메뉴 건너뛰기




Volumn 54, Issue 4, 2011, Pages 618-624

Determination of mixed-mode interfacial fracture toughness for thermal barrier coatings

Author keywords

energy release rate; fracture toughness; interface; mixed mode; multilayer; thermal barrier coating

Indexed keywords

AIR PLASMA SPRAYED; ANALYTICAL EXPRESSIONS; ANALYTICAL SOLUTIONS; CRITICAL ENERGY RELEASE RATE; FINITE ELEMENT ANALYSIS; INTERFACE; INTERFACIAL FAILURES; INTERFACIAL FRACTURE TOUGHNESS; MIXED MODE; PLASTIC WORK; POSITIVE MODE; SHEAR MODES; TEST METHOD;

EID: 79956211526     PISSN: 16747348     EISSN: None     Source Type: Journal    
DOI: 10.1007/s11433-011-4278-0     Document Type: Article
Times cited : (12)

References (26)
  • 1
    • 0034744720 scopus 로고    scopus 로고
    • Mechanics-based scaling laws for the durability of thermal barrier coatings
    • DOI 10.1016/S0079-6425(00)00007-4
    • A. G. Evans M. Y. He J. W. Hutchinson 2001 Mechanics-based scaling laws for the durability of thermal barrier coatings Prog Mater Sci 46 249 271 10.1016/S0079-6425(00)00007-4 (Pubitemid 32264827)
    • (2001) Progress in Materials Science , vol.46 , Issue.3-4 , pp. 249-271
    • Evans, A.G.1    He, M.Y.2    Hutchinson, J.W.3
  • 2
    • 0034743572 scopus 로고    scopus 로고
    • Mechanisms controlling the durability of thermal barrier coatings
    • DOI 10.1016/S0079-6425(00)00020-7, PII S0079642500000207
    • A. G. Evans D. R. Mumm J. W. Hutchinson, et al. 2001 Mechanisms controlling the durability of thermal barrier coatings Prog Mater Sci 46 505 553 10.1016/S0079-6425(00)00020-7 (Pubitemid 32536036)
    • (2001) Progress in Materials Science , vol.46 , Issue.5 , pp. 505-553
    • Evans, A.G.1    Mumm, D.R.2    Hutchinson, J.W.3    Meier, G.H.4    Pettit, F.S.5
  • 3
    • 0343389545 scopus 로고    scopus 로고
    • On the role of imperfections in the failure of a thermal barrier coating made by electron beam deposition
    • 10.1016/S1359-6454(99)00473-5
    • D. R. Mumm A. G. Evans 2000 On the role of imperfections in the failure of a thermal barrier coating made by electron beam deposition Acta Mater 48 1815 1827 10.1016/S1359-6454(99)00473-5
    • (2000) Acta Mater , vol.48 , pp. 1815-1827
    • Mumm, D.R.1    Evans, A.G.2
  • 4
    • 0032626303 scopus 로고    scopus 로고
    • Delamination of multilayer thermal barrier coatings
    • 10.1016/S0167-6636(99)00016-2
    • S. R. Choi J. W. Hutchinson A. G. Evans 1999 Delamination of multilayer thermal barrier coatings Mech Mater 31 431 447 10.1016/S0167-6636(99)00016-2
    • (1999) Mech Mater , vol.31 , pp. 431-447
    • Choi, S.R.1    Hutchinson, J.W.2    Evans, A.G.3
  • 5
    • 0023979063 scopus 로고
    • Elastic fracture-mechanics concepts for interfacial cracks
    • J. R. Rice 1988 Elastic fracture-mechanics concepts for interfacial cracks J Appl Mech-Trans ASME 55 98 103 10.1115/1.3173668 (Pubitemid 18590050)
    • (1988) Journal of Applied Mechanics, Transactions ASME , vol.55 , Issue.1 , pp. 98-103
    • Rice, J.R.1
  • 6
    • 0025421834 scopus 로고
    • Interface crack between 2 elastic layers
    • 10.1007/BF00018123
    • Z. G. Suo J. W. Hutchinson 1990 Interface crack between 2 elastic layers Int J Fract 43 1 18 10.1007/BF00018123
    • (1990) Int J Fract , vol.43 , pp. 1-18
    • Suo, Z.G.1    Hutchinson, J.W.2
  • 7
    • 0032650251 scopus 로고    scopus 로고
    • Modified four-point bending specimen for determining the interface fracture energy for thin, brittle layers
    • 10.1023/A:1007530932726
    • I. Hofinger M. Oechsner H. A. Bahr, et al. 1998 Modified four-point bending specimen for determining the interface fracture energy for thin, brittle layers Int J Fract 92 213 220 10.1023/A:1007530932726
    • (1998) Int J Fract , vol.92 , pp. 213-220
    • Hofinger, I.1    Oechsner, M.2    Bahr, H.A.3
  • 8
    • 0024621114 scopus 로고
    • A test specimen for determining the fracture resistarim of bimaterial interfaces
