메뉴 건너뛰기




Volumn 36, Issue 13, 2011, Pages 8070-8081

Experimental studies on Nafion® 112 single PEM-FCs exposed to freezing conditions

Author keywords

Freezing thawing cycles; MEA Nafion 112; PEM FC polarization curves; Pt migration; Purging

Indexed keywords

ANODE SIDE; AUTOMOBILE APPLICATIONS; BROKEN FIBERS; CATALYTIC LAYERS; DEGRADATION EFFECT; DRY AIR; DRY GAS; EXPERIMENTAL STUDIES; FREEZING CONDITIONS; FREEZING/THAWING; MAXIMUM POWER OUTPUT; PEM-FC POLARIZATION CURVES; PERFORMANCE DEGRADATION; POLYMER ELECTROLYTE MEMBRANE FUEL CELLS; POWER DENSITIES; POWER OUT PUT; PT MIGRATION; PT PARTICLE; SINGLE CELLS; SUB-ZERO TEMPERATURES; WINTER TIME;

EID: 79957597038     PISSN: 03603199     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijhydene.2011.01.182     Document Type: Article
Times cited : (22)

References (66)
  • 1
    • 1542304757 scopus 로고    scopus 로고
    • International activities in DMFC R&D: Status of technologies and potential applications
    • R. Dillon, S. Srinivasan, A.S. Aric, and V. Antonucci International activities in DMFC R&D: status of technologies and potential applications J Power Sources 127 2004 112 116
    • (2004) J Power Sources , vol.127 , pp. 112-116
    • Dillon, R.1    Srinivasan, S.2    Aric, A.S.3    Antonucci, V.4
  • 2
  • 3
    • 2942588627 scopus 로고    scopus 로고
    • Effects of water removal on the performance degradation of PEMFCs Repetitively Brought to <0 °c
    • E.A. Cho, J.-J. Ko, H.Y. Ha, S.-A. Hong, K.-Y. Lee, and T.-W. Lim Effects of water removal on the performance degradation of PEMFCs Repetitively Brought to <0 °C J Electrochem Soc 151 2004 A661 A665
    • (2004) J Electrochem Soc , vol.151
    • Cho, E.A.1    Ko, J.-J.2    Ha, H.Y.3    Hong, S.-A.4    Lee, K.-Y.5    Lim, T.-W.6
  • 4
    • 33748984423 scopus 로고    scopus 로고
    • Effect of sub-freezing temperatures on a PEM fuel cell performance, startup and fuel cell components
    • DOI 10.1016/j.jpowsour.2006.02.075, PII S037877530600382X
    • Q. Yan, H. Toghiani, Y.-W. Lee, K. Liang, and H. Causey Effect of sub-freezing temperatures on a PEM fuel cell performance, startup and fuel cell components J Power Sources 160 2006 1242 1250 (Pubitemid 44441690)
    • (2006) Journal of Power Sources , vol.160 , Issue.2 SPEC. ISS. , pp. 1242-1250
    • Yan, Q.1    Toghiani, H.2    Lee, Y.-W.3    Liang, K.4    Causey, H.5
  • 5
    • 33644771034 scopus 로고    scopus 로고
    • Low temperature operation and influence parameters on the cold start ability of portable PEMFCs
    • DOI 10.1016/j.jpowsour.2005.10.035, PII S0378775305014345, Selected Papers from the Ninth Ulm Electrochemical Days
    • M. Oszcipok, M. Zedda, D. Riemann, and D. Geckeler Low temperature operation and influence parameters on the cold start ability of portable PEMFCs J Power Sources 154 2006 404 411 (Pubitemid 43343796)
    • (2006) Journal of Power Sources , vol.154 , Issue.2 , pp. 404-411
    • Oszcipok, M.1    Zedda, M.2    Riemann, D.3    Geckeler, D.4
  • 6
    • 33845639605 scopus 로고    scopus 로고
    • Behavior of water below the freezing point in PEFCs
    • DOI 10.1016/j.jpowsour.2006.08.026, PII S0378775306015886, Papers presented at the FUEL PROCESSING FOR HYDROGEN PRODUCTION SYMPOSIUM at the 230th American Chemical SocietyNational Meeting
    • Y. Ishikawa, T. Morita, K. Nakata, K. Yoshida, and M. Shiozawa Behavior of water below the freezing point in PEFCs J Power Sources 163 2007 708 712 (Pubitemid 44959590)
    • (2007) Journal of Power Sources , vol.163 , Issue.2 , pp. 708-712
    • Ishikawa, Y.1    Morita, T.2    Nakata, K.3    Yoshida, K.4    Shiozawa, M.5
  • 7
    • 53449098047 scopus 로고    scopus 로고
    • Numerical analyses of non-isothermal self-start behaviors of PEM fuel cells from subfreezing startup temperatures
    • H. Meng Numerical analyses of non-isothermal self-start behaviors of PEM fuel cells from subfreezing startup temperatures Int J Hydrogen Energy 33 2008 5738 5747
    • (2008) Int J Hydrogen Energy , vol.33 , pp. 5738-5747
    • Meng, H.1
  • 8
    • 33845677632 scopus 로고    scopus 로고
    • Gas diffusion layer durability under steady-state and freezing conditions
    • DOI 10.1016/j.jpowsour.2006.09.092, PII S0378775306021318
