메뉴 건너뛰기




Volumn 256, Issue 23, 2010, Pages 7027-7031

Influence of the hydrothermal temperature and pH on the crystallinity of a sputtered hydroxyapatite film

Author keywords

Crystallinity; Hydrothermal; Hydroxyapatite; Sputtering

Indexed keywords

ENERGY DISPERSIVE SPECTROSCOPY; FILM THICKNESS; HYDROXYAPATITE; SCANNING ELECTRON MICROSCOPY; SPUTTERING; X RAY DIFFRACTION;

EID: 77955309245     PISSN: 01694332     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.apsusc.2010.05.018     Document Type: Article
Times cited : (23)

References (30)
  • 2
    • 0028533742 scopus 로고
    • Effect of surface roughness of hydroxyapatite-coated titanium on the bone-implant interface shear strength
    • K. Hayashi, T. Inadome, H. Tsumura, Y. Nakashima, and Y. Sugioka Effect of surface roughness of hydroxyapatite-coated titanium on the bone-implant interface shear strength Biomaterials 15 1994 1187 1191
    • (1994) Biomaterials , vol.15 , pp. 1187-1191
    • Hayashi, K.1    Inadome, T.2    Tsumura, H.3    Nakashima, Y.4    Sugioka, Y.5
  • 3
    • 0032485214 scopus 로고    scopus 로고
    • Comparative push-out test of dense HA implants and HA-coated implants: Findings in a canine study
    • M. Ogiso, Y. Yamashita, and T. Mastumoto Comparative push-out test of dense HA implants and HA-coated implants: findings in a canine study J. Biomed. Mater. Res. 39 1998 364 372
    • (1998) J. Biomed. Mater. Res. , vol.39 , pp. 364-372
    • Ogiso, M.1    Yamashita, Y.2    Mastumoto, T.3
  • 4
    • 0033635916 scopus 로고    scopus 로고
    • Hydroxyapatite-coated bioalloy surfaces: Current status and future challenges
    • G. Lewis Hydroxyapatite-coated bioalloy surfaces: current status and future challenges Bio-Med. Mater. Eng. 10 2000 157 188
    • (2000) Bio-Med. Mater. Eng. , vol.10 , pp. 157-188
    • Lewis, G.1
  • 5
    • 0030088006 scopus 로고    scopus 로고
    • Water vapour-treated hydroxyapatite coatings after plasma spraying and their characteristics
    • Y. Cao, J. Weng, J. Chen, J. Feng, Z. Yang, and X. Zhang Water vapour-treated hydroxyapatite coatings after plasma spraying and their characteristics Biomaterials 17 1996 419 424
    • (1996) Biomaterials , vol.17 , pp. 419-424
    • Cao, Y.1    Weng, J.2    Chen, J.3    Feng, J.4    Yang, Z.5    Zhang, X.6
  • 6
    • 0033635868 scopus 로고    scopus 로고
    • Crystal chemistry of hydroxyapatite deposited on titanium by sputtering technique
    • K. Ozeki, T. Yuhta, H. Aoki, I. Nishimura, and Y. Fukui Crystal chemistry of hydroxyapatite deposited on titanium by sputtering technique Bio-Med. Mater. Eng. 10 2000 221 227
    • (2000) Bio-Med. Mater. Eng. , vol.10 , pp. 221-227
    • Ozeki, K.1    Yuhta, T.2    Aoki, H.3    Nishimura, I.4    Fukui, Y.5
  • 7
    • 0035124739 scopus 로고    scopus 로고
    • Push-out strength of hydroxyapatite coated by sputtering technique in bone
    • K. Ozeki, T. Yuhta, H. Aoki, I. Nishimura, and Y. Fukui Push-out strength of hydroxyapatite coated by sputtering technique in bone Bio-Med. Mater. Eng. 11 2001 63 68
    • (2001) Bio-Med. Mater. Eng. , vol.11 , pp. 63-68
    • Ozeki, K.1    Yuhta, T.2    Aoki, H.3    Nishimura, I.4    Fukui, Y.5
  • 8
    • 0032521085 scopus 로고    scopus 로고
    • In vivo dissolution behavior of various RF magnetron sputtered Ca-P coatings
    • DOI 10.1002/(SICI)1097-4636(19980315)39:4<524::AID-JBM3>3.0.CO;2-L
