Volumn 104, Issue 3, 2011, Pages 1145-1151

Kinetics of thermo-oxidative degradation of polypropylene/aluminum trihydroxide/organo Fe-montmorillonite nanocomposites

Author keywords

Fe montmorillonite; Kinetics of thermo oxidative degradation; Nanocomposite; Polypropylene

Indexed keywords

COMPLEX REACTIONS; FE-MONTMORILLONITE; FLYNN-WALL-OZAWA; KISSINGER; LAST STAGE; ONSET TEMPERATURE; OXIDATIVE DEGRADATION; THERMAL OXIDATIVE DEGRADATION; THERMO-OXIDATIVE DEGRADATION; WHOLE PROCESS;

EID: 79959374638     PISSN: 13886150     EISSN: None     Source Type: Journal    
DOI: 10.1007/s10973-011-1346-7     Document Type: Article
Times cited : (10)

References (21)
  • 1
    • 33144464278 scopus 로고    scopus 로고
    • Properties of polypropylene/aluminum trihydroxide composites containing nanosized organoclay
    • DOI 10.1002/pen.20367
    • N Ristolainen U Hippi J Seppala A Nykanen J Ruokolainen 2005 Properties of polypropylene/aluminum trihydroxide composites containing nanosized organoclay Poly Eng Sci 45 12 1568 1575 10.1002/pen.20367 1:CAS:528: DC%2BD2MXhtlWlt7fP (Pubitemid 43265401)
    • (2005) Polymer Engineering and Science , vol.45 , Issue.12 , pp. 1568-1575
    • Ristolainen, N.1    Hippi, U.2    Seppala, J.3    Nykanen, A.4    Ruokolainen, J.5
  • 2
    • 0242591248 scopus 로고
    • The emergence of magnesium hydroxide as a fire retardant additive
    • The Plastic and Rubber Institute, editor London: Elsevier
    • Rothon R. The emergence of magnesium hydroxide as a fire retardant additive. In: The Plastic and Rubber Institute, editor. Flame Retardants 1990 Conference. London: Elsevier; 1990.
    • (1990) Flame Retardants 1990 Conference
    • Rothon, R.1
  • 3
    • 20544438326 scopus 로고    scopus 로고
    • Catalyzing carbonization of polypropylene itself by supported nickel catalyst during combustion of polypropylene/clay nanocomposite for improving fire retardancy
    • DOI 10.1021/cm047771c
    • T Tang X Chen H Chen X Meng Z Jiang W Bi 2005 Catalyzing carbonization of polypropylene itself by supported nickel catalyst during combustion of polypropylene/clay nanocomposite for improving fire retardancy Chem Mater 17 2799 2802 10.1021/cm047771c 1:CAS:528:DC%2BD2MXjs1Kju7w%3D (Pubitemid 40844682)
    • (2005) Chemistry of Materials , vol.17 , Issue.11 , pp. 2799-2802
    • Tang, T.1    Chen, X.2    Chen, H.3    Meng, X.4    Jiang, Z.5    Bi, W.6
  • 4
    • 0033807613 scopus 로고    scopus 로고
    • Flammability properties of polymer-layered-silicate nanocomposites polypropylene and polystyrene nanocomposites
    • Gilman JW, Jackson CL, Morgan AB, Jr RH, Manias E, Giannelis EP et al., Flammability properties of polymer-layered-silicate nanocomposites polypropylene and polystyrene nanocomposites. Chem Mater. 2000; 12:1866-1873.
    • (2000) Chem Mater. , vol.12 , pp. 1866-1873
    • Gilman, J.W.1    Jackson, C.L.2    Morgan, A.B.3    Jr., R.H.4    Manias, E.5    Giannelis, E.P.6
  • 5
    • 67849128865 scopus 로고    scopus 로고
    • Synergistic flammability and thermal stability of polypropylene/aluminum trihydroxide/Fe-montmorillonite nanocomposites
    • 10.1002/pat.1285 1:CAS:528:DC%2BD1MXks1WntrY%3D
    • QH Kong Y Hu L Song CW Yi 2009 Synergistic flammability and thermal stability of polypropylene/aluminum trihydroxide/Fe-montmorillonite nanocomposites Polym Adv Technol 20 404 409 10.1002/pat.1285 1:CAS:528:DC%2BD1MXks1WntrY%3D
    • (2009) Polym Adv Technol , vol.20 , pp. 404-409
    • Kong, Q.H.1    Hu, Y.2    Song, L.3    Yi, C.W.4
  • 6
    • 0033720281 scopus 로고    scopus 로고
    • Kinetic analysis using multivariate non-linear regression. I. Basic concepts
    • 10.1023/A:1010167626551 1:CAS:528:DC%2BD3cXkvF2qtbo%3D
    • J Opfermann 2000 Kinetic analysis using multivariate non-linear regression. I. Basic concepts J Therm Anal Calorim 60 641 658 10.1023/A:1010167626551 1:CAS:528:DC%2BD3cXkvF2qtbo%3D
