Volumn 18, Issue , 2013, Pages 108-122

Bioresorbable composite screws manufactured via forging process: Pull-out, shear, flexural and degradation characteristics

Author keywords

Bioresorbable; Bone screws; Composite; Forging; Phosphate based glass fibres; Poly lactic acid

Indexed keywords

BIORESORBABLE; BONE SCREW; CHEMICAL DURABILITY; COMPOSITE BARS; DEGRADATION CHARACTERISTICS; DEGRADATION PROCESS; FIBRE MATS; FLEXURAL LOADS; FORGING PROCESS; MASS LOSS; METALLIC SCREWS; PHOSPHATE BASED GLASS; POLY LACTIC ACID; PULL-OUT; PULL-OUT STRENGTH; SCREW HOLE; SHEAR LOADS; WATER UPTAKE;

EID: 84871644474     PISSN: 17516161     EISSN: 18780180     Source Type: Journal    
DOI: 10.1016/j.jmbbm.2012.11.009     Document Type: Article
Times cited : (22)

References (58)
  • 3
    • 48449086835 scopus 로고    scopus 로고
    • Weight loss, ion release and initial mechanical properties of a binary calcium phosphate glass fibre/PCL composite
    • Ahmed I., Parsons A.J., Palmer G., Knowles J.C., Walker G.S., Rudd C.D. Weight loss, ion release and initial mechanical properties of a binary calcium phosphate glass fibre/PCL composite. Acta Biomaterialia 2008, 4(5):1307-1314.
    • (2008) Acta Biomaterialia , vol.4 , Issue.5 , pp. 1307-1314
    • Ahmed, I.1    Parsons, A.J.2    Palmer, G.3    Knowles, J.C.4    Walker, G.S.5    Rudd, C.D.6
  • 5
    • 1242317762 scopus 로고    scopus 로고
    • Processing, characterisation and biocompatibility of iron-phosphate glass fibres for tissue engineering
    • Ahmed I., Collins C.A., Lewis M.P., Olsen I., Knowles J.C. Processing, characterisation and biocompatibility of iron-phosphate glass fibres for tissue engineering. Biomaterials 2004, 25(16):3223-3232.
    • (2004) Biomaterials , vol.25 , Issue.16 , pp. 3223-3232
    • Ahmed, I.1    Collins, C.A.2    Lewis, M.P.3    Olsen, I.4    Knowles, J.C.5
  • 6
    • 0003985424 scopus 로고
    • Standard Test Method for Ignition Loss of Cured Reinforced Resins
    • ASTM D2584-94
    • ASTM D2584-94, Standard Test Method for Ignition Loss of Cured Reinforced Resins, 1994.
    • (1994)
  • 7
    • 67349229089 scopus 로고    scopus 로고
    • Standard Test Method for Transverse Shear Strength of Fiber-reinforced Polymer Matrix Composite Bars
    • ASTM D7617/D7617M-11
    • ASTM D7617/D7617M-11: Standard Test Method for Transverse Shear Strength of Fiber-reinforced Polymer Matrix Composite Bars, 2011.
    • (2011)
  • 8
    • 84871647316 scopus 로고    scopus 로고
    • Standard Specification and Test Methods for Bioabsorbable Plates and Screws for Internal Fixation Implants.
    • ASTM F2502-05
    • ASTM F2502-05 Standard Specification and Test Methods for Bioabsorbable Plates and Screws for Internal Fixation Implants.
  • 11
    • 76649141462 scopus 로고    scopus 로고
    • Cytocompatibility and effect of increasing MgO content in a range of quaternary invert phosphate-based glasses
    • Ahmed I., Parsons A., Jones A., Walker G., Scotchford C., Rudd C. Cytocompatibility and effect of increasing MgO content in a range of quaternary invert phosphate-based glasses. The Journal of Biomaterials Applications 2010, 24(6):555-575.
    • (2010) The Journal of Biomaterials Applications , vol.24 , Issue.6 , pp. 555-575
    • Ahmed, I.1    Parsons, A.2    Jones, A.3    Walker, G.4    Scotchford, C.5    Rudd, C.6
  • 13
    • 84871655292 scopus 로고    scopus 로고
    • Identification and quantification of degradation products from polymeric medical devices
    • BS EN ISO 10993-13
    • BS EN ISO 10993-13, 2010. Biological evaluation of medical devices. Identification and quantification of degradation products from polymeric medical devices.
