Volumn 226, Issue , 2013, Pages 181-188

Preparation of Si-Al/α-FeOOH catalyst from an iron-containing waste and surface-catalytic oxidation of methylene blue at neutral pH value in the presence of H2O2

Author keywords

Fenton like reaction; Grinding wheel ash; Iron oxide; Non radical mechanism; Surface catalytic oxidation

Indexed keywords

ADSORPTIVE CAPACITY; ANALYTICAL REAGENT; CRYSTALLINE STRUCTURE; FENTON-LIKE PROCESS; FENTON-LIKE REACTIONS; OXIDATION MECHANISMS; SCANNING ELECTRON MICROSCOPE; TOTAL ORGANIC CARBON;

EID: 84877895522     PISSN: 13858947     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.cej.2013.04.058     Document Type: Article
Times cited : (48)

References (43)
  • 1
    • 0038507703 scopus 로고    scopus 로고
    • Chemical destruction of MTBE using Fenton's reagent: effect of ferrous iron/hydrogen peroxide ratio
    • Burbano A.A., Dionysiou D.D., Suidan M.T., Richardson T.L. Chemical destruction of MTBE using Fenton's reagent: effect of ferrous iron/hydrogen peroxide ratio. Water Sci. Technol. 2003, 47:165-171.
    • (2003) Water Sci. Technol. , vol.47 , pp. 165-171
    • Burbano, A.A.1    Dionysiou, D.D.2    Suidan, M.T.3    Richardson, T.L.4
  • 2
    • 10644250849 scopus 로고    scopus 로고
    • Oxidation kinetics and effect of pH on the degradation of MTBE with Fenton reagent
    • Burbano A.A., Dionysiou D.D., Suidan M.T., Richardson T.L. Oxidation kinetics and effect of pH on the degradation of MTBE with Fenton reagent. Water Res. 2005, 39:107-118.
    • (2005) Water Res. , vol.39 , pp. 107-118
    • Burbano, A.A.1    Dionysiou, D.D.2    Suidan, M.T.3    Richardson, T.L.4
  • 3
    • 1942525108 scopus 로고    scopus 로고
    • Hydrogen peroxide/iron oxide-induced catalytic oxidation of organic compounds
    • Gurol M.D., Lin S.S. Hydrogen peroxide/iron oxide-induced catalytic oxidation of organic compounds. J. Adv. Oxid. Technol. 2002, 5:147-154.
    • (2002) J. Adv. Oxid. Technol. , vol.5 , pp. 147-154
    • Gurol, M.D.1    Lin, S.S.2
  • 4
    • 80054065086 scopus 로고    scopus 로고
    • Synthesis and characterization of magnetite nanoparticles using waste iron ore tailings for adsorptive removal of dyes from aqueous solution
    • Giri S.K., Das N.N., Pradhan G.C. Synthesis and characterization of magnetite nanoparticles using waste iron ore tailings for adsorptive removal of dyes from aqueous solution. Colloids Surf., A 2011, 389:43-49.
    • (2011) Colloids Surf., A , vol.389 , pp. 43-49
    • Giri, S.K.1    Das, N.N.2    Pradhan, G.C.3
  • 5
    • 54149116505 scopus 로고    scopus 로고
    • Polymer-encapsulated iron oxide nanoparticles as highly efficient Fenton catalysts
    • Shin S., Yoon H., Jang J. Polymer-encapsulated iron oxide nanoparticles as highly efficient Fenton catalysts. Catal. Commun. 2008, 10:178-182.
    • (2008) Catal. Commun. , vol.10 , pp. 178-182
    • Shin, S.1    Yoon, H.2    Jang, J.3
  • 6
    • 78751627718 scopus 로고    scopus 로고
    • New Fe-immobilized natural bentonite plate used as photo-Fenton catalyst for organic pollutant degradation
    • Ferney Gonzalez-Bahamon L., Fernando Hoyos D., Benitez N., Pulgarin C. New Fe-immobilized natural bentonite plate used as photo-Fenton catalyst for organic pollutant degradation. Chemosphere 2011, 82:1185-1189.
    • (2011) Chemosphere , vol.82 , pp. 1185-1189
    • Ferney Gonzalez-Bahamon, L.1    Fernando Hoyos, D.2    Benitez, N.3    Pulgarin, C.4
  • 7
    • 20444372652 scopus 로고    scopus 로고
    • Photo-assisted degradation of anionic and cationic dyes over iron(III)-loaded resin in the presence of hydrogen peroxide
