메뉴 건너뛰기




Volumn 95, Issue 8, 2011, Pages 2228-2237

High temperature oxidation of ZrC-20%MoSi2 in air for future solar receivers

Author keywords

Concentrated solar energy; High temperature; Oxidation; Solar receiver; UHTC; ZrC

Indexed keywords

CONCENTRATED SOLAR ENERGY; HIGH TEMPERATURE; SOLAR RECEIVER; UHTC; ZRC;

EID: 79958097542     PISSN: 09270248     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.solmat.2011.03.028     Document Type: Article
Times cited : (31)

References (20)
  • 1
    • 1342289718 scopus 로고    scopus 로고
    • Porous materials as open volumetric solar receivers: Experimental determination of thermophysical and heat transfer properties
    • DOI 10.1016/S0360-5442(03)00188-9, PII S0360544203001889
    • T. Fend, B. Hoffschmidt, R. Pitz-Paal, O. Reutter, and P. Rietbrock Porous materials as open volumetric solar receivers: experimental determination of thermophysical and heat transfer properties Energy 29 2004 823 833 (Pubitemid 38335469)
    • (2004) Energy , vol.29 , Issue.5-6 , pp. 823-833
    • Fend, T.1    Hoffschmidt, B.2    Pitz-Paal, R.3    Reutter, O.4    Rietbrock, P.5
  • 2
    • 0041544094 scopus 로고    scopus 로고
    • A solar thermal MgO-powder receiver with working temperatures of more than 1600°C: Model investigation by using a laser as an irradiation source
    • PII S0927024896000396
    • V. Verlotski, M. Schaus, and M. Pohl A solar thermal MgO-powder receiver with working temperatures of more than 1600 °C: model investigation by using a laser as an irradiation source Sol. Energy Mater. Sol. Cells 45 1997 227 239 (Pubitemid 127417394)
    • (1997) Solar Energy Materials and Solar Cells , vol.45 , Issue.3 , pp. 227-239
    • Verlotski, V.1    Schaus, M.2    Pohl, M.3
  • 6
    • 0035329816 scopus 로고    scopus 로고
    • Interfacial reaction on oxidation of carbides with formation of carbon
    • DOI 10.1016/S0167-2738(01)00727-5, PII S0167273801007275
    • S. Shimada Interfacial reaction on oxidation of carbides with formation of carbon Solid State Ion. 141142 2001 99 104 (Pubitemid 32605332)
    • (2001) Solid State Ionics , vol.141-142 , pp. 99-104
    • Shimada, S.1
  • 7
    • 0029172168 scopus 로고
    • Formation and microstructure of carbon-containing oxide scales by oxidation of single crystals of zirconium carbide
    • S. Shimada, M. Nishisako, M. Inagaki, and K. Yamamoto Formation and microstructure of carbon-containing oxide scales by oxidation of single crystals of zirconium carbide J. Am. Ceram. Soc 78 1995 41 48
    • (1995) J. Am. Ceram. Soc , vol.78 , pp. 41-48
    • Shimada, S.1    Nishisako, M.2    Inagaki, M.3    Yamamoto, K.4
  • 8
    • 0000697574 scopus 로고    scopus 로고
    • 2 interface by oxidation of ZrC single crystals
    • PII S0008622398000876
    • 2 interface by oxidation of ZrC single crystals Carbon 36 1998 1125 1131 (Pubitemid 128401318)
    • (1998) Carbon , vol.36 , Issue.7-8 , pp. 1125-1131
    • Shimada, S.1    Yoshimatsu, M.2    Inagaki, M.3    Otani, S.4
  • 9
    • 18844375375 scopus 로고    scopus 로고
    • Zirconia growth on zirconium carbide single crystals by oxidation
    • DOI 10.1016/j.surfcoat.2004.05.035, PII S0257897204004402
    • A. Bellucci, D. Gozzi, T. Kimura, T. Noda, and S. Otani Zirconia growth on zirconium carbide single crystals by oxidation Surf. Coat. Technol 197 2005 294 302 (Pubitemid 40696888)
    • (2005) Surface and Coatings Technology , vol.197 , Issue.2-3 , pp. 294-302
    • Bellucci, A.1    Gozzi, D.2    Kimura, T.3    Noda, T.4    Otani, S.5
  • 10
    • 0028439142 scopus 로고
    • Kinetics and mechanism of the oxidation of ZrC
