Volumn 157, Issue 5, 2010, Pages

Enhanced dissolution rate of Pt from a Pt-Zn compound measured by channel flow double electrode

Author keywords

[No Author keywords available]

Indexed keywords

ANODIC BEHAVIOR; CHANNEL FLOW DOUBLE ELECTRODE METHODS; DISSOLUTION RATES; DOUBLE ELECTRODES; HIGH RATE; HYDROMETALLURGICAL RECOVERY; LOW CRYSTALLINITY; ONSET POTENTIAL; PREFERENTIAL DISSOLUTION; PT ELECTRODE; STANDARD HYDROGEN ELECTRODES; SURFACE AREA; SURFACE LAYERS;

EID: 77951163086     PISSN: 00134651     EISSN: None     Source Type: Journal    
DOI: 10.1149/1.3332468     Document Type: Article
Times cited : (18)

References (43)
  • 2
    • 18144421736 scopus 로고    scopus 로고
    • 10.2473/shigentosozai.118.1
    • J. Shibata and A. Okuda, Shigen-to-Sozai, 118, 1 (2002). 10.2473/shigentosozai.118.1
    • (2002) Shigen-to-Sozai , vol.118 , pp. 1
    • Shibata, J.1    Okuda, A.2
  • 3
    • 0034876928 scopus 로고    scopus 로고
    • New convenient dissolution of iron-rhodium alloys using hydrochloric acid containing a small amount of nitric acid without heating for an ICP-AES analysis
    • DOI 10.2116/analsci.17.1011
    • Y. Danzaki and T. Ashino, Anal. Sci. 0910-6340, 17, 1011 (2001). 10.2116/analsci.17.1011 (Pubitemid 32802319)
    • (2001) Analytical Sciences , vol.17 , Issue.8 , pp. 1011-1013
    • Danzaki, Y.1    Ashino, T.2
  • 4
    • 0002971081 scopus 로고    scopus 로고
    • 0920-5861. 10.1016/S0920-5861(98)00171-0
    • J. S. Yoo, Catal. Today 0920-5861, 44, 27 (1998). 10.1016/S0920-5861(98) 00171-0
    • (1998) Catal. Today , vol.44 , pp. 27
    • Yoo, J.S.1
  • 5
    • 0013643473 scopus 로고    scopus 로고
    • Preliminary studies of platinum dissolution from a spent industrial catalyst
    • DOI 10.1016/0926-860X(96)00088-9, PII S0926860X96000889
    • T. N. Angelidis and E. Skouraki, Appl. Catal., A 0926-860X, 142, 387 (1996). 10.1016/0926-860X(96)00088-9 (Pubitemid 126387561)
    • (1996) Applied Catalysis A: General , vol.142 , Issue.2 , pp. 387-395
    • Angelidis, T.N.1    Skouraki, E.2
  • 6
    • 1342264350 scopus 로고    scopus 로고
    • 0304-386X. 10.1016/S0304-386X(03)00141-5
    • M. A. Barakat and M. H. H. Mahmoud, Hydrometallurgy 0304-386X, 72, 179 (2004). 10.1016/S0304-386X(03)00141-5
    • (2004) Hydrometallurgy , vol.72 , pp. 179
    • Barakat, M.A.1    Mahmoud, M.H.H.2
  • 13
    • 0027574648 scopus 로고
    • 0010-938X. 10.1016/0010-938X(93)90280-T
    • H. Kaiser, Corros. Sci. 0010-938X, 34, 683 (1993). 10.1016/0010-938X(93) 90280-T
    • (1993) Corros. Sci. , vol.34 , pp. 683
    • Kaiser, H.1
  • 14
    • 0000432409 scopus 로고    scopus 로고
    • 0010-938X. 10.1016/S0010-938X(97)00016-4
    • K. E. Heusler, Corros. Sci. 0010-938X, 39, 1177 (1997). 10.1016/S0010-938X(97)00016-4
    • (1997) Corros. Sci. , vol.39 , pp. 1177
    • Heusler, K.E.1
  • 15
    • 33746357562 scopus 로고    scopus 로고
    • 4 aqueous solution