    • Lv X.J., Xu Y.M., Lv K.L., Zhang G.C. Photo-assisted degradation of anionic and cationic dyes over iron(III)-loaded resin in the presence of hydrogen peroxide. J. Photochem. Photobiol., A 2005, 173:121-127.
    • (2005) J. Photochem. Photobiol., A , vol.173 , pp. 121-127
    • Lv, X.J.1    Xu, Y.M.2    Lv, K.L.3    Zhang, G.C.4
  • 8
    • 32544434798 scopus 로고    scopus 로고
    • Effect of initial solution pH on the degradation of Orange II using clay-based Fe nanocomposites as heterogeneous photo-Fenton catalyst
    • Feng J.Y., Hu X.J., Yue P.L. Effect of initial solution pH on the degradation of Orange II using clay-based Fe nanocomposites as heterogeneous photo-Fenton catalyst. Water Res. 2006, 40:641-646.
    • (2006) Water Res. , vol.40 , pp. 641-646
    • Feng, J.Y.1    Hu, X.J.2    Yue, P.L.3
  • 9
    • 33746377572 scopus 로고    scopus 로고
    • Fe-pillared clay as a Fenton-type heterogeneous catalyst for cinnamic acid degradation
    • Tabet D., Saidi M., Houari M., Pichat P., Khalaf H. Fe-pillared clay as a Fenton-type heterogeneous catalyst for cinnamic acid degradation. J. Environ. Manage. 2006, 80:342-346.
    • (2006) J. Environ. Manage. , vol.80 , pp. 342-346
    • Tabet, D.1    Saidi, M.2    Houari, M.3    Pichat, P.4    Khalaf, H.5
  • 11
    • 79954425203 scopus 로고    scopus 로고
    • Controlled synthesis, magnetic and sensing properties of hematite nanorods and microcapsules
    • Guo P., Wei Z., Wang B., Ding Y., Li H., Zhang G., Zhao X.S. Controlled synthesis, magnetic and sensing properties of hematite nanorods and microcapsules. Colloids Surf., A 2011, 380:234-240.
    • (2011) Colloids Surf., A , vol.380 , pp. 234-240
    • Guo, P.1    Wei, Z.2    Wang, B.3    Ding, Y.4    Li, H.5    Zhang, G.6    Zhao, X.S.7
  • 12
    • 69249202299 scopus 로고    scopus 로고
    • 3/FeOOH nanostructures with various morphologies by a hydrothermal route and their photocatalytic properties
    • 3/FeOOH nanostructures with various morphologies by a hydrothermal route and their photocatalytic properties. Colloids Surf., A 2009, 348:217-220.
    • (2009) Colloids Surf., A , vol.348 , pp. 217-220
    • Song, L.1    Zhang, S.2
  • 13
    • 71749118976 scopus 로고    scopus 로고
    • Degradation of C.I. Acid Orange 7 by ultrasound enhanced heterogeneous Fenton-like process
    • Zhang H., Fu H., Zhang D. Degradation of C.I. Acid Orange 7 by ultrasound enhanced heterogeneous Fenton-like process. J. Hazard. Mater. 2009, 172:654-660.
    • (2009) J. Hazard. Mater. , vol.172 , pp. 654-660
    • Zhang, H.1    Fu, H.2    Zhang, D.3
  • 16
    • 77955845428 scopus 로고    scopus 로고
    • 4) photocatalytic composites for the degradation of methylene blue dye in dilute aqueous solutions
    • 4) photocatalytic composites for the degradation of methylene blue dye in dilute aqueous solutions. Appl. Catal. B: Environ. 2010, 99:214-221.
    • (2010) Appl. Catal. B: Environ. , vol.99 , pp. 214-221
    • Zhou, B.1    Zhao, X.2    Liu, H.3    Qu, J.4    Huang, C.P.5
  • 18
    • 72249112169 scopus 로고    scopus 로고
    • A silica-supported iron oxide catalyst capable of activating hydrogen peroxide at neutral pH values
    • Pham A.L.-T., Lee C., Doyle F.M., Sedlak D.L. A silica-supported iron oxide catalyst capable of activating hydrogen peroxide at neutral pH values. Environ. Sci. Technol. 2009, 43:8930-8935.
    • (2009) Environ. Sci. Technol. , vol.43 , pp. 8930-8935
    • Pham, A.L.-T.1    Lee, C.2    Doyle, F.M.3    Sedlak, D.L.4
  • 19
    • 33751538043 scopus 로고    scopus 로고
    • Influence of silicon on local structure and morphology of gamma-FeOOH and alpha-FeOOH particles
