Influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites

Author keywords

[No Author keywords available]

Indexed keywords

CRACK INITIATION; CRACK PROPAGATION; FINITE ELEMENT METHOD; INTERFACES (MATERIALS); MATHEMATICAL MODELS; SILICON CARBIDE; TOUGHNESS;

EID: 0343006660     PISSN: 1359835X     EISSN: None     Source Type: Journal    
DOI: 10.1016/S1359-835X(00)00095-6     Document Type: Article
Times cited : (110)

References (47)
  • 1
    • 19944374295 scopus 로고
    • Fibre matrix interphases and interfaces in ceramic matrix composites processed by CVI
    • Naslain R. Fibre matrix interphases and interfaces in ceramic matrix composites processed by CVI. Composite Interface. 1:1993;253-286.
    • (1993) Composite Interface , vol.1 , pp. 253-286
    • Naslain, R.1
  • 2
    • 0025844350 scopus 로고
    • The role of the interface in fiber reinforced brittle matrix
    • Evans A.G., Zok F.W., Davis J.B. The role of the interface in fiber reinforced brittle matrix. Composite Sci Technol. 42:1991;3-24.
    • (1991) Composite Sci Technol , vol.42 , pp. 3-24
    • Evans, A.G.1    Zok, F.W.2    Davis, J.B.3
  • 4
    • 0001129288 scopus 로고    scopus 로고
    • Fracture statistics applied to modelling the nonlinear stress strain behaviour in microcomposites: Influence of interfacial parameters
    • Guillaumat L., Lamon J. Fracture statistics applied to modelling the nonlinear stress strain behaviour in microcomposites: influence of interfacial parameters. Int J Fract. 82:1996;297-316.
    • (1996) Int J Fract , vol.82 , pp. 297-316
    • Guillaumat, L.1    Lamon, J.2
  • 5
    • 0030127397 scopus 로고    scopus 로고
    • Fracture toughness of 2-D woven SiC/SiC CVI-composites with multilayered interphases
    • Droillard C., Lamon J. Fracture toughness of 2-D woven SiC/SiC CVI-composites with multilayered interphases. J Am Ceram Soc. 79:1996;849-858.
    • (1996) J Am Ceram Soc , vol.79 , pp. 849-858
    • Droillard, C.1    Lamon, J.2
  • 6
    • 0029179546 scopus 로고
    • Strong interfaces in CMCS, a condition for efficient multilayered interphases
    • Droillard C., Lamon J., Bourrat X. Strong interfaces in CMCS, a condition for efficient multilayered interphases. Mat Res Soc Symp Proc. 365:1995;371-376.
    • (1995) Mat Res Soc Symp Proc , vol.365 , pp. 371-376
    • Droillard, C.1    Lamon, J.2    Bourrat, X.3
  • 7
    • 0032667825 scopus 로고    scopus 로고
    • Crack deflection in ceramic composites and fiber coating design criteria
    • Kerans R.J., Parthasaraty T.A. Crack deflection in ceramic composites and fiber coating design criteria. Composites Part A. 30:1999;521-524.
    • (1999) Composites Part a , vol.30 , pp. 521-524
    • Kerans, R.J.1    Parthasaraty, T.A.2
  • 8
    • 0032047739 scopus 로고    scopus 로고
    • Interfacial bond strength in Nicalon/C/SiC composites materials as studied by single fiber push-out tests
    • Rebillat F., Lamon J., Naslain R., Lara-curzio E., Ferber M.K., Besman T.M. Interfacial bond strength in Nicalon/C/SiC composites materials as studied by single fiber push-out tests. J Am Ceram Soc. 81:(4):1998;965-978.
    • (1998) J Am Ceram Soc , vol.81 , Issue.4 , pp. 965-978
    • Rebillat, F.1    Lamon, J.2    Naslain, R.3    Lara-Curzio, E.4    Ferber, M.K.5    Besman, T.M.6
  • 9
    • 0031094846 scopus 로고    scopus 로고
    • Damage and failure in ceramic matrix minicomposites: Experimental study and model
    • Lissart N., Lamon J. Damage and failure in ceramic matrix minicomposites: experimental study and model. Acta Mater. 45:(3):1997;1025-1044.
    • (1997) Acta Mater , vol.45 , Issue.3 , pp. 1025-1044
    • Lissart, N.1    Lamon, J.2
  • 10
    • 0031645590 scopus 로고    scopus 로고
    • Tensile static fatigue of 2D SiC/SiC composites with multilayered (PyC/SiC)n interphases at high temperatures in oxidizing atmosphere
    • Pasquier S., Lamon J., Naslain R. Tensile static fatigue of 2D SiC/SiC composites with multilayered (PyC/SiC)n interphases at high temperatures in oxidizing atmosphere. Composites Part A. 29:1998;1157-1164.