    • (2000) J Therm Anal Calorim , vol.60 , pp. 641-658
    • Opfermann, J.1
  • 7
    • 0034667469 scopus 로고    scopus 로고
    • Modelling of nonisothermal kinetics in thermogravimetry
    • 10.1039/b004355i 1:CAS:528:DC%2BD3cXnt1Klur4%3D
    • V Mamleev S Bourbigot M Le Bras S Duquesne J Sestak 2000 Modelling of nonisothermal kinetics in thermogravimetry Phys Chem Chem Phys 2 20 4708 4716 10.1039/b004355i 1:CAS:528:DC%2BD3cXnt1Klur4%3D
    • (2000) Phys Chem Chem Phys , vol.2 , Issue.20 , pp. 4708-4716
    • Mamleev, V.1    Bourbigot, S.2    Le Bras, M.3    Duquesne, S.4    Sestak, J.5
  • 8
    • 10644272683 scopus 로고    scopus 로고
    • Three model-free methods for calculation of activation energy in TG
    • 1:CAS:528:DC%2BD2cXhtVGmt7rF
    • V Mamleev S Bourbigot M Le Bras J Lefevbre 2004 Three model-free methods for calculation of activation energy in TG J Therm Anal Calorim 78 3 1009 1027 1:CAS:528:DC%2BD2cXhtVGmt7rF
    • (2004) J Therm Anal Calorim , vol.78 , Issue.3 , pp. 1009-1027
    • Mamleev, V.1    Bourbigot, S.2    Le Bras, M.3    Lefevbre, J.4
  • 9
    • 0037068086 scopus 로고    scopus 로고
    • Model-free analysis of thermoanalytical data-advantages and limitations
    • JR Opfermann E Kaisersberger HJ Flammersheim 2002 Model-free analysis of thermoanalytical data-advantages and limitations Thermochim Acta 391 1-2 117 127
    • (2002) Thermochim Acta , vol.391 , Issue.12 , pp. 117-127
    • Opfermann, J.R.1    Kaisersberger, E.2    Flammersheim, H.J.3
  • 10
    • 0030283749 scopus 로고    scopus 로고
    • Comprehensive study of the oxidative degradation of an epoxy resin using the degradation front model
    • PII S0141391096000626
    • N Rose M Le Bras S Bourbigot R Delobel B Costes 1996 Comprehensive study of the oxidative degradation of an epoxy resin using the degradation front model Polym Degrad Stab 54 2-3 355 360 10.1016/S0141-3910(96)00062-6 1:CAS:528:DyaK2sXls1altw%3D%3D (Pubitemid 126410881)
    • (1996) Polymer Degradation and Stability , vol.54 , Issue.2-3 SPEC. ISS. , pp. 355-360
    • Rose, N.1    Le Bras, M.2    Bourbigot, S.3    Delober, R.4    Costes, B.5
  • 12
    • 33749213901 scopus 로고
    • Reaction kinetics in differential thermal analysis
    • 10.1021/ac60131a045 1:CAS:528:DyaG1cXivVequw%3D%3D
    • HE Kissinger 1957 Reaction kinetics in differential thermal analysis Anal Chem 29 1702 1706 10.1021/ac60131a045 1:CAS:528:DyaG1cXivVequw%3D%3D
    • (1957) Anal Chem , vol.29 , pp. 1702-1706
    • Kissinger, H.E.1
  • 13
    • 57849133537 scopus 로고    scopus 로고
    • Thermal degradation and combustion behavior of the polyethylene/clay nanocomposite prepared by melt intercalation
    • 10.1007/s10973-008-9355-x 1:CAS:528:DC%2BD1cXhsFWju7nM
    • SM Lomakin IL Dubnikova AN Shchegolikhin GE Zaikov R Kozlowski GM Kim GH Michler 2008 Thermal degradation and combustion behavior of the polyethylene/clay nanocomposite prepared by melt intercalation J Therm Anal Calorim 94 3 719 726 10.1007/s10973-008-9355-x 1:CAS:528:DC%2BD1cXhsFWju7nM
    • (2008) J Therm Anal Calorim , vol.94 , Issue.3 , pp. 719-726
    • Lomakin, S.M.1    Dubnikova, I.L.2    Shchegolikhin, A.N.3    Zaikov, G.E.4    Kozlowski, R.5    Kim, G.M.6    Michler, G.H.7
  • 14
    • 45449119861 scopus 로고    scopus 로고
    • Kinetic study of the thermal degradation of PS/MMT nanocomposites prepared with imidazolium surfactants
    • 10.1007/s10973-007-8577-7 1:CAS:528:DC%2BD1cXksFWls70%3D
    • L Abate I Blanco FA Bottino G Di Pasquale E Fabbri A Orestano A Pollicino 2008 Kinetic study of the thermal degradation of PS/MMT nanocomposites prepared with imidazolium surfactants J Therm Anal Calorim 91 3 681 686 10.1007/s10973-007-8577-7 1:CAS:528:DC%2BD1cXksFWls70%3D
    • (2008) J Therm Anal Calorim , vol.91 , Issue.3 , pp. 681-686
    • Abate, L.1    Blanco, I.2    Bottino, F.A.3    Di Pasquale, G.4    Fabbri, E.5    Orestano, A.6    Pollicino, A.7
