Volumn 6, Issue 4, 2013, Pages 1310-1325

Lithium ion battery anode aging mechanisms

Author keywords

[No Author keywords available]

Indexed keywords

AGING MECHANISM; ANODE ELECTRODES; DEGRADATION MECHANISM; ELECTRODE MATERIAL; LITHIUM IONS; LITHIUM-ION BATTERY; LITHIUM-ION BATTERY ANODES; PASSIVATED SURFACE;

EID: 84880103873     PISSN: None     EISSN: 19961944     Source Type: Journal    
DOI: 10.3390/ma6041310     Document Type: Review
Times cited : (339)

References (101)
  • 1
    • 41849146772 scopus 로고    scopus 로고
    • Material challenges facing electrical energy storage
    • Whittingham, M.S. Material challenges facing electrical energy storage. MRS Bull. 2008, 33, 411-419.
    • (2008) MRS Bull. , vol.33 , pp. 411-419
    • Whittingham, M.S.1
  • 2
    • 44849130726 scopus 로고    scopus 로고
    • Issues and challenges facing rechargeable thin film lithium batteries
    • Patil, A.; Patil, V.; Shin, W.D.; Choi, J.W.; Paik, D.S.; Yoon, J. Issues and challenges facing rechargeable thin film lithium batteries. Mater. Res. Bull. 2008, 43, 1913-1942.
    • (2008) Mater. Res. Bull. , vol.43 , pp. 1913-1942
    • Patil, A.1    Patil, V.2    Shin, W.D.3    Choi, J.W.4    Paik, D.S.5    Yoon, J.6
  • 3
    • 40049108277 scopus 로고    scopus 로고
    • Materials for the next generation lithium ion batteries
    • Shukla, A.K.; Kumar, T.P. Materials for the next generation lithium ion batteries. Curr. Sci. 2008, 94, 314-331.
    • (2008) Curr. Sci. , vol.94 , pp. 314-331
    • Shukla, A.K.1    Kumar, T.P.2
  • 4
    • 0033896106 scopus 로고    scopus 로고
    • Recent development of carbon materials for Li Ion batteries
    • Endo, M.; Kim, C.; Nishimura, K.; Fujino, T.; Miyashita, K. Recent development of carbon materials for Li Ion batteries. Carbon 2000, 38, 183-197.
    • (2000) Carbon , vol.38 , pp. 183-197
    • Endo, M.1    Kim, C.2    Nishimura, K.3    Fujino, T.4    Miyashita, K.5
  • 5
    • 43049123174 scopus 로고    scopus 로고
    • Measuring the salt activity coefficient in Lithium-battery electrolytes
    • Stewart, S.; Newman, J. Measuring the salt activity coefficient in Lithium-battery electrolytes. J. Electrochem. Soc. 2008, 155, A458-A463.
    • (2008) J. Electrochem. Soc. , vol.155
    • Stewart, S.1    Newman, J.2
  • 6
    • 39049093597 scopus 로고    scopus 로고
    • A comparison of solid electrolyte interphase on the artificial graphite anode of the aged and cycled commercial lithium ion cells
    • Lu, M.; Cheng, H.; Yang, Y. A comparison of solid electrolyte interphase on the artificial graphite anode of the aged and cycled commercial lithium ion cells. Eelectrochim. Acta 2008, 53, 3539-3546.
    • (2008) Eelectrochim. Acta , vol.53 , pp. 3539-3546
    • Lu, M.1    Cheng, H.2    Yang, Y.3
  • 7
    • 85016851909 scopus 로고    scopus 로고
    • Performance degradation and gassing of Li4Ti5O12/LiMn2O4 lithium-ion cells
    • Belharouak, I.; Koening, G., Jr.; Tan, T.; Yumoto, H.; Ota, N. Performance degradation and gassing of Li4Ti5O12/LiMn2O4 lithium-ion cells. J. Electrochem. Soc. 2012, 159, 1165-1170.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 1165-1170
    • Belharouak, I.1    Koening, G.2    Tan, T.3    Yumoto, H.4    Ota, N.5
  • 8
    • 0038347500 scopus 로고    scopus 로고
    • Electrochemical behavior of graphite anode at elevated temperature in organic carbonate solution
    • Levi, M.D.; Wang, C.; Gnanara, J.S.; Aurbach, D. Electrochemical behavior of graphite anode at elevated temperature in organic carbonate solution. J. Power Sources 2003, 119, 538-542.
    • (2003) J. Power Sources , vol.119 , pp. 538-542
    • Levi, M.D.1    Wang, C.2    Gnanara, J.S.3    Aurbach, D.4
  • 10
    • 0037079131 scopus 로고    scopus 로고
    • Capacity fade of Sony 18650 cells cycled at elevated temperatures Part II
    • Haran, B.; White, R.; Popov, B.N. Capacity fade of Sony 18650 cells cycled at elevated temperatures Part II. Capacity fade analysis. J. Power Sources 2002, 112, 614-620.
    • (2002) Capacity fade analysis. J. Power Sources , vol.112 , pp. 614-620
    • Haran, B.1    White, R.2    Popov, B.N.3
  • 11
    • 78049366753 scopus 로고    scopus 로고
    • Cycling degradation of automotive LiFePO4 lithium-ion battery
    • Zhang, Y.; Wang, C.; Tang, X. Cycling degradation of automotive LiFePO4 lithium-ion battery. J. Power Sources 2011, 196, 1513-1520.
    • (2011) J. Power Sources , vol.196 , pp. 1513-1520
    • Zhang, Y.1    Wang, C.2    Tang, X.3
  • 12
    • 33645418229 scopus 로고    scopus 로고
    • A study on capacity fading of lithium-ion battery with a manganese positive electrode during cycling
    • Yang, L.; Takahashi, M.; Wang, B. A study on capacity fading of lithium-ion battery with a manganese positive electrode during cycling. Electrochim. Acta 2006, 51, 3228-3234.
