Volumn 51, Issue 1, 2008, Pages 92-100

Investigation of the tribological behavior of polytetrafluoroethylene at cryogenic temperatures

Author keywords

Cryogenic; Friction; PTFE: Space; Seals; Solid Lubrication; Thermal Activation

Indexed keywords


EID: 77957749713     PISSN: 10402004     EISSN: 1547397X     Source Type: Journal    
DOI: 10.1080/10402000701660618     Document Type: Article
Times cited : (31)

References (45)
  • 1
    • 0019902721 scopus 로고
    • Self-lubricating composites for extreme environment applications
    • Gardos, M.N. (1982), “Self-Lubricating Composites for Extreme Environment Applications,” Tribology International, 15, 5, pp 273-283.
    • (1982) Tribology International , vol.15 , Issue.5 , pp. 273-283
    • Gardos, M.N.1
  • 2
    • 0033344765 scopus 로고    scopus 로고
    • Considerations in vacuum tribology (Adhesion, friction, wear, and solid lubrication in vacuum)
    • Miyoshi, K. (1999), “Considerations in Vacuum Tribology (Adhesion, Friction, Wear, and Solid Lubrication in Vacuum),” Tribology International, 32, 11, pp 605-616.
    • (1999) Tribology International , vol.32 , Issue.11 , pp. 605-616
    • Miyoshi, K.1
  • 3
    • 14544283505 scopus 로고    scopus 로고
    • An experimental study of low earth orbit atomic oxygen and ultraviolet radiation effects on a spacecraft material-polytetrafluoroethylene
    • Zhao, X., et al. (2005), “An Experimental Study of Low Earth Orbit Atomic Oxygen and Ultraviolet Radiation Effects on a Spacecraft Material-Polytetrafluoroethylene,” PolymerDegradation and Stability, 88, 2, pp 275-285.
    • (2005) Polymerdegradation and Stability , vol.88 , Issue.2 , pp. 275-285
    • Zhao, X.1
  • 4
    • 0033307271 scopus 로고    scopus 로고
    • Aerospace mechanisms and tribology technology-case study
    • Miyoshi, K. (1999), “Aerospace Mechanisms and Tribology Technology-Case Study,” Tribology International, 32, 11, pp 673-685.
    • (1999) Tribology International , vol.32 , Issue.11 , pp. 673-685
    • Miyoshi, K.1
  • 6
    • 0042469936 scopus 로고
    • Visco-elastic properties and friction of solids-friction of polymers-influence of speed and temperature
    • McLaren, K. and Tabor, D. (1963), “Visco-Elastic Properties and Friction of Solids-Friction of Polymers-Influence of Speed and Temperature,”Nature, 197, 487, pp 856.
    • (1963) Nature , vol.197 , Issue.487 , pp. 856
    • Mc Laren, K.1    Tabor, D.2
  • 7
    • 0026833236 scopus 로고
    • Sliding wear mechanism of polyte-trafluoroethylene (Ptfe) andptfe composites
    • Blanchet, T. and Kennedy, F. (1992), “Sliding Wear Mechanism of Polyte-trafluoroethylene (PTFE) andPTFE Composites,” Wear, 153, 1, pp 229-243.
    • (1992) Wear , vol.153 , Issue.1 , pp. 229-243
    • Blanchet, T.1    Kennedy, F.2
  • 8
    • 34250634129 scopus 로고
    • Friction and transfer of polytetrafluoroethylene
    • Makinson, K. and Tabor, D. (1964), “Friction and Transfer of Polytetrafluoroethylene,” Nature, 201, 491, pp 464.
    • (1964) Nature , vol.201 , Issue.491 , pp. 464
    • Makinson, K.1    Tabor, D.2
  • 9
    • 0031214902 scopus 로고    scopus 로고
    • Thermal fluctuations of ptfe friction and transfer
    • Pleskachevsky, Y.M. and Smurugov, V.A. (1997), “Thermal Fluctuations of PTFE Friction and Transfer,” Wear, 209, 1-2, pp 123-127.