  • 15
    • 0000461518 scopus 로고
    • A new method of analyzing thermogravimetric data
    • 10.1246/bcsj.38.1881 1:CAS:528:DyaF28XjtVyisQ%3D%3D
    • T Ozawa 1965 A new method of analyzing thermogravimetric data Bull Chem Soc Japan 38 1 1881 1886 10.1246/bcsj.38.1881 1:CAS:528:DyaF28XjtVyisQ%3D%3D
    • (1965) Bull Chem Soc Japan , vol.38 , Issue.1 , pp. 1881-1886
    • Ozawa, T.1
  • 16
    • 0000894118 scopus 로고
    • Kinetics of thermal degradation of char-forming plastics from thermogravimetry: Application to phenolic plastic
    • HL Friedman 1964 Kinetics of thermal degradation of char-forming plastics from thermogravimetry: application to phenolic plastic J Polym Sci Part C 6 183 195
    • (1964) J Polym Sci Part C , vol.6 , pp. 183-195
    • Friedman, H.L.1
  • 17
    • 33747607063 scopus 로고    scopus 로고
    • Influence of Fe-MMT on crosslinking and thermal degradation in silicone rubber/clay nanocomposites
    • DOI 10.1002/pat.723
    • Kong QH, Hu Y, Song L, Wang YL, Chen ZY, Wan WC. Influence of Fe-MMT on crosslinking and thermal degradation in silicone rubber/clay nanocomposites. Polym Adv Technol. 2006; 17(6): 463-467. (Pubitemid 44263202)
    • (2006) Polymers for Advanced Technologies , vol.17 , Issue.6 , pp. 463-467
    • Kong, Q.1    Hu, Y.2    Song, L.3    Wang, Y.4    Chen, Z.5    Fan, W.6
  • 18
    • 0035677042 scopus 로고    scopus 로고
    • Studies on the mechanism by which the formation of nanocomposites enhances thermal stability
    • Zhu J, Uhl FM, Morgan AB, Wilkie CA. Studies on the mechanism by which the formation of nanocomposites enhances thermal stability. Chem Mater. 2001; 13(12): 4649-4654.
    • (2001) Chem Mater. , vol.13 , Issue.12 , pp. 4649-4654
    • Zhu, J.1    Uhl, F.M.2    Morgan, A.B.3    Wilkie, C.A.4
  • 19
    • 77949882988 scopus 로고    scopus 로고
    • An assessment of the role of morphology in thermal/thermo-oxidative degradation mechanism of PP/EVA/clay nanocomposites
    • 10.1016/j.polymdegradstab.2010.01.009 1:CAS:528:DC%2BC3cXksVCltL4%3D
    • V Goodarzi SH Jafari HA Khonakdar SA Monemian M Mortazavi 2010 An assessment of the role of morphology in thermal/thermo-oxidative degradation mechanism of PP/EVA/clay nanocomposites Polym Degrad Stab 95 5 859 869 10.1016/j.polymdegradstab.2010.01.009 1:CAS:528:DC%2BC3cXksVCltL4%3D
    • (2010) Polym Degrad Stab , vol.95 , Issue.5 , pp. 859-869
    • Goodarzi, V.1    Jafari, S.H.2    Khonakdar, H.A.3    Monemian, S.A.4    Mortazavi, M.5
  • 20
    • 9444293413 scopus 로고    scopus 로고
    • Thermal oxidative degradation behaviours of flame-retardant copolyesters containing phosphorous linked pendent group/montmorillonite nanocomposites
    • 10.1016/j.polymdegradstab.2004.08.004 1:CAS:528:DC%2BD2cXps1OrsL4%3D
    • DY Wang YZ Wang JS Wang DQ Chen Q Zhou B Yang WY Li 2005 Thermal oxidative degradation behaviours of flame-retardant copolyesters containing phosphorous linked pendent group/montmorillonite nanocomposites Polym Degrad Stab 87 171 176 10.1016/j.polymdegradstab.2004.08.004 1:CAS:528: DC%2BD2cXps1OrsL4%3D
    • (2005) Polym Degrad Stab , vol.87 , pp. 171-176
    • Wang, D.Y.1    Wang, Y.Z.2    Wang, J.S.3    Chen, D.Q.4    Zhou, Q.5    Yang, B.6    Li, W.Y.7
  • 21
    • 4344673400 scopus 로고    scopus 로고
    • Kinetics of the thermal and thermo-oxidative degradation of a polystyrene/clay nanocomposite
    • 10.1002/marc.200300214 1:CAS:528:DC%2BD2cXhvVOhtbY%3D
    • S Vyazovkin I Dranca XW Fan R Advincula 2004 Kinetics of the thermal and thermo-oxidative degradation of a polystyrene/clay nanocomposite Macromol Rapid Comm 25 3 498 503 10.1002/marc.200300214 1:CAS:528:DC%2BD2cXhvVOhtbY%3D
    • (2004) Macromol Rapid Comm , vol.25 , Issue.3 , pp. 498-503
    • Vyazovkin, S.1    Dranca, I.2    Fan, X.W.3    Advincula, R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.