    • (2006) Electrochim. Acta , vol.51 , pp. 3228-3234
    • Yang, L.1    Takahashi, M.2    Wang, B.3
  • 13
    • 84861355816 scopus 로고    scopus 로고
    • Long-term low rate cycling of LiCoO2 graphite Li-ion cells at 55 °C
    • Smith, A.J.; Hannah, M.; Dahn, J.R. Long-term low rate cycling of LiCoO2 graphite Li-ion cells at 55 °C. J. Electrochem. Soc. 2012, 159, 705-710.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 705-710
    • Smith, A.J.1    Hannah, M.2    Dahn, J.R.3
  • 14
    • 26844491391 scopus 로고    scopus 로고
    • Aging characteristics of high-power lithium ion cells with LiNi08Co0.15Al0.05O2 and Li4/3Ti5/3O4 electrodes.
    • Abraham, D.P.; Reynolds, E.M.; Samman, E.; Jansen, A.N.; Dees, D.W. Aging characteristics of high-power lithium ion cells with LiNi0.8Co0.15Al0.05O2 and Li4/3Ti5/3O4 electrodes. Electrochim. Acta 2005, 51, 502-510.
    • (2005) Electrochim. Acta , vol.51 , pp. 502-510
    • Abraham, D.P.1    Reynolds, E.M.2    Samman, E.3    Jansen, A.N.4    Dees, D.W.5
  • 15
    • 84868711373 scopus 로고    scopus 로고
    • Influence of manganese dissolution on the degradation of surface films on edge plane graphite negative -electrodes in lithium -ion batteries
    • Ochida, M.; Domi, Y.; Doi, T.; Tsubouchi, S.; Nakagawa, H.; Yamanaka, T.; Abe, T.; Ogumi, Z. Influence of manganese dissolution on the degradation of surface films on edge plane graphite negative -electrodes in lithium -ion batteries. J. Electrochem. Soc. 2012, 159, A961-A966.
    • (2012) J. Electrochem. Soc. , vol.159
    • Ochida, M.1    Domi, Y.2    Doi, T.3    Tsubouchi, S.4    Nakagawa, H.5    Yamanaka, T.6    Abe, T.7    Ogumi, Z.8
  • 16
    • 33744975480 scopus 로고    scopus 로고
    • Cycle life performance of lithium-ion pouch cells
    • Kumaresan, K.; Guo, O.; Ramada, P.; White, R.E. Cycle life performance of lithium-ion pouch cells. J. Power Sources 2006, 158, 679-688.
    • (2006) J. Power Sources , vol.158 , pp. 679-688
    • Kumaresan, K.1    Guo, O.2    Ramada, P.3    White, R.E.4
  • 18
    • 84872838317 scopus 로고    scopus 로고
    • Lithium-ion batteries working at 85 °C: Aging phenomena and electrode/electrolyte interfaces studied by XPS
    • Bodenes, L.; Dedryvere, R.; Martinez, H.; Fischer, F.; Tessier, C.; Peres, J.P. Lithium-ion batteries working at 85 °C: Aging phenomena and electrode/electrolyte interfaces studied by XPS. J. Electrochem. Soc. 2012, 159, 1739-1746.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 1739-1746
    • Bodenes, L.1    Dedryvere, R.2    Martinez, H.3    Fischer, F.4    Tessier, C.5    Peres, J.P.6
  • 19
    • 0036038215 scopus 로고    scopus 로고
    • The effect of electrolyte temperature on the passivity of the solid electrolyte interphase formed on a graphite
    • Lee, S.; Pyun, S. The effect of electrolyte temperature on the passivity of the solid electrolyte interphase formed on a graphite. Carbon 2002, 40, 2333-2339.
    • (2002) Carbon , vol.40 , pp. 2333-2339
    • Lee, S.1    Pyun, S.2
  • 20
    • 0038555471 scopus 로고    scopus 로고
    • Capacity fade of lithium ion batteries cycled at high discharge rates
    • Ning, G.; Haran, B.; Popov, B.N. Capacity fade of lithium ion batteries cycled at high discharge rates. J. Power Sources 2003, 117, 160-169.
    • (2003) J. Power Sources , vol.117 , pp. 160-169
    • Ning, G.1    Haran, B.2    Popov, B.N.3
  • 23
    • 0034545112 scopus 로고    scopus 로고
    • Characteristics of surface films formed at a mesocarbon microbead electrode in a Li-ion battery
    • Kim, J.S.; Park, Y.T. Characteristics of surface films formed at a mesocarbon microbead electrode in a Li-ion battery. J. Power Sources 2000, 91, 172-176.
    • (2000) J. Power Sources , vol.91 , pp. 172-176
    • Kim, J.S.1    Park, Y.T.2
  • 24
    • 0035702286 scopus 로고    scopus 로고
    • The effect of pulse charge on cycling characteristics of commercial lithium-ion batteries
    • Li, J.; Murphy, E.; Winnick, J.; Kohl, A.P. The effect of pulse charge on cycling characteristics of commercial lithium-ion batteries. J. Power Sources 2001, 102, 302-309.
    • (2001) J. Power Sources , vol.102 , pp. 302-309
    • Li, J.1    Murphy, E.2    Winnick, J.3    Kohl, A.P.4
  • 26
    • 0035698171 scopus 로고    scopus 로고
    • Studies on the cycle life of commercial lithium ion batteries during the charge-discharge cycling
    • Li, J.; Murphy, E.;Winnick, J.; Kohl, P.A. Studies on the cycle life of commercial lithium ion batteries during the charge-discharge cycling. J. Power Sources 2001, 102, 294-301.
    • (2001) J. Power Sources , vol.102 , pp. 294-301
    • Li, J.1    Murphy, E.2    Winnick, J.3    Kohl, P.A.4
  • 27
    • 33750962137 scopus 로고    scopus 로고
    • Studies of cycling behaviour, ageing, and interfacial reactions of LiNi0 5Mn1.5O4 and carbon electrode for lithium-ion 5-V cells.
