메뉴 건너뛰기




Volumn 70, Issue 5, 2010, Pages 734-742

Mechanical and fracture properties of ternary PE/PA6/GF composites

Author keywords

A. Hybrid composites; B. Fracture; C. Stress transfer; D. Fractography; E. Annealing; Short fiber reinforced thermoplastic blends

Indexed keywords

A. HYBRID COMPOSITES; C. STRESS TRANSFER; D. FRACTOGRAPHY; HYBRID COMPOSITES; SHORT FIBER; STRESS TRANSFER;

EID: 77950534822     PISSN: 02663538     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.compscitech.2010.01.004     Document Type: Article
Times cited : (18)

References (25)
  • 1
    • 0021936688 scopus 로고
    • Microstructural efficiency and fracture toughness of short fiber/thermoplastic matrix composites
    • Friedrich K. Microstructural efficiency and fracture toughness of short fiber/thermoplastic matrix composites. Compos Sci Technol 1985, 22:43-74.
    • (1985) Compos Sci Technol , vol.22 , pp. 43-74
    • Friedrich, K.1
  • 2
    • 0024135571 scopus 로고
    • Fracture behavior of injection-molded short and long glass fiber-polyamide 6.6 composites
    • Karger-Kocsis J., Friedrich K. Fracture behavior of injection-molded short and long glass fiber-polyamide 6.6 composites. Compos Sci Technol 1988, 32:293-325.
    • (1988) Compos Sci Technol , vol.32 , pp. 293-325
    • Karger-Kocsis, J.1    Friedrich, K.2
  • 3
    • 0027205921 scopus 로고
    • Instrumented impact fracture and related failure behavior in short- and long-glass-fiber-reinforced polypropylene
    • Karger-Kocsis J. Instrumented impact fracture and related failure behavior in short- and long-glass-fiber-reinforced polypropylene. Compos Sci Technol 1993, 48:273-283.
    • (1993) Compos Sci Technol , vol.48 , pp. 273-283
    • Karger-Kocsis, J.1
  • 4
    • 0030395425 scopus 로고    scopus 로고
    • Effects of hydrothermal aging on the fracture and failure behaviour in short glass fiber-reinforced, toughened poly(butylene terephthalate) composites
    • Czigany T., Mohd Ishak Z.A., Heitz T., Karger-Kocsis J. Effects of hydrothermal aging on the fracture and failure behaviour in short glass fiber-reinforced, toughened poly(butylene terephthalate) composites. Polym Compos 1996, 17(6):900-909.
    • (1996) Polym Compos , vol.17 , Issue.6 , pp. 900-909
    • Czigany, T.1    Mohd Ishak, Z.A.2    Heitz, T.3    Karger-Kocsis, J.4
  • 5
    • 0031250554 scopus 로고    scopus 로고
    • Fracture resistance of polyblends and polyblend matrix composites: part I, unreinforced and fiber-reinforced nylon 6,6/ABS polyblends
    • Nair S.V., Wong S-C., Goettler L.A. Fracture resistance of polyblends and polyblend matrix composites: part I, unreinforced and fiber-reinforced nylon 6,6/ABS polyblends. J Mater Sci 1997, 32:5335-5346.
    • (1997) J Mater Sci , vol.32 , pp. 5335-5346
    • Nair, S.V.1    Wong, S.-C.2    Goettler, L.A.3
  • 6
    • 0031247225 scopus 로고    scopus 로고
    • Fracture resistance of polyblends and polyblend matrix composites: part II, role of the rubber phase in nylon 6,6/ABS alloys
    • Nair S.V., Subramaniam A., Goettler L.A. Fracture resistance of polyblends and polyblend matrix composites: part II, role of the rubber phase in nylon 6,6/ABS alloys. J Mater Sci 1997, 32:5347-5354.
    • (1997) J Mater Sci , vol.32 , pp. 5347-5354
    • Nair, S.V.1    Subramaniam, A.2    Goettler, L.A.3
  • 7
    • 0032187166 scopus 로고    scopus 로고
    • Influence of phase microstructure on the mechanical properties of ternary phase polypropylene composites
    • Hornsby P.R., Premphet K. Influence of phase microstructure on the mechanical properties of ternary phase polypropylene composites. J Appl Polym Sci 1998, 70:587-597.
    • (1998) J Appl Polym Sci , vol.70 , pp. 587-597
    • Hornsby, P.R.1    Premphet, K.2
  • 8
    • 0006374856 scopus 로고    scopus 로고
    • Hydrothermal aging and fracture behaviour of short-glass-fiber-reinforced rubber-toughened poly(butylene terephthalate) composites