    • J.G.C. Wolke, K. de Groot, and J.A. Jansen In vivo dissolution behavior of various RF magnetron sputtered Ca-P coatings J. Biomed. Mater. Res. 39 1998 524 530 (Pubitemid 28079712)
    • (1998) Journal of Biomedical Materials Research , vol.39 , Issue.4 , pp. 524-530
    • Wolke, J.G.C.1    De Groot, K.2    Jansen, J.A.3
  • 9
    • 0031260154 scopus 로고    scopus 로고
    • Influence of rapid heating with infrared radiation on RF magnetron-sputtered calcium phosphate coatings
    • M. Yoshinari, T. Hayakawa, J.G.C. Wolke, K. Nemoto, and J.A. Jansen Influence of rapid heating with infrared radiation on RF magnetron-sputtered calcium phosphate coatings J. Biomed. Mater. Res. 37 1997 60 67
    • (1997) J. Biomed. Mater. Res. , vol.37 , pp. 60-67
    • Yoshinari, M.1    Hayakawa, T.2    Wolke, J.G.C.3    Nemoto, K.4    Jansen, J.A.5
  • 12
    • 0030087954 scopus 로고    scopus 로고
    • Influence of annealing temperature on RF magnetron sputtered calcium phosphate coatings
    • K. van Dijk, H.G. Schaeken, J.G.C. Wolke, and J.A. Jansen Influence of annealing temperature on RF magnetron sputtered calcium phosphate coatings Biomaterials 17 1996 405 410
    • (1996) Biomaterials , vol.17 , pp. 405-410
    • Van Dijk, K.1    Schaeken, H.G.2    Wolke, J.G.C.3    Jansen, J.A.4
  • 14
    • 0032488244 scopus 로고    scopus 로고
    • Hydrothermal-electrochemical deposition of hydroxyapatite
    • S. Ban, and S. Maruo Hydrothermal-electrochemical deposition of hydroxyapatite J. Biomed. Mater. Res. 42 1998 387 395
    • (1998) J. Biomed. Mater. Res. , vol.42 , pp. 387-395
    • Ban, S.1    Maruo, S.2
  • 16
    • 0348109452 scopus 로고    scopus 로고
    • Bone bonding strength of sputtered hydroxyapatite films subjected to a low temperature hydrothermal treatment
    • K. Ozeki, A. Mishima, T. Yuhta, Y. Fukui, and H. Aoki Bone bonding strength of sputtered hydroxyapatite films subjected to a low temperature hydrothermal treatment Bio-Med. Mater. Eng. 13 2003 451 463
    • (2003) Bio-Med. Mater. Eng. , vol.13 , pp. 451-463
    • Ozeki, K.1    Mishima, A.2    Yuhta, T.3    Fukui, Y.4    Aoki, H.5
  • 17
    • 21644434716 scopus 로고    scopus 로고
    • Effect of pH on crystallization of sputtered hydroxyapatite film under hydrothermal conditions at low temperature
    • K. Ozeki, H. Aoki, and Y. Fukui Effect of pH on crystallization of sputtered hydroxyapatite film under hydrothermal conditions at low temperature J. Mater. Sci. 40 2005 2837 2842
    • (2005) J. Mater. Sci. , vol.40 , pp. 2837-2842
    • Ozeki, K.1    Aoki, H.2    Fukui, Y.3
  • 18
    • 0030175775 scopus 로고    scopus 로고
    • Hydroxyapatite coating by dipping method, and bone bonding strength
    • T. Li, J. Lee, T. Kobayashi, and H. Aoki Hydroxyapatite coating by dipping method, and bone bonding strength J. Mater. Sci.: Mater. Med. 7 1996 355 357
    • (1996) J. Mater. Sci.: Mater. Med. , vol.7 , pp. 355-357
    • Li, T.1    Lee, J.2    Kobayashi, T.3    Aoki, H.4
  • 19
    • 0032211086 scopus 로고    scopus 로고
    • Tissue reaction of hydroxyapatite sol to rat molar pulp
    • T. Li, M. Akao, and M. Takagi Tissue reaction of hydroxyapatite sol to rat molar pulp J. Mater. Sci.: Mater. Med. 9 1998 631 642
    • (1998) J. Mater. Sci.: Mater. Med. , vol.9 , pp. 631-642
    • Li, T.1    Akao, M.2    Takagi, M.3
  • 20
    • 0034084101 scopus 로고    scopus 로고
    • Enhanced functions of osteoblasts on nanophase ceramics
    • DOI 10.1016/S0142-9612(00)00075-2, PII S0142961200000752