    • Aurbach, D.; Markovsky, B.; Talyossef, Y.; Salitra, G.; Kim, H.; Choi, S. Studies of cycling behaviour, ageing, and interfacial reactions of LiNi0.5Mn1.5O4 and carbon electrode for lithium-ion 5-V cells. J. Power Sources 2006, 162, 780-789.
    • (2006) J. Power Sources , vol.162 , pp. 780-789
    • Aurbach, D.1    Markovsky, B.2    Talyossef, Y.3    Salitra, G.4    Kim, H.5    Choi, S.6
  • 28
    • 84861354561 scopus 로고    scopus 로고
    • Electrochemical properties and gas evolution behavior of overlithiated Li2NiO2 as cathode active mass for rechargeable Li ion batteries
    • Keun, C.; Yin, R.; Shin, S.; Lee, Y.; Choi, W.; Kim, Y. Electrochemical properties and gas evolution behavior of overlithiated Li2NiO2 as cathode active mass for rechargeable Li ion batteries. J. Electrochem. Soc. 2012, 159, 887-893.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 887-893
    • Keun, C.1    Yin, R.2    Shin, S.3    Lee, Y.4    Choi, W.5    Kim, Y.6
  • 29
    • 34249869036 scopus 로고    scopus 로고
    • Performance degradation of high power lithium ion cells- electrochemistry of harvested electrodes
    • Abraham, D.P.; Knuth, J.L.; Dees, D.W.; Bloom, I. Performance degradation of high power lithium ion cells- electrochemistry of harvested electrodes. J. Power Sources 2007, 170, 465-475.
    • (2007) J. Power Sources , vol.170 , pp. 465-475
    • Abraham, D.P.1    Knuth, J.L.2    Dees, D.W.3    Bloom, I.4
  • 31
    • 48349147825 scopus 로고    scopus 로고
    • Rate capability of lithium intercalation into nano-porous graphitized carbon
    • Yamada, H.; Watanabe, Y.; Moriguchi, I.; Kudo, T. Rate capability of lithium intercalation into nano-porous graphitized carbon. Solid State Ionics 2008, 179, 1706-1709.
    • (2008) Solid State Ionics , vol.179 , pp. 1706-1709
    • Yamada, H.1    Watanabe, Y.2    Moriguchi, I.3    Kudo, T.4
  • 32
    • 0033185360 scopus 로고    scopus 로고
    • Testing of lithium-ion 18650 cells and characterizing/predicting cell performance
    • Fellner, J.P.; Loeber, G.J.; Sandhu, S.S. Testing of lithium-ion 18650 cells and characterizing/predicting cell performance. J. Power Sources 1999, 81, 867-871.
    • (1999) J. Power Sources , vol.81 , pp. 867-871
    • Fellner, J.P.1    Loeber, G.J.2    Sandhu, S.S.3
  • 34
    • 72249121906 scopus 로고    scopus 로고
    • Study of capacity fade of lithium-ion polymer rechargeable batteries with continuous cycling
    • Moss, P.L.; Au, G.; Plichta, E.J.; Zheng, P.J. Study of capacity fade of lithium-ion polymer rechargeable batteries with continuous cycling. J. Electrochem. Soc. 2010, 157, A1-A7.
    • (2010) J. Electrochem. Soc. , vol.157
    • Moss, P.L.1    Au, G.2    Plichta, E.J.3    Zheng, P.J.4
  • 35
    • 81355153808 scopus 로고    scopus 로고
    • Morphology of the solid electrolyte interphase of the graphite I dependency of the formation current
    • Wolfgang, M.; Lu, C.; Novak, P. Morphology of the solid electrolyte interphase of the graphite I dependency of the formation current. J. Electrochem. Soc. 2011, 1478-1482.
    • (2011) J. Electrochem. Soc. , pp. 1478-1482
    • Wolfgang, M.1    Lu, C.2    Novak, P.3
  • 36
    • 81355163959 scopus 로고    scopus 로고
    • Extended cycle life of lithium-ion batteries consisting of lithium insertion electrodes: cycle efficiency versus Ah efficiency
    • Nakura, K.; Ohsugi, Y.; Imazaki, M.; Ariyoshi, K.; Ohzuku, T. Extended cycle life of lithium-ion batteries consisting of lithium insertion electrodes: cycle efficiency versus Ah efficiency. J. Electrochem. Soc. 2011, 158, 1243-1249.
    • (2011) J. Electrochem. Soc. , vol.158 , pp. 1243-1249
    • Nakura, K.1    Ohsugi, Y.2    Imazaki, M.3    Ariyoshi, K.4    Ohzuku, T.5
  • 37
    • 0038729665 scopus 로고    scopus 로고
    • Characterization of high-power lithium-ion cells during constant cycling: Part I cycling performance and electrochemical diagnostics
    • Shim, J.; Striebel, K. Characterization of high-power lithium-ion cells during constant cycling: Part I cycling performance and electrochemical diagnostics. J. Power Sources 2003, 122, 188-194.
    • (2003) J. Power Sources , vol.122 , pp. 188-194
    • Shim, J.1    Striebel, K.2
  • 38
    • 0037167975 scopus 로고    scopus 로고
    • Electrochemical analysis for cycle performance and capacity fading of a lithium-ion battery cycled at elevated temperature
    • Shim, J.; Kostecki, R.; Richardson, T.; Song, X.; Striebel, K.A. Electrochemical analysis for cycle performance and capacity fading of a lithium-ion battery cycled at elevated temperature. J. Power Sources 2002, 112, 222-230.
