Volumn 38, Issue 28, 2013, Pages 12509-12515

Effect of electrotransport treatment on susceptibility of high-strength low alloy steel to hydrogen embrittlement

Author keywords

Electrotransport; Gas chromatography; Hydrogen embrittlement; Low alloy steel; Slow strain rate test

Indexed keywords

ELECTROSTATIC FORCE FIELDS; ELECTROTRANSPORT; ELECTROTRANSPORT THEORY; FRACTURE SURFACE ANALYSIS; HIGH-STRENGTH LOW ALLOY STEELS; HYDROGEN CONCENTRATION; SLOW STRAIN RATE TESTS; ULTIMATE TENSILE STRENGTH;

EID: 84883776679     PISSN: 03603199     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijhydene.2013.07.040     Document Type: Article
Times cited : (10)

References (34)
  • 2
    • 84866465168 scopus 로고    scopus 로고
    • Toward the clean production of hydrogen: Competition among renewable energy sources and nuclear power
    • D.H. Lee Toward the clean production of hydrogen: competition among renewable energy sources and nuclear power Int J Hydrogen Energy 37 2012 15726 15735
    • (2012) Int J Hydrogen Energy , vol.37 , pp. 15726-15735
    • Lee, D.H.1
  • 3
    • 84867891321 scopus 로고    scopus 로고
    • Quantifying the hydrogen embrittlement of pipeline steel for safety considerations
    • L. Briottet, I. Moro, and P. Lemoine Quantifying the hydrogen embrittlement of pipeline steel for safety considerations Int J Hydrogen Energy 37 2012 17616 17623
    • (2012) Int J Hydrogen Energy , vol.37 , pp. 17616-17623
    • Briottet, L.1    Moro, I.2    Lemoine, P.3
  • 4
    • 35348954277 scopus 로고    scopus 로고
    • Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test
    • M. Wang, E. Akiyama, and K. Tsuzaki Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test Corros Sci 49 2007 4081 4097
    • (2007) Corros Sci , vol.49 , pp. 4081-4097
    • Wang, M.1    Akiyama, E.2    Tsuzaki, K.3
  • 5
    • 84655162270 scopus 로고    scopus 로고
    • Development of high pressure gaseous hydrogen storage technologies
    • J. Zheng, X. Liu, P. Xu, P. Liu, Y. Zhao, and J. Yang Development of high pressure gaseous hydrogen storage technologies Int J Hydrogen Energy 37 2012 1048 1057
    • (2012) Int J Hydrogen Energy , vol.37 , pp. 1048-1057
    • Zheng, J.1    Liu, X.2    Xu, P.3    Liu, P.4    Zhao, Y.5    Yang, J.6
  • 6
    • 77949762341 scopus 로고    scopus 로고
    • Effects of grain size on hydrogen environment embrittlement of high strength low alloy steel in 45 MPa gaseous hydrogen
    • K. Takasawa, Y. Wada, R. Ishigaki, and R. Kayano Effects of grain size on hydrogen environment embrittlement of high strength low alloy steel in 45 MPa gaseous hydrogen Mater Trans 51 2010 347 353
    • (2010) Mater Trans , vol.51 , pp. 347-353
    • Takasawa, K.1    Wada, Y.2    Ishigaki, R.3    Kayano, R.4
  • 7
    • 44449100163 scopus 로고    scopus 로고
    • Hydrogen embrittlement of metallic materials in high-pressure hydrogen at normal temperature
    • R. Chen, J. Zheng, P. Xu, F. Kai, and P. Liu Hydrogen embrittlement of metallic materials in high-pressure hydrogen at normal temperature Acta Energiae Solaris Sinica 29 2008 502 508
    • (2008) Acta Energiae Solaris Sinica , vol.29 , pp. 502-508
    • Chen, R.1    Zheng, J.2    Xu, P.3    Kai, F.4    Liu, P.5
  • 8
    • 84860229248 scopus 로고    scopus 로고
    • Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments
    • N.E. Nanninga, Y.S. Levy, E.S. Drexler, R.T. Condon, A.E. Stevenson, and A.J. Slifka Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments Corros Sci 59 2012 1 9
    • (2012) Corros Sci , vol.59 , pp. 1-9
    • Nanninga, N.E.1    Levy, Y.S.2    Drexler, E.S.3    Condon, R.T.4    Stevenson, A.E.5    Slifka, A.J.6
  • 10
    • 0037447645 scopus 로고    scopus 로고
    • Effects of strain rate and temperature on tensile behavior of hydrogen-charged SA508 Cl.3 pressure vessel steel
    • X.Q. Wu, and I.S. Kim Effects of strain rate and temperature on tensile behavior of hydrogen-charged SA508 Cl.3 pressure vessel steel Mater Sci Eng A 348 2003 309 318
    • (2003) Mater Sci Eng A , vol.348 , pp. 309-318
    • Wu, X.Q.1    Kim, I.S.2
  • 11
    • 1642537693 scopus 로고    scopus 로고
    • Role of hydrogen in the sulfide stress-corrosion cracking of pipeline steels