    • (2010) Biological evaluation of medical devices
  • 14
    • 84871656939 scopus 로고    scopus 로고
    • General principles for two-point, three-point and four-point methods.
    • BS ISO 5628
    • BS ISO 5628, 2012. Determination of bending stiffness. General principles for two-point, three-point and four-point methods.
    • (2012) Determination of bending stiffness
  • 17
    • 0028878553 scopus 로고
    • Late degradation tissue response to poly(L-lactide) bone plates and screws
    • Bergsma J.E., de Bruijn W.C., Rozema F.R., Bos R.R.M., Boering G. Late degradation tissue response to poly(L-lactide) bone plates and screws. Biomaterials 1995, 16(1):25-31.
    • (1995) Biomaterials , vol.16 , Issue.1 , pp. 25-31
    • Bergsma, J.E.1    de Bruijn, W.C.2    Rozema, F.R.3    Bos, R.R.M.4    Boering, G.5
  • 18
    • 0034266653 scopus 로고    scopus 로고
    • Flexural properties of fiber reinforced composite using a vacuum/pressure or a manual adaptation manufacturing process
    • Behr M., Rosentritt M., Lang R., Handel G. Flexural properties of fiber reinforced composite using a vacuum/pressure or a manual adaptation manufacturing process. Journal of Dentistry 2000, 28(7):509-514.
    • (2000) Journal of Dentistry , vol.28 , Issue.7 , pp. 509-514
    • Behr, M.1    Rosentritt, M.2    Lang, R.3    Handel, G.4
  • 19
  • 21
    • 33646353199 scopus 로고    scopus 로고
    • The effect of surface area on the degradation rate of nano-fibrous poly(l-lactic acid) foams
    • Chen V.J., Ma P.X. The effect of surface area on the degradation rate of nano-fibrous poly(l-lactic acid) foams. Biomaterials 2006, 27(20):3708-3715.
    • (2006) Biomaterials , vol.27 , Issue.20 , pp. 3708-3715
    • Chen, V.J.1    Ma, P.X.2
  • 22
    • 0028137353 scopus 로고
    • Environmental durability of glass-fiber composites
    • Carol L Environmental durability of glass-fiber composites. Materials Science and Engineering: R: Reports 1994, 13(7):265-323.
    • (1994) Materials Science and Engineering: R: Reports , vol.13 , Issue.7 , pp. 265-323
    • Carol, L.1
  • 24
    • 21344449120 scopus 로고    scopus 로고
    • In vitro properties of PLLA screws and novel bioabsorbable implant with elastic nucleus to replace intervertebral disc
    • Ell V., Kellomaki M., Tormala P. In vitro properties of PLLA screws and novel bioabsorbable implant with elastic nucleus to replace intervertebral disc. Journal of Materials Science: Materials in Medicine 2005, 16:655-662.
    • (2005) Journal of Materials Science: Materials in Medicine , vol.16 , pp. 655-662
    • Ell, V.1    Kellomaki, M.2    Tormala, P.3
  • 25
    • 0032143082 scopus 로고    scopus 로고
    • Composite technology in load-bearing orthopaedic implants
    • Evans S.L., Gregson P.J. Composite technology in load-bearing orthopaedic implants. Biomaterials 1998, 19(15):1329-1342.
    • (1998) Biomaterials , vol.19 , Issue.15 , pp. 1329-1342
    • Evans, S.L.1    Gregson, P.J.2
  • 26
    • 84859034511 scopus 로고    scopus 로고
    • Investigation of crystallinity, molecular weight change, and mechanical properties of PLA/PBG bioresorbable composites as bone fracture fixation plates
    • Felfel R.M., Ahmed I., Parsons A.J., Haque P., Walker G.S., Rudd C.D. Investigation of crystallinity, molecular weight change, and mechanical properties of PLA/PBG bioresorbable composites as bone fracture fixation plates. The Journal of Biomaterials Applications 2012, 26(7):765-789.
    • (2012) The Journal of Biomaterials Applications , vol.26 , Issue.7 , pp. 765-789