    • C. Lee, and W. Mérida Gas diffusion layer durability under steady-state and freezing conditions J Power Sources 164 2007 141 153 (Pubitemid 44959655)
    • (2007) Journal of Power Sources , vol.164 , Issue.1 , pp. 141-153
    • Lee, C.1    Merida, W.2
  • 9
    • 23844495622 scopus 로고    scopus 로고
    • Statistic analysis of operational influences on the cold start behaviour of PEM fuel cells
    • M. Oszcipok, D. Riemann, U. Kronenwett, M. Kreideweis, and M. Zedda Statistic analysis of operational influences on the cold start behaviour of PEM fuel cells J Power Sources 145 2005 407 415
    • (2005) J Power Sources , vol.145 , pp. 407-415
    • Oszcipok, M.1    Riemann, D.2    Kronenwett, U.3    Kreideweis, M.4    Zedda, M.5
  • 10
    • 41949108195 scopus 로고    scopus 로고
    • A review of the main parameters influencing long-term performance and durability of PEM fuel cells
    • W. Schmittinger, and A. Vahidi A review of the main parameters influencing long-term performance and durability of PEM fuel cells J Power Sources 180 2008 1 14
    • (2008) J Power Sources , vol.180 , pp. 1-14
    • Schmittinger, W.1    Vahidi, A.2
  • 11
    • 35748969892 scopus 로고    scopus 로고
    • Physical degradation of membrane electrode assemblies undergoing freeze/thaw cycling: Micro-structure effects
    • DOI 10.1016/j.jpowsour.2007.08.111, PII S0378775307017636, Hybrid Electric Vehicles
    • S. Kim, and M.M. Mench Physical degradation of membrane electrode assemblies undergoing freeze/thaw cycling: micro-structure effects J Power Sources 174 2007 206 220 (Pubitemid 350051659)
    • (2007) Journal of Power Sources , vol.174 , Issue.1 , pp. 206-220
    • Kim, S.1    Mench, M.M.2
  • 12
    • 40049111241 scopus 로고    scopus 로고
    • Physical degradation of membrane electrode assemblies undergoing freeze/thaw cycling: Diffusion media effects
    • S. Kim, B.K. Ahn, and M.M. Mench Physical degradation of membrane electrode assemblies undergoing freeze/thaw cycling: diffusion media effects J Power Sources 179 2008 140 146
    • (2008) J Power Sources , vol.179 , pp. 140-146
    • Kim, S.1    Ahn, B.K.2    Mench, M.M.3
  • 15
    • 44649111826 scopus 로고    scopus 로고
    • Degradation effects in polymer electrolyte membrane fuel cell stacks by sub-zero operation - An in situ and ex situ analysis
    • R. Alink, D. Gerteisen, and M. Oszcipok Degradation effects in polymer electrolyte membrane fuel cell stacks by sub-zero operation - An in situ and ex situ analysis J Power Sources 182 2008 175 187
    • (2008) J Power Sources , vol.182 , pp. 175-187
    • Alink, R.1    Gerteisen, D.2    Oszcipok, M.3
  • 16
    • 34848838589 scopus 로고    scopus 로고
    • ® membranes at low temperature, probed by micro X-ray diffraction
    • DOI 10.1016/j.jpowsour.2007.05.037, PII S0378775307010300
    • ® membranes at low temperature, probed by micro X-ray diffraction J Power Sources 172 2007 587 596 (Pubitemid 47496087)
    • (2007) Journal of Power Sources , vol.172 , Issue.2 , pp. 587-596
    • Pineri, M.1    Gebel, G.2    Davies, R.J.3    Diat, O.4
  • 18
    • 51349109532 scopus 로고    scopus 로고
    • Kinetic investigation of oxygen reduction reaction in sub-freezing acid media
    • W. Song, J. Hou, H. Yu, L. Hao, Z. Shao, and B. Yi Kinetic investigation of oxygen reduction reaction in sub-freezing acid media Int J Hydrogen Energy 33 2008 4844 4848
    • (2008) Int J Hydrogen Energy , vol.33 , pp. 4844-4848
    • Song, W.1    Hou, J.2    Yu, H.3    Hao, L.4    Shao, Z.5    Yi, B.6
  • 19
    • 57249097076 scopus 로고    scopus 로고
    • Experimental and theoretical investigations on a proton exchange membrane fuel cell starting up at subzero temperatures
    • E. Pinton, Y. Fourneron, S. Rosini, and L. Antoni Experimental and theoretical investigations on a proton exchange membrane fuel cell starting up at subzero temperatures J Power Sources 186 2009 80 88
    • (2009) J Power Sources , vol.186 , pp. 80-88
    • Pinton, E.1    Fourneron, Y.2    Rosini, S.3    Antoni, L.4
  • 21
    • 79957594486 scopus 로고    scopus 로고
    • General Motors Corporation. Detroit MI (US) US Patent 6358637
    • General Motors Corporation. Detroit MI (US). Freeze-protecting a fuel cell by vacuum drying. US Patent 6358637; 1999.
