메뉴 건너뛰기




Volumn 7, Issue 2, 2013, Pages 130-138

Preparation and crystallization kinetics of micron-sized Mg(OH)2 in a mixed suspension mixed product removal crystallizer

Author keywords

crystallization kinetics; magnesium hydroxide; micronsized; precipitation

Indexed keywords


EID: 84878272765     PISSN: 20950179     EISSN: 20950187     Source Type: Journal    
DOI: 10.1007/s11705-013-1332-7     Document Type: Article
Times cited : (29)

References (36)
  • 1
    • 0034139888 scopus 로고    scopus 로고
    • Studies on the impact fracture behaviour of flame retardant polymeric material
    • Tai C M, Li R K Y. Studies on the impact fracture behaviour of flame retardant polymeric material. Materials & Design, 2001, 22(1): 15-19.
    • (2001) Materials & Design , vol.22 , Issue.1 , pp. 15-19
    • Tai, C.M.1    Li, R.K.Y.2
  • 2
    • 33751203511 scopus 로고    scopus 로고
    • Structure and properties of polypropylene composites filled with magnesium hydroxide
    • Chen X L, Yu J, Guo S Y. Structure and properties of polypropylene composites filled with magnesium hydroxide. Journal of Applied Polymer Science, 2006, 102(5): 4943-4951.
    • (2006) Journal of Applied Polymer Science , vol.102 , Issue.5 , pp. 4943-4951
    • Chen, X.L.1    Yu, J.2    Guo, S.Y.3
  • 6
    • 0036544983 scopus 로고    scopus 로고
    • Magnesium hydroxide dehydroxylation/carbonation reaction processes: implications for carbon dioxide mineral sequestration
    • Béarat H, McKelvy M J, Chizmeshya A V G, Sharma R, Carpenter R W. Magnesium hydroxide dehydroxylation/carbonation reaction processes: implications for carbon dioxide mineral sequestration. Journal of the American Ceramic Society, 2002, 85(4): 742-748.
    • (2002) Journal of the American Ceramic Society , vol.85 , Issue.4 , pp. 742-748
    • Béarat, H.1    McKelvy, M.J.2    Chizmeshya, A.V.G.3    Sharma, R.4    Carpenter, R.W.5
  • 7
    • 0036027563 scopus 로고    scopus 로고
    • 2 and sucrose on the stability of bovine serum albumin encapsulated in injectable poly (D,L-lactide-co-glycolide) implants
    • 2 and sucrose on the stability of bovine serum albumin encapsulated in injectable poly (D, L-lactide-co-glycolide) implants. Biomaterials, 2002, 23(1): 239-245.
    • (2002) Biomaterials , vol.23 , Issue.1 , pp. 239-245
    • Kang, J.C.1    Schwendeman, S.P.2
  • 9
    • 0029345657 scopus 로고
    • Reduction of nitric oxide over magnesium oxide and dolomite at fluidized bed conditions
    • Olanders B, Strömberg D. Reduction of nitric oxide over magnesium oxide and dolomite at fluidized bed conditions. Energy & Fuels, 1995, 9(4): 680-684.
    • (1995) Energy & Fuels , vol.9 , Issue.4 , pp. 680-684
    • Olanders, B.1    Strömberg, D.2
  • 10
    • 0037102798 scopus 로고    scopus 로고
    • 2 nanocrystallites under hydrothermal conditions and the conversion to MgO nanorods by thermal dehydration
    • 2 nanocrystallites under hydrothermal conditions and the conversion to MgO nanorods by thermal dehydration. Materials Chemistry and Physics, 2002, 76(2): 119-122.
    • (2002) Materials Chemistry and Physics , vol.76 , Issue.2 , pp. 119-122
    • Yan, L.1    Zhuang, J.2    Sun, X.M.3    Deng, Z.X.4    Li, Y.D.5
  • 12
    • 0003173095 scopus 로고    scopus 로고
    • Mechanism of thermal decomposition of magnesium hydroxide
    • L'vov B V, Novichikhin A V, Dyakov A O. Mechanism of thermal decomposition of magnesium hydroxide. Thermochimica Acta, 1998, 315(2): 135-143.
    • (1998) Thermochimica Acta , vol.315 , Issue.2 , pp. 135-143
    • L'vov, B.V.1    Novichikhin, A.V.2    Dyakov, A.O.3
  • 13
    • 1642561700 scopus 로고    scopus 로고
    • Synthesis and characterization of porous magnesium hydroxide and oxide nanoplates
    • Yu J C, Xu A W, Zhang L Z, Song R Q, Wu L. W L. Synthesis and characterization of porous magnesium hydroxide and oxide nanoplates. Journal of Physical Chemistry B, 2004, 108(1): 64-70.
    • (2004) Journal of Physical Chemistry B , vol.108 , Issue.1 , pp. 64-70