    • Felfel, R.M.1    Ahmed, I.2    Parsons, A.J.3    Haque, P.4    Walker, G.S.5    Rudd, C.D.6
  • 30
    • 6944232282 scopus 로고    scopus 로고
    • Biodegradable polymers and composites in biomedical applications: from catgut to tissue engineering. Part 1 Available systems and their properties
    • Gomes M.E., Reis R.L. Biodegradable polymers and composites in biomedical applications: from catgut to tissue engineering. Part 1 Available systems and their properties. International Materials Reviews 2004, 49(5):261-273.
    • (2004) International Materials Reviews , vol.49 , Issue.5 , pp. 261-273
    • Gomes, M.E.1    Reis, R.L.2
  • 31
    • 0033390457 scopus 로고    scopus 로고
    • Interface damage study of hydrothermally aged glass-fibre-reinforced polyester composites
    • Gautier L., Mortaigne B., Bellenger V. Interface damage study of hydrothermally aged glass-fibre-reinforced polyester composites. Composites Science and Technology 1999, 59(16):2329-2337.
    • (1999) Composites Science and Technology , vol.59 , Issue.16 , pp. 2329-2337
    • Gautier, L.1    Mortaigne, B.2    Bellenger, V.3
  • 32
    • 77956899099 scopus 로고    scopus 로고
    • Interfacial properties of phosphate glass fibres/PLA composites: effect of the end functionalities of oligomeric PLA coupling agents
    • Haque P., Parsons A.J., Barker I.A., Ahmed I., Irvine D.J., Walker G.S., Rudd C.D. Interfacial properties of phosphate glass fibres/PLA composites: effect of the end functionalities of oligomeric PLA coupling agents. Composites Science and Technology 2010, 70(13):1854-1860.
    • (2010) Composites Science and Technology , vol.70 , Issue.13 , pp. 1854-1860
    • Haque, P.1    Parsons, A.J.2    Barker, I.A.3    Ahmed, I.4    Irvine, D.J.5    Walker, G.S.6    Rudd, C.D.7
  • 34
    • 33845259122 scopus 로고    scopus 로고
    • Effect of water absorption on the mechanical properties of glass/polyester composites
    • Huang G., Sun H. Effect of water absorption on the mechanical properties of glass/polyester composites. Materials & Design 2007, 28(5):1647-1650.
    • (2007) Materials & Design , vol.28 , Issue.5 , pp. 1647-1650
    • Huang, G.1    Sun, H.2
  • 37
    • 11144272811 scopus 로고    scopus 로고
    • Fixation of osteochondritis dissecans lesions using poly(l-lactic acid)/poly(glycolic acid) copolymer bioabsorbable screws
    • Larsen M.W., Pietrzak W.S., DeLee J.C. Fixation of osteochondritis dissecans lesions using poly(l-lactic acid)/poly(glycolic acid) copolymer bioabsorbable screws. The American Journal of Sports Medicine 2005, 33(1):68-76.
    • (2005) The American Journal of Sports Medicine , vol.33 , Issue.1 , pp. 68-76
    • Larsen, M.W.1    Pietrzak, W.S.2    DeLee, J.C.3
  • 38
    • 0036121228 scopus 로고    scopus 로고
    • The influence of short-term water storage on the flexural properties of unidirectional glass fiber-reinforced composites
    • Lassila L.V.J., Nohrström T., Vallittu P.K. The influence of short-term water storage on the flexural properties of unidirectional glass fiber-reinforced composites. Biomaterials 2002, 23(10):2221-2229.
    • (2002) Biomaterials , vol.23 , Issue.10 , pp. 2221-2229
    • Lassila, L.V.J.1    Nohrström, T.2    Vallittu, P.K.3
  • 39
    • 0034580276 scopus 로고    scopus 로고
    • Synthetic biodegradable polymers as orthopedic devices
    • Middleton J.C., Tipton A.J. Synthetic biodegradable polymers as orthopedic devices. Biomaterials 2000, 21(23):2335-2346.
    • (2000) Biomaterials , vol.21 , Issue.23 , pp. 2335-2346
