메뉴 건너뛰기




Volumn 17, Issue 2, 2010, Pages 555-565

Evaluating resistance of polymeric materials for outdoor applications to corona and ozone

Author keywords

Composite insulation; Corona; Housing material; Outdoor insulation; Ozone

Indexed keywords

COMPOSITE INSULATION; CORONA DISCHARGES; HOUSING MATERIAL; HOUSING MATERIALS; MONITORING CHANGE; OUTDOOR INSULATION; POLYMERIC MATERIAL; TEST CONDITION;

EID: 77951552802     PISSN: 10709878     EISSN: None     Source Type: Journal    
DOI: 10.1109/TDEI.2010.5448112     Document Type: Article
Times cited : (66)

References (62)
  • 2
    • 84966331530 scopus 로고    scopus 로고
    • Material properties for non-ceramic outdoor insulation: State of the art
    • CIGRE WG D1.14
    • CIGRE WG D1.14, "Material properties for non-ceramic outdoor insulation: State of the art", Technical Brochure No. 255, 2004.
    • (2004) Technical Brochure , Issue.255
  • 3
    • 0014629557 scopus 로고
    • Photodecomposition of polymethylsiloxane
    • D. A. Delman, M. Landy, and B. B. Simms, "Photodecomposition of polymethylsiloxane", J. Polymer Sci., Vol. 7, pp. 3375-3386, 1969.
    • (1969) J. Polymer. Sci. , vol.7 , pp. 3375-3386
    • Delman, D.A.1    Landy, M.2    Simms, B.B.3
  • 4
    • 0014863714 scopus 로고
    • Hydroxylation of polymethylsiloxane surfaces by oxidizing plasmas
    • R. J. Hollahan and L. G. Carlson, "Hydroxylation of polymethylsiloxane surfaces by oxidizing plasmas", Appl. Polymer Sci., Vol. 14, p. 2499-2508, 1970.
    • (1970) Appl. Polymer. Sci. , vol.14 , pp. 2499-2508
    • Hollahan, R.J.1    Carlson, L.G.2
  • 6
    • 33747854637 scopus 로고    scopus 로고
    • Surface degradation of silicone rubber exposed to corona discharge
    • DOI 10.1109/TPS.2006.876498
    • Y. Zhu, M. Otsubo, C. Honda, and S. Tanaka, "Loss and recovery in hydrophobicity of silicone rubber exposed to corona discharge", Polymer Degradation and Stability, Vol. 91, pp. 1448-1454, 2006. (Pubitemid 44283354)
    • (2006) IEEE Transactions on Plasma Science , vol.91 , pp. 1094-1098
    • Zhu, Y.1    Haji, K.2    Otsubo, M.3    Honda, C.4
  • 7
    • 0028375279 scopus 로고
    • Chemical changes at the surface of RTV silicone rubber coatings on insulators during dry-band arcing
    • S.-H. Kim, E. A. Cherney, R. Hackam, and K. G. Rutherford, "Chemical changes at the surface of RTV silicone rubber coatings on insulators during dry-band arcing", IEEE Trans. Dielectr. Electr. Insul., Vol. 1, pp. 106-23, 1994.