    • Yu, J.C.1    Xu, A.W.2    Zhang, L.Z.3    Song, R.Q.4    Wu, L.W.L.5
  • 14
    • 34047183044 scopus 로고    scopus 로고
    • 2 nanostructures via natural oxidation of Mg metal in formamide/water mixture
    • 2 nanostructures via natural oxidation of Mg metal in formamide/water mixture. Materials Research Bulletin, 2007, 42(6): 1153-1158.
    • (2007) Materials Research Bulletin , vol.42 , Issue.6 , pp. 1153-1158
    • Zou, G.L.1    Liu, R.2    Chen, W.X.3    Xu, Z.D.4
  • 16
    • 55349084773 scopus 로고    scopus 로고
    • Influence of solvents on the hydrothermal formation of one-dimensional magnesium hydroxide
    • Sun X T, Xiang L, Zhu W C, Liu Q. Influence of solvents on the hydrothermal formation of one-dimensional magnesium hydroxide. Crystal Research and Technology, 2008, 43(10): 1057-1061.
    • (2008) Crystal Research and Technology , vol.43 , Issue.10 , pp. 1057-1061
    • Sun, X.T.1    Xiang, L.2    Zhu, W.C.3    Liu, Q.4
  • 20
    • 2942544280 scopus 로고    scopus 로고
    • Controlled growth of three morphological structures of magnesium hydroxide nanoparticles by wet precipitation method
    • Lv J P, Qiu L Z, Qu B J. Controlled growth of three morphological structures of magnesium hydroxide nanoparticles by wet precipitation method. Journal of Crystal Growth, 2004, 267(3-4): 676-684.
    • (2004) Journal of Crystal Growth , vol.267 , Issue.3-4 , pp. 676-684
    • Lv, J.P.1    Qiu, L.Z.2    Qu, B.J.3
  • 21
    • 0037297828 scopus 로고    scopus 로고
    • Morphological study of magnesium hydroxide nanoparticles precipitated in dilute aqueous solution
    • Henrist C, Mathieu J P, Vogels C, Rulmont A, Cloots R. Morphological study of magnesium hydroxide nanoparticles precipitated in dilute aqueous solution. Journal of Crystal Growth, 2003, 249(1): 321-330.
    • (2003) Journal of Crystal Growth , vol.249 , Issue.1 , pp. 321-330
    • Henrist, C.1    Mathieu, J.P.2    Vogels, C.3    Rulmont, A.4    Cloots, R.5
  • 25
    • 84984297074 scopus 로고
    • Precipitation of magnesium hydroxide
    • Söhnel O, Mareček J. Precipitation of magnesium hydroxide. Kristall und Technik, 1978, 13(3): 253-262.
    • (1978) Kristall Und Technik , vol.13 , Issue.3 , pp. 253-262
    • Söhnel, O.1    Mareček, J.2
  • 27
  • 30
    • 80053969999 scopus 로고    scopus 로고
    • Morphology control and growth mechanism of magnesium hydroxide nanoparticles via a simple wet precipitation method
    • Wang P P, Li C H, Gong H Y, Wang H Q, Liu J R. Morphology control and growth mechanism of magnesium hydroxide nanoparticles via a simple wet precipitation method. Ceramics International, 2011, 37(8): 3365-3370.
    • (2011) Ceramics International , vol.37 , Issue.8 , pp. 3365-3370
    • Wang, P.P.1    Li, C.H.2    Gong, H.Y.3    Wang, H.Q.4    Liu, J.R.5
  • 31
    • 41249095465 scopus 로고    scopus 로고
    • Magnesium hydroxide nanoparticles with controlled morphologies via wet coprecipitation
    • Chen D H, Zhu L Y, Zhang H P, Xu K, Chen M C. Magnesium hydroxide nanoparticles with controlled morphologies via wet coprecipitation. Materials Chemistry and Physics, 2008, 109(2-3): 224-229.
    • (2008) Materials Chemistry and Physics , vol.109 , Issue.2-3 , pp. 224-229
    • Chen, D.H.1    Zhu, L.Y.2    Zhang, H.P.3    Xu, K.4    Chen, M.C.5
  • 33
    • 85023815298 scopus 로고
    • Crystal growth in aqueous solutions1: II-Experimental
    • McCabe W L. Crystal growth in aqueous solutions1: II-Experimental. Industrial & Engineering Chemistry, 1929, 21(2): 112-119.
    • (1929) Industrial & Engineering Chemistry , vol.21 , Issue.2 , pp. 112-119
    • McCabe, W.L.1
  • 34
    • 85024686441 scopus 로고
    • Crystal growth in aqueous solutions1: I-Theory
    • McCabe W L. Crystal growth in aqueous solutions1: I-Theory. Industrial & Engineering Chemistry, 1929, 21(1): 30-33.
    • (1929) Industrial & Engineering Chemistry , vol.21 , Issue.1 , pp. 30-33
    • McCabe, W.L.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.