Volumn 3, Issue 2, 2010, Pages 800-814

Stability of nanocrystalline spark plasma sintered 3Y-TZP

Author keywords

3Y TZP; Degradation; Grain size; Phase transformation

Indexed keywords

3Y-TZP; GRAIN SIZE; HYDROTHERMAL AGEING; NANOCRYSTALLINES; NEAR SURFACE REGIONS; RELATIVE DENSITY; RESULTING MATERIALS; SOAKING TIME;

EID: 78649468247     PISSN: None     EISSN: 19961944     Source Type: Journal    
DOI: 10.3390/ma3020800     Document Type: Article
Times cited : (32)

References (41)
  • 1
    • 0033873591 scopus 로고    scopus 로고
    • Transformation toughening in zirconia-containing ceramics
    • Hannink, R.H.J.; Nelly, P.M.; Muddle, B.C. Transformation toughening in zirconia-containing ceramics. J. Am. Ceram. Soc. 2000, 83, 461-487.
    • (2000) J. Am. Ceram. Soc , vol.83 , pp. 461-487
    • Hannink, R.H.J.1    Nelly, P.M.2    Muddle, B.C.3
  • 2
    • 0019044985 scopus 로고
    • Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageing
    • Kobayashi, K.; Kuwajima, H.; Masaki, T. Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageing. Solid State Ion. 1980, 3, 489-493.
    • (1980) Solid State Ion , vol.3 , pp. 489-493
    • Kobayashi, K.1    Kuwajima, H.2    Masaki, T.3
  • 3
    • 0036061888 scopus 로고    scopus 로고
    • The martensitic transformation in ceramics: Its role in transformation toughening
    • Kelly, P.M.; Rose, L.R.F. The martensitic transformation in ceramics: Its role in transformation toughening. Prog. Mater. Sci. 2002, 47, 463-557.
    • (2002) Prog. Mater. Sci , vol.47 , pp. 463-557
    • Kelly, P.M.1    Rose, L.R.F.2
  • 5
    • 0035418342 scopus 로고    scopus 로고
    • Hydrothermal degradation mechanism of tetragonal zirconia
    • Guo, X. Hydrothermal degradation mechanism of tetragonal zirconia. J. Mat. Sci. 2001, 36, 3737-3744.
    • (2001) J. Mat. Sci , vol.36 , pp. 3737-3744
    • Guo, X.1
  • 6
    • 17844386116 scopus 로고    scopus 로고
    • Stability of Y-TZP during hydrothermal treatment: Neutron experiments and stability considerations
    • Schubert, H.; Frey, F. Stability of Y-TZP during hydrothermal treatment: Neutron experiments and stability considerations. J. Eur. Ceram. Soc. 2005, 25, 1597-1602.
    • (2005) J. Eur. Ceram. Soc , vol.25 , pp. 1597-1602
    • Schubert, H.1    Frey, F.2
  • 8
    • 0029237462 scopus 로고
    • Environmental degradation of zirconia ceramics
    • Lawson, S. Environmental degradation of zirconia ceramics. J. Eur. Ceram. Soc. 1995, 15, 485-502.
    • (1995) J. Eur. Ceram. Soc , vol.15 , pp. 485-502
    • Lawson, S.1
  • 12
    • 34547381199 scopus 로고    scopus 로고
    • Low-temperature degradation of zirconia and implications for biomedical implants
    • Chevalier, J.; Laurent, G.; Sylvain, D. Low-temperature degradation of zirconia and implications for biomedical implants. Annu. Rev. Mater. Res. 2007, 37, 1-32.
    • (2007) Annu. Rev. Mater. Res , vol.37 , pp. 1-32
    • Chevalier, J.1    Laurent, G.2    Sylvain, D.3
  • 13
    • 0033886246 scopus 로고    scopus 로고
    • Sintering Behavior Of Nanocrystalline zirconia prepared by chemical vapor synthesis
    • Vladimir, V.S.; Markus, W.; Horst, H. Sintering Behavior Of Nanocrystalline zirconia prepared by chemical vapor synthesis. J. Am. Ceram. Soc. 2000, 83, 729-736.
    • (2000) J. Am. Ceram. Soc , vol.83 , pp. 729-736
    • Vladimir, V.S.1    Markus, W.2    Horst, H.3
  • 14
    • 0000587728 scopus 로고    scopus 로고
    • Low-temperature sintering and microstructural development of nanocrystalline Y-TZP powders
    • Duran, P.; Villegas, M.; Capel, F.; Recio, P.; Moure, C. Low-temperature sintering and microstructural development of nanocrystalline Y-TZP powders. J. Eur. Ceram. Soc. 1996, 16, 945-952.
