Volumn 47, Issue 23, 2013, Pages 13712-13720

Depassivation of aged Fe0 by ferrous ions: Implications to contaminant degradation

Author keywords

[No Author keywords available]

Indexed keywords

CONTAMINANT DEGRADATION; CORROSION CURRENT; CORROSION POTENTIALS; CRYSTALLINE PHASIS; OPEN CIRCUIT POTENTIAL; POLARIZATION RESISTANCES; RATE OF REDUCTION; SURFACE DISSOLUTION;

EID: 84889833625     PISSN: 0013936X     EISSN: 15205851     Source Type: Journal    
DOI: 10.1021/es403709v     Document Type: Article
Times cited : (74)

References (45)
  • 1
    • 0030220248 scopus 로고    scopus 로고
    • Kinetics of halogenated organic compound degradation by iron metal
    • Johnson, T. L.; Scherer, M. M.; Tratnyek, P. G. Kinetics of halogenated organic compound degradation by iron metal Environ. Sci. Technol. 1996, 30, 2634-2640
    • (1996) Environ. Sci. Technol. , vol.30 , pp. 2634-2640
    • Johnson, T.L.1    Scherer, M.M.2    Tratnyek, P.G.3
  • 3
    • 0035388045 scopus 로고    scopus 로고
    • Mass transport effects on the kinetics of nitrobenzene reduction by iron metal
    • Scherer, M. M.; Johnson, K. M.; Westall, J. C.; Tratnyek, P. G. Mass transport effects on the kinetics of nitrobenzene reduction by iron metal Environ. Sci. Technol. 2001, 35, 2804-2811
    • (2001) Environ. Sci. Technol. , vol.35 , pp. 2804-2811
    • Scherer, M.M.1    Johnson, K.M.2    Westall, J.C.3    Tratnyek, P.G.4
  • 4
    • 0032146653 scopus 로고    scopus 로고
    • Nitrate reduction by metallic iron
    • Huang, C. P.; Wang, H. W.; Chiu, P. C. Nitrate reduction by metallic iron Water Res. 1998, 32, 2257-2264
    • (1998) Water Res. , vol.32 , pp. 2257-2264
    • Huang, C.P.1    Wang, H.W.2    Chiu, P.C.3
  • 6
    • 0034307593 scopus 로고    scopus 로고
    • Performance evaluation of a zerovalent iron reactive barrier: Mineralogical characteristics
    • Phillips, D. H.; Gu, B.; Watson, D. B.; Roh, Y.; Liang, L.; Lee, S. Y. Performance evaluation of a zerovalent iron reactive barrier: Mineralogical characteristics Environ. Sci. Technol. 2000, 34, 4169-4176
    • (2000) Environ. Sci. Technol. , vol.34 , pp. 4169-4176
    • Phillips, D.H.1    Gu, B.2    Watson, D.B.3    Roh, Y.4    Liang, L.5    Lee, S.Y.6
  • 7
    • 0037108315 scopus 로고    scopus 로고
    • Effects of carbonate species on the kinetics of dechlorination of 1,1,1-trichloroethane by zero-valent iron
    • Agrawal, A.; Ferguson, W. J.; Gardner, B. O.; Christ, J. A.; Bandstra, J. Z.; Tratnyek, P. G. Effects of carbonate species on the kinetics of dechlorination of 1,1,1-trichloroethane by zero-valent iron Environ. Sci. Technol. 2002, 36, 4326-4333
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 4326-4333
    • Agrawal, A.1    Ferguson, W.J.2    Gardner, B.O.3    Christ, J.A.4    Bandstra, J.Z.5    Tratnyek, P.G.6
  • 8
    • 0042208360 scopus 로고    scopus 로고
    • Effects of oxide coating and selected cations on nitrate reduction by iron metal
    • Huang, Y. H.; Zhang, T. C.; Shea, P. J.; Comfort, S. D. Effects of oxide coating and selected cations on nitrate reduction by iron metal J. Environ. Qual. 2003, 32, 1306-1315
    • (2003) J. Environ. Qual. , vol.32 , pp. 1306-1315
    • Huang, Y.H.1    Zhang, T.C.2    Shea, P.J.3    Comfort, S.D.4
  • 9
    • 0037114999 scopus 로고    scopus 로고