    • 10.1115/1.3176069
    • P. G. Charalambides J. Lund A. G. Evans, et al. 1989 A test specimen for determining the fracture resistarim of bimaterial interfaces J Appl Mech-Trans ASME 56 77 82 10.1115/1.3176069
    • (1989) J Appl Mech-Trans ASME , vol.56 , pp. 77-82
    • Charalambides, P.G.1    Lund, J.2    Evans, A.G.3
  • 9
    • 0035957778 scopus 로고    scopus 로고
    • Measurement of interfacial toughness in thermal barrier coating systems by indentation
    • DOI 10.1016/S0013-7944(00)00130-2, PII S0013794400001302
    • A. Vasinonta J. L. Beuth 2001 Measurement of interfacial toughness in thermal barrier coating systems by indentation Eng Fract Mech 68 843 860 10.1016/S0013-7944(00)00130-2 (Pubitemid 32406549)
    • (2001) Engineering Fracture Mechanics , vol.68 , Issue.7 , pp. 843-860
    • Vasinonta, A.1    Beuth, J.L.2
  • 10
    • 67749133629 scopus 로고    scopus 로고
    • Interfacial fracture toughness of APS bond coat/substrate under high temperature
    • 10.1007/s10704-008-9294-3 05640155
    • H. Y. Qi X. G. Yang Y. M. Wang 2009 Interfacial fracture toughness of APS bond coat/substrate under high temperature Int J Fract 157 71 80 10.1007/s10704-008-9294-3 05640155
    • (2009) Int J Fract , vol.157 , pp. 71-80
    • Qi, H.Y.1    Yang, X.G.2    Wang, Y.M.3
  • 11
    • 23844527153 scopus 로고    scopus 로고
    • Measurement of interfacial shear mechanical properties in thermal barrier coating systems by a barb pullout method
    • DOI 10.1016/j.scriptamat.2005.07.012, PII S1359646205004203
    • S. Q. Guo D. R. Mumm A. M. Karlsson, et al. 2005 Measurement of interfacial shear mechanical properties in thermal barrier coating systems by a barb pullout method Scrip Mater 53 1043 1048 10.1016/j.scriptamat.2005.07.012 (Pubitemid 41162525)
    • (2005) Scripta Materialia , vol.53 , Issue.9 , pp. 1043-1048
    • Guo, S.Q.1    Mumm, D.R.2    Karlsson, A.M.3    Kagawa, Y.4
  • 12
    • 36249016746 scopus 로고    scopus 로고
    • Analysis of a "barb test" for measuring the mixed-mode delamination toughness of coatings
    • DOI 10.1016/j.actamat.2007.08.052, PII S1359645407006003
    • Y. F. Liu Y. Kagawa A. G. Evans 2008 Analysis of a "barb test" for measuring the mixed-mode delamination toughness of coatings Acta Mater 56 43 49 10.1016/j.actamat.2007.08.052 (Pubitemid 350123099)
    • (2008) Acta Materialia , vol.56 , Issue.1 , pp. 43-49
    • Liu, Y.-F.1    Kagawa, Y.2    Evans, A.G.3
  • 13
    • 0033187930 scopus 로고    scopus 로고
    • A modified mixed-mode bending specimen for the interfacial fracture testing of dissimilar materials
    • W. O. Soboyejo G. Y. Lu S. Chengalva, et al. 1999 A modified mixed-mode bending specimen for the interfacial fracture testing of dissimilar materials Fatigue Fract Eng M 22 799 810
    • (1999) Fatigue Fract Eng M , vol.22 , pp. 799-810
    • Soboyejo, W.O.1    Lu, G.Y.2    Chengalva, S.3
  • 14
    • 0001844390 scopus 로고    scopus 로고
    • A single leg bending test for interfacial fracture toughness determination
    • B. D. Davidson V. Sundararaman 1996 A single leg bending test for interfacial fracture toughness determination Int J Fract 78 193 210 10.1007/BF00034525 (Pubitemid 126712875)
    • (1996) International Journal of Fracture , vol.78 , Issue.2 , pp. 193-210
    • Davidson, B.D.1    Sundararaman, V.2
  • 15
    • 34047231305 scopus 로고    scopus 로고
    • Mixed-mode interfacial fracture toughness for thermal barrier coating
    • DOI 10.1016/j.engfracmech.2006.10.021, PII S0013794406004127
    • M. Arai Y. Kajima K. Kishimoto 2007 Mixed-mode interfacial fracture toughness for thermal barrier coating Eng Fract Mech 74 2055 2069 10.1016/j.engfracmech.2006.10.021 (Pubitemid 46534812)
    • (2007) Engineering Fracture Mechanics , vol.74 , Issue.13 , pp. 2055-2069
    • Arai, M.1    Okajima, Y.2    Kishimoto, K.3
  • 16
    • 33748438529 scopus 로고    scopus 로고