    • (1994) IEEE Trans. Dielectr. Electr. Insul. , vol.1 , pp. 106-23
    • Kim, S.-H.1    Cherney, E.A.2    Hackam, R.3    Rutherford, K.G.4
  • 10
    • 0033307859 scopus 로고    scopus 로고
    • Hydrophobicity recovery of polydimethylsiloxane after repeated exposure to corona discharges. Influence of crosslink density
    • H. Hillborg and U. W. Gedde, "Hydrophobicity recovery of polydimethylsiloxane after repeated exposure to corona discharges. Influence of crosslink density", IEEE Conf. Electr. Insul. Dielectr. Phenomena (CEIDP), Austin, TX, USA, pp. 751-755, 1999. (Pubitemid 30539775)
    • (1999) Conference on Electrical Insulation and Dielectric Phenomena (CEIDP), Annual Report , vol.2 , pp. 751-755
    • Hillborg, H.1    Gedde, U.W.2
  • 12
    • 0343337272 scopus 로고    scopus 로고
    • Hydrophobic recovery of polydimethylsiloxane after exposure to partial discharges as a function of crosslink density
    • DOI 10.1016/S0032-3861(01)00202-6, PII S0032386101002026
    • H. Hillborg, M. Sandelin, and U. W. Gedde, "Hydrophobic recovery of polydimethylsiloxane after exposure to partial discharges as a function of crosslink density", Polymer, Vol. 42, pp. 7349-7362, 2001. (Pubitemid 32479783)
    • (2001) Polymer , vol.42 , Issue.17 , pp. 7349-7362
    • Hillborg, H.1    Sandelin, M.2    Gedde, U.W.3
  • 15
    • 0035974207 scopus 로고    scopus 로고
    • Characterisation of low molar mass siloxanes extracted from crosslinked polydimethylsiloxanes exposed to corona discharges
    • PII S0032386101004517
    • H. Hillborg, S. Karlsson, and U. W. Gedde, "Characterisation of low molar mass siloxanes extracted from crosslinked polydimethylsiloxanes exposed to corona discharges", Polymer, Vol. 42, pp. 8883-8889, Oct. 2001. (Pubitemid 32728823)
    • (2001) Polymer , vol.42 , Issue.21 , pp. 8883-8889
    • Hillborg, H.1    Karlsson, S.2    Gedde, U.W.3
  • 16
    • 0035578070 scopus 로고    scopus 로고
    • The mechanisms of hydrophobic recovery of polydimethylsiloxane elastomers exposed to partial electrical discharges
    • DOI 10.1006/jcis.2001.7909
    • J. Kim, M. K. Chaudhury, M. J. Owen, and T. Orbeck, "The mechanisms of hydrophobic recovery of polydimethylsiloxane elastomers exposed to partial electrical discharges", J. Colloid Interface Sci., Vol. 244, p. 200-207, 2001. (Pubitemid 33144976)
    • (2001) Journal of Colloid and Interface Science , vol.244 , Issue.1 , pp. 200-207
    • Kim, J.1    Chaudhury, M.K.2    Owen, M.J.3    Orbeck, T.4
  • 17
    • 0037397861 scopus 로고    scopus 로고
    • Hydrophobic transfer of RTV silicone rubber aged in single and multiple environmental stresses and the behavior of LMW silicone fluid
    • S. Kumagai and N. Yoshimura, "Hydrophobic transfer of RTV silicone rubber aged in single and multiple environmental stresses and the behavior of LMW silicone fluid", IEEE Transactions on Power Delivery, vol. 18, pp. 506-516, 2003.
    • (2003) IEEE Transactions on Power Delivery , vol.18 , pp. 506-516
    • Kumagai, S.1    Yoshimura, N.2
  • 20
    • 0032759627 scopus 로고    scopus 로고
    • Water drop corona effects on full-scale 500 kV non-ceramic insulators
    • A. J. Phillips, D. J. Childs, and H. M. Schneider, "Water drop corona effects on full-scale 500 kV non-ceramic insulators", IEEE Trans. Power Delivery, Vol. 14, pp. 258-265, 1999.
    • (1999) IEEE Trans. Power Delivery , vol.14 , pp. 258-265
    • Phillips, A.J.1    Childs, D.J.2    Schneider, H.M.3
  • 21
    • 0008819175 scopus 로고    scopus 로고
    • Surface ageing mechanisms and their relationship to service performance of silicone rubber insulation
    • London, UK
    • J. P. Reynders, I. R. Jandrell, and S. M. Reynders, "Surface ageing mechanisms and their relationship to service performance of silicone rubber insulation", 11th Intern. Symposium High Voltage Engineering (ISH), London, UK, pp. 54-58, 1999.
    • (1999) 11th Intern. Symposium High Voltage Engineering (ISH) , pp. 54-58
    • Reynders, J.P.1    Jandrell, I.R.2    Reynders, S.M.3
  • 23
    • 0035307921 scopus 로고    scopus 로고
    • A study of partial discharges from water droplets on a silicone rubber insulating surface
    • I. J. S. Lopes, S. H. Jayaram, and E. A. Cherney, "A study of partial discharges from water droplets on a silicone rubber insulating surface", IEEE Trans. Dielectr. Electr. Insul., Vol. 8, pp. 262-268, 2001.