    • (1996) J. Eur. Ceram. Soc , vol.16 , pp. 945-952
    • Duran, P.1    Villegas, M.2    Capel, F.3    Recio, P.4    Moure, C.5
  • 15
    • 49849106788 scopus 로고    scopus 로고
    • Densification and grain growth of nanocrystalline 3YTZP during two-step sintering
    • Mehdi, M.; Simchi, A.; Golestani-fard, F. Densification and grain growth of nanocrystalline 3YTZP during two-step sintering. J. Eur. Ceram. Soc. 2008, 28, 2933-2939.
    • (2008) J. Eur. Ceram. Soc , vol.28 , pp. 2933-2939
    • Mehdi, M.1    Simchi, A.2    Golestani-fard, F.3
  • 16
    • 0035906759 scopus 로고    scopus 로고
    • Hydroxide synthesis, colloidal processing and sintering of nano-size 3y-Tzp powder
    • Oleg, V.; Yoshio, S. Hydroxide synthesis, colloidal processing and sintering of nano-size 3y-Tzp powder. Scr. Mater. 2001, 44, 2219-2223.
    • (2001) Scr. Mater , vol.44 , pp. 2219-2223
    • Oleg, V.1    Yoshio, S.2
  • 17
    • 19244380601 scopus 로고    scopus 로고
    • Phase stability of nanostructured tetragonal zirconia polycrystals versus temperature and water vapor
    • 136-137
    • Djurado, E.; Dessemond, L.; Roux, C. Phase stability of nanostructured tetragonal zirconia polycrystals versus temperature and water vapor. Solid State Ion. 2000 136-137, 1249-1254.
    • (2000) Solid State Ion , pp. 1249-1254
    • Djurado, E.1    Dessemond, L.2    Roux, C.3
  • 18
    • 0035216810 scopus 로고    scopus 로고
    • Low temperature phase transformation of nanocrystalline tetragonal ZrO2 by neutrons and Raman Scattering studies
    • Ritter, C.; Dianoux, A.J.; Lucazeau, G. Low temperature phase transformation of nanocrystalline tetragonal ZrO2 by neutrons and Raman Scattering studies. Int. J. Inorg. Mater. 2001, 3, 647-654.
    • (2001) Int. J. Inorg. Mater , vol.3 , pp. 647-654
    • Ritter, C.1    Dianoux, A.J.2    Lucazeau, G.3
  • 19
    • 0032182099 scopus 로고    scopus 로고
    • Phase transformation in Y2O3-partially-stabilized ZrO2 polycrystals of various grain sizes during low-temperature aging in water
    • Li, J.F.; Watanabe, R. Phase transformation in Y2O3-partially-stabilized ZrO2 polycrystals of various grain sizes during low-temperature aging in water. J. Am. Ceram. Soc. 1998, 81, 2687-2691.
    • (1998) J. Am. Ceram. Soc , vol.81 , pp. 2687-2691
    • Li, J.F.1    Watanabe, R.2
  • 20
    • 0242575980 scopus 로고    scopus 로고
    • Mechanical properties and low temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing
    • Munoz, S.J.; Balmori, R.H.; Jaramillo, V.D.; Iga, T.; Schneider, G.A. Mechanical properties and low temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing. J. Mater. Res. 2003, 18, 2415-2426.
    • (2003) J. Mater. Res , vol.18 , pp. 2415-2426
    • Munoz, S.J.1    Balmori, R.H.2    Jaramillo, V.D.3    Iga, T.4    Schneider, G.A.5
  • 21
    • 84987368881 scopus 로고
    • Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction
    • Toraya, H.; Yoshimura, M.; Somiya, S. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction. J. Am. Ceram. Soc. 1984, 67, 119-121.
    • (1984) J. Am. Ceram. Soc , vol.67 , pp. 119-121
    • Toraya, H.1    Yoshimura, M.2    Somiya, S.3
  • 23
    • 0026875935 scopus 로고
    • An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments
    • Oliver, W.C.; Pharr, G.M.; An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J. Mater. Res. 1992, 7, 1564-1583.
    • (1992) J Mater. Res , vol.7 , pp. 1564-1583
    • Oliver, W.C.1    Pharr, G.M.2
  • 24
    • 0040633110 scopus 로고    scopus 로고
    • Measurement of mechanical properties by ultra-low load indentation