    • (1997) Wear , vol.209 , Issue.1-2 , pp. 123-127
    • Pleskachevsky, Y.M.1    Smurugov, V.A.2
  • 10
    • 0026933891 scopus 로고
    • On ptfe transfer and thermoactivation mechanism of wear
    • Smurugov, V., et al. (1992), “On PTFE Transfer and Thermoactivation Mechanism of Wear,” Wear, 158, 1-2, pp 61-69.
    • (1992) Wear , vol.158 , Issue.1-2 , pp. 61-69
    • Smurugov, V.1
  • 11
    • 34250631027 scopus 로고
    • Sliding experiments with polytetrafluoroethylene
    • Steijn, R. (1968), “Sliding Experiments with Polytetrafluoroethylene,” ASLE Transactions, 11, 3, pp 235.
    • (1968) ASLE Transactions , vol.11 , Issue.3 , pp. 235
    • Steijn, R.1
  • 12
    • 17944404718 scopus 로고
    • Mechanism of wear of poytetrafluoroethylene
    • Tanaka, K., Uchiyama, Y. and Toyooka, S. (1973), “Mechanism of Wear of Poytetrafluoroethylene,” Wear, 23, 2, pp 153-172.
    • (1973) Wear , vol.23 , Issue.2 , pp. 153-172
    • Tanaka, K.1    Uchiyama, Y.2    Toyooka, S.3
  • 13
    • 0032058241 scopus 로고    scopus 로고
    • Friction and wear at low temperatures
    • Gradt, T., et al. (1998), “Friction and Wear at Low Temperatures,” International Journal ofHydrogen Energy, 23, 5, pp 397-403.
    • (1998) International Journal Ofhydrogen Energy , vol.23 , Issue.5 , pp. 397-403
    • Gradt, T.1
  • 14
    • 0032052954 scopus 로고    scopus 로고
    • Tribological behaviour of materials at cryogenic temperatures
    • Hubner, W., et al. (1998), “Tribological Behaviour of Materials at Cryogenic Temperatures,” Wear, 216, 2, pp 150-159.
    • (1998) Wear , vol.216 , Issue.2 , pp. 150-159
    • Hubner, W.1
  • 15
    • 0026206267 scopus 로고
    • Friction and wear of polymeric materials at 293-k, 77-k and 4.2-k
    • Michael, P., Rabinowicz, E. and Iwasa, Y. (1991), “Friction and Wear of Polymeric Materials at 293-K, 77-K and 4.2-K,” Cryogenics, 31, 8, pp 695-704.
    • (1991) Cryogenics , vol.31 , Issue.8 , pp. 695-704
    • Michael, P.1    Rabinowicz, E.2    Iwasa, Y.3
  • 16
    • 0035297659 scopus 로고    scopus 로고
    • Low temperature tribology at the b. Verkin institute for low temperature physics and engineering (historical review)
    • Ostrovskaya, Y., etal. (2001), “Low Temperature Tribology at the B. Verkin Institute for Low Temperature Physics and Engineering (Historical Review),” Tribology International 34, 4, pp 265-276.
    • (2001) Tribology International , vol.34 , Issue.4 , pp. 265-276
    • Ostrovskaya, Y.1
  • 17
    • 0036647493 scopus 로고    scopus 로고
    • Friction and wear of ptfe composites at cryogenic temperatures
    • Theiler, G., et al. (2002), “Friction and Wear of PTFE Composites at Cryogenic Temperatures,” Tribology International 35, 7, pp 449-458.
    • (2002) Tribology International , vol.35 , Issue.7 , pp. 449-458
    • Theiler, G.1
  • 19
    • 31444434333 scopus 로고    scopus 로고
    • Cryogenic friction behavior of ptfe based solid lubricant composites
    • McCook, N.L., et al. (2005), “Cryogenic Friction Behavior of PTFE Based Solid Lubricant Composites,” Tribology Letters, 20, 2, pp 109-113.