    • Formation of ferrihydrite and associated iron corrosion products in permeable reactive barriers of zero-valent iron
    • Furukawa, Y.; Kim, J. W.; Watkins, J.; Wilkin, R. T. Formation of ferrihydrite and associated iron corrosion products in permeable reactive barriers of zero-valent iron Environ. Sci. Technol. 2002, 36, 5469-5475
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 5469-5475
    • Furukawa, Y.1    Kim, J.W.2    Watkins, J.3    Wilkin, R.T.4
  • 10
    • 80051664649 scopus 로고    scopus 로고
    • Recovery of iron/iron oxide nanoparticles from solution: Comparison of methods and their effects
    • Nurmi, J. T.; Sarathy, V.; Tratnyek, P. G.; Baer, D. R.; Amonette, J. E.; Karkamkar, A. Recovery of iron/iron oxide nanoparticles from solution: comparison of methods and their effects J. Nanopart. Res. 2011, 13, 1937-1952
    • (2011) J. Nanopart. Res. , vol.13 , pp. 1937-1952
    • Nurmi, J.T.1    Sarathy, V.2    Tratnyek, P.G.3    Baer, D.R.4    Amonette, J.E.5    Karkamkar, A.6
  • 11
    • 35948973102 scopus 로고    scopus 로고
    • Catalytic reduction of chlorobenzenes with Pd/Fe nanoparticles: Reactive sites, catalyst stability, particle aging, and regeneration
    • Zhu, B. W.; Lim, T. T. Catalytic reduction of chlorobenzenes with Pd/Fe nanoparticles: Reactive sites, catalyst stability, particle aging, and regeneration Environ. Sci. Technol. 2007, 41, 7523-7529
    • (2007) Environ. Sci. Technol. , vol.41 , pp. 7523-7529
    • Zhu, B.W.1    Lim, T.T.2
  • 12
    • 78449231950 scopus 로고    scopus 로고
    • Use of dithionite to extend the reactive lifetime of nanoscale zero-valent iron treatment systems
    • Xie, Y.; Cwiertny, D. M. Use of dithionite to extend the reactive lifetime of nanoscale zero-valent iron treatment systems Environ. Sci. Technol. 2010, 44, 8649-8655
    • (2010) Environ. Sci. Technol. , vol.44 , pp. 8649-8655
    • Xie, Y.1    Cwiertny, D.M.2
  • 13
    • 34247253302 scopus 로고    scopus 로고
    • Regeneration of iron for trichloroethylene reduction by Shewanella alga BrY
    • Shin, H. Y.; Singhal, N.; Park, J. W. Regeneration of iron for trichloroethylene reduction by Shewanella alga BrY Chemosphere 2007, 68, 1129-1134
    • (2007) Chemosphere , vol.68 , pp. 1129-1134
    • Shin, H.Y.1    Singhal, N.2    Park, J.W.3
  • 14
    • 84869179662 scopus 로고    scopus 로고
    • Enhanced biotransformation of DDTs by an iron- and humic-reducing bacteria Aeromonas hydrophila HS01 upon addition of goethite and anthraquinone-2,6-disulphonic disodium salt (AQDS)
    • Cao, F.; Liu, T. X.; Wu, C. Y.; Li, F. B.; Li, X. M.; Yu, H. Y.; Tong, H.; Chen, M. J. Enhanced biotransformation of DDTs by an iron- and humic-reducing bacteria Aeromonas hydrophila HS01 upon addition of goethite and anthraquinone-2,6-disulphonic disodium salt (AQDS) J. Agric. Food Chem. 2012, 60, 11238-11244
    • (2012) J. Agric. Food Chem. , vol.60 , pp. 11238-11244
    • Cao, F.1    Liu, T.X.2    Wu, C.Y.3    Li, F.B.4    Li, X.M.5    Yu, H.Y.6    Tong, H.7    Chen, M.J.8
  • 15
    • 36349015385 scopus 로고    scopus 로고
    • Adsorption and surface oxidation of Fe(II) on metal (hydr)oxides
    • Hiemstra, T.; Riemsdijk, W. H. Adsorption and surface oxidation of Fe(II) on metal (hydr)oxides Geochim. Cosmochim. Acta 2007, 71, 5913-5933
    • (2007) Geochim. Cosmochim. Acta , vol.71 , pp. 5913-5933
