Post-yield fracture behaviour of PA-6/LDPE-g-MA/nanoclay ternary nanocomposites: Semiductile-to-ductile transition

Author keywords

Deformation; Fracture; Microstructure; Polymer; Toughness

Indexed keywords

CRACKS; DEFORMATION; FRACTURE; FRACTURE MECHANICS; MICROSTRUCTURE; NANOCOMPOSITES; NANOSTRUCTURED MATERIALS; POLYMERS; TOUGHNESS;

EID: 84869886138     PISSN: 10229760     EISSN: 15728935     Source Type: Journal    
DOI: 10.1007/s10965-012-0038-8     Document Type: Article
Times cited : (6)

References (39)
  • 1
    • 2342498961 scopus 로고
    • Impact fracture mechanisms in polymer blends: Rubber-toughened nylon
    • Wu S (1983) Impact fracture mechanisms in polymer blends: rubber-toughened nylon. J Polymer Sci Pol Phys Edition 21: 699-716
    • (1983) J Polymer Sci Pol Phys Edition , vol.21 , pp. 699-716
    • Wu, S.1
  • 2
    • 33646131400 scopus 로고    scopus 로고
    • Comparison of fracture behavior of nylon 6 versus an amorphous polyamide toughened with maleated poly (ethylene-1-octene) elastomers
    • Huang JJ, Paul DR (2006) Comparison of fracture behavior of nylon 6 versus an amorphous polyamide toughened with maleated poly (ethylene-1-octene) elastomers. Polymer 47:3505-3519
    • (2006) Polymer , vol.47 , pp. 3505-3519
    • Huang, J.J.1    Paul, D.R.2
  • 3
    • 30144446021 scopus 로고    scopus 로고
    • Temperature dependence of crack initiation fracture toughness of various nanoparticles filled polyamide 66
    • Zhang H, Zhang Z, Yang JL, Friedrich K (2006) Temperature dependence of crack initiation fracture toughness of various nanoparticles filled polyamide 66. Polymer 47:679-689
    • (2006) Polymer , vol.47 , pp. 679-689
    • Zhang, H.1    Zhang, Z.2    Yang, J.L.3    Friedrich, K.4
  • 4
    • 0036711113 scopus 로고    scopus 로고
    • Toughness of nanoscale and multiscale polyamide 66 composites
    • Nair SV, Goettler LA, Lysek BA (2002) Toughness of nanoscale and multiscale polyamide 66 composites. Polymer Eng Sci 42:1872-1882
    • (2002) Polymer Eng Sci , vol.42 , pp. 1872-1882
    • Nair, S.V.1    Goettler, L.A.2    Lysek, B.A.3
  • 5
    • 33644701862 scopus 로고    scopus 로고
    • Embrittlement mechanisms of nylon 66/organoclay nanocomposites prepared by melt compounding process
    • Chen L, Phang IY, Wong SC, Lv PF, Liu T (2006) Embrittlement mechanisms of nylon 66/organoclay nanocomposites prepared by melt compounding process. Mater Manuf Process 22:153-158
    • (2006) Mater Manuf Process , vol.22 , pp. 153-158
    • Chen, L.1    Phang, I.Y.2    Wong, S.C.3    Lv, P.F.4    Liu, T.5
  • 6
    • 33645910518 scopus 로고    scopus 로고
    • Rubber toughening of nylon 6 nanocomposites
    • Ahn YC, Paul DR (2006) Rubber toughening of nylon 6 nanocomposites. Polymer 47:2830-2838
    • (2006) Polymer , vol.47 , pp. 2830-2838
    • Ahn, Y.C.1    Paul, D.R.2
  • 7
    • 84855326227 scopus 로고    scopus 로고
    • Mechanical and thermal behavior of polyamide 6/silicon carbide nanocomposites toughened with maletaed styrene-ethylene-butylene-styrene elastomer
    • Liao CZ, Tjong SC (2011) Mechanical and thermal behavior of polyamide 6/silicon carbide nanocomposites toughened with maletaed styrene-ethylene-butylene-styrene elastomer. Fatig Fract Eng Mater Struct 35:56-63
    • (2011) Fatig Fract Eng Mater Struct , vol.35 , pp. 56-63
    • Liao, C.Z.1    Tjong, S.C.2
  • 8
    • 12344253183 scopus 로고    scopus 로고
    • Essential fracture work of nylon 6-silicate nanocomposites
    • Qiao Y, Avlar S, Chakravarthula SS (2005) Essential fracture work of nylon 6-silicate nanocomposites. J Appl Polymer Sci 95: 815-819
    • (2005) J Appl Polymer Sci , vol.95 , pp. 815-819
    • Qiao, Y.1    Avlar, S.2    Chakravarthula, S.S.3
  • 11
    • 39149104638 scopus 로고    scopus 로고
