메뉴 건너뛰기




Volumn 13, Issue 6, 2011, Pages 507-516

Effect of multiple coats of ultra-mild all-in-one adhesives on bond strength to dentin covered with two different smear layer thicknesses

Author keywords

All in one adhesives; Bond strength; Dentin; Microtensile; Smear layer

Indexed keywords

TOOTH CEMENT;

EID: 84857024972     PISSN: 14615185     EISSN: 17579988     Source Type: Journal    
DOI: 10.3290/j.jad.a19814     Document Type: Article
Times cited : (27)

References (38)
  • 2
    • 0036580872 scopus 로고    scopus 로고
    • One-year clinical performance of a self-etching adhesive in class V resin composites cured by two methods
    • Brackett WW, Covey DA, St Germain HA, Jr. One-year clinical performance of a self-etching adhesive in class V resin composites cured by two methods. Oper Dent 2002;27;218-222.
    • (2002) Oper Dent , vol.27 , pp. 218-222
    • Brackett, W.W.1    Covey, D.A.2    St Germain, H.A.3
  • 6
    • 0035462366 scopus 로고    scopus 로고
    • "No-bottle" vs "multibottle" dentin adhesives--a microtensile bond strength and morphological study
    • Frankenberger R, Perdigao J, Rosa BT, Lopes M. "No-bottle" vs "multibottle" dentin adhesives--a microtensile bond strength and morphological study. Dent Mater 2001;17;373-380.
    • (2001) Dent Mater , vol.17 , pp. 373-380
    • Frankenberger, R.1    Perdigao, J.2    Rosa, B.T.3    Lopes, M.4
  • 7
    • 15244345686 scopus 로고    scopus 로고
    • Evidence of chemical bonding to hydroxyapatite by phosphoric acid esters
    • Fu B, Sun X, Qian W, Shen Y, Chen R, Hannig M. Evidence of chemical bonding to hydroxyapatite by phosphoric acid esters. Biomaterials 2005;26;5104-5110.
    • (2005) Biomaterials , vol.26 , pp. 5104-5110
    • Fu, B.1    Sun, X.2    Qian, W.3    Shen, Y.4    Chen, R.5    Hannig, M.6
  • 9
    • 0035379488 scopus 로고    scopus 로고
    • Microtensile bond strength of two single-step adhesive systems to bur-prepared dentin
    • Inoue H, Inoue S, Uno S, Takahashi A, Koase K, Sano H. Microtensile bond strength of two single-step adhesive systems to bur-prepared dentin. J Adhes Dent 2001;3;129-136.
    • (2001) J Adhes Dent , vol.3 , pp. 129-136
    • Inoue, H.1    Inoue, S.2    Uno, S.3    Takahashi, A.4    Koase, K.5    Sano, H.6
  • 14
    • 0035286367 scopus 로고    scopus 로고
    • Bonding to dentin with a self-etching primer: The effect of smear layers
    • Koibuchi H, Yasuda N, Nakabayashi N. Bonding to dentin with a self-etching primer: the effect of smear layers. Dent Mater 2001;17; 122-126.
    • (2001) Dent Mater , vol.17 , pp. 122-126
    • Koibuchi, H.1    Yasuda, N.2    Nakabayashi, N.3
  • 15
  • 18
    • 9644258869 scopus 로고    scopus 로고
    • Spatially resolved photopolymerization kinetics and oxygen inhibition in dental adhesives
    • Nunes TG, Ceballos L, Osorio R, Toledano M. Spatially resolved photopolymerization kinetics and oxygen inhibition in dental adhesives. Biomaterials 2005;26;1809-1817.
    • (2005) Biomaterials , vol.26 , pp. 1809-1817
    • Nunes, T.G.1    Ceballos, L.2    Osorio, R.3    Toledano, M.4
  • 19
    • 0035405652 scopus 로고    scopus 로고
    • Effects of different burs on dentin bond strengths of self-etching primer bonding systems
    • Ogata M, Harada N, Yamaguchi S, Nakajima M, Pereira PN, Tagami J. Effects of different burs on dentin bond strengths of self-etching primer bonding systems. Oper Dent 2001;26;375-382.
    • (2001) Oper Dent , vol.26 , pp. 375-382
    • Ogata, M.1    Harada, N.2    Yamaguchi, S.3    Nakajima, M.4    Pereira, P.N.5    Tagami, J.6
  • 21
    • 0035463789 scopus 로고    scopus 로고
    • Aggressiveness of contemporary self-etching adhesives. Part II: Etching effects on unground enamel
    • Pashley DH, Tay FR. Aggressiveness of contemporary self-etching adhesives. Part II: etching effects on unground enamel. Dent Mater 2001;17;430-444.
    • (2001) Dent Mater , vol.17 , pp. 430-444
    • Pashley, D.H.1    Tay, F.R.2
  • 22
    • 0036479738 scopus 로고    scopus 로고
    • Effects of one versus two applications of an unfilled, all-in-one adhesive on dentine bonding
    • Pashley EL, Agee KA, Pashley DH, Tay FR. Effects of one versus two applications of an unfilled, all-in-one adhesive on dentine bonding. J Dent 2002;30;83-90.