    • Hiemstra, T.1    Riemsdijk, W.H.2
  • 17
    • 0037089028 scopus 로고    scopus 로고
    • Reduction of polyhalogenated methanes by surface-bound Fe(II) in aqueous suspensions of iron oxides
    • Pecher, K.; Haderlein, S. B.; Schwarzenbach, R. P. Reduction of polyhalogenated methanes by surface-bound Fe(II) in aqueous suspensions of iron oxides Environ. Sci. Technol. 2002, 36, 1734-1741
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 1734-1741
    • Pecher, K.1    Haderlein, S.B.2    Schwarzenbach, R.P.3
  • 18
    • 0027061953 scopus 로고
    • The cycling of iron in natural environments: Considerations based on laboratory studies of heterogeneous redox processes
    • Stumm, W.; Sulzberger, B. The cycling of iron in natural environments: Considerations based on laboratory studies of heterogeneous redox processes Geochim. Cosmochim. Acta 1992, 56, 3233-3257
    • (1992) Geochim. Cosmochim. Acta , vol.56 , pp. 3233-3257
    • Stumm, W.1    Sulzberger, B.2
  • 20
  • 21
    • 4143068994 scopus 로고    scopus 로고
    • Abiotic degradation of pentachloronitrobenzene by Fe(II): Reactions on goethite and iron oxide nanoparticles
    • Klupinski, T. P.; Chin, Y. P.; Traina, S. J. Abiotic degradation of pentachloronitrobenzene by Fe(II): Reactions on goethite and iron oxide nanoparticles Environ. Sci. Technol. 2004, 38, 4353-4360
    • (2004) Environ. Sci. Technol. , vol.38 , pp. 4353-4360
    • Klupinski, T.P.1    Chin, Y.P.2    Traina, S.J.3
  • 23
    • 33646037326 scopus 로고    scopus 로고
    • Ferrous iron sorption by hydrous metal oxides
    • Nano, G. V.; Strathmann, T. J. Ferrous iron sorption by hydrous metal oxides J. Colloid Interface Sci. 2006, 297, 443-454
    • (2006) J. Colloid Interface Sci. , vol.297 , pp. 443-454
    • Nano, G.V.1    Strathmann, T.J.2
  • 24
    • 79951665528 scopus 로고    scopus 로고
    • Effect of amorphous Fe(III) oxide transformation on the Fe(II)-mediated reduction of U(VI)
    • Boland, D. D.; Collins, R. N.; Payne, T. E.; Waite, T. D. Effect of amorphous Fe(III) oxide transformation on the Fe(II)-mediated reduction of U(VI) Environ. Sci. Technol. 2011, 45, 1327-1333
    • (2011) Environ. Sci. Technol. , vol.45 , pp. 1327-1333
    • Boland, D.D.1    Collins, R.N.2    Payne, T.E.3    Waite, T.D.4
  • 25
    • 84882690607 scopus 로고    scopus 로고
    • An in situ quick-EXAFS and redox potential study of the Fe(II)-catalysed transformation of ferrihydrite
    • 10.1016/j.colsurfa.2013.02.009
    • Boland, D. D.; Collins, R. N.; Glover, C. J.; Waite, T. D. An in situ quick-EXAFS and redox potential study of the Fe(II)-catalysed transformation of ferrihydrite Colloids Surf., A 2013, 10.1016/j.colsurfa.2013.02.009
    • (2013) Colloids Surf., A
    • Boland, D.D.1    Collins, R.N.2    Glover, C.J.3    Waite, T.D.4
  • 26
    • 84880122402 scopus 로고    scopus 로고
    • 0 by inorganic salts: Implications to contaminant degradation in seawater
    • 0 by inorganic salts: Implications to contaminant degradation in seawater Environ. Sci. Technol. 2013, 47, 7350-7356
    • (2013) Environ. Sci. Technol. , vol.47 , pp. 7350-7356
    • Liu, T.X.1    Li, X.M.2    Waite, T.D.3
  • 28
    • 37549045698 scopus 로고    scopus 로고
    • Electrochemical studies of packed iron powder electrodes: Effects of common constituents of natural waters on corrosion potential
