Volumn 36, Issue , 2012, Pages 289-295

Mechanical properties and microstructure of 3D orthogonal quartz fiber reinforced silica composites fabricated by silicasol-infiltration-sintering

Author keywords

A. Ceramic matrix composites; E. Mechanical; F. Microstructure

Indexed keywords

3D ORTHOGONAL; AVERAGE VALUES; CRACK DEFLECTIONS; CRISTOBALITES; DAMAGE FEATURES; E. MECHANICAL; F. MICROSTRUCTURE; FIBER PULL OUT; FLEXURAL LOADING; FLEXURE STRENGTH; FRACTURE SURFACES; LONG FIBER; LOW TEMPERATURES; MATRIX CRACK; PROPERTIES AND MICROSTRUCTURES; QUARTZ FIBERS; ROOM TEMPERATURE; SHEAR LOADINGS; SILICA COMPOSITES; WEAK INTERFACE;

EID: 84855410627     PISSN: 02641275     EISSN: 18734197     Source Type: Journal    
DOI: 10.1016/j.matdes.2011.11.022     Document Type: Article
Times cited : (49)

References (33)
  • 2
    • 77956176793 scopus 로고    scopus 로고
    • Interfacial microstructure and mechanical properties of joining electroless nickel plated quartz fibers reinforced silica composite to invar
    • Zhao L., Zhang L.X., Tian X.Y., He P., Feng J.C. Interfacial microstructure and mechanical properties of joining electroless nickel plated quartz fibers reinforced silica composite to invar. Mater Des 2011, 32:382-387.
    • (2011) Mater Des , vol.32 , pp. 382-387
    • Zhao, L.1    Zhang, L.X.2    Tian, X.Y.3    He, P.4    Feng, J.C.5
  • 3
    • 0031630327 scopus 로고    scopus 로고
    • The design of the fibre-matrix interfacial zone in ceramic matrix composites
    • Naslain R.R. The design of the fibre-matrix interfacial zone in ceramic matrix composites. Composites Part A 1998, 29A:1145-1155.
    • (1998) Composites Part A , vol.29 A , pp. 1145-1155
    • Naslain, R.R.1
  • 4
    • 33947370306 scopus 로고    scopus 로고
    • High strength three-dimensional silica fiber reinforced silicon nitride-based composites via polyhydridomethylsilazane pyrolysis
    • Qi G.J., Zhang C.R., Hu H.F. High strength three-dimensional silica fiber reinforced silicon nitride-based composites via polyhydridomethylsilazane pyrolysis. Ceram Int 2007, 33:891-894.
    • (2007) Ceram Int , vol.33 , pp. 891-894
    • Qi, G.J.1    Zhang, C.R.2    Hu, H.F.3
  • 5
    • 50249116191 scopus 로고    scopus 로고
    • Manufacturing of weft-knitted fabric reinforced composite materials: a review
    • Pamuk G., Ceken F. Manufacturing of weft-knitted fabric reinforced composite materials: a review. Mater Manuf Process 2008, 23:635-640.
    • (2008) Mater Manuf Process , vol.23 , pp. 635-640
    • Pamuk, G.1    Ceken, F.2
  • 6
    • 53349162985 scopus 로고    scopus 로고
    • Microstructures and mechanical properties of a low-cost three-dimensional needled carbon/silicon carbide composite
    • Cai Y.Z., Xu Y.D., Li B., Fan S.W., Zhang L.T., Cheng L.F., et al. Microstructures and mechanical properties of a low-cost three-dimensional needled carbon/silicon carbide composite. Mater Sci Eng A 2008, 497:278-282.
    • (2008) Mater Sci Eng A , vol.497 , pp. 278-282
    • Cai, Y.Z.1    Xu, Y.D.2    Li, B.3    Fan, S.W.4    Zhang, L.T.5    Cheng, L.F.6
  • 7
    • 62949215509 scopus 로고    scopus 로고
    • Effects of ablation at different regions in three-dimensional orthogonal C/SiC composites ablated by oxyacetylene torch at 1800°C
    • Yan B., Chen Z.F., Zhu J.X., Zhang J.Z., Jiang Y. Effects of ablation at different regions in three-dimensional orthogonal C/SiC composites ablated by oxyacetylene torch at 1800°C. J Mater Process Technol 2009, 209(7):3438-3443.
    • (2009) J Mater Process Technol , vol.209 , Issue.7 , pp. 3438-3443
    • Yan, B.1    Chen, Z.F.2    Zhu, J.X.3    Zhang, J.Z.4    Jiang, Y.5
  • 8
    • 77957020260 scopus 로고    scopus 로고
    • Fatigue behavior of non-crimp 3D orthogonal weave and multi-layer plain weave E-glass reinforced composites
    • Carvelli V., Gramellini G., Lomov S.V., Bogdanovich A.E., Mungalov D.D., Verpoest I. Fatigue behavior of non-crimp 3D orthogonal weave and multi-layer plain weave E-glass reinforced composites. Compos Sci Technol 2010, 70(14):2068-2076.
    • (2010) Compos Sci Technol , vol.70 , Issue.14 , pp. 2068-2076