    • Mohd Ishak Z.A., Ishiaku U.S., Karger-Kocsis J. Hydrothermal aging and fracture behaviour of short-glass-fiber-reinforced rubber-toughened poly(butylene terephthalate) composites. Compos Sci Technol 2000, 60:803-815.
    • (2000) Compos Sci Technol , vol.60 , pp. 803-815
    • Mohd Ishak, Z.A.1    Ishiaku, U.S.2    Karger-Kocsis, J.3
  • 9
    • 0037138327 scopus 로고    scopus 로고
    • Fracture behaviour of rubber-modified injection molded poly(butylene terephthalate) with and without short glass fiber reinforcement
    • Yow B.N., Ishiaku U.S., Mohd Ishak Z.A., Karger-Kocsis J. Fracture behaviour of rubber-modified injection molded poly(butylene terephthalate) with and without short glass fiber reinforcement. J Appl Polym Sci 2002, 84:1233-1244.
    • (2002) J Appl Polym Sci , vol.84 , pp. 1233-1244
    • Yow, B.N.1    Ishiaku, U.S.2    Mohd Ishak, Z.A.3    Karger-Kocsis, J.4
  • 10
    • 0036567564 scopus 로고    scopus 로고
    • Mechanical behaviour and fracture toughness evaluation of maleic anhydride compatibilized short glass fiber/SEBS/polypropylene hybrid composites
    • Tjong S.C., Xu S-A., Li R.K-Y., Mai Y.W. Mechanical behaviour and fracture toughness evaluation of maleic anhydride compatibilized short glass fiber/SEBS/polypropylene hybrid composites. Compos Sci Technol 2002, 62:831-840.
    • (2002) Compos Sci Technol , vol.62 , pp. 831-840
    • Tjong, S.C.1    Xu, S.-A.2    Li, R.K.-Y.3    Mai, Y.W.4
  • 11
    • 0036857783 scopus 로고    scopus 로고
    • Short glass fiber-reinforced polyamide 6,6 composites toughened with maleated SEBS
    • Tjong S.C., Xu S-A., Li R.K-Y., Mai Y-W. Short glass fiber-reinforced polyamide 6,6 composites toughened with maleated SEBS. Compos Sci Technol 2002, 62:2017-2027.
    • (2002) Compos Sci Technol , vol.62 , pp. 2017-2027
    • Tjong, S.C.1    Xu, S.-A.2    Li, R.K.-Y.3    Mai, Y.-W.4
  • 12
    • 0037172872 scopus 로고    scopus 로고
    • Effect of glass fiber surface chemistry on the mechanical properties of glass fiber reinforced, rubber-toughened nylon 6
    • Laura D.M., Keskkula H., Barlow J.W., Paul D.R. Effect of glass fiber surface chemistry on the mechanical properties of glass fiber reinforced, rubber-toughened nylon 6. Polymer 2002, 43:4673-4687.
    • (2002) Polymer , vol.43 , pp. 4673-4687
    • Laura, D.M.1    Keskkula, H.2    Barlow, J.W.3    Paul, D.R.4
  • 13
    • 1542709186 scopus 로고    scopus 로고
    • Essential work of fracture (EWF) analysis for short glass fiber reinforced and rubber toughened nylon-6
    • Ching E.C.Y., Li R.K.-Y., Tjong C.S., Mai Y.-W. Essential work of fracture (EWF) analysis for short glass fiber reinforced and rubber toughened nylon-6. Polym Eng Sci 2003, 43(3):558-569.
    • (2003) Polym Eng Sci , vol.43 , Issue.3 , pp. 558-569
    • Ching, E.C.Y.1    Li, R.K.-Y.2    Tjong, C.S.3    Mai, Y.-W.4
  • 14
    • 77950541951 scopus 로고    scopus 로고
    • Glass fiber reinforced thermoplastic blends. PhD dissertation, Technical University of Delft, Dept Nanostructured Materials, 2628 BL Delft, The Netherlands;
    • Malchev PG. Glass fiber reinforced thermoplastic blends. PhD dissertation, Technical University of Delft, Dept Nanostructured Materials, 2628 BL Delft, The Netherlands; 2008.
    • (2008)
    • Malchev, P.G.1
  • 15
    • 0033076038 scopus 로고    scopus 로고
    • Long fiber reinforcement of polypropilene/polystyrene blends
    • Inberg J.P.F., Hunse P.H., Gaymans R.J. Long fiber reinforcement of polypropilene/polystyrene blends. Polym Eng Sci 1999, 39(2):340-346.
    • (1999) Polym Eng Sci , vol.39 , Issue.2 , pp. 340-346
    • Inberg, J.P.F.1    Hunse, P.H.2    Gaymans, R.J.3
  • 16
    • 0028992115 scopus 로고
    • Fracture toughness and failure mechanisms in unreinforced and long-glass-fiber-reinforced PA66/PP blends