    • Microdeformation and fracture mechanisms in polyamide-6/Organoclay nanocomposites
    • He C, Liu T, Tjiu WC, Sue HJ, Yee AF (2008) Microdeformation and fracture mechanisms in polyamide-6/Organoclay nanocomposites. Macromolecules 41:193-202
    • (2008) Macromolecules , vol.41 , pp. 193-202
    • He, C.1    Liu, T.2    Tjiu, W.C.3    Sue, H.J.4    Yee, A.F.5
  • 12
    • 33751536486 scopus 로고    scopus 로고
    • Impact essential work of fracture of polypropylene/montmorillonite nanocomposites toughened with SEBS-g-MA elastomer
    • Bao SP, Tjong SC (2007) Impact essential work of fracture of polypropylene/montmorillonite nanocomposites toughened with SEBS-g-MA elastomer. Composites: Part A 38:378-387
    • (2007) Composites: Part A , vol.38 , pp. 378-387
    • Bao, S.P.1    Tjong, S.C.2
  • 13
    • 33644504195 scopus 로고    scopus 로고
    • Rubber toughening of polyamide 6/organoclay nanocomposites obtained by melt blending
    • Baldi F, Bignotti F, Tieghi G, Ricco T (2006) Rubber toughening of polyamide 6/organoclay nanocomposites obtained by melt blending. J Appl Polymer Sci 99:3406-3416
    • (2006) J Appl Polymer Sci , vol.99 , pp. 3406-3416
    • Baldi, F.1    Bignotti, F.2    Tieghi, G.3    Ricco, T.4
  • 14
    • 14644399228 scopus 로고    scopus 로고
    • Impact fracture toughness of polyamide-6/montmorillonite nanocomposites toughened with a maleated styrene/ethylene butylene/styrene elastomer
    • Tjong SC, Bao SP (2005) Impact fracture toughness of polyamide-6/montmorillonite nanocomposites toughened with a maleated styrene/ethylene butylene/styrene elastomer. J Polymer Sci B Polymer Phys 43:585-595
    • (2005) J Polymer Sci B Polymer Phys , vol.43 , pp. 585-595
    • Tjong, S.C.1    Bao, S.P.2
  • 15
    • 54249122164 scopus 로고    scopus 로고
    • Impact and tensile energies of fracture in polymer-clay nanocomposites
    • Chen B, Evans-Julian RG (2008) Impact and tensile energies of fracture in polymer-clay nanocomposites. Polymer 49:5113-5118
    • (2008) Polymer , vol.49 , pp. 5113-5118
    • Chen, B.1    Evans-Julian, R.G.2
  • 16
    • 33746776746 scopus 로고    scopus 로고
    • Morphology and fracture behaviour of polyethylene/Mg-Al layered double hydroxide (LDH) nanocomposites
    • Costa FR, Satapathy BK,Wagenknecht U,Weidisch R, Heinrich G (2006) Morphology and fracture behaviour of polyethylene/Mg-Al layered double hydroxide (LDH) nanocomposites. Eur Polymer J 42:2140-2152
    • (2006) Eur Polymer J , vol.42 , pp. 2140-2152
    • Costa, F.R.1    Satapathy, B.K.2    Wagenknecht, U.3    Weidisch, R.4    Heinrich, G.5
  • 18
    • 0033893498 scopus 로고    scopus 로고
    • Impact fracture morphology of nylon 6 toughened with a maleated polyethylene-octane elastomer
    • Yu ZZ, Ke YC, Ou YC, Hu GH (2000) Impact fracture morphology of nylon 6 toughened with a maleated polyethylene-octane elastomer. J Appl Polymer Sci 76:1285-1295
    • (2000) J Appl Polymer Sci , vol.76 , pp. 1285-1295
    • Yu, Z.Z.1    Ke, Y.C.2    Ou, Y.C.3    Hu, G.H.4
  • 19
    • 77950534822 scopus 로고    scopus 로고
    • Mechanical and fracture properties of ternary PE/PA6/GF composites
    • Malchev PG, de Vos G, Picken SJ, Gotsis AD (2010) Mechanical and fracture properties of ternary PE/PA6/GF composites. Compos Sci Tech 70:734-742
    • (2010) Compos Sci Tech , vol.70 , pp. 734-742
    • Malchev, P.G.1    de Vos, G.2    Picken, S.J.3    Gotsis, A.D.4
  • 20
    • 49149115105 scopus 로고    scopus 로고
    • The influence of reactive compatibilization on uniaxial large strain deformation and fracture behavior of polyamide 6 and poly (ethylene-co-butyl acrylate) blends
    • Balamurugan GP, Maiti SN (2008) The influence of reactive compatibilization on uniaxial large strain deformation and fracture behavior of polyamide 6 and poly (ethylene-co-butyl acrylate) blends. Polymer Test 27:752-764