    • (1998) Composites Part a , vol.29 , pp. 1157-1164
    • Pasquier, S.1    Lamon, J.2    Naslain, R.3
  • 11
    • 85031557168 scopus 로고    scopus 로고
    • Influence of strong fiber-coating interfaces on the mechanical behavior and lifetime of Hi-Nicalon/(PyC-SiC)n/SiC minicomposites
    • (in press)
    • Bertrand S., Pailler R., Lamon J. Influence of strong fiber-coating interfaces on the mechanical behavior and lifetime of Hi-Nicalon/(PyC-SiC)n/SiC minicomposites. J Am Ceram Soc. 2000;. (in press).
    • (2000) J Am Ceram Soc
    • Bertrand, S.1    Pailler, R.2    Lamon, J.3
  • 12
    • 0032707239 scopus 로고    scopus 로고
    • Interfacial behavior during creep of microcomposites at elevated temperatures
    • Rugg K.L., Tressler R.E., Lamon J. Interfacial behavior during creep of microcomposites at elevated temperatures. J Eur Ceram Soc. 19:1999;2297-2303.
    • (1999) J Eur Ceram Soc , vol.19 , pp. 2297-2303
    • Rugg, K.L.1    Tressler, R.E.2    Lamon, J.3
  • 13
    • 0024884622 scopus 로고
    • Crack deflection at an interface between dissimilar elastic materials
    • He M.Y., Hutchinson J.W. Crack deflection at an interface between dissimilar elastic materials. Int J Solid Struct. 25:1989;1053-1067.
    • (1989) Int J Solid Struct , vol.25 , pp. 1053-1067
    • He, M.Y.1    Hutchinson, J.W.2
  • 14
    • 0026407057 scopus 로고
    • A micromechanics analysis of cracks in unidirectional fiber composites
    • Ahmad J. A micromechanics analysis of cracks in unidirectional fiber composites. J Appl Mech. 58:1991;964-972.
    • (1991) J Appl Mech , vol.58 , pp. 964-972
    • Ahmad, J.1
  • 15
    • 0027039837 scopus 로고
    • Crack growth at interfaces in bimaterial systems and composites
    • Popejoy D.B., Dharani L.R., Tang H. Crack growth at interfaces in bimaterial systems and composites. Int J Solids Struct. 29:(24):1992;3113-3123.
    • (1992) Int J Solids Struct , vol.29 , Issue.24 , pp. 3113-3123
    • Popejoy, D.B.1    Dharani, L.R.2    Tang, H.3
  • 16
    • 0001791973 scopus 로고
    • Crack deflection at an interface between two orthotropic media
    • Gupta V., Argon A.S., Suo Z. Crack deflection at an interface between two orthotropic media. J Appl Mech. 59:1992;79-87.
    • (1992) J Appl Mech , vol.59 , pp. 79-87
    • Gupta, V.1    Argon, A.S.2    Suo, Z.3
  • 17
    • 0028485551 scopus 로고
    • Energy criterium for crack deflection at an interface between two orthotropic media
    • Martinez D., Gupta V. Energy criterium for crack deflection at an interface between two orthotropic media. J Mech Phys Solids. 42:1994;1247-1271.
    • (1994) J Mech Phys Solids , vol.42 , pp. 1247-1271
    • Martinez, D.1    Gupta, V.2
  • 18
    • 0028730620 scopus 로고
    • Crack deflection at an interface between dissimilar elastic materials: Role of residual stresses
    • He M.Y., Evans A.G., Hutchinson J.W. Crack deflection at an interface between dissimilar elastic materials: role of residual stresses. Int J Solids Struct. 31:1994;3443-3455.
    • (1994) Int J Solids Struct , vol.31 , pp. 3443-3455
    • He, M.Y.1    Evans, A.G.2    Hutchinson, J.W.3
  • 19
    • 0028500423 scopus 로고
    • Deflection and penetration of cracks at an interface between two dissimilar materials
    • Tullock D.L., Reimanis I.E., Graham A.L., Petrovic J.J. Deflection and penetration of cracks at an interface between two dissimilar materials. Acta Metall Mater. 42:1994;3245-3252.
    • (1994) Acta Metall Mater , vol.42 , pp. 3245-3252
    • Tullock, D.L.1    Reimanis, I.E.2    Graham, A.L.3    Petrovic, J.J.4
  • 20
    • 0029273504 scopus 로고
    • The effect of flaws on the propagation of cracks at bi-material interfaces
    • Mammoli A.A., Graham; A.L., Reimanis I.E., Tullock D.L. The effect of flaws on the propagation of cracks at bi-material interfaces. Acta Metall Mater. 43:(3):1995;1149-1156.
