Metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting

Author keywords

Bending test; Bonding; Co Cr; Metal ceramic; Selective laser melting (Slm); Sem

Indexed keywords

ALLOY; CHROMIUM DERIVATIVE; SILICON;

EID: 84862820519     PISSN: 03005712     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jdent.2012.02.006     Document Type: Article
Times cited : (91)

References (20)
  • 3
    • 77950070633 scopus 로고    scopus 로고
    • A study of the microstructural evolution during selective laser melting of Ti-6Al-4V
    • L. Thijs, F. Verhaeghe, T. Craeghs, J.V. Humbeeck, and J.P. Kruth A study of the microstructural evolution during selective laser melting of Ti-6Al-4V Acta Materialia 58 2010 3303 3312
    • (2010) Acta Materialia , vol.58 , pp. 3303-3312
    • Thijs, L.1    Verhaeghe, F.2    Craeghs, T.3    Humbeeck, J.V.4    Kruth, J.P.5
  • 4
    • 0029355343 scopus 로고
    • Cellular response to metallic ions released from nickel-chromium dental alloys
    • J.D. Bumgardner, and L.C. Lucas Cellular response to metallic ions released from nickel-chromium dental alloys Journal of Dental Research 74 1995 1521 1527
    • (1995) Journal of Dental Research , vol.74 , pp. 1521-1527
    • Bumgardner, J.D.1    Lucas, L.C.2
  • 6
    • 0023967360 scopus 로고
    • Causes of failure following oral rehabilitation: Biological versus technical factors
    • J.R. Strub, S. Stiffler, and P. Scharer Causes of failure following oral rehabilitation: biological versus technical factors Quintessence International 19 1988 215 222
    • (1988) Quintessence International , vol.19 , pp. 215-222
    • Strub, J.R.1    Stiffler, S.2    Scharer, P.3
  • 10
    • 0032009273 scopus 로고    scopus 로고
    • Porcelain adherence vs force to failure for palladium-gallium alloys: A critique of metal-ceramic bond testing
    • E. Papazoglou, and W.A. Brantley Porcelain adherence vs force to failure for palladium-gallium alloys: a critique of metal-ceramic bond testing Dental Materials 14 1998 112 119
    • (1998) Dental Materials , vol.14 , pp. 112-119
    • Papazoglou, E.1    Brantley, W.A.2
  • 11
  • 12
    • 75149145382 scopus 로고    scopus 로고
    • Bond strength and interfacial characterization of eight low fusing porcelains to cp Ti
    • S. Zinelis, X. Barmpagadaki, V. Vergos, M. Chakmakchi, and G. Eliades Bond strength and interfacial characterization of eight low fusing porcelains to cp Ti Dental Materials 26 2010 264 273
    • (2010) Dental Materials , vol.26 , pp. 264-273
    • Zinelis, S.1    Barmpagadaki, X.2    Vergos, V.3    Chakmakchi, M.4    Eliades, G.5
  • 14
    • 79952164265 scopus 로고    scopus 로고
    • Fracture load of titanium crowns coated with gold or titanium nitride and bonded to low-fusing porcelain
    • H.P. Lim, J.H. Kim, K.M. Lee, and S.W. Park Fracture load of titanium crowns coated with gold or titanium nitride and bonded to low-fusing porcelain The Journal of Prosthetic Dentistry 105 2011 164 170
    • (2011) The Journal of Prosthetic Dentistry , vol.105 , pp. 164-170
    • Lim, H.P.1    Kim, J.H.2    Lee, K.M.3    Park, S.W.4
  • 15
    • 0037364451 scopus 로고    scopus 로고
    • Fracture reasons in ceramic-fused-to-metal restorations
    • M. Ozcan Fracture reasons in ceramic-fused-to-metal restorations Journal of Oral Rehabilitation 30 2003 265 269
    • (2003) Journal of Oral Rehabilitation , vol.30 , pp. 265-269
    • Ozcan, M.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.