    • (2002) J. Power Sources , vol.112 , pp. 222-230
    • Shim, J.1    Kostecki, R.2    Richardson, T.3    Song, X.4    Striebel, K.A.5
  • 40
    • 0037048823 scopus 로고    scopus 로고
    • Study on capacity fade factors of lithium secondary batteries using LiNi07 Co0.3O2 and graphite-coke hybrid carbon.
    • Kida, Y.; Kinoshita, A.; Yanagida, K.; Funahashi, A.; Nohma, T.; Yonezu, I. Study on capacity fade factors of lithium secondary batteries using LiNi0.7 Co0.3O2 and graphite-coke hybrid carbon. Electrochim. Acta 2002, 47, 4157-4162.
    • (2002) Electrochim. Acta , vol.47 , pp. 4157-4162
    • Kida, Y.1    Kinoshita, A.2    Yanagida, K.3    Funahashi, A.4    Nohma, T.5    Yonezu, I.6
  • 41
    • 79961025905 scopus 로고    scopus 로고
    • Influence of particle size on the self-discharge behavior of graphite electrodes in lithium-ion batteries
    • Utsunomiya, T.; Hatozaki, O.; Yoshimoto, N.; Egashira, M.; Morita, M. Influence of particle size on the self-discharge behavior of graphite electrodes in lithium-ion batteries. J. Power Sources 2011, 196, 8675-8682.
    • (2011) J. Power Sources , vol.196 , pp. 8675-8682
    • Utsunomiya, T.1    Hatozaki, O.2    Yoshimoto, N.3    Egashira, M.4    Morita, M.5
  • 42
    • 24944564651 scopus 로고    scopus 로고
    • Study the fading mechanism of LiMn2O4 battery with spherical and flake type graphite as anode material
    • Wu, H.C.; Guo, Z.Z.; Wen, H.P.; Yang, M.Y. Study the fading mechanism of LiMn2O4 battery with spherical and flake type graphite as anode material. J. Power Sources 2005, 146, 736-740.
    • (2005) J. Power Sources , vol.146 , pp. 736-740
    • Wu, H.C.1    Guo, Z.Z.2    Wen, H.P.3    Yang, M.Y.4
  • 43
    • 0042878542 scopus 로고    scopus 로고
    • Comparison of the capacity fade of Sony US 18650 cells charged with different protocols
    • Sikha, G.; Ramadass, P.; Haran, B.S.; White, R.E.; Popov, B.N. Comparison of the capacity fade of Sony US 18650 cells charged with different protocols. J. Power Sources 2003, 122, 67-76.
    • (2003) J. Power Sources , vol.122 , pp. 67-76
    • Sikha, G.1    Ramadass, P.2    Haran, B.S.3    White, R.E.4    Popov, B.N.5
  • 44
    • 0036608149 scopus 로고    scopus 로고
    • Low-temperature characterization of lithium-ion carbon anodes via microperturbation measurement
    • Wang, C.; Appleby, A.J.; Little, F.E. Low-temperature characterization of lithium-ion carbon anodes via microperturbation measurement. J. Electrochem. Soc. 2002, 149, 754-760.
    • (2002) J. Electrochem. Soc. , vol.149 , pp. 754-760
    • Wang, C.1    Appleby, A.J.2    Little, F.E.3
  • 45
    • 65949122946 scopus 로고    scopus 로고
    • Cycle-life characterization of automotive lithium-ion batteries with LiNiO2
    • Zhang, Y.; Wang, C.Y. Cycle-life characterization of automotive lithium-ion batteries with LiNiO2. J. Electrochem. Soc. 2009, 156, 527-535.
    • (2009) J. Electrochem. Soc. , vol.156 , pp. 527-535
    • Zhang, Y.1    Wang, C.Y.2
  • 46
    • 38749117522 scopus 로고    scopus 로고
    • Studies on degradation of Li-ion batteries by the use of micro reference electrodes
    • Zhou, J.; Notten, P.H.L. Studies on degradation of Li-ion batteries by the use of micro reference electrodes. J. Power Sources 2008, 177, 553-560.
    • (2008) J. Power Sources , vol.177 , pp. 553-560
    • Zhou, J.1    Notten, P.H.L.2
  • 47
    • 36148986030 scopus 로고    scopus 로고
    • Low temperature study of lithium-ion cells using LiySn micro-reference electrode
    • Jasen, N.A.; Dees, D.W.; Abraham, D.P.; Amine, K.; Henriksen, G.L. Low temperature study of lithium-ion cells using LiySn micro-reference electrode. J. Power Sources 2007, 174, 373-379.
    • (2007) J. Power Sources , vol.174 , pp. 373-379
    • Jasen, N.A.1    Dees, D.W.2    Abraham, D.P.3    Amine, K.4    Henriksen, G.L.5
  • 48
    • 79551596158 scopus 로고    scopus 로고
    • A study on the cause of deterioration in float-charged lithium-ion batteries using LiMn2O4 as a cathode active material
    • Tsujikawa, T.; Yabuta, K.; Matsushita, T.; Arakawa, M.; Hayashi, K. A study on the cause of deterioration in float-charged lithium-ion batteries using LiMn2O4 as a cathode active material. J. Electrochem. Soc. 2011, 158, 322-325.
    • (2011) J. Electrochem. Soc. , vol.158 , pp. 322-325
    • Tsujikawa, T.1    Yabuta, K.2    Matsushita, T.3    Arakawa, M.4    Hayashi, K.5
  • 51
    • 33644819143 scopus 로고    scopus 로고
    • Diagnostic evaluation of detrimental phenomena in high-power lithium-ion batteries
    • Kostecki, R.; Lei, J.; McLarnon, F.; Shim, J.; Striebel, K. Diagnostic evaluation of detrimental phenomena in high-power lithium-ion batteries. J. Electrochem. Soc. 2006, 153, A669-A672.