    • (2001) IEEE Trans. Dielectr. Electr. Insul. , vol.8 , pp. 262-268
    • Lopes, I.J.S.1    Jayaram, S.H.2    Cherney, E.A.3
  • 24
    • 0036645049 scopus 로고    scopus 로고
    • DC corona discharge from water droplets on a hydrophobic surface
    • DOI 10.1016/S0304-3886(01)00217-0, PII S0304388601002170, Selected papers from the 4th IEJ-ESA joint symposium on Electrostatics
    • Y. Higashiyama, S. Yanase, and T. Sugimoto, "DC corona discharge from water droplets on a hydrophobic surface", J. Electrostatics, Vol. 55, pp. 351-360, 2002. (Pubitemid 34714628)
    • (2002) Journal of Electrostatics , vol.55 , Issue.3-4 , pp. 351-360
    • Higashiyama, Y.1    Yanase, S.2    Sugimoto, T.3
  • 27
    • 33846542387 scopus 로고    scopus 로고
    • Behavior of water droplet on electrically stressed polymeric coating surface
    • DOI 10.1016/j.surfcoat.2006.07.116, PII S0257897206007286
    • Z. Yong, M. Otsubo, and C. Honda, "Behavior of water droplet on electrically stressed polymeric coating surface", Surface and Coatings Technology, Vol. 201, pp. 5541-5546, 2007. (Pubitemid 46158594)
    • (2007) Surface and Coatings Technology , vol.201 , pp. 5541-5546
    • Zhu, Y.1    Otsubo, M.2    Honda, C.3
  • 29
    • 0033706921 scopus 로고    scopus 로고
    • An experimental approach to the estimation of the long term corona performance of non-ceramic insulator housings
    • Anaheim, CA, USA
    • V. M. Moreno and R. S. Goror, "An experimental approach to the estimation of the long term corona performance of non-ceramic insulator housings", IEEE Intern. Symposium Electr. Insul., Anaheim, CA, USA, pp. 193-196, 2000.
    • (2000) IEEE Intern. Symposium Electr. Insul. , pp. 193-196
    • Moreno, V.M.1    Goror, R.S.2
  • 30
    • 0035248713 scopus 로고    scopus 로고
    • Effect of long-term corona on non-ceramic outdoor insulator housing materials
    • V. M. Moreno and R. S. Gorur, "Effect of long-term corona on non-ceramic outdoor insulator housing materials", IEEE Trans. Dielectr. Electr. Insul., Vol. 8, pp. 117-128, 2001.
    • (2001) IEEE Trans. Dielectr. Electr. Insul. , vol.8 , pp. 117-128
    • Moreno, V.M.1    Gorur, R.S.2
  • 31
    • 77951539132 scopus 로고    scopus 로고
    • Applying technology for better reliability; Materials testing and evaluation
    • Shanghai China
    • Ohio Brass, "Applying technology for better reliability; Materials testing and evaluation", World Insulator Congress, Shanghai China, pp. 245-253, 2001.
    • (2001) World Insulator Congress , pp. 245-253
    • Brass, O.1
  • 32
    • 0011774823 scopus 로고    scopus 로고
    • Hydrophobic Cycloaliphatic epoxy - Latest findings and future developments
    • Shanghai China
    • C. Beisele, "Hydrophobic Cycloaliphatic epoxy - latest findings and future developments", World Insulator Congress, Shanghai China, pp. 141-153, 2001.
    • (2001) World Insulator Congress , pp. 141-153
    • Beisele, C.1
  • 33
    • 84969802812 scopus 로고    scopus 로고
    • The hydrophobicity of silicone rubber insulators subjected to water droplet corona under HVDC potential
    • Kunming, China
    • N. M. Ijumba, A. C. Britten, and J. P. Swartz, "The hydrophobicity of silicone rubber insulators subjected to water droplet corona under HVDC potential", Intern. Conf. Power System Technology, Kunming, China, pp. 1884-1889, 2002.
