277.
    • (2002) Compos. Part B , vol.33 , pp. 263-277
    • Lau, K.T.1    Hui, D.2
  • 3
    • 0000110877 scopus 로고    scopus 로고
    • New carbon materials for research technology
    • Scharff P. New carbon materials for research technology. Carbon 1998, 36:481-486.
    • (1998) Carbon , vol.36 , pp. 481-486
    • Scharff, P.1
  • 4
  • 5
    • 49849089583 scopus 로고    scopus 로고
    • Fracture toughness and fatigue life of MWCNT/epoxy composites
    • Yu N., Zhang Z.H., He S.Y. Fracture toughness and fatigue life of MWCNT/epoxy composites. Mater. Sci. Eng. A 2008, 494:380-384.
    • (2008) Mater. Sci. Eng. A , vol.494 , pp. 380-384
    • Yu, N.1    Zhang, Z.H.2    He, S.Y.3
  • 6
    • 0036405046 scopus 로고    scopus 로고
    • Failure mechanisms of carbon nanotube/epoxy composites pretreated in different temperature environments
    • Lau K.T., Shi S.Q. Failure mechanisms of carbon nanotube/epoxy composites pretreated in different temperature environments. Carbon 2002, 40:2961-2973.
    • (2002) Carbon , vol.40 , pp. 2961-2973
    • Lau, K.T.1    Shi, S.Q.2
  • 7
    • 0032800017 scopus 로고    scopus 로고
    • Development of a dispersion process for carbon nanotubes in an epoxy matrix and the resulting electrical properties
    • Sandler J., Shaffer M.S.P., Prasse T., Bauhofer W., Schulte K., Windle A.H. Development of a dispersion process for carbon nanotubes in an epoxy matrix and the resulting electrical properties. Polymer 1999, 40:5967-5971.
    • (1999) Polymer , vol.40 , pp. 5967-5971
    • Sandler, J.1    Shaffer, M.S.P.2    Prasse, T.3    Bauhofer, W.4    Schulte, K.5    Windle, A.H.6
  • 8
    • 44549086570 scopus 로고    scopus 로고
    • Reinforcement with carbon nanotubes in aluminium matrix composites
    • Choi H.J., Kwon G.B., Lee G.Y., Bae D.H. Reinforcement with carbon nanotubes in aluminium matrix composites. Scr. Mater. 2008, 59:360-363.
    • (2008) Scr. Mater. , vol.59 , pp. 360-363
    • Choi, H.J.1    Kwon, G.B.2    Lee, G.Y.3    Bae, D.H.4
  • 9
    • 33845270397 scopus 로고    scopus 로고
    • Processing and properties of carbon nanotubes reinforced aluminium composites
    • Deng C.F., Wang D.Z., Zhang X.X., Li A.B. Processing and properties of carbon nanotubes reinforced aluminium composites. Mater. Sci. Eng. A 2007, 444:138-145.
    • (2007) Mater. Sci. Eng. A , vol.444 , pp. 138-145
    • Deng, C.F.1    Wang, D.Z.2    Zhang, X.X.3    Li, A.B.4
  • 10
    • 24144445603 scopus 로고    scopus 로고
    • Strengthening in carbon nanotube aluminium (CNT/Al) composites
    • George R., Kashyap K.T., Rahul R., Yamdagni S. Strengthening in carbon nanotube aluminium (CNT/Al) composites. Scr. Mater. 2005, 53:1159-1163.
    • (2005) Scr. Mater. , vol.53 , pp. 1159-1163
    • George, R.1    Kashyap, K.T.2    Rahul, R.3    Yamdagni, S.4
  • 11
    • 37349072878 scopus 로고    scopus 로고
    • Carbon nanotube-reinforced aluminium strips
    • Esavi A.M.K., El Boradi M.A. Carbon nanotube-reinforced aluminium strips. Compos. Sci. Technol. 2008, 68:486-492.
    • (2008) Compos. Sci. Technol. , vol.68 , pp. 486-492
    • Esavi, A.M.K.1    El Boradi, M.A.2
  • 13
    • 7044272921 scopus 로고    scopus 로고
    • CNT-reinforced ceramics and metals
    • Curtin W.A., Sheldon B.W. CNT-reinforced ceramics and metals. Mater. Today 2004, 11:44-49.
    • (2004) Mater. Today , vol.11 , pp. 44-49
    • Curtin, W.A.1    Sheldon, B.W.2
  • 15
    • 33947374723 scopus 로고    scopus 로고
    • Reinforcement of mullite matrix with multi-walled carbon nanotubes
    • Wang J., Kou H., Liu X., Pan Y., Guo J. Reinforcement of mullite matrix with multi-walled carbon nanotubes. Ceram. Int. 2007, 33:719-722.