    • Pharr, G.M. Measurement of mechanical properties by ultra-low load indentation. Mat. Sci. Eng. A. 1998, 253, 151-159.
    • (1998) Mat. Sci. Eng. A , vol.253 , pp. 151-159
    • Pharr, G.M.1
  • 25
    • 11244331765 scopus 로고    scopus 로고
    • Spark plasma sintering and characterization of bulk nanostructured fully stabilized zirconia. Part I Densification studies.
    • Anselmi-tamburini, U.; Garay, J.E.; Munir, Z.A.; Tacca, A.; Maglia, F.; Spinolo, G. Spark plasma sintering and characterization of bulk nanostructured fully stabilized zirconia. Part I. Densification studies. J. Mater. Res. 2004, 19, 3255-3262.
    • (2004) J. Mater. Res. , vol.19 , pp. 3255-3262
    • Anselmi-tamburini, U.1    Garay, J.E.2    Munir, Z.A.3    Tacca, A.4    Maglia, F.5    Spinolo, G.6
  • 27
    • 51649111622 scopus 로고    scopus 로고
    • Spark plasma sintering of a commercially available granulated zirconia powder. II. Microstructure after sintering and ionic conductivity
    • Bernard-granger, G.; Guizard, C.; Surble, S.; Baldinozzi, G.; Addad, A. Spark plasma sintering of a commercially available granulated zirconia powder. II. Microstructure after sintering and ionic conductivity. Acta Mater. 2008, 56. 4658-4672.
    • (2008) Acta Mater , vol.56 , pp. 4658-4672
    • Bernard-granger, G.1    Guizard, C.2    Surble, S.3    Baldinozzi, G.4    Addad, A.5
  • 28
    • 0019058952 scopus 로고
    • Elastic/plastic indentation damage in ceramics: The median/radial crack system
    • Lawn, B.R.; Evans, A.G.; Marshall, D.B. Elastic/plastic indentation damage in ceramics: The median/radial crack system. J. Am. Ceram. Soc. 1980, 63, 574-581.
    • (1980) J. Am. Ceram. Soc , vol.63 , pp. 574-581
    • Lawn, B.R.1    Evans, A.G.2    Marshall, D.B.3
  • 29
    • 67349181721 scopus 로고    scopus 로고
    • Indentation techniques for evaluating the fracture toughness of biomaterials and hard tissues
    • Kruzica, J.J.; Kimb, D.K.; Koesterc, K.J.; Ritchie, R.O. Indentation techniques for evaluating the fracture toughness of biomaterials and hard tissues. J. Mech. Beh. Bio. Med. Mat. 2009, 2, 384-395.
    • (2009) J. Mech. Beh. Bio. Med. Mat , vol.2 , pp. 384-395
    • Kruzica, J.J.1    Kimb, D.K.2    Koesterc, K.J.3    Ritchie, R.O.4
  • 30
    • 54249149533 scopus 로고    scopus 로고
    • Effect of grain size on mechanical properties of 3Y-TZP ceramics
    • Trunec, M. Effect of grain size on mechanical properties of 3Y-TZP ceramics. Ceramics 2008, 52, 165-171.
    • (2008) Ceramics , vol.52 , pp. 165-171
    • Trunec, M.1
  • 31
    • 34548481996 scopus 로고    scopus 로고
    • Effect of grain size on mechanical properties of submicrometer 3Y-TZP: Fracture strength and hydrothermal degradation
    • Eichler, J.; Rodel, J.; Eisele, U.; Hoffman, M. Effect of grain size on mechanical properties of submicrometer 3Y-TZP: Fracture strength and hydrothermal degradation. J. Am. Ceram. Soc. 2007, 90, 2830-2836.
    • (2007) J. Am. Ceram. Soc , vol.90 , pp. 2830-2836
    • Eichler, J.1    Rodel, J.2    Eisele, U.3    Hoffman, M.4
  • 32
    • 0022751718 scopus 로고
    • Mechanical properties of Y2O3-stabilized tetragonal ZrO2 polycrystals after aging at high temperature
    • Masaki, T. Mechanical properties of Y2O3-stabilized tetragonal ZrO2 polycrystals after aging at high temperature. J. Am. Ceram. Soc. 1986, 69, 519-522.
    • (1986) J. Am. Ceram. Soc , vol.69 , pp. 519-522
    • Masaki, T.1
  • 33
    • 50149093027 scopus 로고    scopus 로고
    • Quantification of hydrothermal degradation in zirconia by nanoindentation
    • Gaillard, Y.; Jiménez-pique, E.; Soldera, F.; Mucklich, F.; Anglada, M. Quantification of hydrothermal degradation in zirconia by nanoindentation. Acta Mater. 2008, 56, 4206-4216.