    • (2002) Intern. Conf. Power System Technology , pp. 1884-1889
    • Ijumba, N.M.1    Britten, A.C.2    Swartz, J.P.3
  • 34
    • 0141739271 scopus 로고    scopus 로고
    • Positron annihilation spectroscopy study of high-voltage polydimethylsiloxane (PDMS) insulators
    • DOI 10.1016/S0969-806X(03)00204-4
    • P. E. Mallon, C. J. Greyling, W. Vosloo, and Y. C. Jean, "Positron annihilation spectroscopy study of high-voltage polydimethylsiloxane (PDMS) insulators", Radiation Phys. Chem., Vol. 68, pp. 453-456, 2003. (Pubitemid 37162439)
    • (2003) Radiation Physics and Chemistry , vol.68 , Issue.3-4 , pp. 453-456
    • Mallon, P.E.1    Greyling, C.J.2    Vosloo, W.3    Jean, Y.C.4
  • 35
    • 10044277071 scopus 로고    scopus 로고
    • Tracking the hydrophobicity recovery of PDMS compounds using the adhesive force determined by AFM force distance measurements
    • DOI 10.1016/j.polymer.2004.11.012, PII S0032386104011024
    • M. Meincken, T. A. Berhane, and P. E. Mallon, "Tracking the hydrophobicity recovery of PDMS compounds using the adhesive force determined by AFM force distance measurements", Polymer, Vol. 46, pp. 203-8, 2005. (Pubitemid 39602712)
    • (2005) Polymer , vol.46 , Issue.1 , pp. 203-208
    • Meincken, M.1    Berhane, T.A.2    Mallon, P.E.3
  • 36
    • 33747854637 scopus 로고    scopus 로고
    • Surface degradation of silicone rubber exposed to corona discharge
    • DOI 10.1109/TPS.2006.876498
    • Z. Yong, K. Haji, M. Otsubo, and C. Honda, "Surface degradation of silicone rubber exposed to corona discharge", IEEE Trans. Plasma Sci., Vol. 34, pp. 1094-8, 2006. (Pubitemid 44283354)
    • (2006) IEEE Transactions on Plasma Science , vol.34 , pp. 1094-1098
    • Zhu, Y.1    Haji, K.2    Otsubo, M.3    Honda, C.4
  • 37
    • 33747854637 scopus 로고    scopus 로고
    • Surface degradation of silicone rubber exposed to corona discharge
    • DOI 10.1109/TPS.2006.876498
    • Z. Yong, M. Otsubo, and C. Honda, "Degradation of polymeric materials exposed to corona discharges", Polymer Testing, Vol. 25, pp. 313-317, 2006. (Pubitemid 44283354)
    • (2006) IEEE Transactions on Plasma Science , vol.34 , pp. 1094-1098
    • Zhu, Y.1    Haji, K.2    Otsubo, M.3    Honda, C.4
  • 38
    • 0029220039 scopus 로고
    • Physical and chemical aspects of partial discharges and their effects on materials
    • M. Goldman, A. Goldman, and J. Gatellet, "Physical and chemical aspects of partial discharges and their effects on materials", IEE Proc. Sci., Measurement and Technology, Vol. 142, pp. 11-16, 1995.
    • (1995) IEE Proc. Sci., Measurement and Technology , vol.142 , pp. 11-16
    • Goldman, M.1    Goldman, A.2    Gatellet, J.3
  • 40
    • 0037300002 scopus 로고    scopus 로고
    • Impact of corona on the long-term performance of nonceramic insulators
    • V. M. Moreno and R. S. Gorur, "Impact of corona on the long-term performance of nonceramic insulators", IEEE Trans. Dielectr. Electr. Insul., Vol. 10, pp. 80-95, 2003.
    • (2003) IEEE Trans. Dielectr. Electr. Insul. , vol.10 , pp. 80-95
    • Moreno, V.M.1    Gorur, R.S.2
  • 41
    • 10644221880 scopus 로고    scopus 로고
    • Hydrophobic recovery of UV/ozone treated poly (dimethylsiloxane) : Adhesion studies by contact mechanics and mechanism of surface modification
    • A. Olah, H. Hillborg, and G. J. Vancso, "Hydrophobic recovery of UV/ozone treated poly (dimethylsiloxane) : adhesion studies by contact mechanics and mechanism of surface modification", Appl. Surface Sci., Vol. 239, pp. 410-423, 2005.