    • (2008) Polymer Test , vol.27 , pp. 752-764
    • Balamurugan, G.P.1    Maiti, S.N.2
  • 21
    • 0037466569 scopus 로고    scopus 로고
    • Impact fracture toughness of short glass fiber-reinforced polyamide 6,6 hybrid composites containing elastomer particles using essential work of fracture concept
    • Tjong SC, Xu SA, Mai YW (2003) Impact fracture toughness of short glass fiber-reinforced polyamide 6,6 hybrid composites containing elastomer particles using essential work of fracture concept. Mater Sci Eng A 347:338-345
    • (2003) Mater Sci Eng A , vol.347 , pp. 338-345
    • Tjong, S.C.1    Xu, S.A.2    Mai, Y.W.3
  • 22
    • 33847023032 scopus 로고    scopus 로고
    • Fracture mechanisms and fracture toughness in semicrystalline polymer nanocomposites
    • Cotterell B, Chia JYH, Hbaieb K (2007) Fracture mechanisms and fracture toughness in semicrystalline polymer nanocomposites. Eng Fract Mech 74:1054-1078
    • (2007) Eng Fract Mech , vol.74 , pp. 1054-1078
    • Cotterell, B.1    Chia, J.Y.H.2    Hbaieb, K.3
  • 23
    • 0032103756 scopus 로고    scopus 로고
    • Fracture behaviour of some rubber-toughened nylon 6 blends
    • Kayano Y, Keskkula H, Paul DR (1998) Fracture behaviour of some rubber-toughened nylon 6 blends. Polymer 39:2835-2845
    • (1998) Polymer , vol.39 , pp. 2835-2845
    • Kayano, Y.1    Keskkula, H.2    Paul, D.R.3
  • 24
    • 10444223802 scopus 로고    scopus 로고
    • Application of the essential work of fracture concept to nanostructured polymer materials
    • Lach R, Schneider K, Weidisch R, Janke A, Knoll K (2005) Application of the essential work of fracture concept to nanostructured polymer materials. Eur Polymer J 41(2):383
    • (2005) Eur Polymer J , vol.41 , Issue.2 , pp. 383
    • Lach, R.1    Schneider, K.2    Weidisch, R.3    Janke, A.4    Knoll, K.5
  • 25
    • 80053997240 scopus 로고    scopus 로고
    • Microstructural correlations to micromechanical properties of PA-6/LDPE-g-MA/nanoclay ternary nanocomposites
    • Dayma N, Satapathy BK (2012) Microstructural correlations to micromechanical properties of PA-6/LDPE-g-MA/nanoclay ternary nanocomposites. Mater Des 33:510-522
    • (2012) Mater Des , vol.33 , pp. 510-522
    • Dayma, N.1    Satapathy, B.K.2
  • 26
    • 0026171091 scopus 로고
    • Essential work of fracture and J-integral measurements for ductile polymers
    • Mai YW, Powell P (1991) Essential work of fracture and J-integral measurements for ductile polymers. J Polymer Sci, Part B: Polymer Phys 29:785-793
    • (1991) J Polymer Sci, Part B: Polymer Phys , vol.29 , pp. 785-793
    • Mai, Y.W.1    Powell, P.2
  • 28
    • 0022793082 scopus 로고
    • On the essential work of ductile fracture in polymers
    • Mai YW, Cotterell B (1986) On the essential work of ductile fracture in polymers. Int J Fract 32:105-125
    • (1986) Int J Fract , vol.32 , pp. 105-125
    • Mai, Y.W.1    Cotterell, B.2
  • 29
    • 0041379171 scopus 로고    scopus 로고
    • Work of fracture of high impact polystyrene (HIPS) film under plane stress conditions
    • Hashemi S (2003) Work of fracture of high impact polystyrene (HIPS) film under plane stress conditions. J Mater Sci 38: 3055-3062
    • (2003) J Mater Sci , vol.38 , pp. 3055-3062
    • Hashemi, S.1
  • 30
    • 0001860610 scopus 로고    scopus 로고
    • Deformation mechanisms in rubbertoughened polymers
    • Paul DR, Bucknall CB (eds), 2nd edn. Wiley, New York
    • Bucknall CB (2000) Deformation mechanisms in rubbertoughened polymers. In: Paul DR, Bucknall CB (eds) Polymer blends, vol 2, 2nd edn. Wiley, New York, p 83
    • (2000) Polymer blends , vol.2 , pp. 83
    • Bucknall, C.B.1
  • 31
    • 0021607182 scopus 로고
    • Fracture mechanics of polymers
    • ISBN 0853126852
    • Williams JG (1984) Fracture mechanics of polymers. Halsted, New York. ISBN 0853126852