    • V.Y. Chernov, V.D. Makarenko, and L.S. Shlapak Role of hydrogen in the sulfide stress-corrosion cracking of pipeline steels Mater Sci 39 2003 144 147
    • (2003) Mater Sci , vol.39 , pp. 144-147
    • Chernov, V.Y.1    Makarenko, V.D.2    Shlapak, L.S.3
  • 12
    • 2442660695 scopus 로고    scopus 로고
    • Effect of post- weld heat treatment on the microstructure and hydrogen permeation of 13CrNiMo steels
    • C. Gesnouin, A. Hazarabedian, P. Bruzzoni, J. Ovejero-García, P. Bilmes, and C. Llorente Effect of post- weld heat treatment on the microstructure and hydrogen permeation of 13CrNiMo steels Corros Sci 46 2004 1633 1647
    • (2004) Corros Sci , vol.46 , pp. 1633-1647
    • Gesnouin, C.1    Hazarabedian, A.2    Bruzzoni, P.3    Ovejero-García, J.4    Bilmes, P.5    Llorente, C.6
  • 13
    • 0023995459 scopus 로고
    • Surface modification: A potential new approach to combating hydrogen induced fracture in steel
    • B.E. Wilde, and T. Shimada Surface modification: a potential new approach to combating hydrogen induced fracture in steel Scripta Met 22 1988 551 556
    • (1988) Scripta Met , vol.22 , pp. 551-556
    • Wilde, B.E.1    Shimada, T.2
  • 14
    • 0020193851 scopus 로고
    • X-ray-induced release of hydrogen in lithium-exposed stainless steel
    • T. Miki, M. Touge, and M. Ikeya X-ray-induced release of hydrogen in lithium-exposed stainless steel J Nucl Mater 110 1982 150 157
    • (1982) J Nucl Mater , vol.110 , pp. 150-157
    • Miki, T.1    Touge, M.2    Ikeya, M.3
  • 15
    • 84855710018 scopus 로고    scopus 로고
    • 2 coated iron studied by electrochemical penetration and desorption techniques
    • 2 coated iron studied by electrochemical penetration and desorption techniques Int J Hydrogen Energy 37 2012 1826 1835
    • (2012) Int J Hydrogen Energy , vol.37 , pp. 1826-1835
    • Voloshchuk, I.1    Zakroczymski, T.2
  • 16
    • 33750629862 scopus 로고    scopus 로고
    • Studies on inhibition of hydrogen-induced cracking of linepipe steels
    • M. Elboujdaîni, V.S. Sastri, and J.R. Perumareddi Studies on inhibition of hydrogen-induced cracking of linepipe steels Corrosion 62 2006 29 34
    • (2006) Corrosion , vol.62 , pp. 29-34
    • Elboujdaîni, M.1    Sastri, V.S.2    Perumareddi, J.R.3
  • 17
    • 67349272757 scopus 로고    scopus 로고
    • Hydrogen and helium removal retained in stainless steel by neon glow discharge
    • Y. Yamauchi, K. Takeda, Y. Nobuta, and T. Hino Hydrogen and helium removal retained in stainless steel by neon glow discharge J Nucl Mater 390-391 2009 1048 1050
    • (2009) J Nucl Mater , vol.390-391 , pp. 1048-1050
    • Yamauchi, Y.1    Takeda, K.2    Nobuta, Y.3    Hino, T.4
  • 18
    • 84872027276 scopus 로고    scopus 로고
    • Electrochemical hydrogen discharge of high-strength low alloy steel for high-pressure gaseous hydrogen storage tank: Effect of discharging temperature
    • T.H. Nam, J.G. Kim, and Y.S. Choi Electrochemical hydrogen discharge of high-strength low alloy steel for high-pressure gaseous hydrogen storage tank: effect of discharging temperature Int J Hydrogen Energy 38 2013 999 1003
    • (2013) Int J Hydrogen Energy , vol.38 , pp. 999-1003
    • Nam, T.H.1    Kim, J.G.2    Choi, Y.S.3
  • 22
    • 84880033953 scopus 로고    scopus 로고
    • Low-cycle fatigue behaviors of two heats of SA508 Gr.1a low alloy steel in 310 C air and deoxygenated water-effects of dynamic strain aging and microstructure
    • H. Jang, J.H. Kim, C.H. Jang, J.G. Lee, and T.S. Kim Low-cycle fatigue behaviors of two heats of SA508 Gr.1a low alloy steel in 310 C air and deoxygenated water-effects of dynamic strain aging and microstructure Mater Sci Eng A 580 2013 41 50
    • (2013) Mater Sci Eng A , vol.580 , pp. 41-50
    • Jang, H.1    Kim, J.H.2    Jang, C.H.3    Lee, J.G.4    Kim, T.S.5
  • 23
    • 44249083535 scopus 로고    scopus 로고
    • Effect of cyclic strain rate and sulfides on environmentally assisted cracking behaviors of SA508 Gr.1A low alloy steel in deoxygenated water at 310 C