    • (2005) Appl. Surface Sci. , vol.239 , pp. 410-423
    • Olah, A.1    Hillborg, H.2    Vancso, G.J.3
  • 42
    • 77951609535 scopus 로고
    • International Electrotechnical Commission, Recommended test methods for determining the relative resistance of insulating materials to breakdown by surface discharges IEC 60343
    • International Electrotechnical Commission, Recommended test methods for determining the relative resistance of insulating materials to breakdown by surface discharges (IEC 60343), 1992.
    • (1992)
  • 43
    • 9144253355 scopus 로고    scopus 로고
    • Impact of corona on the long-term performance of nonceramic insulators
    • V. M. Moreno, R. S. Gorur, and A. Kroese, "Impact of corona on the long-term performance of nonceramic insulators", IEEE Trans. Dielectr. Electr. Insul., Vol. 11, pp. 913-915, 2004.
    • (2004) IEEE Trans. Dielectr. Electr. Insul. , vol.11 , pp. 913-915
    • Moreno, V.M.1    Gorur, R.S.2    Kroese, A.3
  • 44
    • 0032688010 scopus 로고    scopus 로고
    • AC and DC performance of polymeric housing materials for HV outdoor insulators
    • V. M. Moreno and R. S. Gorur, "AC and DC performance of polymeric housing materials for HV outdoor insulators", IEEE Trans. Dielectr. Electr. Insul., Vol. 6, pp. 342-350, 1999.
    • (1999) IEEE Trans. Dielectr. Electr. Insul. , vol.6 , pp. 342-350
    • Moreno, V.M.1    Gorur, R.S.2
  • 45
    • 0033354497 scopus 로고    scopus 로고
    • Accelerated corona discharge performance of polymer compounds used in high voltage outdoor insulators
    • Austin, TX, USA
    • V. M. Moreno and R. S. Gorur, "Accelerated corona discharge performance of polymer compounds used in high voltage outdoor insulators", IEEE Conf. Electr. Insul. Dielectr. Phenomena (CEIDP), Austin, TX, USA, pp. 731-734, 1999.
    • (1999) IEEE Conf. Electr. Insul. Dielectr. Phenomena (CEIDP) , pp. 731-734
    • Moreno, V.M.1    Gorur, R.S.2
  • 47
    • 58049126576 scopus 로고    scopus 로고
    • Effects of corona discharge on surface deterioration of silicone rubber insulator under reduced pressures
    • Piscataway, NJ, USA
    • B. X. Du, L. Yong, and R. L. Wang, "Effects of corona discharge on surface deterioration of silicone rubber insulator under reduced pressures", Intern. Symposium on Electr. Insul. Materials, Piscataway, NJ, USA, pp. 271-274, 2008.
    • (2008) Intern. Symposium on Electr. Insul. Materials , pp. 271-274
    • Du, B.X.1    Yong, L.2    Wang, R.L.3
  • 48
    • 50249137637 scopus 로고    scopus 로고
    • Surface degradation of styrene acrylonitrile exposed to corona discharge
    • M. A. Handala and O. Lamrous, "Surface degradation of styrene acrylonitrile exposed to corona discharge", European Trans. Electr. Power, Vol. 18, pp. 494-505, 2008.
    • (2008) European Trans. Electr. Power , vol.18 , pp. 494-505
    • Handala, M.A.1    Lamrous, O.2
  • 50
    • 0010765455 scopus 로고
    • Mechanism of the ozone formations in a near liquid nitrogen temperature medium pressure glow discharge positive column
    • J. S. Chang and S. Masuda, "Mechanism of the ozone formations in a near liquid nitrogen temperature medium pressure glow discharge positive column", Pure Appl. Chem., Vol. 60, No. 5, pp. 645-650, 1980.
    • (1980) Pure Appl. Chem. , vol.60 , Issue.5 , pp. 645-650
    • Chang, J.S.1    Masuda, S.2
  • 51
    • 0004205118 scopus 로고
    • Amsterdam, The Netherlands: Elsevier Science
    • M. Horvath, Ozone. Amsterdam, The Netherlands: Elsevier Science, 1980.