    • Middleton, J.C.1    Tipton, A.J.2
  • 40
    • 0031555488 scopus 로고    scopus 로고
    • Fiber-matrix interface studies on bioabsorbable composite materials for internal fixation of bone fractures. II. A new method using laser scanning confocal microscopy
    • Michael A.S., Chu C.C. Fiber-matrix interface studies on bioabsorbable composite materials for internal fixation of bone fractures. II. A new method using laser scanning confocal microscopy. Journal of Biomedical Materials Research 1997, 37(3):353-362.
    • (1997) Journal of Biomedical Materials Research , vol.37 , Issue.3 , pp. 353-362
    • Michael, A.S.1    Chu, C.C.2
  • 42
    • 77955060404 scopus 로고    scopus 로고
    • Bioactive composites based on calcium phosphates for bone regeneration
    • Navarro M., Planell J.A. Bioactive composites based on calcium phosphates for bone regeneration. Key Engineering Materials 2010, 441:203-233.
    • (2010) Key Engineering Materials , vol.441 , pp. 203-233
    • Navarro, M.1    Planell, J.A.2
  • 45
  • 51
    • 0034845979 scopus 로고    scopus 로고
    • Bioresorbable devices made of forged composites of hydroxyapatite (HA) particles and poly -lactide (PLLA). Part II: practical properties of miniscrews and miniplates
    • Shikinami Y., Okuno M. Bioresorbable devices made of forged composites of hydroxyapatite (HA) particles and poly -lactide (PLLA). Part II: practical properties of miniscrews and miniplates. Biomaterials 2001, 22(23):3197-3211.
    • (2001) Biomaterials , vol.22 , Issue.23 , pp. 3197-3211
    • Shikinami, Y.1    Okuno, M.2
  • 54
    • 0029341450 scopus 로고
    • The interface region in glass fibre-reinforced epoxy resin composites: 2. Water absorption, voids and the interface
    • Thomason J.L. The interface region in glass fibre-reinforced epoxy resin composites: 2. Water absorption, voids and the interface. Composites 1995, 26(7):477-485.
    • (1995) Composites , vol.26 , Issue.7 , pp. 477-485
    • Thomason, J.L.1
  • 55
    • 0036738361 scopus 로고    scopus 로고
    • Self-reinforced bioabsorbable versus metallic fixation systems for metacarpal and phalangeal fractures: A biomechanical study
    • Waris E., Ashammakhi N., Raatikainen T., Törmälä P., Santavirta S., Konttinen Y.T. Self-reinforced bioabsorbable versus metallic fixation systems for metacarpal and phalangeal fractures: A biomechanical study. The Journal of Hand Surgery 2002, 27(5):902-909.
    • (2002) The Journal of Hand Surgery , vol.27 , Issue.5 , pp. 902-909
    • Waris, E.1    Ashammakhi, N.2    Raatikainen, T.3    Törmälä, P.4    Santavirta, S.5    Konttinen, Y.T.6
  • 57
    • 34347407883 scopus 로고    scopus 로고
    • Water absorption behavior and its influence on properties of GRP pipe
    • Yao J., Ziegmann G. Water absorption behavior and its influence on properties of GRP pipe. Journal of Composite Materials 2007, 41(8):993-1008.
    • (2007) Journal of Composite Materials , vol.41 , Issue.8 , pp. 993-1008
    • Yao, J.1    Ziegmann, G.2
  • 58
    • 0038748339 scopus 로고    scopus 로고
    • Structure and morphology changes during in vitro degradation of electrospun poly(glycolide-co-lactide) nanofiber membrane
    • Zong X., Ran S., Kim K.-S., Fang D., Hsiao B.S., Chu B. Structure and morphology changes during in vitro degradation of electrospun poly(glycolide-co-lactide) nanofiber membrane. Biomacromolecules 2003, 4(2):416-423.
    • (2003) Biomacromolecules , vol.4 , Issue.2 , pp. 416-423
    • Zong, X.1    Ran, S.2    Kim, K.-S.3    Fang, D.4    Hsiao, B.S.5    Chu, B.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.