    • (1984) Halsted, New York
    • Williams, J.G.1
  • 32
    • 0033686701 scopus 로고    scopus 로고
    • Temperature dependence of essential and non-essential work of fracture parameters for polycarbonate films
    • Hashemi S, Williams JG (2000) Temperature dependence of essential and non-essential work of fracture parameters for polycarbonate films. Plast Rubber Compos 29:294-302
    • (2000) Plast Rubber Compos , vol.29 , pp. 294-302
    • Hashemi, S.1    Williams, J.G.2
  • 33
    • 33747168471 scopus 로고    scopus 로고
    • Essential work of fracture and failure mechanisms of polypropylene claynanocomposites
    • Bureau MN, Ton-That MT, Perrin-Sarazin F (2006) Essential work of fracture and failure mechanisms of polypropylene claynanocomposites. Eng Fract Mech 73:2360-2374
    • (2006) Eng Fract Mech , vol.73 , pp. 2360-2374
    • Bureau, M.N.1    Ton-That, M.T.2    Perrin-Sarazin, F.3
  • 34
    • 79951509535 scopus 로고    scopus 로고
    • Effects of unfolded and intercalated halloysites on mechanical properties of halloysite-epoxy nanocomposites
    • Tang Y, Deng S, Ye L, Yang C, Yuan Q, Zhang J, Zhao C (2011) Effects of unfolded and intercalated halloysites on mechanical properties of halloysite-epoxy nanocomposites. Composites: Part A 42:345-354
    • (2011) Composites: Part A , vol.42 , pp. 345-354
    • Tang, Y.1    Deng, S.2    Ye, L.3    Yang, C.4    Yuan, Q.5    Zhang, J.6    Zhao, C.7
  • 35
    • 0034139479 scopus 로고    scopus 로고
    • Influence on nanofillers on the deformation process in layered silicate/polyamide-12 nanocomposites
    • Kim GM, Lee DH, Hoffmann B, Kressler J, Stoppelmann G (2001) Influence on nanofillers on the deformation process in layered silicate/polyamide-12 nanocomposites. Polymer 42:1095-1100
    • (2001) Polymer , vol.42 , pp. 1095-1100
    • Kim, G.M.1    Lee, D.H.2    Hoffmann, B.3    Kressler, J.4    Stoppelmann, G.5
  • 36
    • 84865319517 scopus 로고    scopus 로고
    • Unsaturated polyester-based hybrid nanocomposite: Fracture behavior and tensile properties
    • Ahmadi M, Moghbeli MR, Shokrieh MM (2012) Unsaturated polyester-based hybrid nanocomposite: fracture behavior and tensile properties. J Polymer Res 19:1-12
    • (2012) J Polymer Res , vol.19 , pp. 1-12
    • Ahmadi, M.1    Moghbeli, M.R.2    Shokrieh, M.M.3
  • 37
    • 6344270191 scopus 로고    scopus 로고
    • Morphology and fracture behavior of intercalated epoxy/clay nanocomposites
    • Liu T, Tjiu WC, Tong Y, He C, Goh SS, Chung TS (2004) Morphology and fracture behavior of intercalated epoxy/clay nanocomposites. J Appl Polymer Sci 94:1236-1244
    • (2004) J Appl Polymer Sci , vol.94 , pp. 1236-1244
    • Liu, T.1    Tjiu, W.C.2    Tong, Y.3    He, C.4    Goh, S.S.5    Chung, T.S.6
  • 38
    • 38349045863 scopus 로고    scopus 로고
    • The location and extent of exfoliation of clay on the fracture mechanisms in nylon 66-based ternary nanocomposites
    • Dasari A, Yu ZZ, Mai YW, Yang M (2008) The location and extent of exfoliation of clay on the fracture mechanisms in nylon 66-based ternary nanocomposites. J Nanosci Nanotechnol 8:1901-1912
    • (2008) J Nanosci Nanotechnol , vol.8 , pp. 1901-1912
    • Dasari, A.1    Yu, Z.Z.2    Mai, Y.W.3    Yang, M.4
  • 39
    • 4444247069 scopus 로고    scopus 로고
    • The role of plasticizer on the exfoliation and dispersion and fracture behavior of clay particles in PVC matrix: A comprehensive morphological study
    • Yalcin B, CalmakM (2004) The role of plasticizer on the exfoliation and dispersion and fracture behavior of clay particles in PVC matrix: a comprehensive morphological study. Polymer 45:6623-6638
    • (2004) Polymer , vol.45 , pp. 6623-6638
    • Yalcin, B.1    Calmak, M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.