    • T.J. Webster, R.W. Siegel, and R. Bizios Enhanced functions of osteoblasts on nanophase ceramics Biomaterials 21 2000 1803 1810 (Pubitemid 30365044)
    • (2000) Biomaterials , vol.21 , Issue.17 , pp. 1803-1810
    • Webster, T.J.1    Ergun, C.2    Doremus, R.H.3    Siegel, R.W.4    Bizios, R.5
  • 21
    • 0000843012 scopus 로고    scopus 로고
    • Direct growth rate measurement of hydroxyapatite single crystal by moiré phase shift interferometry
    • N. Kanzaki, K. Onuma, A. Ito, K. Teraoka, T. Tateishi, and S. Tsutsumi Direct growth rate measurement of hydroxyapatite single crystal by moiré phase shift interferometry J. Phys. Chem. B 102 1998 6471 6476
    • (1998) J. Phys. Chem. B , vol.102 , pp. 6471-6476
    • Kanzaki, N.1    Onuma, K.2    Ito, A.3    Teraoka, K.4    Tateishi, T.5    Tsutsumi, S.6
  • 22
    • 0035426488 scopus 로고    scopus 로고
    • Crystal orientation of hydroxyapatite induced by ordered carboxyl groups
    • K. Sato, T. Kogure, Y. Kumagai, and J. Tanaka Crystal orientation of hydroxyapatite induced by ordered carboxyl groups J. Colloid Interface Sci. 240 2001 133 138
    • (2001) J. Colloid Interface Sci. , vol.240 , pp. 133-138
    • Sato, K.1    Kogure, T.2    Kumagai, Y.3    Tanaka, J.4
  • 24
    • 0001698827 scopus 로고
    • Hydrothermal growth of calcium hydroxyapatite single crystals
    • M. Mengeot, M.L. Harvill, and O.R. Gilliam Hydrothermal growth of calcium hydroxyapatite single crystals J. Cryst. Growth 19 1973 199 203
    • (1973) J. Cryst. Growth , vol.19 , pp. 199-203
    • Mengeot, M.1    Harvill, M.L.2    Gilliam, O.R.3
  • 25
    • 0010009584 scopus 로고
    • Progress in efforts to grow large single crystals of hydroxyapatite
    • J.F. Kirn, and H. Leidheiser Progress in efforts to grow large single crystals of hydroxyapatite J. Cryst. Growth 2 1968 111 112
    • (1968) J. Cryst. Growth , vol.2 , pp. 111-112
    • Kirn, J.F.1    Leidheiser, H.2
  • 26
    • 0036013935 scopus 로고    scopus 로고
    • Morphological regulation and crystal growth of hydrothermal- electrochemically deposited apatite
    • S. Ban, and J. Hasegawa Morphological regulation and crystal growth of hydrothermal-electrochemically deposited apatite Biomaterials 23 2002 2965 2972
    • (2002) Biomaterials , vol.23 , pp. 2965-2972
    • Ban, S.1    Hasegawa, J.2
  • 28
    • 0017857760 scopus 로고
    • Synthetic hydroxyapatite-solubility product and stoichiometry of dissolution
    • L.C. Bell, H. Mika, and B.J. Kruger Synthetic hydroxyapatite-solubility product and stoichiometry of dissolution Arch. Oral Biol. 23 1978 329 336
    • (1978) Arch. Oral Biol. , vol.23 , pp. 329-336
    • Bell, L.C.1    Mika, H.2    Kruger, B.J.3
  • 29
    • 0033105609 scopus 로고    scopus 로고
    • Solubility and ion activity product of calcium phosphate minerals
    • W.F. Jaynes, P.A. Moore Jr., and D.M. Miller Solubility and ion activity product of calcium phosphate minerals J. Eviron. Qual. 28 1999 530 536
    • (1999) J. Eviron. Qual. , vol.28 , pp. 530-536
    • Jaynes, W.F.1    Moore Jr., P.A.2    Miller, D.M.3
  • 30
    • 0024779881 scopus 로고
    • The hydroxyapatite solubility product of human dental enamel as a function of pH in the range 4.6-7.6 at 20 °c
    • M.J. Larsen, and S.J. Jensen The hydroxyapatite solubility product of human dental enamel as a function of pH in the range 4.6-7.6 at 20 °C Arch. Oral Biol. 34 1989 957 961
    • (1989) Arch. Oral Biol. , vol.34 , pp. 957-961
    • Larsen, M.J.1    Jensen, S.J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.