    • (1999) Freeze-protecting A Fuel Cell by Vacuum Drying
  • 22
    • 79957610059 scopus 로고    scopus 로고
    • Energy Partners LC. Palm Beach FL (US) Patent WO/2000/065676
    • Energy Partners LC. Palm Beach FL (US). Freeze tolerant fuel cell system and method. Patent WO/2000/065676; 2000.
    • (2000) Freeze Tolerant Fuel Cell System and Method
  • 27
    • 33750002473 scopus 로고    scopus 로고
    • Analysis of PEMFC freeze degradation at -20 °C after gas purging
    • DOI 10.1016/j.jpowsour.2006.07.010, PII S0378775306012365
    • J. Hou, H. Yu, S. Zhang, S. Sun, H. Wang, and B. Yi Analysis of PEMFC freeze degradation at -20 °C after gas purging J Power Sources 162 2006 513 520 (Pubitemid 44573749)
    • (2006) Journal of Power Sources , vol.162 , Issue.1 , pp. 513-520
    • Hou, J.1    Yu, H.2    Zhang, S.3    Sun, S.4    Wang, H.5    Yi, B.6    Ming, P.7
  • 28
    • 36549084024 scopus 로고    scopus 로고
    • Investigation of resided water effects on PEM fuel cell after cold start
    • DOI 10.1016/j.ijhydene.2007.05.004, PII S036031990700287X
    • J. Hou, B. Yi, H. Yu, L. Hao, W. Song, and Y. Fu Investigation of resided water effects on PEM fuel cell after cold start Int J Hydrogen Energy 32 2007 4503 4509 (Pubitemid 350180187)
    • (2007) International Journal of Hydrogen Energy , vol.32 , Issue.17 , pp. 4503-4509
    • Hou, J.1    Yi, B.2    Yu, H.3    Hao, L.4    Song, W.5    Fu, Y.6    Shao, Z.7
  • 29
    • 33845996602 scopus 로고    scopus 로고
    • Effects of freeze/thaw cycles and gas purging method on polymer electrolyte membrane fuel cells
    • S. Zang, B. Yi, and P. Ming Effects of freeze/thaw cycles and gas purging method on polymer electrolyte membrane fuel cells Chin J Chem Eng 14 2006 802 805
    • (2006) Chin J Chem Eng , vol.14 , pp. 802-805
    • Zang, S.1    Yi, B.2    Ming, P.3
  • 30
    • 33846219162 scopus 로고    scopus 로고
    • Effects of purging on the degradation of PEMFCs operating with repetitive on/off cycles
    • S.-Y. Lee, E.A. Cho, J.-H. Lee, H.-J. Kim, T.-H. Lim, and I.-H. Oh Effects of purging on the degradation of PEMFCs operating with repetitive on/off cycles J Electrochem Soc 154 2007 B194 B200
    • (2007) J Electrochem Soc , vol.154
    • Lee, S.-Y.1    Cho, E.A.2    Lee, J.-H.3    Kim, H.-J.4    Lim, T.-H.5    Oh, I.-H.6
  • 31
    • 33947180961 scopus 로고    scopus 로고
    • Characteristics of subzero startup and water/ice formation on the catalyst layer in a polymer electrolyte fuel cell
    • DOI 10.1016/j.electacta.2007.01.038, PII S0013468607001569
    • S. Ge, and C.Y. Wang Characteristics of subzero startup and water/ice formation on the catalyst layer in a PEMFC Electrochim Acta 52 2007 4825 4835 (Pubitemid 46412299)
    • (2007) Electrochimica Acta , vol.52 , Issue.14 , pp. 4825-4835
    • Ge, S.1    Wang, C.-Y.2
  • 32
    • 48249121079 scopus 로고    scopus 로고
    • Water removal from a PEFC during gas purge
    • K. Tajiri, C.-Y. Wang, and Y. Tabuchi Water removal from a PEFC during gas purge Electrochim Acta 53 2008 6337 6343
    • (2008) Electrochim Acta , vol.53 , pp. 6337-6343
    • Tajiri, K.1    Wang, C.-Y.2    Tabuchi, Y.3
  • 33
    • 77951023854 scopus 로고    scopus 로고
    • Degradation behaviors of polymer electrolyte membrane fuel cell under freeze/thaw cycles