    • (2008) Acta Mater , vol.56 , pp. 4206-4216
    • Gaillard, Y.1    Jiménez-pique, E.2    Soldera, F.3    Mucklich, F.4    Anglada, M.5
  • 34
    • 33748691349 scopus 로고    scopus 로고
    • R-curve behaviour of 2Y-TZP with submicron grain size
    • Eichler, J.; Hoffman, M.; Eisele, U.; Rodel, J. R-curve behaviour of 2Y-TZP with submicron grain size. J. Eur. Ceram. Soc. 2006, 26, 3575-3582.
    • (2006) J. Eur. Ceram. Soc , vol.26 , pp. 3575-3582
    • Eichler, J.1    Hoffman, M.2    Eisele, U.3    Rodel, J.4
  • 35
    • 0037300394 scopus 로고    scopus 로고
    • Crystallite and grain-size-dependent phase transformations in yttria-doped zirconia
    • Suresh, A.; Mayo, M.J.; Porter, W.D.; Rawn, C.J. Crystallite and grain-size-dependent phase transformations in yttria-doped zirconia. J. Am. Ceram. Soc. 2003, 86, 360-362.
    • (2003) J. Am. Ceram. Soc , vol.86 , pp. 360-362
    • Suresh, A.1    Mayo, M.J.2    Porter, W.D.3    Rawn, C.J.4
  • 36
    • 0022751690 scopus 로고
    • Significance of internal stresses for the martensitic transformation in yttria-stabilized tetragonal zirconia polycrystals during degradation
    • Schmauder, S.; Schubert, H. Significance of internal stresses for the martensitic transformation in yttria-stabilized tetragonal zirconia polycrystals during degradation. J. Am. Ceram. Soc. 1986, 69, 534-540.
    • (1986) J. Am. Ceram. Soc , vol.69 , pp. 534-540
    • Schmauder, S.1    Schubert, H.2
  • 37
    • 0039284782 scopus 로고
    • Microstructural investigations on the stability of ytrria stabilised tetragonal zirconia
    • Advances in Ceramics, Science and Technology of Zirconia III; Somiya, S., Yamamoto, N., Yanagida, H., Eds.; American ceramic society Inc.: Columbus, OH, USA
    • Schubert, H.; Petzow, G. Microstructural investigations on the stability of ytrria stabilised tetragonal zirconia. In Advances in Ceramics, Science and Technology of Zirconia III; Somiya, S., Yamamoto, N., Yanagida, H., Eds.; American ceramic society Inc.: Columbus, OH, USA, 1988; Volume 24, pp. 21-28.
    • (1988) , vol.24 , pp. 21-28
    • Schubert, H.1    Petzow, G.2
  • 38
    • 0028449599 scopus 로고
    • Grinding of ceramics: The effect on their strength properties
    • Maksond, T.M.A.; Morgan, J.E. Grinding of ceramics: The effect on their strength properties. J. Matter. Process. Technol. 1994, 43, 65-67.
    • (1994) J. Matter. Process. Technol , vol.43 , pp. 65-67
    • Maksond, T.M.A.1    Morgan, J.E.2
  • 39
    • 0027541322 scopus 로고
    • Strength and residual stress of Mg-PSZ after grinding
    • Van Den Berg, P.H.J.; De With, G. Strength and residual stress of Mg-PSZ after grinding. Wear 1993, 160, 301-308.
    • (1993) Wear , vol.160 , pp. 301-308
    • Den Berg, P.H.J.V.1    De With, G.2
  • 40
    • 0030159286 scopus 로고    scopus 로고
    • Effects of surface-finishing condition and annealing on transformation sensitivity of a 3 mol % Y2O3 stabilized tetragonal zirconia surface under interaction of lubricant
    • Sato, T.; Besshi, T.; Tada, Y. Effects of surface-finishing condition and annealing on transformation sensitivity of a 3 mol % Y2O3 stabilized tetragonal zirconia surface under interaction of lubricant. Wear 1996, 194, 204-211.
    • (1996) Wear , vol.194 , pp. 204-211
    • Sato, T.1    Besshi, T.2    Tada, Y.3
  • 41
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TPZ zirconia ceramic
    • Kosmac, T.; Oblak, C.; Jevnikar, P.; Funduk, N.; Marion, L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TPZ zirconia ceramic. Dent. Mat. 1999, 15, 426-433.
    • (1999) Dent. Mat , vol.15 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.