    • H. Jang, H.C. Cho, C.H. Jang, T.S. Kim, and C.K. Moon Effect of cyclic strain rate and sulfides on environmentally assisted cracking behaviors of SA508 Gr.1A low alloy steel in deoxygenated water at 310 C Nucl Eng Technol 40 2008 225 232
    • (2008) Nucl Eng Technol , vol.40 , pp. 225-232
    • Jang, H.1    Cho, H.C.2    Jang, C.H.3    Kim, T.S.4    Moon, C.K.5
  • 24
    • 29244470480 scopus 로고    scopus 로고
    • Study on hydrogen absorption of pipeline steel under cathodic charging
    • M. Yan, and Y. Weng Study on hydrogen absorption of pipeline steel under cathodic charging Corros Sci 48 2006 432 444
    • (2006) Corros Sci , vol.48 , pp. 432-444
    • Yan, M.1    Weng, Y.2
  • 25
    • 67650162674 scopus 로고    scopus 로고
    • Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials
    • S. Bechtle, M. Kumar, B.P. Somerday, M.E. Launey, and R.O. Ritchie Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials Acta Mater 57 2009 4148 4157
    • (2009) Acta Mater , vol.57 , pp. 4148-4157
    • Bechtle, S.1    Kumar, M.2    Somerday, B.P.3    Launey, M.E.4    Ritchie, R.O.5
  • 26
    • 79960706895 scopus 로고    scopus 로고
    • Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging
    • D. Pérez Escobar, C. Miñambres, L. Duprez, K. Verbeken, and M. Verhaege Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging Corros Sci 53 2011 3166 3176
    • (2011) Corros Sci , vol.53 , pp. 3166-3176
    • Pérez Escobar, D.1    Miñambres, C.2    Duprez, L.3    Verbeken, K.4    Verhaege, M.5
  • 27
    • 34548475127 scopus 로고    scopus 로고
    • Hemispherical bubbles growth on electrochemically charged aluminum with hydrogen
    • P. Rozenak Hemispherical bubbles growth on electrochemically charged aluminum with hydrogen Int J Hydrogen Energy 32 2007 2816 2823
    • (2007) Int J Hydrogen Energy , vol.32 , pp. 2816-2823
    • Rozenak, P.1
  • 28
    • 0000436675 scopus 로고    scopus 로고
    • Transgranular stress corrosion cracking of X-80 and X-52 pipeline steels in dilute aqueous solution with near-neutral pH
    • B. Gu, W.Z. Yu, J.L. Luo, and X. Mao Transgranular stress corrosion cracking of X-80 and X-52 pipeline steels in dilute aqueous solution with near-neutral pH Corrosion 55 1999 312 318
    • (1999) Corrosion , vol.55 , pp. 312-318
    • Gu, B.1    Yu, W.Z.2    Luo, J.L.3    Mao, X.4
  • 30
    • 47749149418 scopus 로고
    • Comparative study of methods for determining the diffusible hydrogen content in welds
    • L.C. Abreu, P.J. Modenesi, and P.V. Marques Comparative study of methods for determining the diffusible hydrogen content in welds Welding Int 9 1995 26 31
    • (1995) Welding Int , vol.9 , pp. 26-31
    • Abreu, L.C.1    Modenesi, P.J.2    Marques, P.V.3
  • 31
    • 0004801222 scopus 로고    scopus 로고
    • NACE TM0177-96, NACE International Houston, Texas
    • 2S environments 1996 NACE International Houston, Texas
    • (1996) 2S Environments
  • 32
    • 47749098053 scopus 로고    scopus 로고
    • Effect of microstructure on hydrogen-induced cracking of linepipe steels
    • S.U. Koh, H.G. Jung, K.B. Kang, G.T. Park, and K.Y. Kim Effect of microstructure on hydrogen-induced cracking of linepipe steels Corrosion 64 2008 574 585
    • (2008) Corrosion , vol.64 , pp. 574-585
    • Koh, S.U.1    Jung, H.G.2    Kang, K.B.3    Park, G.T.4    Kim, K.Y.5
  • 33
    • 47349102472 scopus 로고    scopus 로고
    • Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel
    • G.T. Park, S.U. Koh, H.G. Jung, and K.Y. Kim Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel Corros Sci 50 2008 1865 1871
    • (2008) Corros Sci , vol.50 , pp. 1865-1871
    • Park, G.T.1    Koh, S.U.2    Jung, H.G.3    Kim, K.Y.4
  • 34
    • 79955774118 scopus 로고    scopus 로고
    • Influence of the applied stress rate on the stress corrosion cracking of 4340 and 3.5NiCrMoV steels under conditions of cathodic hydrogen charging
    • S. Ramamurthy, W.M.L. Lau, and A. Atrens Influence of the applied stress rate on the stress corrosion cracking of 4340 and 3.5NiCrMoV steels under conditions of cathodic hydrogen charging Corros Sci 53 2011 2419 2429
    • (2011) Corros Sci , vol.53 , pp. 2419-2429
    • Ramamurthy, S.1    Lau, W.M.L.2    Atrens, A.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.