Volumn 31, Issue 14, 2011, Pages 2733-2739

Gas tight sintered material for high temperature sublimation setups

Author keywords

Carbides; Porosity; Refractories; Sintering; Thermal expansion

Indexed keywords

ALN; CERAMIC DISCS; FINE POWDERS; GRAIN SIZE; GROWTH CONDITIONS; HIGH TEMPERATURE; RELATIVE DENSITY; SINTERED MATERIALS; THERMAL EXPANSION COEFFICIENTS;

EID: 80051469467     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2010.12.013     Document Type: Article
Times cited : (8)

References (20)
  • 1
    • 0030410873 scopus 로고    scopus 로고
    • Progress and prospects of group-III nitride semiconductors
    • Mohammad S.N., Morkoc H. Progress and prospects of group-III nitride semiconductors. Prog Quant Electr 1996, 20:361-525.
    • (1996) Prog Quant Electr , vol.20 , pp. 361-525
    • Mohammad, S.N.1    Morkoc, H.2
  • 2
    • 0031222709 scopus 로고    scopus 로고
    • Comparison of the oxidation behaviour of two dense hot isostatically pressed tantalum carbide materials
    • Desmaison-Brut M., Alexandre N., Desmaison J. Comparison of the oxidation behaviour of two dense hot isostatically pressed tantalum carbide materials. J Eur Ceram Soc 1997, 17:1325-1334.
    • (1997) J Eur Ceram Soc , vol.17 , pp. 1325-1334
    • Desmaison-Brut, M.1    Alexandre, N.2    Desmaison, J.3
  • 3
    • 70349202046 scopus 로고    scopus 로고
    • Mechanical properties and rapid consolidation of binderless nanostructured TaC
    • Kim B.R., Woo K.D., Doh J.M., Yoon J.K., Shon I.J., Yoon J.K., Shon I.J. Mechanical properties and rapid consolidation of binderless nanostructured TaC. Ceram Int 2009, 35:3395-3400.
    • (2009) Ceram Int , vol.35 , pp. 3395-3400
    • Kim, B.R.1    Woo, K.D.2    Doh, J.M.3    Yoon, J.K.4    Shon, I.J.5    Yoon, J.K.6    Shon, I.J.7
  • 5
    • 76049107594 scopus 로고    scopus 로고
    • Pressureless sintering of tantalum carbide ceramics without additives
    • Liu J.X., Kan Y.M., Zhang G.J. Pressureless sintering of tantalum carbide ceramics without additives. J Am Ceram Soc 2010, 93(2):370-373.
    • (2010) J Am Ceram Soc , vol.93 , Issue.2 , pp. 370-373
    • Liu, J.X.1    Kan, Y.M.2    Zhang, G.J.3
  • 6
    • 57649215255 scopus 로고    scopus 로고
    • Densification, mechanical properties and oxidation resistance of TaC-TaB2 ceramics
    • Zhang X.H., Hilmas G.E., Fahrenholtz W.G. Densification, mechanical properties and oxidation resistance of TaC-TaB2 ceramics. J Am Ceram Soc 2008, 91(12):4129-4132.
    • (2008) J Am Ceram Soc , vol.91 , Issue.12 , pp. 4129-4132
    • Zhang, X.H.1    Hilmas, G.E.2    Fahrenholtz, W.G.3
  • 7
    • 57349173065 scopus 로고    scopus 로고
    • Densification and mechanical properties of TaC-based ceramics
    • Zhang X.H., Hilmas G.E., Fahrenholtz W.G. Densification and mechanical properties of TaC-based ceramics. Mater Sci Eng A 2009, 501(1-2):37-43.
    • (2009) Mater Sci Eng A , vol.501 , Issue.1-2 , pp. 37-43
    • Zhang, X.H.1    Hilmas, G.E.2    Fahrenholtz, W.G.3
  • 8
    • 33846537903 scopus 로고    scopus 로고
    • Hot pressing of tantalum carbide with and without sintering additives
    • Zhang X.H., Hilmas G.E., Fahrenholtz W.G. Hot pressing of tantalum carbide with and without sintering additives. J Am Ceram Soc 2007, 90(2):393-401.
    • (2007) J Am Ceram Soc , vol.90 , Issue.2 , pp. 393-401
    • Zhang, X.H.1    Hilmas, G.E.2    Fahrenholtz, W.G.3
  • 10
    • 80051470839 scopus 로고    scopus 로고
    • Personal communication. FCT Ingenieurkeramik GmbH, Germany.
    • Berroth K. Personal communication. FCT Ingenieurkeramik GmbH, Germany.
    • Berroth, K.1
  • 12
    • 70349202046 scopus 로고    scopus 로고
    • Mechanical properties and rapid consolidation of binderless nanostructured tantalum carbide
    • Kim B.R., Woo K.D., Doh J.M., Yoon J.K., Shon I.J. Mechanical properties and rapid consolidation of binderless nanostructured tantalum carbide. Ceram Int 2009, 35:3395-3400.
    • (2009) Ceram Int , vol.35 , pp. 3395-3400
    • Kim, B.R.1    Woo, K.D.2    Doh, J.M.3    Yoon, J.K.4    Shon, I.J.5
  • 13
    • 80051469677 scopus 로고    scopus 로고
    • .
    • http://www.knovel.com/web/.
  • 14
    • 80051475157 scopus 로고
    • Chemie der Elemente. 1. Auflage, ISBN 3-527-26169-9;
    • Greenwood NN, Earnshaw A. Chemie der Elemente. 1. Auflage, ISBN 3-527-26169-9; 1988. p. 1260.
    • (1988) , pp. 1260
    • Greenwood, N.N.1    Earnshaw, A.2
  • 15
    • 80051469565 scopus 로고    scopus 로고
    • .
    • http://www.dguv.de/ifa/stoffdatenbank/index.jsp.
  • 16
    • 80051475559 scopus 로고    scopus 로고
    • .
    • http://www.chemicalbook.com/ChemicalProductProperty_DE_CB2174365.htm.
  • 17
    • 80051469970 scopus 로고
    • Chemie der Elemente. 1. Edition, ISBN 3-527-26169-9;
    • Greenwood NN, Earnshaw A. Chemie der Elemente. 1. Edition, ISBN 3-527-26169-9; 1988. p. 1291.
    • (1988) , pp. 1291
    • Greenwood, N.N.1    Earnshaw, A.2
  • 19
    • 0037962205 scopus 로고
    • Ternary phase equilibrium in transition metal-Boron-carbon-silicon systems
    • Rudy E. Ternary phase equilibrium in transition metal-Boron-carbon-silicon systems. AFML 1969.
    • (1969) AFML
    • Rudy, E.1
  • 20
    • 0007726320 scopus 로고
    • Untersuchungen im System Tantal-Wolfram-Kohlenstoff
    • Rudy E., Rudy E., Benesovsky F. Untersuchungen im System Tantal-Wolfram-Kohlenstoff. Mh Chem 1962, 93:1176-1195.
    • (1962) Mh Chem , vol.93 , pp. 1176-1195
    • Rudy, E.1    Rudy, E.2    Benesovsky, F.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.