    • (2006) J. Electrochem. Soc. , vol.153
    • Kostecki, R.1    Lei, J.2    McLarnon, F.3    Shim, J.4    Striebel, K.5
  • 52
    • 80052077448 scopus 로고    scopus 로고
    • Aging of a commercial graphite LiFePO4 cell
    • Safari, M.; Delacourt, C. Aging of a commercial graphite LiFePO4 cell. J. Electrochem. Soc. 2011, 158, 1123-1135.
    • (2011) J. Electrochem. Soc. , vol.158 , pp. 1123-1135
    • Safari, M.1    Delacourt, C.2
  • 53
    • 80054030177 scopus 로고    scopus 로고
    • The use of elevated temperature storage experiments to learn about parasitic reaction in wound LiCoO2/graphite cells
    • Sinha, N.N.; Smith, A.J.; Burns, J.C.; Gaurav, J.; Eberman, K.W.; Scott, E.; Gardner, J.P.; Dahn, J.R. The use of elevated temperature storage experiments to learn about parasitic reaction in wound LiCoO2/graphite cells. J. Electrochem. Soc. 2011, 158, 1194-1201.
    • (2011) J. Electrochem. Soc. , vol.158 , pp. 1194-1201
    • Sinha, N.N.1    Smith, A.J.2    Burns, J.C.3    Gaurav, J.4    Eberman, K.W.5    Scott, E.6    Gardner, J.P.7    Dahn, J.R.8
  • 54
    • 84875442846 scopus 로고    scopus 로고
    • The rate of active lithium loss from a soft carbon negative electrode as a function of temperature, time and electrode potential
    • Sinha, N.N.; Marks, T.H.; Dahn, H.M.; Smith, A.J.; Burn, J.C.; Coyle, D.J.; Dahn, J.J.; Dahn, J.R. The rate of active lithium loss from a soft carbon negative electrode as a function of temperature, time and electrode potential. J. Electrochem. Soc. 2012, 159, 1672-1681.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 1672-1681
    • Sinha, N.N.1    Marks, T.H.2    Dahn, H.M.3    Smith, A.J.4    Burn, J.C.5    Coyle, D.J.6    Dahn, J.J.7    Dahn, J.R.8
  • 55
    • 0142079683 scopus 로고    scopus 로고
    • The complex electrochemistry of graphite electrodes in lithium-ion batteries
    • Novak, P.; Lanz, M.; Allia, D.; Rykart, B.; Paniz, J.; Haas, O. The complex electrochemistry of graphite electrodes in lithium-ion batteries. J. Power Sources 2001, 97, 39-46.
    • (2001) J. Power Sources , vol.97 , pp. 39-46
    • Novak, P.1    Lanz, M.2    Allia, D.3    Rykart, B.4    Paniz, J.5    Haas, O.6
  • 56
    • 0033075180 scopus 로고    scopus 로고
    • M TEM Study of Electrochemical Cycling-Induced Damage and Disorder in LiCoO2 Cathodes for Rechargeable Lithium Batteries
    • Wang, H.; Jang, Y.; Huang, B.; Sadoway, R.D.; Chiang, Y.M TEM Study of Electrochemical Cycling-Induced Damage and Disorder in LiCoO2 Cathodes for Rechargeable Lithium Batteries. J. Electrochem. Soc. 1999, 146, 473-480.
    • (1999) J. Electrochem. Soc. , vol.146 , pp. 473-480
    • Wang, H.1    Jang, Y.2    Huang, B.3    Sadoway, R.D.4    Chiang, Y.5
  • 58
    • 24944561887 scopus 로고    scopus 로고
    • Capacity fading of lithiated graphite electrodes studied by a combination of electroanalytical methods, Raman spectroscopy and SEM
    • Markervich, E.; Salitra, G.; Levi, M.D.; Aurbach, D. Capacity fading of lithiated graphite electrodes studied by a combination of electroanalytical methods, Raman spectroscopy and SEM. J. Power Sources 2005, 146, 146-150.
    • (2005) J. Power Sources , vol.146 , pp. 146-150
    • Markervich, E.1    Salitra, G.2    Levi, M.D.3    Aurbach, D.4
  • 59
  • 60
    • 0031248974 scopus 로고    scopus 로고
    • Irreversible capacity loss of graphite electrode in lithium-ion batteries
    • Chang, Y.; Li, H.; Wu, L.; Lu, T. Irreversible capacity loss of graphite electrode in lithium-ion batteries. J. Power Sources 1997, 68, 187-190.
    • (1997) J. Power Sources , vol.68 , pp. 187-190
    • Chang, Y.1    Li, H.2    Wu, L.3    Lu, T.4
  • 61
    • 1842578969 scopus 로고    scopus 로고
    • The dependence of natural graphite anode performance on electrode density
    • Shim, J.; Striebel, A.K. The dependence of natural graphite anode performance on electrode density. J. Power Sources 2004, 130, 247-253.
    • (2004) J. Power Sources , vol.130 , pp. 247-253
    • Shim, J.1    Striebel, A.K.2
  • 62
    • 84875550853 scopus 로고    scopus 로고
    • Influence of Fe(II) species in electrolyte on performance of graphite anode for lithium-ion batteries
    • Lai, Y.; Cao, Z.; Haishen, S.; Zhang, Z.; Chen, X.; Lu, H.; Jia, M.; Li, J. Influence of Fe(II) species in electrolyte on performance of graphite anode for lithium-ion batteries. J. Electrochem. Soc. 2012, 159, 1961-1966.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 1961-1966
    • Lai, Y.1    Cao, Z.2    Haishen, S.3    Zhang, Z.4    Chen, X.5    Lu, H.6    Jia, M.7    Li, J.8
  • 63
    • 79961149240 scopus 로고    scopus 로고
    • Novel cell design for combined in situ acoustic emission and x-ray diffraction study during electrochemical cycling of batteries
    • Rhodes, K.; Kirkham, M.; Meisner, R.; Parish, M.C.; Dudney, N. Novel cell design for combined in situ acoustic emission and x-ray diffraction study during electrochemical cycling of batteries. Rev. Sci. Instrum. 2011, 82, 75-107.