    • (2002) J Dent , vol.30 , pp. 83-90
    • Pashley, E.L.1    Agee, K.A.2    Pashley, D.H.3    Tay, F.R.4
  • 23
    • 0036366708 scopus 로고    scopus 로고
    • In vivo influence of residual moisture on microtensile bond strengths of one-bottle adhesives
    • Perdigao J, Geraldeli S, Carmo AR, Dutra HR. In vivo influence of residual moisture on microtensile bond strengths of one-bottle adhesives. J Esthet Restor Dent 2002;14;31-38.
    • (2002) J Esthet Restor Dent , vol.14 , pp. 31-38
    • Perdigao, J.1    Geraldeli, S.2    Carmo, A.R.3    Dutra, H.R.4
  • 24
    • 0032175779 scopus 로고    scopus 로고
    • Influence of different etching times on hybrid layer formation and tensile bond strength
    • Pioch T, Stotz S, Buff E, Duschner H, Staehle HJ. Influence of different etching times on hybrid layer formation and tensile bond strength. Am J Dent 1998;11;202-206.
    • (1998) Am J Dent , vol.11 , pp. 202-206
    • Pioch, T.1    Stotz, S.2    Buff, E.3    Duschner, H.4    Staehle, H.J.5
  • 25
    • 0032109479 scopus 로고    scopus 로고
    • Resin-infiltrated dentin layer formation of new bonding systems
    • Prati C, Chersoni S, Mongiorgi R, Pashley DH. Resin-infiltrated dentin layer formation of new bonding systems. Oper Dent 1998;23;185-194.
    • (1998) Oper Dent , vol.23 , pp. 185-194
    • Prati, C.1    Chersoni, S.2    Mongiorgi, R.3    Pashley, D.H.4
  • 27
    • 0038655298 scopus 로고    scopus 로고
    • Effect of smear layer thickness on bond strength mediated by three all-in-one self-etching priming adhesives
    • Tani C, Finger WJ. Effect of smear layer thickness on bond strength mediated by three all-in-one self-etching priming adhesives. J Adhes Dent 2002;4;283-289.
    • (2002) J Adhes Dent , vol.4 , pp. 283-289
    • Tani, C.1    Finger, W.J.2
  • 28
    • 0035405736 scopus 로고    scopus 로고
    • Aggressiveness of contemporary self-etching systems. I: Depth of penetration beyond dentin smear layers
    • Tay FR, Pashley DH. Aggressiveness of contemporary self-etching systems. I: Depth of penetration beyond dentin smear layers. Dent Mater 2001;17;296-308.
    • (2001) Dent Mater , vol.17 , pp. 296-308
    • Tay, F.R.1    Pashley, D.H.2
  • 29
    • 0642275700 scopus 로고    scopus 로고
    • Have dentin adhesives become too hydrophilic?
    • Tay FR, Pashley DH. Have dentin adhesives become too hydrophilic? J Can Dent Assoc, 2003;69;726-731.
    • (2003) J Can Dent Assoc , vol.69 , pp. 726-731
    • Tay, F.R.1    Pashley, D.H.2
  • 30
    • 0034208769 scopus 로고    scopus 로고
    • Effect of smear layers on the bonding of a self-etching primer to dentin
    • Tay FR, Carvalho R, Sano H, Pashley DH. Effect of smear layers on the bonding of a self-etching primer to dentin. J Adhes Dent 2000;2; 99-116.
    • (2000) J Adhes Dent , vol.2 , pp. 99-116
    • Tay, F.R.1    Carvalho, R.2    Sano, H.3    Pashley, D.H.4
  • 31
    • 0034208378 scopus 로고    scopus 로고
    • An ultrastructural study of the influence of acidity of self-etching primers and smear layer thickness on bonding to intact dentin
    • Tay FR, Sano H, Carvalho R, Pashley EL, Pashley DH. An ultrastructural study of the influence of acidity of self-etching primers and smear layer thickness on bonding to intact dentin. J Adhes Dent 2000;2;83-98.
    • (2000) J Adhes Dent , vol.2 , pp. 83-98
    • Tay, F.R.1    Sano, H.2    Carvalho, R.3    Pashley, E.L.4    Pashley, D.H.5
  • 33
    • 3342886383 scopus 로고    scopus 로고
    • Durability of three simplified adhesive systems in Class V non-carious cervical dentin lesions
    • van Dijken JW. Durability of three simplified adhesive systems in Class V non-carious cervical dentin lesions. Am J Dent 2004;17;27-32.
    • (2004) Am J Dent , vol.17 , pp. 27-32
    • van Dijken, J.W.1
  • 38
    • 46049111485 scopus 로고    scopus 로고
    • Effect of dentinal surface preparation on bond strength of self-etching adhesives
    • Yiu CK, Hiraishi N, King NM, Tay FR. Effect of dentinal surface preparation on bond strength of self-etching adhesives. J Adhes Dent 2008;10;173-182.
    • (2008) J Adhes Dent , vol.10 , pp. 173-182
    • Yiu, C.K.1    Hiraishi, N.2    King, N.M.3    Tay, F.R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.