    • Carvelli, V.1    Gramellini, G.2    Lomov, S.V.3    Bogdanovich, A.E.4    Mungalov, D.D.5    Verpoest, I.6
  • 9
    • 42249113316 scopus 로고    scopus 로고
    • Modeling and experimental verification of dielectric constant for three-dimensional woven composites
    • Yao L., Wang X., Liang F., Wu R., Hu B., Feng Y.N., et al. Modeling and experimental verification of dielectric constant for three-dimensional woven composites. Compos Sci Technol 2008, 68:1794-1799.
    • (2008) Compos Sci Technol , vol.68 , pp. 1794-1799
    • Yao, L.1    Wang, X.2    Liang, F.3    Wu, R.4    Hu, B.5    Feng, Y.N.6
  • 11
  • 12
    • 0035427190 scopus 로고    scopus 로고
    • Infiltration processing of fiber reinforced composites: governing phenomena
    • Michaud V., Mortensen A. Infiltration processing of fiber reinforced composites: governing phenomena. Composites Part A 2001, 32:981-996.
    • (2001) Composites Part A , vol.32 , pp. 981-996
    • Michaud, V.1    Mortensen, A.2
  • 13
    • 84903333813 scopus 로고    scopus 로고
    • ASTM International. ASTM C1341 - 06. Standard test method for flexural properties of continuous fiber-reinforced advanced ceramic composites
    • ASTM International. ASTM C1341 - 06. Standard test method for flexural properties of continuous fiber-reinforced advanced ceramic composites. American Society for Testing and Materials; 2006.
    • (2006) American Society for Testing and Materials.
  • 14
    • 0003890882 scopus 로고    scopus 로고
    • ASTM International. ASTM D5379 - 05. Standard test method for shear properties of composite materials by the V-notched beam method
    • ASTM International. ASTM D5379 - 05. Standard test method for shear properties of composite materials by the V-notched beam method. American Society for Testing and Materials; 2005.
    • (2005) American Society for Testing and Materials.
  • 16
    • 33748294160 scopus 로고    scopus 로고
    • Continuous silica fiber reinforced silica composites densified by polymer-derived silicon nitride: mechanical properties
    • Qi G.J., Zhang C.R., Hu H.F. Continuous silica fiber reinforced silica composites densified by polymer-derived silicon nitride: mechanical properties. J Non-Cryst Solids 2006, 352:3794-3798.
    • (2006) J Non-Cryst Solids , vol.352 , pp. 3794-3798
    • Qi, G.J.1    Zhang, C.R.2    Hu, H.F.3
  • 17
    • 0346606786 scopus 로고    scopus 로고
    • Materials design and processing of high temperature ceramic matrix composites: state of the art and future trends
    • Naslain R. Materials design and processing of high temperature ceramic matrix composites: state of the art and future trends. Adv Compos Mater 1999, 8(1):3-16.
    • (1999) Adv Compos Mater , vol.8 , Issue.1 , pp. 3-16
    • Naslain, R.1
  • 18
    • 0348013351 scopus 로고    scopus 로고
    • Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview
    • Naslain R. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview. Compos Sci Technol 2004, 64(2):155-170.
    • (2004) Compos Sci Technol , vol.64 , Issue.2 , pp. 155-170
    • Naslain, R.1
  • 20
    • 0025521737 scopus 로고
    • Crack stability in simply supported four-point and three-point loaded beams of brittle materials
    • Baratta F.I., Dunlay W.A. Crack stability in simply supported four-point and three-point loaded beams of brittle materials. Mech Mater 1990, 10:149-159.
    • (1990) Mech Mater , vol.10 , pp. 149-159
    • Baratta, F.I.1    Dunlay, W.A.2
  • 21
    • 0030242990 scopus 로고    scopus 로고
    • Crack stability and its effect on fracture toughness of hot pressed silicon nitride beam specimens
    • Bar-On I., Baratta F.I., Cho K. Crack stability and its effect on fracture toughness of hot pressed silicon nitride beam specimens. J Am Ceram Soc 1996, 79:2300-2308.
    • (1996) J Am Ceram Soc , vol.79 , pp. 2300-2308
    • Bar-On, I.1    Baratta, F.I.2    Cho, K.3
  • 22
    • 0042132063 scopus 로고    scopus 로고
    • Fracture toughness of ceramics and ceramic composites
    • Gogotsi G.A. Fracture toughness of ceramics and ceramic composites. Ceram Int 2003, 29:777-784.
    • (2003) Ceram Int , vol.29 , pp. 777-784
    • Gogotsi, G.A.1
  • 23