    • (2011) Rev. Sci. Instrum. , vol.82 , pp. 75-107
    • Rhodes, K.1    Kirkham, M.2    Meisner, R.3    Parish, M.C.4    Dudney, N.5
  • 64
    • 62849113706 scopus 로고    scopus 로고
    • Scanning spreading resistance characterization of aged Li-ion batteries using atomic force microscopy
    • Nagpure, S.C.; Bhushan, B.; Babu, S.; Rizzoni, G. Scanning spreading resistance characterization of aged Li-ion batteries using atomic force microscopy. Scripta Mater. 2009, 60, 933-936.
    • (2009) Scripta Mater. , vol.60 , pp. 933-936
    • Nagpure, S.C.1    Bhushan, B.2    Babu, S.3    Rizzoni, G.4
  • 65
    • 0029272301 scopus 로고
    • Factor affecting the capacity retention of lithium-ion cells
    • Ohzuku, T.; Ueda, A.; Yamamoto, N.; Yasunobu, I. Factor affecting the capacity retention of lithium-ion cells. J. Power Sources 1995, 54, 99-102.
    • (1995) J. Power Sources , vol.54 , pp. 99-102
    • Ohzuku, T.1    Ueda, A.2    Yamamoto, N.3    Yasunobu, I.4
  • 66
    • 0001635538 scopus 로고    scopus 로고
    • Surface film formation on graphite negative electrode in lithium-ion batteries
    • Jeong, S.K.; Inaba, M.; Takeshi, A.; Ogumi, Z. Surface film formation on graphite negative electrode in lithium-ion batteries. J. Electrochem. Soc. 2001, 148, A989-A993.
    • (2001) J. Electrochem. Soc. , vol.148
    • Jeong, S.K.1    Inaba, M.2    Takeshi, A.3    Ogumi, Z.4
  • 67
    • 77049086515 scopus 로고    scopus 로고
    • Rate capability of graphite materials as negative electrodes in lithium ion capacitors
    • Silvakkumar, S.R.; Nerkar, J.Y. Rate capability of graphite materials as negative electrodes in lithium ion capacitors. Electrochim. Acta 2010, 55, 3330-3335.
    • (2010) Electrochim. Acta , vol.55 , pp. 3330-3335
    • Silvakkumar, S.R.1    Nerkar, J.Y.2
  • 70
    • 0033184942 scopus 로고    scopus 로고
    • Characterization of the ambient and elevated temperature performance of graphite electrode
    • Anderson, A.M.; Edstrom, K.; Thomas, J.O. Characterization of the ambient and elevated temperature performance of graphite electrode. J. Power Sources 1999, 81-82, 8-12.
    • (1999) J. Power Sources , vol.81-82 , pp. 8-12
    • Anderson, A.M.1    Edstrom, K.2    Thomas, J.O.3
  • 71
    • 0030287394 scopus 로고    scopus 로고
    • Rate effect on lithium-ion graphite electrode performance
    • Tran, T.D.; Feikert, J.H.; Pekala, R.W. Rate effect on lithium-ion graphite electrode performance. J. Appl. Electrochem. 1996, 26, 1161-1167.
    • (1996) J. Appl. Electrochem. , vol.26 , pp. 1161-1167
    • Tran, T.D.1    Feikert, J.H.2    Pekala, R.W.3
  • 72
    • 61549110194 scopus 로고    scopus 로고
    • Effect of particle size on the thermal stability of lithiated graphite
    • Park, Y.; Lee, S. Effect of particle size on the thermal stability of lithiated graphite. Electrochim. Acta 2009, 54, 3339-3343.
    • (2009) Electrochim. Acta , vol.54 , pp. 3339-3343
    • Park, Y.1    Lee, S.2
  • 73
    • 58849086617 scopus 로고    scopus 로고
    • Correlations between surface properties of graphite and the first cycle specific charge loss in lithium-ion batteries
    • Nga, S.H.; Vix-Guterl, C.; Bernardo, P.H.; Tran, N.; Ufheil, J.; Buqa, H.; Dentzer, J.; Gadiou, R.; Spahr, M.E.; Goers, D.; et al. Correlations between surface properties of graphite and the first cycle specific charge loss in lithium-ion batteries. Carbon 2009, 47, 705-712.
    • (2009) Carbon , vol.47 , pp. 705-712
    • Nga, S.H.1    Vix-Guterl, C.2    Bernardo, P.H.3    Tran, N.4    Ufheil, J.5    Buqa, H.6    Dentzer, J.7    Gadiou, R.8    Spahr, M.E.9    Goers, D.10
  • 74
    • 0035396160 scopus 로고    scopus 로고
    • Relation between surface properties, pore structure and first cycle charge loss of graphite as negative electrode in lithium-ion batteries
    • Joho, F.; Rykart, B.; Wilhem, H.; Novak, P.; Spahr, M.E.; Monnier, A. Relation between surface properties, pore structure and first cycle charge loss of graphite as negative electrode in lithium-ion batteries. J. Power Sources 2001, 97, 78-82.
    • (2001) J. Power Sources , vol.97 , pp. 78-82
    • Joho, F.1    Rykart, B.2    Wilhem, H.3    Novak, P.4    Spahr, M.E.5    Monnier, A.6
  • 75
    • 0038348469 scopus 로고    scopus 로고
    • On the behaviour of different types of graphite anodes
    • Aurbach, D.; Teller, H.; Koltypin, M.; Levi, E. On the behaviour of different types of graphite anodes. J. Power Sources 2003, 119-121, 2-7.
