메뉴 건너뛰기




Volumn 33, Issue 13-14, 2013, Pages 2689-2698

Strength degradation and failure limits of dense and porous ceramic membrane materials

Author keywords

Ceramics; Failure; Lifetime; Membranes; Strength

Indexed keywords

CERAMICS; ELEVATED TEMPERATURE; LIFETIME; PERMEATION PROPERTIES; POROUS CERAMIC MEMBRANES; STRENGTH; STRENGTH DEGRADATION; SUBCRITICAL CRACK GROWTH;

EID: 84879845670     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2013.04.018     Document Type: Article
Times cited : (56)

References (40)
  • 2
    • 78650736674 scopus 로고    scopus 로고
    • Comparative thermodynamic analysis and integration issues of CCS steam power plants based on oxy-combustion with cryogenic or membrane based air separation
    • Pfaff I., Kather A. Comparative thermodynamic analysis and integration issues of CCS steam power plants based on oxy-combustion with cryogenic or membrane based air separation. Energy Procedia 2009, 1(February (1)):495-502.
    • (2009) Energy Procedia , vol.1 , Issue.1 , pp. 495-502
    • Pfaff, I.1    Kather, A.2
  • 3
    • 27544486687 scopus 로고    scopus 로고
    • Perovskite hollow-fiber membranes for the production of oxygen-enriched air
    • Wang H., Werth S., Schiestel T., Caro J. Perovskite hollow-fiber membranes for the production of oxygen-enriched air. Angew Chem Int Ed 2005, 44(42):6906-6909.
    • (2005) Angew Chem Int Ed , vol.44 , Issue.42 , pp. 6906-6909
    • Wang, H.1    Werth, S.2    Schiestel, T.3    Caro, J.4
  • 4
    • 0042925338 scopus 로고    scopus 로고
    • Dense ceramic membranes for methane conversion
    • Bouwmeester H.J.M. Dense ceramic membranes for methane conversion. Catal Today 2003, 82(July (1-4)):141-150.
    • (2003) Catal Today , vol.82 , Issue.1-4 , pp. 141-150
    • Bouwmeester, H.J.M.1
  • 5
    • 61649108523 scopus 로고    scopus 로고
    • Oxidative coupling of methane using catalyst modified dense perovskite membrane reactors
    • Olivier L., Haag S., Mirodatos C., van Veen A.C. Oxidative coupling of methane using catalyst modified dense perovskite membrane reactors. Catal Today 2009, 142(April (1-2)):34-41.
    • (2009) Catal Today , vol.142 , Issue.1-2 , pp. 34-41
    • Olivier, L.1    Haag, S.2    Mirodatos, C.3    van Veen, A.C.4
  • 6
    • 0036494232 scopus 로고    scopus 로고
    • Controlled oxidative coupling of methane by ionic conducting ceramic membrane
    • Akin F.T., Lin Y.S. Controlled oxidative coupling of methane by ionic conducting ceramic membrane. Catal Lett 2002, 78(1):239-242.
    • (2002) Catal Lett , vol.78 , Issue.1 , pp. 239-242
    • Akin, F.T.1    Lin, Y.S.2
  • 8
    • 78650516207 scopus 로고    scopus 로고
    • High performance perovskite hollow fibres for oxygen separation
    • Leo A., Smart S., Liu S., Diniz da Costa J.C. High performance perovskite hollow fibres for oxygen separation. J Membr Sci 2011, 368(February (1-2)):64-68.
    • (2011) J Membr Sci , vol.368 , Issue.1-2 , pp. 64-68
    • Leo, A.1    Smart, S.2    Liu, S.3    Diniz da Costa, J.C.4
  • 12
    • 79955660653 scopus 로고    scopus 로고
    • 2-δ+Co (x=0.1, 0.2) and evaluation as oxygen-transport membrane
    • 2-δ+Co (x=0.1, 0.2) and evaluation as oxygen-transport membrane. Chem Mater 2011, 23(May (9)):2333-2343.
    • (2011) Chem Mater , vol.23 , Issue.9 , pp. 2333-2343
    • Balaguer, M.1    Solis, C.2    Serra, J.3
  • 16
    • 0034578811 scopus 로고    scopus 로고
    • Homogeneous porous perovskite supports for thin dense oxygen separation membranes
    • van der Haar L.M., Verweij H. Homogeneous porous perovskite supports for thin dense oxygen separation membranes. J Membr Sci 2000, 180(December (1)):147-155.
    • (2000) J Membr Sci , vol.180 , Issue.1 , pp. 147-155
    • van der Haar, L.M.1    Verweij, H.2
  • 17
    • 84866248743 scopus 로고    scopus 로고
    • Einsatz keramischer BSCF-Membranen in einem transportablen Sauerstoff- Erzeuger
    • HvB, Section 8.10.1.1
    • Kriegel R. Einsatz keramischer BSCF-Membranen in einem transportablen Sauerstoff- Erzeuger. DKG Handbuch Technische Keramische Werkstoffe 2010, HvB, Section 8.10.1.1.
    • (2010) DKG Handbuch Technische Keramische Werkstoffe
    • Kriegel, R.1
  • 19
    • 0003400331 scopus 로고
    • Ceramics: mechanical performance and lifetime prediction
    • Pergamon Press, Oxford, 1557-70
    • Danzer R. Ceramics: mechanical performance and lifetime prediction. Encyclopedia of materials science and engineering 1993, Pergamon Press, Oxford, 1557-70.
    • (1993) Encyclopedia of materials science and engineering
    • Danzer, R.1
  • 20
    • 84866766651 scopus 로고    scopus 로고
    • Sub-critical crack growth in alumina - a comparison of different measurement and evaluation methods