    • Nurmi, J. T.; Tratnyek, P. G. Electrochemical studies of packed iron powder electrodes: Effects of common constituents of natural waters on corrosion potential Corros. Sci. 2008, 50, 144-154
    • (2008) Corros. Sci. , vol.50 , pp. 144-154
    • Nurmi, J.T.1    Tratnyek, P.G.2
  • 29
    • 2942657609 scopus 로고    scopus 로고
    • Packed powder electrodes for characterizing the reactivity of granular iron in borate solutions
    • Nurmi, J. T.; Bandstra, J. Z.; Tratnyek, P. G. Packed powder electrodes for characterizing the reactivity of granular iron in borate solutions J. Electrochem. Soc. 2004, 151, 347-353
    • (2004) J. Electrochem. Soc. , vol.151 , pp. 347-353
    • Nurmi, J.T.1    Bandstra, J.Z.2    Tratnyek, P.G.3
  • 31
    • 0347333641 scopus 로고    scopus 로고
    • The role of oxides in reduction reactions at the metal-water interface
    • Sparks, D. L. Grundl, T. J. American Chemical Society: Washington, DC, ACS Symposium Series - 322
    • Scherer, M. M.; Balko, B. A.; Tratnyek, P. G. The role of oxides in reduction reactions at the metal-water interface. In Mineral-Water Interfacial Reactions: Kinetics and Mechanisms; Sparks, D. L.; Grundl, T. J., Eds.; American Chemical Society: Washington, DC, 1998; ACS Symposium Series, Vol. 715, pp 301-322.
    • (1998) Mineral-Water Interfacial Reactions: Kinetics and Mechanisms , vol.715 , pp. 301
    • Scherer, M.M.1    Balko, B.A.2    Tratnyek, P.G.3
  • 33
    • 26844532416 scopus 로고    scopus 로고
    • Modeling the dynamics of fermentation and respiratory processes in a groundwater plume of phenolic contaminants interpreted from laboratory- to field-scale
    • Watson, I. A.; Oswald, S. E.; Banwart, S. A.; Crouch, R. S.; Thornton, S. F. Modeling the dynamics of fermentation and respiratory processes in a groundwater plume of phenolic contaminants interpreted from laboratory- to field-scale Environ. Sci. Technol. 2005, 39, 8829-8839
    • (2005) Environ. Sci. Technol. , vol.39 , pp. 8829-8839
    • Watson, I.A.1    Oswald, S.E.2    Banwart, S.A.3    Crouch, R.S.4    Thornton, S.F.5
  • 34
    • 0023804377 scopus 로고
    • Role of surface speciation in the low-temperature dissolution of minerals
    • Blum, A. E.; Lasaga, A. C. Role of surface speciation in the low-temperature dissolution of minerals Nature 1988, 331, 431-433
    • (1988) Nature , vol.331 , pp. 431-433
    • Blum, A.E.1    Lasaga, A.C.2
  • 36
    • 0022901661 scopus 로고
    • The coordination chemistry of weathering: II. Dissolution of Fe(III) oxides
    • Zinder, B.; Furrer, G.; Stumm, W. The coordination chemistry of weathering: II. Dissolution of Fe(III) oxides Geochim. Cosmochim. Acta 1986, 50, 1861-1869
    • (1986) Geochim. Cosmochim. Acta , vol.50 , pp. 1861-1869
    • Zinder, B.1    Furrer, G.2    Stumm, W.3
  • 37
    • 4544255728 scopus 로고    scopus 로고
    • Spectroscopic evidence for Fe(II)-Fe(III) electron transfer at the iron oxide-water interface
    • Williams, A. G. B.; Scherer, M. M. Spectroscopic evidence for Fe(II)-Fe(III) electron transfer at the iron oxide-water interface Environ. Sci. Technol. 2004, 38, 4782-4790
    • (2004) Environ. Sci. Technol. , vol.38 , pp. 4782-4790
    • Williams, A.G.B.1    Scherer, M.M.2
  • 38
    • 64349120216 scopus 로고    scopus 로고
    • Atom exchange between aqueous Fe(II) and goethite: An Fe isotope tracer study