    • (2003) J. Power Sources , vol.119-121 , pp. 2-7
    • Aurbach, D.1    Teller, H.2    Koltypin, M.3    Levi, E.4
  • 76
    • 0033740440 scopus 로고    scopus 로고
    • Charaterization of commercial size cylindrical Li-ion cell with a reference electrode
    • Wu, Q.; Lu, W.; Prakash, J. Charaterization of commercial size cylindrical Li-ion cell with a reference electrode. J. Power Sources 2000, 88, 237-242.
    • (2000) J. Power Sources , vol.88 , pp. 237-242
    • Wu, Q.1    Lu, W.2    Prakash, J.3
  • 77
    • 0005370973 scopus 로고    scopus 로고
    • A study of capacity fades in cylindrical and prismatic lithium-ion batteries
    • Rubino, S.R.; Gan, H.; Takeuchi, S.E. A study of capacity fades in cylindrical and prismatic lithium-ion batteries. J. Electrochem. Soc. 2001, 148, 1029-1033.
    • (2001) J. Electrochem. Soc. , vol.148 , pp. 1029-1033
    • Rubino, S.R.1    Gan, H.2    Takeuchi, S.E.3
  • 78
    • 0038347414 scopus 로고    scopus 로고
    • Effect of electrode density on cycle performance and irreversible capacity loss for natural graphite anode in lithium-ion batteries
    • Shim, J.; Striebel, A.K. Effect of electrode density on cycle performance and irreversible capacity loss for natural graphite anode in lithium-ion batteries. J. Power Sources 2003, 119, 934-937.
    • (2003) J. Power Sources , vol.119 , pp. 934-937
    • Shim, J.1    Striebel, A.K.2
  • 79
    • 0000014535 scopus 로고    scopus 로고
    • Abuse Testing of Lithium-Ion Batteries Characterization of the Overcharge Reaction of LiCoO2/Graphite Cells
    • Leising, A.R.; Palazzo, M.J.; Takeuchi, S.E.; Takeuchi, J.K. Abuse Testing of Lithium-Ion Batteries Characterization of the Overcharge Reaction of LiCoO2/Graphite Cells. J. Electrochem. Soc. 2001, 148, 838-844.
    • (2001) J. Electrochem. Soc. , vol.148 , pp. 838-844
    • Leising, A.R.1    Palazzo, M.J.2    Takeuchi, S.E.3    Takeuchi, J.K.4
  • 80
    • 0035700249 scopus 로고    scopus 로고
    • DEMS study of gas evolution at thick graphite electrodes for lithium-ion batteries: The effect of the ?-butyrolactone
    • Lanz, M.; Novak, P. DEMS study of gas evolution at thick graphite electrodes for lithium-ion batteries: The effect of the ?-butyrolactone. J. Power Sources 2001, 102, 277-282.
    • (2001) J. Power Sources , vol.102 , pp. 277-282
    • Lanz, M.1    Novak, P.2
  • 82
    • 0036898777 scopus 로고    scopus 로고
    • Live scanning electron microscope observation of dendrite growth in lithium polymer cells
    • Dolle, M.; Sannier, L.; Beaudion, B.; Trentin, M. Live scanning electron microscope observation of dendrite growth in lithium polymer cells. J. Electrochem. Soc. 2002, 5, 286-289.
    • (2002) J. Electrochem. Soc. , vol.5 , pp. 286-289
    • Dolle, M.1    Sannier, L.2    Beaudion, B.3    Trentin, M.4
  • 83
    • 79955137580 scopus 로고    scopus 로고
    • Effects of electrolyte composition on lithium plating in lithium-ion cells
    • Smart, M.C.; Ratnakumar, B.V. Effects of electrolyte composition on lithium plating in lithium-ion cells. J. Electrochem. Soc. 2011, 158, 379-389.
    • (2011) J. Electrochem. Soc. , vol.158 , pp. 379-389
    • Smart, M.C.1    Ratnakumar, B.V.2
  • 84
    • 62349136663 scopus 로고    scopus 로고
    • Electrochemical properties and Li deposition morphologies of surface modified graphite after grinding
    • Honbo, H.; Takei, K.; Ishii, Y.; Nishida, T. Electrochemical properties and Li deposition morphologies of surface modified graphite after grinding. J. Power Sources 2009, 189, 337-343.
    • (2009) J. Power Sources , vol.189 , pp. 337-343
    • Honbo, H.1    Takei, K.2    Ishii, Y.3    Nishida, T.4
  • 86
    • 0032202686 scopus 로고    scopus 로고
    • In situ scanning electron microscope observation of interfaces within plastic lithium batteries
    • Ornini, F.; Pasquier, D.A.; Beaudion, B.; Tarason, J.M.; Trentin, M. In situ scanning electron microscope observation of interfaces within plastic lithium batteries. J. Power Sources 1998, 76, 19-29.
    • (1998) J. Power Sources , vol.76 , pp. 19-29
    • Ornini, F.1    Pasquier, D.A.2    Beaudion, B.3    Tarason, J.M.4    Trentin, M.5
  • 88
    • 9344268863 scopus 로고    scopus 로고
    • Observation of dendritic growth on Li powder anode using the optical cell
    • Kim, W.; Yoon, W. Observation of dendritic growth on Li powder anode using the optical cell. Electrochim. Acta 2004, 50, 541-545.
    • (2004) Electrochim. Acta , vol.50 , pp. 541-545
    • Kim, W.1    Yoon, W.2
  • 89
    • 84875496556 scopus 로고    scopus 로고
    • Electrochemical behavior of Li-powder anode in high Li capacity used
    • Kong, S.; Kim, B.; Yoon, W. Electrochemical behavior of Li-powder anode in high Li capacity used. J. Electrochem. Soc. 2012, 159, 1551-1553.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 1551-1553
    • Kong, S.1    Kim, B.2    Yoon, W.3
  • 90
    • 77958036913 scopus 로고    scopus 로고
    • In situ NMR observation of the formation of metallic microstructure in lithium batteries
    • Bhattacharyya, R.; Key, B.; Chen, H.; Best, A.S.; Hollenkamp, A.F.; Grey, C.P. In situ NMR observation of the formation of metallic microstructure in lithium batteries. Nat. Mater. 2010, 9, 504-510.