    • Lube T., Baierl R.G.A. Sub-critical crack growth in alumina - a comparison of different measurement and evaluation methods. Berg Huettenmaenn Monatsh 2011, 156(November (11)):450-456.
    • (2011) Berg Huettenmaenn Monatsh , vol.156 , Issue.11 , pp. 450-456
    • Lube, T.1    Baierl, R.G.A.2
  • 24
    • 84987266075 scopus 로고
    • A statistical distribution function of wide applicability
    • Weibull W. A statistical distribution function of wide applicability. J Appl Mech 1951, 18:293-297.
    • (1951) J Appl Mech , vol.18 , pp. 293-297
    • Weibull, W.1
  • 25
    • 0027001424 scopus 로고
    • A general strength distribution function for brittle materials
    • Danzer R. A general strength distribution function for brittle materials. J Eur Ceram Soc 1992, 10(6):461-472.
    • (1992) J Eur Ceram Soc , vol.10 , Issue.6 , pp. 461-472
    • Danzer, R.1
  • 26
    • 0026367073 scopus 로고
    • Statistical and systematical errors in the strength determination of brittle materials
    • Bongartz K., Schuster H. Statistical and systematical errors in the strength determination of brittle materials. Materialwiss Werkstofftech 1991, 22(12):449-461.
    • (1991) Materialwiss Werkstofftech , vol.22 , Issue.12 , pp. 449-461
    • Bongartz, K.1    Schuster, H.2
  • 29
    • 84875621973 scopus 로고    scopus 로고
    • Subcritical crack growth in low temperature co-fired ceramics under biaxial loading
    • Bermejo R., Supancic P., Krautgasser C., Morrell R., Danzer R. Subcritical crack growth in low temperature co-fired ceramics under biaxial loading. Eng Fract Mech 2013, 100(March):108-121.
    • (2013) Eng Fract Mech , vol.100 , Issue.MARCH , pp. 108-121
    • Bermejo, R.1    Supancic, P.2    Krautgasser, C.3    Morrell, R.4    Danzer, R.5
  • 31
    • 79952615558 scopus 로고    scopus 로고
    • Subcritical crack growth behavior of a perovskite-type oxygen transport ceramic membrane
    • Nagabhushana N., Nithyanantham T., Bandopadhyay S., Zhang J. Subcritical crack growth behavior of a perovskite-type oxygen transport ceramic membrane. Int J Appl Ceram Technol 2011, 8(2):390-397.
    • (2011) Int J Appl Ceram Technol , vol.8 , Issue.2 , pp. 390-397
    • Nagabhushana, N.1    Nithyanantham, T.2    Bandopadhyay, S.3    Zhang, J.4
  • 32
    • 0344671623 scopus 로고    scopus 로고
    • Tape casting of high dielectric ceramic composite substrates for microelectronics application
    • Tok A.I.Y., Boey F.Y.C., Khor K.A. Tape casting of high dielectric ceramic composite substrates for microelectronics application. J Mater Eng Perform 1999, 89-90(May):508-512.
    • (1999) J Mater Eng Perform , Issue.MAY , pp. 508-512
    • Tok, A.I.Y.1    Boey, F.Y.C.2    Khor, K.A.3
  • 33
    • 0004777628 scopus 로고
    • Synthesis, forming and characterization of ceramic materials for the planar solid oxide fuel cell (SOFC)
    • Kountouros P., Förthmann R., Naoumidis A., Stochniol G., Syskakis E. Synthesis, forming and characterization of ceramic materials for the planar solid oxide fuel cell (SOFC). Ionics 1995, 1(January (1)):40-50.
    • (1995) Ionics , vol.1 , Issue.JANUARY 1 , pp. 40-50
    • Kountouros, P.1    Förthmann, R.2    Naoumidis, A.3    Stochniol, G.4    Syskakis, E.5
  • 35
    • 79959242543 scopus 로고    scopus 로고
    • Ring-on-ring testing of thin, curved bi-layered materials
    • Pećanac G., Bause T., Malzbender J. Ring-on-ring testing of thin, curved bi-layered materials. J Eur Ceram Soc 2011, 31(October (12)):2037-2042.
    • (2011) J Eur Ceram Soc , vol.31 , Issue.OCTOBER 12 , pp. 2037-2042
    • Pećanac, G.1    Bause, T.2    Malzbender, J.3
  • 36
    • 0018519639 scopus 로고
    • Uniaxial data for statistical comparisons of a ceramic's strength
    • Biaxial
    • Giovan M.N., Sines G., Biaxial Uniaxial data for statistical comparisons of a ceramic's strength. J Am Ceram Soc 1979, 62(9-10):510-515.
    • (1979) J Am Ceram Soc , vol.62 , Issue.9-10 , pp. 510-515
    • Giovan, M.N.1    Sines, G.2
  • 37
    • 0001621198 scopus 로고
    • Thermal shock and fracture in ceramics
    • Davidge R.W., Tappin G. Thermal shock and fracture in ceramics. Brit Ceram Trans J 1967, 66:405-422.
    • (1967) Brit Ceram Trans J , vol.66 , pp. 405-422
    • Davidge, R.W.1    Tappin, G.2
  • 40
    • 84866793152 scopus 로고    scopus 로고
    • Direct observation of ferroelastic domain effects in LSCF perovskites
    • Huang B.X., Steinbrech R.W., Malzbender J. Direct observation of ferroelastic domain effects in LSCF perovskites. Solid State Ionics 2012, 228(November):32-36.
    • (2012) Solid State Ionics , vol.228 , Issue.NOVEMBER , pp. 32-36
    • Huang, B.X.1    Steinbrech, R.W.2    Malzbender, J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.