    • (2007) Ceram. Int. , vol.33 , pp. 719-722
    • Wang, J.1    Kou, H.2    Liu, X.3    Pan, Y.4    Guo, J.5
  • 17
    • 0346256571 scopus 로고    scopus 로고
    • Stabilization of cubic zirconia by carbon nanotubes
    • Luo T.Y., Liang T.X., Li C.S. Stabilization of cubic zirconia by carbon nanotubes. Mater. Sci. Eng. A 2004, 366:206-209.
    • (2004) Mater. Sci. Eng. A , vol.366 , pp. 206-209
    • Luo, T.Y.1    Liang, T.X.2    Li, C.S.3
  • 18
    • 33947393157 scopus 로고    scopus 로고
    • Gas-phase growth of diameter-controlled carbon nanotubes
    • Kim S.H., Zachariah M.R. Gas-phase growth of diameter-controlled carbon nanotubes. Mater. Lett. 2007, 61:2079-2083.
    • (2007) Mater. Lett. , vol.61 , pp. 2079-2083
    • Kim, S.H.1    Zachariah, M.R.2
  • 19
    • 0038033665 scopus 로고
    • Single shell carbon nanotubes of one nanometer diameter
    • Iijima S., Ichihashi T. Single shell carbon nanotubes of one nanometer diameter. Nature 1993, 363:603-605.
    • (1993) Nature , vol.363 , pp. 603-605
    • Iijima, S.1    Ichihashi, T.2
  • 20
    • 58149212911 scopus 로고
    • Catalytic growth of single-walled nanotubes by laser vaporization
    • Guo T., Nikolaev P., Thess A., Colbert D.T. Catalytic growth of single-walled nanotubes by laser vaporization. Chem. Phys. Lett. 1995, 243:49-54.
    • (1995) Chem. Phys. Lett. , vol.243 , pp. 49-54
    • Guo, T.1    Nikolaev, P.2    Thess, A.3    Colbert, D.T.4
  • 21
    • 33745278573 scopus 로고    scopus 로고
    • Morphologies and microstructures of free-like carbon produced at different reaction conditions in a CVD process
    • Ma H.L., Su D.S., Klein-Hoffmann A., Jin G.H., Guo X.Y. Morphologies and microstructures of free-like carbon produced at different reaction conditions in a CVD process. Carbon 2006, 44:2254-2260.
    • (2006) Carbon , vol.44 , pp. 2254-2260
    • Ma, H.L.1    Su, D.S.2    Klein-Hoffmann, A.3    Jin, G.H.4    Guo, X.Y.5
  • 23
    • 84925066303 scopus 로고    scopus 로고
    • Cambridge University Press, United Kingdom
    • Harris P.J.F. Carbon Nanotube Science 2009, 55. Cambridge University Press, United Kingdom.
    • (2009) Carbon Nanotube Science , pp. 55
    • Harris, P.J.F.1
  • 26
    • 14744289721 scopus 로고    scopus 로고
    • Fabrication of carbon nanotube reinforced alumina matrix nanocomposite by sol-gel process
    • Chan B., Cha S.I., Kim K.T., Lee K.H., Hong S.H. Fabrication of carbon nanotube reinforced alumina matrix nanocomposite by sol-gel process. Mater. Sci. Eng. A 2005, 395:124-128.
    • (2005) Mater. Sci. Eng. A , vol.395 , pp. 124-128
    • Chan, B.1    Cha, S.I.2    Kim, K.T.3    Lee, K.H.4    Hong, S.H.5
  • 27
    • 22544474430 scopus 로고    scopus 로고
    • Strengthening and toughening of carbon nanotube reinforced alumina nanocomposite fabricated by molecular level mixing process
    • Cha S.I., Kim K.T., Lee K.H., Mo C.B., Hong S.H. Strengthening and toughening of carbon nanotube reinforced alumina nanocomposite fabricated by molecular level mixing process. Scr. Mater. 2005, 53:793-797.
    • (2005) Scr. Mater. , vol.53 , pp. 793-797
    • Cha, S.I.1    Kim, K.T.2    Lee, K.H.3    Mo, C.B.4    Hong, S.H.5
  • 28
    • 36249011344 scopus 로고    scopus 로고
    • The effect of process parameters on the Liquid Flame Spray generated titania nanoparticles
    • Aromaa M., Keskinen H., Mäkelä J.M. The effect of process parameters on the Liquid Flame Spray generated titania nanoparticles. Biomol. Eng. 2007, 24:543-548.