    • Kwon S.K., Shinoda K., Suzuki S., Waseda Y. Influence of silicon on local structure and morphology of gamma-FeOOH and alpha-FeOOH particles. Corros. Sci. 2007, 49:1513-1526.
    • (2007) Corros. Sci. , vol.49 , pp. 1513-1526
    • Kwon, S.K.1    Shinoda, K.2    Suzuki, S.3    Waseda, Y.4
  • 20
    • 33645450208 scopus 로고    scopus 로고
    • Highly active heterogeneous Fenton catalyst using iron oxide nanoparticles immobilized in alumina coated mesoporous silica
    • Lim H., Lee J., Jin S., Kim J., Yoon J., Hyeon T. Highly active heterogeneous Fenton catalyst using iron oxide nanoparticles immobilized in alumina coated mesoporous silica. Chem. Commun. 2006, 463-465.
    • (2006) Chem. Commun. , pp. 463-465
    • Lim, H.1    Lee, J.2    Jin, S.3    Kim, J.4    Yoon, J.5    Hyeon, T.6
  • 21
    • 77949266524 scopus 로고    scopus 로고
    • Catalytic oxidation of methyl orange by an amorphous FeOOH catalyst developed from a high iron-containing fly ash
    • Li Y., Zhang F.-S. Catalytic oxidation of methyl orange by an amorphous FeOOH catalyst developed from a high iron-containing fly ash. Chem. Eng. J. 2010, 158:148-153.
    • (2010) Chem. Eng. J. , vol.158 , pp. 148-153
    • Li, Y.1    Zhang, F.-S.2
  • 22
    • 84877899709 scopus 로고    scopus 로고
    • Heterogeneous Fenton process using steel industry wastes for methyl orange degradation
    • Ali M.E.M., Gad-Allah T.A., Badawy M.I. Heterogeneous Fenton process using steel industry wastes for methyl orange degradation. Appl. Water Sci. 2013, 3:263-270.
    • (2013) Appl. Water Sci. , vol.3 , pp. 263-270
    • Ali, M.E.M.1    Gad-Allah, T.A.2    Badawy, M.I.3
  • 23
    • 34247521747 scopus 로고    scopus 로고
    • Comparative study for the removal of methylene blue via adsorption and photocatalytic degradation
    • El-Sharkawy E.A., Soliffian A.Y., Al-Amer K.M. Comparative study for the removal of methylene blue via adsorption and photocatalytic degradation. J. Colloid Interf. Sci. 2007, 310:498-508.
    • (2007) J. Colloid Interf. Sci. , vol.310 , pp. 498-508
    • El-Sharkawy, E.A.1    Soliffian, A.Y.2    Al-Amer, K.M.3
  • 25
    • 70249119225 scopus 로고    scopus 로고
    • Arsenic (V) removal from aqueous system using adsorbent developed from a high iron-containing fly ash
    • Li Y., Zhang F.-S., Xiu F.-R. Arsenic (V) removal from aqueous system using adsorbent developed from a high iron-containing fly ash. Sci. Total Environ. 2009, 407:5780-5786.
    • (2009) Sci. Total Environ. , vol.407 , pp. 5780-5786
    • Li, Y.1    Zhang, F.-S.2    Xiu, F.-R.3
  • 27
    • 38449094857 scopus 로고    scopus 로고
    • Characterization and field emission performance of electrochemically synthesized FeOOH nanowalls
    • Chin K.C., Cui H., Sow C.H., Sheu F.S., van L.H., Gao X., Wee A.T.S. Characterization and field emission performance of electrochemically synthesized FeOOH nanowalls. J. Nanosci. Nanotechnol. 2007, 7:3301-3306.
    • (2007) J. Nanosci. Nanotechnol. , vol.7 , pp. 3301-3306
    • Chin, K.C.1    Cui, H.2    Sow, C.H.3    Sheu, F.S.4    van, L.H.5    Gao, X.6    Wee, A.T.S.7
  • 29
    • 0035696153 scopus 로고    scopus 로고
    • Effects of surface modification of alpha-FeOOH powder on the sintering process of ferrite compacts
    • Uekawa N., Fukuda S., Kakegawa K., Sasaki Y. Effects of surface modification of alpha-FeOOH powder on the sintering process of ferrite compacts. Phys. Chem. Chem. Phys. 2001, 3:5596-5601.
    • (2001) Phys. Chem. Chem. Phys. , vol.3 , pp. 5596-5601
    • Uekawa, N.1    Fukuda, S.2    Kakegawa, K.3    Sasaki, Y.4
  • 30
    • 80051947334 scopus 로고    scopus 로고
    • ZnO/montmorillonite for photocatalytic and photochemical degradation of methylene blue