    • M. Luo, C. Huang, W. Liu, Z. Luo, and M. Pan Degradation behaviors of polymer electrolyte membrane fuel cell under freeze/thaw cycles Int J Hydrogen Energy 35 2010 2986 2993
    • (2010) Int J Hydrogen Energy , vol.35 , pp. 2986-2993
    • Luo, M.1    Huang, C.2    Liu, W.3    Luo, Z.4    Pan, M.5
  • 35
    • 77951106278 scopus 로고    scopus 로고
    • Cold start analysis of polymer electrolyte membrane fuel cells
    • K. Jiao, and X. Li Cold start analysis of polymer electrolyte membrane fuel cells Int J Hydrogen Energy 35 2010 5077 5094
    • (2010) Int J Hydrogen Energy , vol.35 , pp. 5077-5094
    • Jiao, K.1    Li, X.2
  • 36
    • 77955296098 scopus 로고    scopus 로고
    • Characteristics of proton exchange membrane fuel cells cold start with silica in cathode catalyst layers
    • Z. Miao, H. Yu, W. Song, L. Hao, Z. Shao, and Q. Shen Characteristics of proton exchange membrane fuel cells cold start with silica in cathode catalyst layers Int J Hydrogen Energy 35 2010 5552 5557
    • (2010) Int J Hydrogen Energy , vol.35 , pp. 5552-5557
    • Miao, Z.1    Yu, H.2    Song, W.3    Hao, L.4    Shao, Z.5    Shen, Q.6
  • 37
    • 77957335492 scopus 로고    scopus 로고
    • Effect of catalytic ink on sub-freezing endurance of PEMFCs
    • W. Song, H. Yu, L. Hao, B. Yi, and Z. Shao Effect of catalytic ink on sub-freezing endurance of PEMFCs Int J Hydrogen Energy 35 2010 11129 11137
    • (2010) Int J Hydrogen Energy , vol.35 , pp. 11129-11137
    • Song, W.1    Yu, H.2    Hao, L.3    Yi, B.4    Shao, Z.5
  • 38
    • 43049125787 scopus 로고    scopus 로고
    • Water removal characteristics of proton exchange membrane fuel cells using a dry gas purging method
    • S.-Y. Lee, S.-U. Kim, H.-J. Kim, J.H. Jang, I.-H. Oh, and E.A. Cho Water removal characteristics of proton exchange membrane fuel cells using a dry gas purging method J Power Sources 180 2008 784 790
    • (2008) J Power Sources , vol.180 , pp. 784-790
    • Lee, S.-Y.1    Kim, S.-U.2    Kim, H.-J.3    Jang, J.H.4    Oh, I.-H.5    Cho, E.A.6
  • 40
    • 48949117591 scopus 로고    scopus 로고
    • Progress in the US DOE fuel cell subprogram efforts in polymer electrolyte fuel cells
    • J. Marcinkoski, J.P. Kopasz, and T.G. Benjamin Progress in the US DOE fuel cell subprogram efforts in polymer electrolyte fuel cells Int J Hydrogen Energy 33 2008 3894 3902
    • (2008) Int J Hydrogen Energy , vol.33 , pp. 3894-3902
    • Marcinkoski, J.1    Kopasz, J.P.2    Benjamin, T.G.3
  • 41
    • 38049087430 scopus 로고    scopus 로고
    • Fuel cell systems for transportation: Status and trends
    • R.K. Ahluwalia, and X. Wang Fuel cell systems for transportation: status and trends J Power Sources 177 2008 167 176
    • (2008) J Power Sources , vol.177 , pp. 167-176
    • Ahluwalia, R.K.1    Wang, X.2
  • 48
    • 0024000178 scopus 로고
    • Change of Pt distribution in the active components of phosphoric acid fuel cell
    • J. Aragane, T. Murahashi, and T. Odaka Change of Pt distribution in the active components of phosphoric acid fuel cell J Electrochem Soc 135 1988 844 850 (Pubitemid 18604278)
    • (1988) Journal of the Electrochemical Society , vol.135 , Issue.4 , pp. 844-850
    • Aragane, J.1    Murahashi, T.2    Odaka, T.3
  • 49
    • 27944444164 scopus 로고    scopus 로고
    • Instability of Pt/C electrocatalysts in proton exchange membrane fuel cells: A mechanistic investigation