    • (2005) Tribology Letters , vol.20 , Issue.2 , pp. 109-113
    • Mc Cook, N.L.1
  • 20
    • 0037532408 scopus 로고    scopus 로고
    • A study on the friction and wear behavior of ptfe filled with alumina nanoparticles
    • Sawyer, W.G., et al. (2003), “A Study on the Friction and Wear Behavior of PTFE Filled with Alumina Nanoparticles,” Wear, 254, 5-6, pp 573-580.
    • (2003) Wear , vol.254 , Issue.5-6 , pp. 573-580
    • Sawyer, W.G.1
  • 21
    • 18844400297 scopus 로고    scopus 로고
    • Tribological sensitivity of ptfe/alumina nanocomposites to a range of traditional surface finishes
    • Burris, D.L. and Sawyer, W.G. (2005), “Tribological Sensitivity of PTFE/Alumina Nanocomposites to a Range of Traditional Surface Finishes,” Tribology Transactions, 48, 2, pp 147-153.
    • (2005) Tribology Transactions , vol.48 , Issue.2 , pp. 147-153
    • Burris, D.L.1    Sawyer, W.G.2
  • 22
    • 22244453762 scopus 로고    scopus 로고
    • The difficulty of measuring low friction: Uncertainty analysis for friction coefficient measurements
    • Schmitz, T., etal. (2005), “The Difficulty of Measuring Low Friction: Uncertainty Analysis for Friction Coefficient Measurements,” Tribology Transactions, 127, 3, pp 673-678.
    • (2005) Tribology Transactions , vol.127 , Issue.3 , pp. 673-678
    • Schmitz, T.1
  • 23
    • 33750992146 scopus 로고    scopus 로고
    • Tribological behavior of peek components with compositionally graded peek/ptfe surfaces
    • Burris, D. and Sawyer, W. (2007), “Tribological Behavior of PEEK Components with Compositionally Graded PEEK/PTFE Surfaces,” Wear, 262, 1-2, pp 220-224.
    • (2007) Wear , vol.262 , Issue.1-2 , pp. 220-224
    • Burris, D.1    Sawyer, W.2
  • 25
    • 0031153322 scopus 로고    scopus 로고
    • Thin film thermocouple arrays for sliding surface temperature measurement
    • Kennedy, F.E., Frusescu, D. and Li, J.Y. (1997), “Thin Film Thermocouple Arrays for Sliding Surface Temperature Measurement,” Wear, 207, 1-2, pp 46-54.
    • (1997) Wear , vol.207 , Issue.1-2 , pp. 46-54
    • Kennedy, F.E.1    Frusescu, D.2    Li, J.Y.3
  • 26
    • 34547215730 scopus 로고    scopus 로고
    • Macroscopic evidence of thermally activated friction with polytetrafluoroethylene
    • Burris, D.L., Perry, S.S. and Sawyer, W.G. (2007), “Macroscopic Evidence of Thermally Activated Friction with Polytetrafluoroethylene” Tribology Letters, 27, pp 323-328.
    • (2007) Tribology Letters , vol.27 , pp. 323-328
    • Burris, D.L.1    Perry, S.S.2    Sawyer, W.G.3
  • 27
    • 15944404291 scopus 로고    scopus 로고
    • Structural surprises in friction-deposited films of poly(Tetrafluoroethylene)
    • Breiby, D., et al. (2005), “Structural Surprises in Friction-Deposited Films of Poly(tetrafluoroethylene),” Macromolecules, 38, 6, pp 2383-2390.
    • (2005) Macromolecules , vol.38 , Issue.6 , pp. 2383-2390
    • Breiby, D.1
  • 28
    • 33746843161 scopus 로고    scopus 로고
    • The effect of crystallinity on the fracture of polytetrafluoroethylene (Ptfe)
    • Brown, E., et al. (2006), “The Effect of Crystallinity on the Fracture of Polytetrafluoroethylene (PTFE),” Material Science and Engineering C-Biomimetic and Supramolecular Systems, 26, 8, pp 1338-1343.
    • (2006) Material Science and Engineering C-Biomimetic and Supramolecular Systems , vol.26 , Issue.8 , pp. 1338-1343
    • Brown, E.1
  • 29
    • 33645104912 scopus 로고    scopus 로고
    • The crystal structure of polytetrafluoroethylene, forms i and iv
    • Clark, E. (2006), “The Crystal Structure of Polytetrafluoroethylene, Forms I and IV,” Journal of Macromolecular Science Part B-Physics, 45, 2, pp 201-213.