    • Harima T., Friedrich K. Fracture toughness and failure mechanisms in unreinforced and long-glass-fiber-reinforced PA66/PP blends. Compos Sci Technol 1995, 53:423-430.
    • (1995) Compos Sci Technol , vol.53 , pp. 423-430
    • Harima, T.1    Friedrich, K.2
  • 17
    • 0032074687 scopus 로고    scopus 로고
    • Ifluence of weathering on unreinforced and short glass fiber reinforced thermoplastic polyester
    • Choi N.S., Takahashi K., Oschmann D., Karger-Kocsis J., Friedrich K. Ifluence of weathering on unreinforced and short glass fiber reinforced thermoplastic polyester. J Mater Sci 1998, 33:2529-2535.
    • (1998) J Mater Sci , vol.33 , pp. 2529-2535
    • Choi, N.S.1    Takahashi, K.2    Oschmann, D.3    Karger-Kocsis, J.4    Friedrich, K.5
  • 18
    • 0033075294 scopus 로고    scopus 로고
    • Essential fracture work of short fiber reinforced polymer blends
    • Wong S.-C., Mai Y.-M. Essential fracture work of short fiber reinforced polymer blends. Polym Eng Sci 1999, 39(2):356-364.
    • (1999) Polym Eng Sci , vol.39 , Issue.2 , pp. 356-364
    • Wong, S.-C.1    Mai, Y.-M.2
  • 19
    • 28544431608 scopus 로고    scopus 로고
    • Effect of PA6,6/PP ratio on the mechanical properties of short glass fiber reinforced and rubber-toughened polyamide 6,6/polypropylene blends
    • Fu S.-Y., Lauke B., Li R.K,.-Y., Mai Y.-W. Effect of PA6,6/PP ratio on the mechanical properties of short glass fiber reinforced and rubber-toughened polyamide 6,6/polypropylene blends. Composites: Part B 2006, 73:182-190.
    • (2006) Composites: Part B , vol.73 , pp. 182-190
    • Fu, S.-Y.1    Lauke, B.2    Li, R.K.,.-Y.3    Mai, Y.-W.4
  • 20
    • 0034522463 scopus 로고    scopus 로고
    • Interfacial component of glass fiber in ternary composites of GF/PC/PP: effect of the preferential encapsulation of glass fiber
    • Noh C.-H., Yoon B.S., Suh M.H., Lee S.H. Interfacial component of glass fiber in ternary composites of GF/PC/PP: effect of the preferential encapsulation of glass fiber. Polymer 2001, 42:2695-2700.
    • (2001) Polymer , vol.42 , pp. 2695-2700
    • Noh, C.-H.1    Yoon, B.S.2    Suh, M.H.3    Lee, S.H.4
  • 21
    • 17544368575 scopus 로고    scopus 로고
    • Mechanical properties of short fiber reinforced thermoplastic blends
    • Malchev P.G., David C.T., Picken S.J., Gotsis A.D. Mechanical properties of short fiber reinforced thermoplastic blends. Polymer 2005, 46:3895-3905.
    • (2005) Polymer , vol.46 , pp. 3895-3905
    • Malchev, P.G.1    David, C.T.2    Picken, S.J.3    Gotsis, A.D.4
  • 22
    • 34748890121 scopus 로고    scopus 로고
    • Evolution of the morphology and the mechanical properties of ternary PE/PA6/GF composites during annealing
    • Malchev P.G., de Vos G., Norder B., Picken S.J., Gotsis A.D. Evolution of the morphology and the mechanical properties of ternary PE/PA6/GF composites during annealing. Polymer 2007, 48(21):6294-6303.
    • (2007) Polymer , vol.48 , Issue.21 , pp. 6294-6303
    • Malchev, P.G.1    de Vos, G.2    Norder, B.3    Picken, S.J.4    Gotsis, A.D.5
  • 23
    • 35348984864 scopus 로고    scopus 로고
    • The effect of annealing on the melt rheology of ternary PE/PA6/GF composites
    • Malchev P.G., Norder B., Picken S.J., Gotsis A.D. The effect of annealing on the melt rheology of ternary PE/PA6/GF composites. Polymer 2007, 48(23):6834-6842.
    • (2007) Polymer , vol.48 , Issue.23 , pp. 6834-6842
    • Malchev, P.G.1    Norder, B.2    Picken, S.J.3    Gotsis, A.D.4
  • 25
    • 0036465939 scopus 로고    scopus 로고
    • The effect of interface characteristics on the morphology, rheology and thermal behaviour of three-component polymer alloys
    • Fisher I., Siegmann A., Narkis M. The effect of interface characteristics on the morphology, rheology and thermal behaviour of three-component polymer alloys. Polym Compos 2002, 23(1):34-48.
    • (2002) Polym Compos , vol.23 , Issue.1 , pp. 34-48
    • Fisher, I.1    Siegmann, A.2    Narkis, M.3