Volumn 20, Issue 11, 2011, Pages 1837-1849

In vivo biostability of polymeric spine implants: Retrieval analyses from a United States investigational device exemption study

Author keywords

Biodegradation; Biostability; Dynamic stabilization; Polycarbonate urethane; Polyethylene terephthalate

Indexed keywords

POLYCARBONATE URETHANE; POLYETHYLENE TEREPHTHALATE; POLYMER; UNCLASSIFIED DRUG;

EID: 84855195889     PISSN: 09406719     EISSN: 14320932     Source Type: Journal    
DOI: 10.1007/s00586-011-1812-8     Document Type: Article
Times cited : (16)

References (32)
  • 1
    • 0022404209 scopus 로고
    • Titanium-aluminium-niobium alloy, development for biocompatible, high strength surgical implants
    • Semlitsch M, Staub F, Weber H (1985) Titanium-aluminium-niobium alloy, development for biocompatible, high strength surgical implants. Biomed Tech (Berl) 30:334-339 (Pubitemid 16189147)
    • (1985) Biomedizinische Technik , vol.30 , Issue.12 , pp. 334-339
    • Semlitsch, M.1    Staub, F.2    Weber, H.3
  • 2
    • 0031906445 scopus 로고    scopus 로고
    • Assessment of press-fit hip femoral components retrieved at autopsy
    • Lester DK, Campbell P, Ehya A et al (1998) Assessment of pressfit hip femoral components retrieved at autopsy. Orthopedics 21(1):27-33 (Pubitemid 28063561)
    • (1998) Orthopedics , vol.21 , Issue.1 , pp. 27-33
    • Lester, D.K.1    Campbell, P.2    Ehya, A.3    Rude, R.K.4
  • 3
    • 0036035142 scopus 로고    scopus 로고
    • The dynamic neutralization system for the spine: A multi-center study of a novel non-fusion system
    • Stoll TM, Dubois G, Schwarzenbach O (2002) The dynamic neutralization system for the spine: a multi-center study of a novel non-fusion system. Eur Spine J 11(Suppl 2):170-178
    • (2002) Eur Spine J , vol.11 , Issue.SUPPL. 2 , pp. 170-178
    • Stoll, T.M.1    Dubois, G.2    Schwarzenbach, O.3
  • 4
    • 13444300930 scopus 로고    scopus 로고
    • Clinical experience with the dynesys semirigid fixation system for the lumbar spine: Surgical and patient-oriented outcome in 50 cases after an average of 2 years
    • DOI 10.1097/01.brs.0000152584.46266.25
    • Grob D, Benini A, Junge A et al (2005) Clinical experience with the Dynesys semirigid fixation system for the lumbar spine: surgical and patient-oriented outcome in 50 cases after an average of 2 years. Spine 30:324-331 (Pubitemid 40209259)
    • (2005) Spine , vol.30 , Issue.3 , pp. 324-331
    • Grob, D.1    Benini, A.2    Junge, A.3    Mannion, A.F.4
  • 5
    • 33748564646 scopus 로고    scopus 로고
    • Mechanical concepts for disc regeneration
    • Schnake KJ, Putzier M, Haas NP et al (2006) Mechanical concepts for disc regeneration. Eur Spine J 15(Suppl 3):354-360
    • (2006) Eur Spine J , vol.15 , Issue.SUPPL. 3 , pp. 354-360
    • Schnake, K.J.1    Putzier, M.2    Haas, N.P.3
  • 6
    • 33645513258 scopus 로고    scopus 로고
    • The surgical treatment of the lumbar disc prolapse: Nucleotomy with additional transpedicular dynamic stabilization versus nucleotomy alone
    • Putzier M, Schneider SV, Funk JF et al (2005) The surgical treatment of the lumbar disc prolapse: nucleotomy with additional transpedicular dynamic stabilization versus nucleotomy alone. Spine 30:E109-E114
    • (2005) Spine , vol.30
    • Putzier, M.1    Schneider, S.V.2    Funk, J.F.3
  • 7
    • 84855186275 scopus 로고    scopus 로고
    • last access on February 20th, 2011
    • http://www.fda.gov/AdvisoryCommittees/CommitteesMeetingMaterials/ MedicalDevices/MedicalDevicesAdvisoryCommittee/ OrthopaedicandRehabilitationDevicesPanel/ucm147056.htm, last access on February 20th, 2011
  • 8
    • 2442651557 scopus 로고    scopus 로고
    • Poly(carbonate urethane) and poly(ether urethane) biodegradation: In vivo studies
    • Christenson EM, Dadsetan M, Wiggins M et al (2004) Poly(carbonate urethane) and poly(ether urethane) biodegradation: in vivo studies. J Biomed Mater Res A 69:407-416