    • G. Rama Rao, and V. Venugopal Kinetics and mechanism of the oxidation of ZrC J. Alloys Compd. 206 1994 237 242
    • (1994) J. Alloys Compd. , vol.206 , pp. 237-242
    • Rama Rao, G.1    Venugopal, V.2
  • 11
    • 84886365935 scopus 로고
    • High-temperature oxidation. IV. Zirconium and hafnium carbides
    • J.B. Berkowitz-Mattuck High-temperature oxidation. IV. Zirconium and hafnium carbides J. Electrochem. Soc. 114 1967 1030 1033
    • (1967) J. Electrochem. Soc. , vol.114 , pp. 1030-1033
    • Berkowitz-Mattuck, J.B.1
  • 12
    • 0025508134 scopus 로고
    • Oxidation kinetics of zirconium carbide at relatively low temperatures
    • S. Shimada, and T. Ishil Oxidation kinetics of zirconium carbide at relatively low temperatures J. Am. Ceram. Soc. 73 1990 2804 2808
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 2804-2808
    • Shimada, S.1    Ishil, T.2
  • 13
    • 0032660705 scopus 로고    scopus 로고
    • Oxidation kinetics of refractory carbides at low oxygen partial pressures
    • D. Gozzi, M. Montozzi, and P. Cignini Oxidation kinetics of refractory carbides at low oxygen partial pressures Solid State Ion. 123 1999 11 18
    • (1999) Solid State Ion. , vol.123 , pp. 11-18
    • Gozzi, D.1    Montozzi, M.2    Cignini, P.3
  • 14
    • 84975353152 scopus 로고
    • The oxidation kinetics of zirconium diboride and zirconium carbide at high temperatures
    • A.K. Kuriakose, and J.L. Margrave The oxidation kinetics of zirconium diboride and zirconium carbide at high temperatures J. Electrochem. Soc. 111 1964 827 831
    • (1964) J. Electrochem. Soc. , vol.111 , pp. 827-831
    • Kuriakose, A.K.1    Margrave, J.L.2
  • 15
    • 0029656765 scopus 로고    scopus 로고
    • Determination of the Active-to-Passive Transition in the Oxidation of Silicon Carbide in Standard and Microwave-Excited Air
    • DOI 10.1016/0955-2219(95)00104-2
    • M.J.H. Balat Determination of the active-to-passive transition in the oxidation of silicon carbide in standard and microwave-excited air J. Eur. Ceram. Soc. 16 1996 55 62 (Pubitemid 126403344)
    • (1996) Journal of the European Ceramic Society , vol.16 , Issue.1 , pp. 55-62
    • Balat, M.J.H.1
  • 16
    • 77953542256 scopus 로고    scopus 로고
    • In situ microscopy observation of liquid flow, zirconia growth, and CO bubble formation during high temperature oxidation of zirconium diboridesilicon carbide
    • S. Gangireddy, S.N. Karlsdottir, S.J. Norton, J.C. Tucker, and J.W. Halloran In situ microscopy observation of liquid flow, zirconia growth, and CO bubble formation during high temperature oxidation of zirconium diboridesilicon carbide J. Eur. Ceram. Soc. 30 2010 2365 2374
    • (2010) J. Eur. Ceram. Soc. , vol.30 , pp. 2365-2374
    • Gangireddy, S.1    Karlsdottir, S.N.2    Norton, S.J.3    Tucker, J.C.4    Halloran, J.W.5
  • 17
    • 48749120518 scopus 로고    scopus 로고
    • Microstructure and properties of pressureless sintered ZrC-based materials
    • L. Silvestroni, and D. Sciti Microstructure and properties of pressureless sintered ZrC-based materials J. Mater. Res 26 2008 1882 1889
    • (2008) J. Mater. Res , vol.26 , pp. 1882-1889
    • Silvestroni, L.1    Sciti, D.2
  • 19
    • 77953961270 scopus 로고    scopus 로고
    • High temperature oxidation of SiC under helium with low-pressure oxygen - Part 1: Sintered α-SiC
    • L. Charpentier, M. Balat-Pichelin, and F. Audubert High temperature oxidation of SiC under helium with low-pressure oxygen - part 1: sintered α-SiC J. Eur. Ceram. Soc. 30 2010 2653 2660
    • (2010) J. Eur. Ceram. Soc. , vol.30 , pp. 2653-2660
    • Charpentier, L.1    Balat-Pichelin, M.2    Audubert, F.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.