    • (1995) Acta Metall Mater , vol.43 , Issue.3 , pp. 1149-1156
    • Mammoli, A.A.1    Graham, A.L.2    Reimanis, I.E.3    Tullock, D.L.4
  • 21
    • 0032214103 scopus 로고    scopus 로고
    • Criteria for crack deflection/penetration for fiber-reinforced ceramic matrix composites
    • Ahn B.K., Curtin W.A., Parthasaraty T.A., Dutton R.E. Criteria for crack deflection/penetration for fiber-reinforced ceramic matrix composites. Comp Sci and Technology. 59:1998;1775-1784.
    • (1998) Comp Sci and Technology , vol.59 , pp. 1775-1784
    • Ahn, B.K.1    Curtin, W.A.2    Parthasaraty, T.A.3    Dutton, R.E.4
  • 22
    • 0030270440 scopus 로고    scopus 로고
    • Growth of interface defects and its effects on crack deflection and toughening criteria
    • Lee W., Howard S.J., Clegg W.J. Growth of interface defects and its effects on crack deflection and toughening criteria. Acta Metall Mater. 44:(10):1996;3905-3922.
    • (1996) Acta Metall Mater , vol.44 , Issue.10 , pp. 3905-3922
    • Lee, W.1    Howard, S.J.2    Clegg, W.J.3
  • 23
    • 0032073548 scopus 로고    scopus 로고
    • Single and double deflections of cracks at the carbon-carbon/BN coating interfaces in ceramic-matrix composites
    • Kumar S., Singh R.N. Single and double deflections of cracks at the carbon-carbon/BN coating interfaces in ceramic-matrix composites. J Am Ceram Soc. 81:(5):1998;1329-1338.
    • (1998) J Am Ceram Soc , vol.81 , Issue.5 , pp. 1329-1338
    • Kumar, S.1    Singh, R.N.2
  • 24
    • 5244380008 scopus 로고
    • Microtextures of interfaces related to mechanical properties in ceramic fiber reinforced ceramic matrix composites
    • In: Bunsell AR, Jamet JF, Massiah A, editors EACM, Bordeaux, France
    • Monthioux M, Cojean D. Microtextures of interfaces related to mechanical properties in ceramic fiber reinforced ceramic matrix composites. In: Bunsell AR, Jamet JF, Massiah A, editors. Proceedings of the 5th European conference on composite materials (ECCM-5). EACM, Bordeaux, France, 1992. p. 729-34.
    • (1992) Proceedings of the 5th European Conference on Composite Materials , vol.ECCM-5 , pp. 729-734
    • Monthioux, M.1    Cojean, D.2
  • 25
    • 85031559282 scopus 로고    scopus 로고
    • Properties of multilayered interphases in SiC/SiC CVI composites with "weak" and "strong" interfaces
    • (in press)
    • Rebillat F., Lamon J., Naslain R., Lara-curzio E., Ferber M.K., Besman T.M. Properties of multilayered interphases in SiC/SiC CVI composites with "weak" and "strong" interfaces. J Am Ceram Soc. 2000;. (in press).
    • (2000) J Am Ceram Soc
    • Rebillat, F.1    Lamon, J.2    Naslain, R.3    Lara-Curzio, E.4    Ferber, M.K.5    Besman, T.M.6
  • 26
    • 0029780161 scopus 로고    scopus 로고
    • Effect of interfacial strength on crack-fiber interaction behavior in ceramic matrix composites
    • Kumaria S., Singh R.N. Effect of interfacial strength on crack-fiber interaction behavior in ceramic matrix composites. J Am Ceram Soc. 79:(1):1996;199-208.
    • (1996) J Am Ceram Soc , vol.79 , Issue.1 , pp. 199-208
    • Kumaria, S.1    Singh, R.N.2
  • 29
    • 0026745262 scopus 로고
    • Matrix crack initiation in ceramic matrix composites Part II : Models and simulation results
    • Wang A.S.D., Huang X.G., Barsoum M.W. Matrix crack initiation in ceramic matrix composites Part II : Models and simulation results. Composite Sci Tech. 44:1992;271-282.
    • (1992) Composite Sci Tech , vol.44 , pp. 271-282
    • Wang, A.S.D.1    Huang, X.G.2    Barsoum, M.W.3
  • 31
    • 0002472599 scopus 로고    scopus 로고
    • Asymptotic analysis of a spontaneous crack growth. Application to a blunt crack
    • D. Durban, & J.R.A. Pearson. Dordrecht: Kluwer Academic
    • Leguillon D. Asymptotic analysis of a spontaneous crack growth. Application to a blunt crack. Durban D., Pearson J.R.A. Proc. IUTAM Symposium on non-linear singularities in deformation and flow. 1999;169-180 Kluwer Academic, Dordrecht.