    • The determination of the delamination resistance in thermal barrier coating system by four-point bending tests
    • DOI 10.1016/j.surfcoat.2005.12.023, PII S0257897205013903
    • Y. Yamazaki A. Schmidt A. Scholz 2006 The determination of the delamination resistance in thennal barrier coating system by four-point bending tests Surf Coat Tech 201 744 754 10.1016/j.surfcoat.2005.12.023 (Pubitemid 44340771)
    • (2006) Surface and Coatings Technology , vol.201 , Issue.3-4 , pp. 744-754
    • Yamazaki, Y.1    Schmidt, A.2    Scholz, A.3
  • 18
    • 0024032029 scopus 로고
    • Elastic-plastic analysis of cracks on bimaterial interfaces: Part 1. Small-Scale Yielding
    • C. F. Shih R. J. Asaro 1988 Elastic-plastic analysis of cracks on bimaterial interfaces 1. Small-Scale Yielding J Appl Mech-Trans ASME 55 299 316 10.1115/1.3173676 (Pubitemid 18646470)
    • (1988) Journal of Applied Mechanics, Transactions ASME , vol.55 , Issue.2 , pp. 299-316
    • Shih, C.F.1    Asaro, R.J.2
  • 19
    • 79956226039 scopus 로고    scopus 로고
    • ABAQUS/Standard. Hinnitt, Karlsson & Sorensen, Inc. Providence (RI)
    • ABAQUS/Standard: Users's Manual. Version 6.9. Providence (RI): Hinnitt, Karlsson & Sorensen, Inc. 2009
    • (2009) Users's Manual. Version 6.9
  • 20
    • 0000919351 scopus 로고
    • On the analysis of mixed-mode failure
    • 1992IJFr.54.269C
    • M. Charalambides A. J. Kinloch Y. Wang, et al. 1992 On the analysis of mixed-mode failure Int J Fracture 54 269 291 1992IJFr...54..269C
    • (1992) Int J Fracture , vol.54 , pp. 269-291
    • Charalambides, M.1    Kinloch, A.J.2    Wang, Y.3
  • 21
    • 0025461953 scopus 로고
    • Experimental-determination of interfacial toughness curves using Brazil-Nut-Sandwiches
    • 10.1016/0956-7151(90)90200-Z
    • J. S. Wang Z. Suo 1990 Experimental-determination of interfacial toughness curves using Brazil-Nut-Sandwiches Acta Metall Mater 38 1279 1290 10.1016/0956-7151(90)90200-Z
    • (1990) Acta Metall Mater , vol.38 , pp. 1279-1290
    • Wang, J.S.1    Suo, Z.2
  • 22
    • 0030408924 scopus 로고    scopus 로고
    • Residual stresses in thermal spray coatings and their effect on interfacial adhesion: A review of recent work
    • T. W. Clyne S. C. Gill 1996 Residual stresses in thermal spray coatings and their effect on interfacial adhesion: A review of recent work J Therm Spray Tech 5 401 418 10.1007/BF02645271 1996JTST....5..401C (Pubitemid 126591516)
    • (1996) Journal of Thermal Spray Technology , vol.5 , Issue.4 , pp. 401-418
    • Clyne, T.W.1    Gill, S.C.2
  • 23
    • 0026219801 scopus 로고
    • Biaxial loading experiments for determining interfacial fracture toughness
    • K. M. Liechti Y. S. Chai 1991 Biaxial loading experiments for determining interfacial fracture-toughness J Appl Mech-Trans ASME 58 680 687 10.1115/1.2897248 (Pubitemid 21708482)
    • (1991) Journal of Applied Mechanics, Transactions ASME , vol.58 , Issue.3 , pp. 680-687
    • Liechti, K.M.1    Chai, Y.-S.2
  • 24
    • 33748431401 scopus 로고    scopus 로고
    • The effect of self-assembled monolayers on interfacial fracture
    • DOI 10.1115/1.1940662
    • A. W. Mello K. M. Liechti 2006 The effect of self-assembled monolayers on interfacial fracture J Appl Mech-Trans ASME 73 860 870 10.1115/1.1940662 1111.74555 (Pubitemid 44343287)
    • (2006) Journal of Applied Mechanics, Transactions ASME , vol.73 , Issue.5 , pp. 860-870
    • Mello, A.W.1    Liechti, K.M.2
  • 25
    • 0002432484 scopus 로고    scopus 로고
    • Asymmetric shielding mechanisms in the mixed-mode fracture of a glass/epoxy interface
    • J. G. Swadener K. M. Liechti 1998 Asymmetric shielding mechanisms in the mixed-mode fracture of a glass/epoxy interface J Appl Mech-Trans ASME 65 25 29 10.1115/1.2789035 (Pubitemid 128728544)
    • (1998) Journal of Applied Mechanics, Transactions ASME , vol.65 , Issue.1 , pp. 25-29
    • Swadener, J.G.1    Liechti, K.M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.