    • (2007) Biomol. Eng. , vol.24 , pp. 543-548
    • Aromaa, M.1    Keskinen, H.2    Mäkelä, J.M.3
  • 29
    • 11144357963 scopus 로고    scopus 로고
    • Generation of metal and metal oxide nanoparticles by liquid flame spray process
    • Mäkelä J.M., Keskinen H., Forsblom T., Keskinen J. Generation of metal and metal oxide nanoparticles by liquid flame spray process. J. Mater. Sci. 2004, 39:2783-4788.
    • (2004) J. Mater. Sci. , vol.39 , pp. 2783-4788
    • Mäkelä, J.M.1    Keskinen, H.2    Forsblom, T.3    Keskinen, J.4
  • 34
    • 58249136857 scopus 로고    scopus 로고
    • 2 composite powders by calcining an emulsion precursor at 1100°C
    • 2 composite powders by calcining an emulsion precursor at 1100°C. J. Alloys Compd. 2008, 469:10-12.
    • (2008) J. Alloys Compd. , vol.469 , pp. 10-12
    • Chandradass, J.1    Bae, D.S.2
  • 36
    • 0030564396 scopus 로고    scopus 로고
    • Simultaneous determination of composition and thickness of thin iron-oxide films from XPS Fe 2p spectra
    • Graat P.C.J., Somers M.A.J. Simultaneous determination of composition and thickness of thin iron-oxide films from XPS Fe 2p spectra. Appl. Surf. Sci. 1996, 100:36-40.
    • (1996) Appl. Surf. Sci. , vol.100 , pp. 36-40
    • Graat, P.C.J.1    Somers, M.A.J.2
  • 38
    • 33846188118 scopus 로고    scopus 로고
    • Extent of charge ordering by Mössbauer spectroscopy and high-intensity high-resolution powder diffraction
    • Karen P., Gustafsson K., Lindén J. Extent of charge ordering by Mössbauer spectroscopy and high-intensity high-resolution powder diffraction. J. Solid State Chem. 2007, 180:138-147.
    • (2007) J. Solid State Chem. , vol.180 , pp. 138-147
    • Karen, P.1    Gustafsson, K.2    Lindén, J.3
  • 39
    • 73549100422 scopus 로고    scopus 로고
    • High-strength metal nanomagnets for diagnostics and medicine
    • Herrmann I.K., Grass R.N., Stark W.J. High-strength metal nanomagnets for diagnostics and medicine. Nanomedicine 2009, 4:787-798.
    • (2009) Nanomedicine , vol.4 , pp. 787-798
    • Herrmann, I.K.1    Grass, R.N.2    Stark, W.J.3
  • 41
    • 34047142103 scopus 로고    scopus 로고
    • Purity assessment of multiwalled carbon nanotubes by Raman spectroscopy
    • DiLeo R.A., Landi B.J., Raffaelle R.P. Purity assessment of multiwalled carbon nanotubes by Raman spectroscopy. J. Appl. Phys. 2007, 101:064307.
    • (2007) J. Appl. Phys. , vol.101 , pp. 064307
    • DiLeo, R.A.1    Landi, B.J.2    Raffaelle, R.P.3
  • 43
    • 29744470918 scopus 로고    scopus 로고
    • Radial-breathing-like phonon modes of double-walled carbon nanotubes
    • Wu G., Zhou J., Dong J. Radial-breathing-like phonon modes of double-walled carbon nanotubes. Phys. Rev. B 2005, 72:115418.
    • (2005) Phys. Rev. B , vol.72 , pp. 115418
    • Wu, G.1    Zhou, J.2    Dong, J.3
  • 44
    • 0000534809 scopus 로고    scopus 로고
    • Thermogravimetric analysis of the oxidation of multiwalled carbon nanotubes: evidence for the role of defect sites in carbon nanotube chemistry
    • Bom D., Andrews R., Jacques D., Aanthony J., Chen B., Meier M.S., Selegue J.P. Thermogravimetric analysis of the oxidation of multiwalled carbon nanotubes: evidence for the role of defect sites in carbon nanotube chemistry. Nano Lett. 2002, 2:615-619.
    • (2002) Nano Lett. , vol.2 , pp. 615-619
    • Bom, D.1    Andrews, R.2    Jacques, D.3    Aanthony, J.4    Chen, B.5    Meier, M.S.6    Selegue, J.P.7


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.