    • (2006) Journal of Macromolecular Science Part B-Physics , vol.45 , Issue.2 , pp. 201-213
    • Clark, E.1
  • 30
    • 0020115870 scopus 로고
    • X-ray-diffraction study of crystal transformation and molecular disorder in poly(Tetrafluoroethylene)
    • Yamamoto, T. and Hara, T. (1982), “X-Ray-Diffraction Study of Crystal Transformation and Molecular Disorder in Poly(tetrafluoroethylene),” Polymer, 23, 4, pp 521-528.
    • (1982) Polymer , vol.23 , Issue.4 , pp. 521-528
    • Yamamoto, T.1    Hara, T.2
  • 31
    • 0000214489 scopus 로고
    • The fine structure of polytetrafluoroethylene
    • Bunn, C., Cobbold, A. and Palmer, R. (1958), “The Fine Structure of Polytetrafluoroethylene,” Journal ofPolymer Science, 28, 117, pp 365-376.
    • (1958) Journal Ofpolymer Science , vol.28 , Issue.117 , pp. 365-376
    • Bunn, C.1    Cobbold, A.2    Palmer, R.3
  • 32
    • 36949090256 scopus 로고
    • Structures of molecules and crystals of fluorocarbons
    • Bunn, C. and Howells, E. (1954), “Structures of Molecules and Crystals of Fluorocarbons,” Nature, 174, 4429, pp 549-551.
    • (1954) Nature , vol.174 , Issue.4429 , pp. 549-551
    • Bunn, C.1    Howells, E.2
  • 33
    • 0032788038 scopus 로고    scopus 로고
    • The molecular conformations of polytetrafluoroethy-lene: Forms ii and iv
    • Clark, E. (1999), “The Molecular Conformations of Polytetrafluoroethy-lene: Forms II and IV,” Polymer, 40, 16, pp 4659-4665.
    • (1999) Polymer , vol.40 , Issue.16 , pp. 4659-4665
    • Clark, E.1
  • 34
    • 0019635191 scopus 로고
    • Energy calculations of the crystal-structure of the low-temperature phase (Ii) of polytetrafluoroethylene
    • Farmer, B. and Eby, R. (1981), “Energy Calculations of the Crystal-Structure of the Low-Temperature Phase (II) of Polytetrafluoroethylene,” Polymer, 22, 11, pp 1487-1495.
    • (1981) Polymer , vol.22 , Issue.11 , pp. 1487-1495
    • Farmer, B.1    Eby, R.2
  • 35
    • 0028413594 scopus 로고
    • Chain reorientation in poly(Tetrafluoroethylene) by mobile twin-helix reversal defects
    • Kimmig, M., Strobl, G. and Stuhn, B. (1994), “Chain Reorientation in Poly(tetrafluoroethylene) by Mobile Twin-Helix Reversal Defects,” Macromolecules, 27, 9, pp 2481-2495.
    • (1994) Macromolecules , vol.27 , Issue.9 , pp. 2481-2495
    • Kimmig, M.1    Strobl, G.2    Stuhn, B.3
  • 36
    • 0019632752 scopus 로고
    • Crystal-strcture of the low-temperature phase(Ii) of polytetrafluoroethylene
    • Weeks, J., Clark, E. and Eby, R. (1981), “Crystal-Strcture of the Low-Temperature Phase(II) of Polytetrafluoroethylene,” Polymer, 22, 11, pp 1480-1486.
    • (1981) Polymer , vol.22 , Issue.11 , pp. 1480-1486
    • Weeks, J.1    Clark, E.2    Eby, R.3
  • 37
    • 0019632945 scopus 로고
    • Disorder in the crystal-structures of phase-1 and phase-2 of copolymers of tetrafluoroethylene and hexaflu-oropropylene
    • Weeks, J., Eby, R. and Clark, E. (1981), “Disorder in the Crystal-Structures of Phase-1 and Phase-2 of Copolymers of Tetrafluoroethylene and Hexaflu-oropropylene,” Polymer, 22, 11, pp 1496-1499.