    • (2004) J Biomed Mater Res A , vol.69 , pp. 407-416
    • Christenson, E.M.1    Dadsetan, M.2    Wiggins, M.3
  • 10
    • 1942436763 scopus 로고    scopus 로고
    • Long-term in vivo biostability of poly(dimethylsiloxane)/ poly(hexamethylene oxide) mixed macrodiol-based polyurethane elastomers
    • DOI 10.1016/j.biomaterials.2004.01.004, PII S0142961204000055
    • Simmons A, Hyvarinen J, Odell RA et al (2004) Long-term in vivo biostability of poly(dimethylsiloxane)/poly(hexamethylene oxide) mixed macrodiol-based polyurethane elastomers. Biomaterials 25(20):4887-4900 (Pubitemid 38520819)
    • (2004) Biomaterials , vol.25 , Issue.20 , pp. 4887-4900
    • Simmons, A.1    Hyvarinen, J.2    Odell, R.A.3    Martin, D.J.4    Gunatillake, P.A.5    Noble, K.R.6    Poole-Warren, L.A.7
  • 11
    • 0004270932 scopus 로고    scopus 로고
    • Surface characterization of polyurethanes
    • Lamba NMK, Woodhouse KA, Cooper SL (eds). CRC Press, Boca Raton, FL
    • Lamba NMK, Woodhouse KA, Cooper SL (1998) Surface characterization of polyurethanes. In: Lamba NMK, Woodhouse KA, Cooper SL (eds) Polyurethanes in biomedical applications. CRC Press, Boca Raton, FL, pp 91-114
    • (1998) Polyurethanes in Biomedical Applications , pp. 91-114
    • Lamba, N.M.K.1    Woodhouse, K.A.2    Cooper, S.L.3
  • 12
    • 0033118636 scopus 로고    scopus 로고
    • Synergistic effects of oxidative environments and mechanical stress on in vitro stability of polyetherurethanes and polycarbonateurethanes
    • DOI 10.1002/(SICI)1097-4636(199904)45:1<62::AID-JBM9>3.0.CO;2-F
    • Fare S, Petrini P, Motta A et al (1999) Synergistic effects of oxidative environments and mechanical stress on in vitro stability of polyether urethanes and polycarbonate urethanes. J Biomed Mater Res 45:62-74 (Pubitemid 29068440)
    • (1999) Journal of Biomedical Materials Research , vol.45 , Issue.1 , pp. 62-74
    • Fare, S.1    Petrini, P.2    Motta, A.3    Cigada, A.4    Tanzi, M.C.5
  • 14
    • 0031281407 scopus 로고    scopus 로고
    • In-vivo degradation of polyurethanes: Transmission-FTIR microscopic characterization of polyurethanes sectioned by cryomicrotomy
    • DOI 10.1016/S0142-9612(97)00083-5, PII S0142961297000835
    • McCarthy SJ, Meijs GF, Mitchell N et al (1997) In vivo degradation of polyurethanes: transmission-FTIR microscopic characterization of polyurethanes sectioned by cryomicrotomy. Biomaterials 18:1387-1409 (Pubitemid 27480602)
    • (1997) Biomaterials , vol.18 , Issue.21 , pp. 1387-1409
    • McCarthy, S.J.1    Meijs, G.F.2    Mitchell, N.3    Gunatillake, P.A.4    Heath, G.5    Brandwood, A.6    Schindhelm, K.7
  • 15
    • 0033624751 scopus 로고    scopus 로고
    • In vitro stability of polyether and polycarbonate urethanes
    • DOI 10.1106/7TJU-H1YA-4NYT-XL84
    • Tanzi MC, Fare S, Petrini P (2000) In vitro stability of polyether and polycarbonate urethanes. J Biomater Appl 14:325-348 (Pubitemid 30594801)
    • (2000) Journal of Biomaterials Applications , vol.14 , Issue.4 , pp. 325-348
    • Tanzi, M.C.1    Fare, S.2    Petrini, P.3
  • 16
    • 0035889832 scopus 로고    scopus 로고
    • Hydrolytic degradation of poly(carbonate)-urethanes by monocyte-derived macrophages
    • DOI 10.1016/S0142-9612(01)00049-7, PII S0142961201000497
    • Labow RS, Meek E, Santerre JP (2001) Hydrolytic degradation of poly(carbonate)-urethanes by monocyte-derived macrophages. Biomaterials 22:3025-3033 (Pubitemid 32768710)
    • (2001) Biomaterials , vol.22 , Issue.22 , pp. 3025-3033
    • Labow, R.S.1    Meek, E.2    Santerre, J.P.3
  • 17
    • 0021505618 scopus 로고
    • Molecular weight characterization of virgin and explanted polyester arterial prostheses
    • Paarek JM, Guidoin R, Aubin M et al (1984) Molecular weight characterization of virgin and explanted polyester arterial prostheses. J Biomed Mater Res 18:881-894 (Pubitemid 14013161)