    • 0000193476 scopus 로고    scopus 로고
    • Critical notch-root radius effect in SENB-S fracture toughness testing
    • Damani R., Gstrain R., Danzer R. Critical notch-root radius effect in SENB-S fracture toughness testing. J Eur Ceram Soc 1996, 16:695-702.
    • (1996) J Eur Ceram Soc , vol.16 , pp. 695-702
    • Damani, R.1    Gstrain, R.2    Danzer, R.3
  • 24
    • 84903346556 scopus 로고    scopus 로고
    • ASTM International. ASTM C1421 - 01b. Standard test methods for determination of fracture toughness of advanced ceramics at ambient temperature
    • ASTM International. ASTM C1421 - 01b. Standard test methods for determination of fracture toughness of advanced ceramics at ambient temperature. American Society for Testing and Materials; 2007.
    • (2007) American Society for Testing and Materials.
  • 26
    • 3042627463 scopus 로고    scopus 로고
    • Fracture behaviour of 2D-weaved, silica-silica continuous fibre-reinforced, ceramic-matrix composites (CFCCs)
    • Prasad N.E., Kumari S., Kamat S.V., Vijayakumar M., Malakondaiah G. Fracture behaviour of 2D-weaved, silica-silica continuous fibre-reinforced, ceramic-matrix composites (CFCCs). Eng Fract Mech 2004, 71:2589-2605.
    • (2004) Eng Fract Mech , vol.71 , pp. 2589-2605
    • Prasad, N.E.1    Kumari, S.2    Kamat, S.V.3    Vijayakumar, M.4    Malakondaiah, G.5
  • 27
    • 0346409067 scopus 로고    scopus 로고
    • The importance of damage and slow crack growth in the creep behavior of ceramic matrix composites
    • Chermant J.L., Boitier G. The importance of damage and slow crack growth in the creep behavior of ceramic matrix composites. Adv Compos Mater 1999, 8:77-85.
    • (1999) Adv Compos Mater , vol.8 , pp. 77-85
    • Chermant, J.L.1    Boitier, G.2
  • 28
    • 0343006660 scopus 로고    scopus 로고
    • The influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites
    • Carrere N., Martin E., Lamon J. The influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites. Composites Part A 2000, 31:1179-1190.
    • (2000) Composites Part A , vol.31 , pp. 1179-1190
    • Carrere, N.1    Martin, E.2    Lamon, J.3
  • 29
    • 0032584519 scopus 로고    scopus 로고
    • Conditions for matrix crack deflection at an interface in ceramic matrix composites
    • Martin E., Peters P.W.M., Leguillon D., Quenisset J.M. Conditions for matrix crack deflection at an interface in ceramic matrix composites. Mater Sci Eng A 1998, 250:291-302.
    • (1998) Mater Sci Eng A , vol.250 , pp. 291-302
    • Martin, E.1    Peters, P.W.M.2    Leguillon, D.3    Quenisset, J.M.4
  • 30
    • 0032214103 scopus 로고    scopus 로고
    • Criteria for crack deflection/penetration criteria for fiber-reinforced ceramic matrix composites
    • Ahn B.K., Curtin W.A., Parthasarathy T.A., Dutton R.E. Criteria for crack deflection/penetration criteria for fiber-reinforced ceramic matrix composites. Compos Sci Technol 1998, 58:1775-1784.
    • (1998) Compos Sci Technol , vol.58 , pp. 1775-1784
    • Ahn, B.K.1    Curtin, W.A.2    Parthasarathy, T.A.3    Dutton, R.E.4
  • 31
    • 70349208817 scopus 로고    scopus 로고
    • Sol-gel approach to near-net-shape oxide-oxide composites reinforced with short alumina fibres - the effect of crystallization
    • Naskar M.K., Basu K., Chatterjee M. Sol-gel approach to near-net-shape oxide-oxide composites reinforced with short alumina fibres - the effect of crystallization. Ceram Int 2009, 35:3073-3079.
    • (2009) Ceram Int , vol.35 , pp. 3073-3079
    • Naskar, M.K.1    Basu, K.2    Chatterjee, M.3
  • 32
    • 77953963245 scopus 로고    scopus 로고
    • Microstructural evolution of coating-modified 3D C/SiC composites after annealing in wet oxygen at different temperatures
    • Li S.W., Feng Z.D., Liu Y.S., Yang W.B., Zhang W.H., Cheng L.F., et al. Microstructural evolution of coating-modified 3D C/SiC composites after annealing in wet oxygen at different temperatures. Corros Sci 2010, 52:2837-2845.
    • (2010) Corros Sci , vol.52 , pp. 2837-2845
    • Li, S.W.1    Feng, Z.D.2    Liu, Y.S.3    Yang, W.B.4    Zhang, W.H.5    Cheng, L.F.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.