    • (1980) Ozone
    • Horvath, M.1
  • 52
    • 77951527876 scopus 로고
    • International Organization for Standardization, Rubber, vulcanized or thermoplastic - Resistance to ozone cracking - Part 1: Static strain test ISO 1431-1
    • International Organization for Standardization, Rubber, vulcanized or thermoplastic - Resistance to ozone cracking - Part 1: Static strain test (ISO 1431-1), 1989.
    • (1989)
  • 53
    • 77951617834 scopus 로고
    • International Organization for Standardization, Rubber, vulcanized or thermoplastic - Resistance to ozone cracking - Part 2: Dynamic strain test ISO 1431-2
    • International Organization for Standardization, Rubber, vulcanized or thermoplastic - Resistance to ozone cracking - Part 2: Dynamic strain test (ISO 1431-2), 1994.
    • (1994)
  • 54
    • 77951590556 scopus 로고    scopus 로고
    • International organization for standardization
    • Resistance to ozone cracking - Part 3: Reference and alternative methods for determining the ozone concentration in laboratory test chambers ISO 1431-3
    • International Organization for Standardization, Rubber, vulcanized or thermoplastic - Resistance to ozone cracking - Part 3: Reference and alternative methods for determining the ozone concentration in laboratory test chambers (ISO 1431-3), 2000.
    • (2000) Rubber, Vulcanized Or Thermoplastic
  • 55
    • 77951524456 scopus 로고    scopus 로고
    • American Society for Testing and Materials, Standard test method for rubber deterioration - surface ozone cracking in a chamber ASTM D1149-99
    • American Society for Testing and Materials, Standard test method for rubber deterioration - surface ozone cracking in a chamber (ASTM D1149-99).
  • 56
    • 77951617135 scopus 로고    scopus 로고
    • Deutsches Institut für Normung, Prüfung von kautschuk und elastomeren-bestimmung der beständigkeit gegen rissbildung unter ozoneinwirkung-teil 1: statische beanspruchung DIN 53509-1, in German
    • Deutsches Institut für Normung, Prüfung von kautschuk und elastomeren-bestimmung der beständigkeit gegen rissbildung unter ozoneinwirkung-teil 1: statische beanspruchung (DIN 53509-1, in German), 2001.
    • (2001)
  • 57
    • 77951551692 scopus 로고
    • Deutsches Institut für Normung, Prüfung von kautschuk und elastomeren-bestimmung der beständigkeit gegen rissbildung unter ozoneinwirkung-teil 2: Referenz-verfahren zur bestimmung der ozonkonzentration in prufkammern DIN 53509-2, in German
    • Deutsches Institut für Normung, Prüfung von kautschuk und elastomeren-bestimmung der beständigkeit gegen rissbildung unter ozoneinwirkung-teil 2: Referenz-verfahren zur bestimmung der ozonkonzentration in prufkammern (DIN 53509-2, in German), 1994.
    • (1994)
  • 58
    • 0032070218 scopus 로고    scopus 로고
    • Automated system for power measurement in the silent discharge
    • PII S0093999498041176
    • R. Feng, G. S. P. Castle, and S. Jayaram, "Automated system for power measurement in the silent discharge", IEEE Trans. Industry Applications, Vol. 34, pp. 563-570, 1998. (Pubitemid 128740187)
    • (1998) IEEE Transactions on Industry Applications , vol.34 , Issue.3 , pp. 563-570
    • Feng, R.1    Castle, G.S.P.2    Jayaram, S.3
  • 60
    • 77951591530 scopus 로고    scopus 로고
    • Tokyo Japan: Komyo Rikagaku Kogyo K. K.
    • KITAGAWA Gas Detector Tube System Handbook. Tokyo Japan: Komyo Rikagaku Kogyo K. K., 2008 (http://www.komyokk.co.jp).
    • (2008) KITAGAWA Gas Detector Tube System Handbook
  • 61
    • 0029304597 scopus 로고
    • Partial discharge XX. Partial discharges in air. II. Selection of line conductors
    • N. G. Trinh, "Partial discharge XX. Partial discharges in air. II. Selection of line conductors", IEEE Electr. Insul. Mag., Vol. 11, pp. 5-11, 1995.
    • (1995) IEEE Electr. Insul. Mag. , vol.11 , pp. 5-11
    • Trinh, N.G.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.