    • (1984) Journal of Biomedical Materials Research , vol.18 , Issue.8 , pp. 881-894
    • Maarek, J.M.1    Guidoin, R.2
  • 18
    • 0026938679 scopus 로고
    • Rubber abrasion and wear
    • Muhr AH, Roberts AD (1992) Rubber abrasion and wear. Wear 158:213-228 (Pubitemid 23586514)
    • (1992) Wear , vol.158 , Issue.1-2 , pp. 213-228
    • Muhr, A.H.1    Roberts, A.D.2
  • 19
    • 0035885544 scopus 로고    scopus 로고
    • Enzyme-induced biodegradation of polycarbonate polyurethanes: Dependence on hard-segment concentration
    • DOI 10.1002/1097-4636(20010915)56:4<516::AID-JBM1123>3.0.CO;2-B
    • Tang YW, Labow RS, Santerre JP (2001) Enzyme-induced biodegradation of polycarbonate polyurethanes: dependence on hard-segment concentration. J Biomed Mater Res 56(4):516-528 (Pubitemid 32606011)
    • (2001) Journal of Biomedical Materials Research , vol.56 , Issue.4 , pp. 516-528
    • Tang, Y.W.1    Labow, R.S.2    Santerre, J.P.3
  • 20
    • 0024100474 scopus 로고    scopus 로고
    • Biostability of polyurethane elastomers: A critical review
    • Szycher M (1998) Biostability of polyurethane elastomers: a critical review. J Biomater Appl 3:297
    • (1998) J Biomater Appl , vol.3 , pp. 297
    • Szycher, M.1
  • 21
    • 0024097873 scopus 로고
    • Factors and interactions affecting the performance of polyurethane elastomers in medical devices
    • Coury AJ, Slaikeu PC, Cahalan PT et al (1988) Factors and interactions affecting the performance of polyurethane elastomers in medical devices. J Biomater Appl 3(2):130-179
    • (1988) J Biomater Appl , vol.3 , Issue.2 , pp. 130-179
    • Coury, A.J.1    Slaikeu, P.C.2    Cahalan, P.T.3
  • 22
    • 84947413779 scopus 로고
    • A review of biostability and carcinogenicity of polyurethanes in medicine and the new generation of biostable polyurethanes
    • Pinchuk L (1995) A review of biostability and carcinogenicity of polyurethanes in medicine and the new generation of biostable polyurethanes. J Biomater Sci Polym Edn 6(3):225-267
    • (1995) J Biomater Sci Polym Edn , vol.6 , Issue.3 , pp. 225-267
    • Pinchuk, L.1
  • 24
    • 23644440286 scopus 로고    scopus 로고
    • Understanding the biodegradation of polyurethanes: From classical implants to tissue engineering materials
    • DOI 10.1016/j.biomaterials.2005.05.079, PII S0142961205004692, Canadian Biomaterials Research
    • Santerre JP, Woodhouse K, Laroche G et al (2005) Understanding the biodegradation of polyurethanes: from classical implants to tissue engineering materials. Biomaterials 26(35):7457-7470 (Pubitemid 41133597)
    • (2005) Biomaterials , vol.26 , Issue.35 , pp. 7457-7470
    • Santerre, J.P.1    Woodhouse, K.2    Laroche, G.3    Labow, R.S.4
  • 27
    • 20344380629 scopus 로고
    • Degradation studies of polyethylene therephthalate
    • McMahon W, Birdsall HA, Johnson GR et al (1959) Degradation studies of polyethylene therephthalate. J Chem Eng Data 4:57-79
    • (1959) J Chem Eng Data , vol.4 , pp. 57-79
    • McMahon, W.1    Birdsall, H.A.2    Johnson, G.R.3
  • 28
    • 52549109020 scopus 로고    scopus 로고
    • Microstructural changes in polyester biotextiles during implantation in humans
    • King MW, Zhang Z, Guidoin R (2001) Microstructural changes in polyester biotextiles during implantation in humans. J Text Appar Technol Manag 1:1-8
    • (2001) J Text Appar Technol Manag , vol.1 , pp. 1-8
    • King, M.W.1    Zhang, Z.2    Guidoin, R.3
  • 32
    • 84855186276 scopus 로고    scopus 로고
    • Analysis of retrievals of a dynamic stabilization system for the spine
    • Trommsdorff U, Koettig P (2005) Analysis of retrievals of a dynamic stabilization system for the spine. EuroSpine, Annual Meeting
    • (2005) EuroSpine, Annual Meeting
    • Trommsdorff, U.1    Koettig, P.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.