    • (1999) Proc. IUTAM Symposium on Non-linear Singularities in Deformation and Flow , pp. 169-180
    • Leguillon, D.1
  • 33
    • 0018047794 scopus 로고
    • On the problem of crack extension in brittle solids under general loading
    • S. Nemat-Nasser. New York: Pergamon Press
    • Palaniswamy K., Knauss W.G. On the problem of crack extension in brittle solids under general loading. Nemat-Nasser S. Mechanics Today. 1978;87-145 Pergamon Press, New York.
    • (1978) Mechanics Today , pp. 87-145
    • Palaniswamy, K.1    Knauss, W.G.2
  • 34
    • 0029251147 scopus 로고
    • Microcomposite test procedure for evaluating the interface properties of ceramic matrix composites
    • Lamon J., Rebillat F., Evans A.G. Microcomposite test procedure for evaluating the interface properties of ceramic matrix composites. J Am Ceram Soc. 78:(2):1995;401-405.
    • (1995) J Am Ceram Soc , vol.78 , Issue.2 , pp. 401-405
    • Lamon, J.1    Rebillat, F.2    Evans, A.G.3
  • 36
    • 0001374881 scopus 로고
    • Asymptotic approximations to crack problems
    • G.C. Sih. Gronigen, Holland: Noordhoff International
    • Benthem J.P., Koiter W.T. Asymptotic approximations to crack problems. Sih G.C. Method of analysis and solutions of crack problems. 1973;131-178 Noordhoff International, Gronigen, Holland.
    • (1973) Method of Analysis and Solutions of Crack Problems , pp. 131-178
    • Benthem, J.P.1    Koiter, W.T.2
  • 39
    • 0029528027 scopus 로고
    • Asymptotic stresses around a crack tip at the interface between planar or cylindrical bodies
    • Pagano N.J., Kaw A.K. Asymptotic stresses around a crack tip at the interface between planar or cylindrical bodies. Int J Fract. 71:1995;151-164.
    • (1995) Int J Fract , vol.71 , pp. 151-164
    • Pagano, N.J.1    Kaw, A.K.2
  • 41
    • 0029325961 scopus 로고
    • Thermal residual stresses in ceramic matrix composites - I. Axisymmetrical model and finite element analysis
    • Bobet J.L., Lamon J. Thermal residual stresses in ceramic matrix composites - I. Axisymmetrical model and finite element analysis. Acta metall mater. 43:1995;2241-2253.
    • (1995) Acta Metall Mater , vol.43 , pp. 2241-2253
    • Bobet, J.L.1    Lamon, J.2
  • 42
    • 84986398326 scopus 로고
    • Determination of fracture toughness in 2-D woven SiC matrix composites made by chemical vapor infiltration
    • Droillard C., Voisard P., Heibst C., Lamon J. Determination of fracture toughness in 2-D woven SiC matrix composites made by chemical vapor infiltration. J Am Ceram Soc. 78:1995;1201-1211.
    • (1995) J Am Ceram Soc , vol.78 , pp. 1201-1211
    • Droillard, C.1    Voisard, P.2    Heibst, C.3    Lamon, J.4
  • 43
    • 0003097104 scopus 로고
    • Characterization and control of the fiber-matrix interface in ceramic matrix composites
    • Lowden RA. Characterization and control of the fiber-matrix interface in ceramic matrix composites, Report ORNL/TM 11039, 1989.
    • (1989) Report ORNL/TM 11039
    • Lowden, R.A.1
  • 44
    • 0005214925 scopus 로고    scopus 로고
    • Interfaces in metal matrix composites
    • S. Mall, & T. Nicholas. Technomic
    • Majumdar B.S. Interfaces in metal matrix composites. Mall S., Nicholas T. Titanium matrix composites. 1996;Technomic.
    • (1996) Titanium Matrix Composites
    • Majumdar, B.S.1
  • 45
    • 0022715695 scopus 로고
    • Fracture toughness anisotropy of a pyrolitic carbon
    • Sakai M., Bradt R.C., Fischbach D.B. Fracture toughness anisotropy of a pyrolitic carbon. J Mater Sci. 21:1986;1491-1501.
    • (1986) J Mater Sci , vol.21 , pp. 1491-1501
    • Sakai, M.1    Bradt, R.C.2    Fischbach, D.B.3
  • 47
    • 0001144361 scopus 로고
    • A mechanism for the control of crack propagation in all brittle systems
    • Cook J., Gordon J.E. A mechanism for the control of crack propagation in all brittle systems. Proc Roy Soc A. 282:1964;508-520.
    • (1964) Proc Roy Soc a , vol.282 , pp. 508-520
    • Cook, J.1    Gordon, J.E.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.