    • (1981) Polymer , vol.22 , Issue.11 , pp. 1496-1499
    • Weeks, J.1    Eby, R.2    Clark, E.3
  • 38
    • 15744374226 scopus 로고    scopus 로고
    • The role of crystalline phase on fracture and microstructure evolution of polytetrafluoroethy-lene (Ptfe)
    • Brown, E.N. and Dattelbaum, D.M. (2005), “The Role of Crystalline Phase on Fracture and Microstructure Evolution of Polytetrafluoroethy-lene (PTFE),” Polymer, 46, 9, pp 3056-3068.
    • (2005) Polymer , vol.46 , Issue.9 , pp. 3056-3068
    • Brown, E.N.1    Dattelbaum, D.M.2
  • 39
    • 36849128279 scopus 로고
    • Friction of teflon sliding on teflon
    • Flom, D. and Porile, N. (1955), “Friction of Teflon Sliding on Teflon,” Journal ofApplied Physics, 26, 9, pp 1088-1092.
    • (1955) Journal Ofapplied Physics , vol.26 , Issue.9 , pp. 1088-1092
    • Flom, D.1    Porile, N.2
  • 40
    • 18144434454 scopus 로고    scopus 로고
    • Differential application of wear models to fractional thin films
    • Blanchet, T.A. and Sawyer, W.G. (2001), “Differential Application of Wear Models to Fractional Thin Films,” Wear, 250, pp 1003-1008.
    • (2001) Wear , vol.250 , pp. 1003-1008
    • Blanchet, T.A.1    Sawyer, W.G.2
  • 41
    • 3543070036 scopus 로고    scopus 로고
    • Fractional coverage model for the adsorption and removal of gas species and application to superlow friction diamond-like carbon
    • Dickrell, P.L., Sawyer, W.G. and Erdemir, A. (2004), “Fractional Coverage Model for the Adsorption and Removal of Gas Species and Application to Superlow Friction Diamond-Like Carbon,” Journal of Tribology-Transactions ofthe Asme, 126, 3, pp 615-619.
    • (2004) Journal of Tribology-Transactions Ofthe Asme , vol.126 , Issue.3 , pp. 615-619
    • Dickrell, P.L.1    Sawyer, W.G.2    Erdemir, A.3
  • 42
    • 1542605224 scopus 로고    scopus 로고
    • Fracture toughness evaluation of polytetrafluoroethy-lene
    • Joyce, J. (2003), “Fracture Toughness Evaluation of Polytetrafluoroethy-lene,” Polymer Engineering and Science, 43, 10, pp 1702-1714.
    • (2003) Polymer Engineering and Science , vol.43 , Issue.10 , pp. 1702-1714
    • Joyce, J.1
  • 44
    • 24044488606 scopus 로고
    • Glass-transition of poly(Tetrafluoroethylene)
    • Lau, S.F., Wesson, J.P and Wunderlich, B. (1984), “Glass-Transition of Poly(Tetrafluoroethylene),” Macromolecules, 17, 5, pp 1102-1104.
    • (1984) Macromolecules , vol.17 , Issue.5 , pp. 1102-1104
    • Lau, S.F.1    Wesson, J.P.2    Wunderlich, B.3
  • 45
    • 0032123786 scopus 로고    scopus 로고
    • The temperature dependence of the local free volume in polyethylene and polytetraflu-oroethylene: A positron lifetime study
    • Dlubek, G., Saarinen, K. and Fretwell, H.M. (1998), “The Temperature Dependence of the Local Free Volume in Polyethylene and Polytetraflu-oroethylene: A Positron Lifetime Study,” Journal of Polymer Science Part B-PolymerPhysics, 36, 9, pp 1513-1528.
    • (1998) Journal of Polymer Science Part B-PolymerPhysics , vol.36 , Issue.9 , pp. 1513-1528
    • Dlubek, G.1    Saarinen, K.2    Fretwell, H.M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.