    • (2010) Nat. Mater. , vol.9 , pp. 504-510
    • Bhattacharyya, R.1    Key, B.2    Chen, H.3    Best, A.S.4    Hollenkamp, A.F.5    Grey, C.P.6
  • 91
    • 84859301601 scopus 로고    scopus 로고
    • Overcharge effect on morphology and structure of carbon electrodes for lithium-ion batteries
    • Lu, W.; Carmen, M.; Liu, N.; Vaughely, T.J.; Jansen, A.; Dees, D.W. Overcharge effect on morphology and structure of carbon electrodes for lithium-ion batteries. J. Electrochem. Soc. 2012, 159, 566-570.
    • (2012) J. Electrochem. Soc. , vol.159 , pp. 566-570
    • Lu, W.1    Carmen, M.2    Liu, N.3    Vaughely, T.J.4    Jansen, A.5    Dees, D.W.6
  • 92
    • 33646462726 scopus 로고    scopus 로고
    • Studies on charging lithium-ion cells at low temperatures
    • Fan, J.; Tan, S. Studies on charging lithium-ion cells at low temperatures. J. Electrochem. Soc. 2006, 153, 1081-1092.
    • (2006) J. Electrochem. Soc. , vol.153 , pp. 1081-1092
    • Fan, J.1    Tan, S.2
  • 93
    • 0033184677 scopus 로고    scopus 로고
    • Key factors for the cycling stability of graphite intercalation electrodes for lithium-ion batteries
    • Joho, F.; Rykart, B.; Imhof, R.; Novak, P.; Spahr, M.E.; Monnier, A. Key factors for the cycling stability of graphite intercalation electrodes for lithium-ion batteries. J. Power Sources 1999, 81, 243-247.
    • (1999) J. Power Sources , vol.81 , pp. 243-247
    • Joho, F.1    Rykart, B.2    Imhof, R.3    Novak, P.4    Spahr, M.E.5    Monnier, A.6
  • 94
    • 65449126355 scopus 로고    scopus 로고
    • Effect of carbon coating on thermal stability of natural graphite spheres used as anode materials in lithium-ion batteries
    • Park, Y.; Bang, H.J.; Oh, S.; Sun, Y.; Lee, S. Effect of carbon coating on thermal stability of natural graphite spheres used as anode materials in lithium-ion batteries. J. Power Sources 2009, 190, 553-557.
    • (2009) J. Power Sources , vol.190 , pp. 553-557
    • Park, Y.1    Bang, H.J.2    Oh, S.3    Sun, Y.4    Lee, S.5
  • 96
    • 0034966150 scopus 로고    scopus 로고
    • Reduction of irreversible capacity of a graphite anode by the CVD process
    • Natarajan, C.; Fujimoto, H.; Tokumitsu, K.; Mabuchi, A.; Kasuh, T. Reduction of irreversible capacity of a graphite anode by the CVD process. Carbon 2001, 39, 1409-1413.
    • (2001) Carbon , vol.39 , pp. 1409-1413
    • Natarajan, C.1    Fujimoto, H.2    Tokumitsu, K.3    Mabuchi, A.4    Kasuh, T.5
  • 97
    • 3142773547 scopus 로고    scopus 로고
    • The effect of compression on natural graphite anode performance and matrix conductivity
    • Striebel, K.A.; Sierra, A.; Shim, J.; Wang, C.W.; Saatry, A.M. The effect of compression on natural graphite anode performance and matrix conductivity. J. Power Sources 2004, 234, 241-251.
    • (2004) J. Power Sources , vol.234 , pp. 241-251
    • Striebel, K.A.1    Sierra, A.2    Shim, J.3    Wang, C.W.4    Saatry, A.M.5
  • 98
    • 33846192863 scopus 로고    scopus 로고
    • Electrochemical characterization of thermally oxidized natural graphite anodes in lithium-ion batteries
    • Shim, J.; Striebel, K.A. Electrochemical characterization of thermally oxidized natural graphite anodes in lithium-ion batteries. J. Power Sources 2007,164, 862-867.
    • (2007) J. Power Sources , vol.164 , pp. 862-867
    • Shim, J.1    Striebel, K.A.2
  • 99
    • 0037130601 scopus 로고    scopus 로고
    • Factors that affect cycle life and possible degradation mechanisms of a Li-ion cell based on LiCoO2
    • Choi, S.S.; Lim, H.S. Factors that affect cycle life and possible degradation mechanisms of a Li-ion cell based on LiCoO2. J. Power Sources 2002, 111, 130-136.
    • (2002) J. Power Sources , vol.111 , pp. 130-136
    • Choi, S.S.1    Lim, H.S.2
  • 100
    • 77953687092 scopus 로고    scopus 로고
    • Low-temperature behavior of graphite-tin composite anodes for Li-ion batteries
    • Nobili, F.; Mancini, M.; Dsoke, S.; Tossici, R.; Marassi, R. Low-temperature behavior of graphite-tin composite anodes for Li-ion batteries. J. Power Sources 2010, 195, 7090-7097.
    • (2010) J. Power Sources , vol.195 , pp. 7090-7097
    • Nobili, F.1    Mancini, M.2    Dsoke, S.3    Tossici, R.4    Marassi, R.5
  • 101
    • 0033185355 scopus 로고    scopus 로고
    • The study of irreversible capacity in lithium-ion anodes prepared with thermally oxidized graphite
    • Rubino, R.S.; Takeuchi, S.E. The study of irreversible capacity in lithium-ion anodes prepared with thermally oxidized graphite. J. Power Sources 1999, 81, 373-377.
    • (1999) J. Power Sources , vol.81 , pp. 373-377
    • Rubino, R.S.1    Takeuchi, S.E.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.