    • P.J. Ferreira, R. Makharia, S. Kocha, H. Gasteiger, D. Morgan, and G.J. la O' Instability of Pt/C electrocatalysts in proton exchange membrane fuel cells: a mechanistic investigation J Electrochem Soc 152 2005 A2256 A2271
    • (2005) J Electrochem Soc , vol.152
    • Ferreira, P.J.1    Makharia, R.2    Kocha, S.3    Gasteiger, H.4    Morgan, D.5    La, O.'.G.J.6
  • 50
    • 33846608718 scopus 로고    scopus 로고
    • Formation mechanism of Pt single-crystal nanoparticles in proton exchange membrane fuel cells
    • P.J. Ferreira, and Y. Shao-Hornb Formation mechanism of Pt single-crystal nanoparticles in proton exchange membrane fuel cells Electrochem Solid-State Lett 10 2007 B60 B63
    • (2007) Electrochem Solid-State Lett , vol.10
    • Ferreira, P.J.1    Shao-Hornb, Y.2
  • 51
  • 52
    • 50949115781 scopus 로고    scopus 로고
    • The influence of the electrochemical stressing (potential step and potential-static holding) on the degradation of polymer electrolyte membrane fuel cell electrocatalysts
    • Y. Shao, R. Kou, J. Wang, V.V. Viswanathan, J.H. Kwak, and J. Liu The influence of the electrochemical stressing (potential step and potential-static holding) on the degradation of polymer electrolyte membrane fuel cell electrocatalysts J Power Sources 185 2008 280 286
    • (2008) J Power Sources , vol.185 , pp. 280-286
    • Shao, Y.1    Kou, R.2    Wang, J.3    Viswanathan, V.V.4    Kwak, J.H.5    Liu, J.6
  • 56
    • 0039990040 scopus 로고    scopus 로고
    • Morphological variation of platinum catalysts in phosphotungstic acid fuel cell
    • PII S0378775397026967
    • P. Staiti, A.S. Aric, V. Antonucci, and S. Hocevar Morphological variation of platinum catalysts in phosphotungstic acid fuel cell J Power Sources 70 1998 91 101 (Pubitemid 128374712)
    • (1998) Journal of Power Sources , vol.70 , Issue.1 , pp. 91-101
    • Staiti, P.1    Arico, A.S.2    Antonucci, V.3    Hocevar, S.4
  • 60
    • 39149127963 scopus 로고    scopus 로고
    • Modeling of PEM fuel cell Pt/C catalyst degradation
    • W. Bi, and T.F. Fuller Modeling of PEM fuel cell Pt/C catalyst degradation J Power Sources 178 2008 188 196
    • (2008) J Power Sources , vol.178 , pp. 188-196
    • Bi, W.1    Fuller, T.F.2
  • 63
    • 33750007305 scopus 로고    scopus 로고
    • Durability study of proton exchange membrane fuel cells under dynamic testing conditions with cyclic current profile
    • DOI 10.1016/j.jpowsour.2006.07.007, PII S0378775306012493
    • D. Liu, and S. Case Durability study of proton exchange membrane fuel cells under dynamic testing conditions with cyclic current profile J Power Sources 162 2006 521 531 (Pubitemid 44573761)
    • (2006) Journal of Power Sources , vol.162 , Issue.1 , pp. 521-531
    • Liu, D.1    Case, S.2
  • 64
    • 20344367747 scopus 로고    scopus 로고
    • Microstructural changes of membrane electrode assemblies during PEFC durability testing at high humidity conditions
    • J. Xie, D.L. Wood, K.L. More, P. Atanassov, and R.L. Borup Microstructural changes of membrane electrode assemblies during PEFC durability testing at high humidity conditions J Electrochem Soc 152 2005 A1011 A1020
    • (2005) J Electrochem Soc , vol.152
    • Xie, J.1    Wood, D.L.2    More, K.L.3    Atanassov, P.4    Borup, R.L.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.