    • Handler, R. M.; Beard, B. L.; Johnson, C. M.; Scherer, M. M. Atom exchange between aqueous Fe(II) and goethite: An Fe isotope tracer study Environ. Sci. Technol. 2009, 43, 1102-1107
    • (2009) Environ. Sci. Technol. , vol.43 , pp. 1102-1107
    • Handler, R.M.1    Beard, B.L.2    Johnson, C.M.3    Scherer, M.M.4
  • 40
    • 0036469556 scopus 로고    scopus 로고
    • Kinetics of nitrate, nitrite, and Cr(VI) reduction by iron metal
    • Alowitz, M. J.; Scherer, M. M. Kinetics of nitrate, nitrite, and Cr(VI) reduction by iron metal Environ. Sci. Technol. 2002, 36, 299-306
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 299-306
    • Alowitz, M.J.1    Scherer, M.M.2
  • 41
    • 33646751915 scopus 로고    scopus 로고
    • Kinetic and microscopic studies of reductive transformations of organic contaminants on goethite
    • Chun, C. L.; Leepenn, R.; Arnold, W. Kinetic and microscopic studies of reductive transformations of organic contaminants on goethite Environ. Sci. Technol. 2006, 40, 3299-3304
    • (2006) Environ. Sci. Technol. , vol.40 , pp. 3299-3304
    • Chun, C.L.1    Leepenn, R.2    Arnold, W.3
  • 42
    • 33747469555 scopus 로고    scopus 로고
    • QSAR study of the reduction of nitroaromatics by Fe(II) species
    • Colón, D.; Weber, E. J.; Anderson, J. L. QSAR study of the reduction of nitroaromatics by Fe(II) species Environ. Sci. Technol. 2006, 40, 4976-4982
    • (2006) Environ. Sci. Technol. , vol.40 , pp. 4976-4982
    • Colón, D.1    Weber, E.J.2    Anderson, J.L.3
  • 43
    • 77949915302 scopus 로고    scopus 로고
    • Enhanced reductive dechlorination of DDT in an anaerobic system of dissimilatory iron-reducing bacteria and iron oxide
    • Li, F. B.; Li, X. M.; Zhou, S. G.; Zhuang, L.; Cao, F.; Huang, D. Y.; Xu, W.; Liu, T. X.; Feng, C. H. Enhanced reductive dechlorination of DDT in an anaerobic system of dissimilatory iron-reducing bacteria and iron oxide Environ. Pollut. 2010, 158, 1733-1740
    • (2010) Environ. Pollut. , vol.158 , pp. 1733-1740
    • Li, F.B.1    Li, X.M.2    Zhou, S.G.3    Zhuang, L.4    Cao, F.5    Huang, D.Y.6    Xu, W.7    Liu, T.X.8    Feng, C.H.9
  • 44
    • 47049083957 scopus 로고    scopus 로고
    • Oxygenation of Fe(II) in natural waters revisited: Kinetic modeling approaches, rate constant estimation and the importance of various reaction pathways
    • Pham, A. N.; Waite, T. D. Oxygenation of Fe(II) in natural waters revisited: Kinetic modeling approaches, rate constant estimation and the importance of various reaction pathways Geochim. Cosmochim. Acta 2008, 72, 3616-3630
    • (2008) Geochim. Cosmochim. Acta , vol.72 , pp. 3616-3630
    • Pham, A.N.1    Waite, T.D.2
  • 45
    • 84864677107 scopus 로고    scopus 로고
    • Influence of anionic cosolutes and pH on nanoscale zerovalent iron longevity: Time scales and mechanisms of reactivity loss toward 1,1,1,2-tetrachloroethane and Cr(VI)
    • Xie, Y.; Cwiertny, D. M. Influence of anionic cosolutes and pH on nanoscale zerovalent iron longevity: Time scales and mechanisms of reactivity loss toward 1,1,1,2-tetrachloroethane and Cr(VI) Environ. Sci. Technol. 2012, 46, 8365-8373
    • (2012) Environ. Sci. Technol. , vol.46 , pp. 8365-8373
    • Xie, Y.1    Cwiertny, D.M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.