    • Fatimah I., Wang S., Wulandari D. ZnO/montmorillonite for photocatalytic and photochemical degradation of methylene blue. Appl. Clay Sci. 2011, 53:553-560.
    • (2011) Appl. Clay Sci. , vol.53 , pp. 553-560
    • Fatimah, I.1    Wang, S.2    Wulandari, D.3
  • 31
    • 79551683643 scopus 로고    scopus 로고
    • 2 as a reusable heterogeneous Fenton-like catalyst
    • 2 as a reusable heterogeneous Fenton-like catalyst. Desalination 2011, 269:284-290.
    • (2011) Desalination , vol.269 , pp. 284-290
    • Ji, F.1    Li, C.2    Zhang, J.3    Deng, L.4
  • 34
    • 34948839999 scopus 로고    scopus 로고
    • Probing methylene blue photocatalytic degradation by adsorbed ethanol with in situ IR
    • Yu Z., Chuang S.S.C. Probing methylene blue photocatalytic degradation by adsorbed ethanol with in situ IR. J. Phys. Chem. C 2007, 111:13813-13820.
    • (2007) J. Phys. Chem. C , vol.111 , pp. 13813-13820
    • Yu, Z.1    Chuang, S.S.C.2
  • 35
    • 0037362977 scopus 로고    scopus 로고
    • Catalyzed oxidation of arsenic(III) by hydrogen peroxide on the surface of ferrihydrite: An in situ ATR-FTIR study
    • Voegelin A., Hug S.J. Catalyzed oxidation of arsenic(III) by hydrogen peroxide on the surface of ferrihydrite: An in situ ATR-FTIR study. Environ. Sci. Technol. 2003, 37:972-978.
    • (2003) Environ. Sci. Technol. , vol.37 , pp. 972-978
    • Voegelin, A.1    Hug, S.J.2
  • 36
    • 0037782275 scopus 로고    scopus 로고
    • Iron-catalyzed oxidation of arsenic(III) by oxygen and by hydrogen peroxide: pH-dependent formation of oxidants in the Fenton reaction
    • Hug S.J., Leupin O. Iron-catalyzed oxidation of arsenic(III) by oxygen and by hydrogen peroxide: pH-dependent formation of oxidants in the Fenton reaction. Environ. Sci. Technol. 2003, 37:2734-2742.
    • (2003) Environ. Sci. Technol. , vol.37 , pp. 2734-2742
    • Hug, S.J.1    Leupin, O.2
  • 38
    • 0036469048 scopus 로고    scopus 로고
    • Iron oxide surface-catalyzed oxidation of ferrous iron by monochloramine: implications of oxide type and carbonate on reactivity
    • Vikesland P.J., Valentine R.L. Iron oxide surface-catalyzed oxidation of ferrous iron by monochloramine: implications of oxide type and carbonate on reactivity. Environ. Sci. Technol. 2002, 36:512-519.
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 512-519
    • Vikesland, P.J.1    Valentine, R.L.2
  • 41
    • 0141739755 scopus 로고    scopus 로고
    • A method for preparing silica-containing iron(III) oxide adsorbents for arsenic removal
    • Zeng L. A method for preparing silica-containing iron(III) oxide adsorbents for arsenic removal. Water Res. 2003, 37:4351-4358.
    • (2003) Water Res. , vol.37 , pp. 4351-4358
    • Zeng, L.1
  • 42
    • 34547909673 scopus 로고    scopus 로고
    • Characteristic low-temperature magnetic properties of aluminous goethite [α-(Fe, Al)OOH] explained
    • Liu Q., Yu Y., Torrent J., Roberts A.P., Pan Y., Zhu R. Characteristic low-temperature magnetic properties of aluminous goethite [α-(Fe, Al)OOH] explained. J. Geophys. Res. 2006, 111.
    • (2006) J. Geophys. Res. , vol.111
    • Liu, Q.1    Yu, Y.2    Torrent, J.3    Roberts, A.P.4    Pan, Y.5    Zhu, R.6
  • 43
    • 64549125206 scopus 로고    scopus 로고
    • The crystal chemistry of Al-bearing goethites: an infrared spectroscopic study
    • Blanch A.J., Quinton J.S., Lenehan C.E., Pring A. The crystal chemistry of Al-bearing goethites: an infrared spectroscopic study. Min. Mag. 2008, 72:1043-1056.
    • (2008) Min. Mag. , vol.72 , pp. 1043-1056
    • Blanch, A.J.1    Quinton, J.S.2    Lenehan, C.E.3    Pring, A.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.