    • DOI 10.1016/j.corsci.2005.08.020, PII S0010938X05002672
    • E. Sidot, N. Souissi, L. Bousselmi, E. Triki, and L. Robbiola, Corros. Sci. 0010-938X, 48, 2241 (2006). 10.1016/j.corsci.2005.08.020 (Pubitemid 44109844)
    • (2006) Corrosion Science , vol.48 , Issue.8 , pp. 2241-2257
    • Sidot, E.1    Souissi, N.2    Bousselmi, L.3    Triki, E.4    Robbiola, L.5
  • 16
    • 33746256999 scopus 로고    scopus 로고
    • Electrochemical behavior of multicomponent amorphous and nanocrystalline Zr-based alloys in different environments
    • DOI 10.1016/j.corsci.2005.09.001, PII S0010938X05002714
    • K. Mondal, B. S. Murty, and U. K. Chatterjee, Corros. Sci. 0010-938X, 48, 2212 (2006). 10.1016/j.corsci.2005.09.001 (Pubitemid 44093485)
    • (2006) Corrosion Science , vol.48 , Issue.8 , pp. 2212-2225
    • Mondal, K.1    Murty, B.S.2    Chatterjee, U.K.3
  • 18
    • 3042515574 scopus 로고    scopus 로고
    • De-alloying of type 316 stainless steel in hot, concentrated sodium hydroxide solution
    • DOI 10.1016/j.corsci.2004.01.011, PII S0010938X04000125
    • J. Deakin, Z. Dong, B. Lynch, and R. C. Newman, Corros. Sci. 0010-938X, 46, 2117 (2004). 10.1016/j.corsci.2004.01.011 (Pubitemid 39168822)
    • (2004) Corrosion Science , vol.46 , Issue.9 , pp. 2117-2133
    • Deakin, J.1    Dong, Z.2    Lynch, B.3    Newman, R.C.4
  • 19
    • 0037401635 scopus 로고    scopus 로고
    • Mechanism of dissolution of a Cu-13Sn alloy in low aggressive conditions
    • DOI 10.1016/S0010-938X(02)00207-X, PII S0010938X0200207X
    • I. Mabille, A. Bertrand, E. M. M. Sutter, and C. Fiaud, Corros. Sci. 0010-938X, 45, 855 (2003). 10.1016/S0010-938X(02)00207-X (Pubitemid 36122320)
    • (2003) Corrosion Science , vol.45 , Issue.5 , pp. 855-866
    • Mabille, I.1    Bertrand, A.2    Sutter, E.M.M.3    Fiaud, C.4
  • 20
    • 0035371921 scopus 로고    scopus 로고
    • Comparison of the spontaneous and anodic processes during dissolution of brass
    • DOI 10.1016/S0010-938X(00)00130-X, PII S0010938X0000130X
    • L. Burzynska, Corros. Sci. 0010-938X, 43, 1053 (2001). 10.1016/S0010-938X(00)00130-X (Pubitemid 32434809)
    • (2001) Corrosion Science , vol.43 , Issue.6 , pp. 1053-1069
    • Burzynska, L.1
  • 21
    • 33748973369 scopus 로고    scopus 로고
    • Influence of composition on corrosion behavior of as-cast Cu-Zr alloys in HCl solution
    • DOI 10.1016/j.electacta.2006.05.047, PII S0013468606006244
    • H. Lu, Y. Li, and F. Wang, Electrochim. Acta 0013-4686, 52, 474 (2006). 10.1016/j.electacta.2006.05.047 (Pubitemid 44441226)
    • (2006) Electrochimica Acta , vol.52 , Issue.2 , pp. 474-480
    • Lu, H.-B.1    Li, Y.2    Wang, F.-H.3
  • 22
    • 0037024039 scopus 로고    scopus 로고
    • Electrochemical behavior of brass in 0.1 M NaCl
    • DOI 10.1016/S0169-4332(02)00258-1, PII S0169433202002581
    • M. Kabasakaloglu, T. Kiyak, O. Sendil, and A. Asan, Appl. Surf. Sci. 0169-4332, 193, 167 (2002). 10.1016/S0169-4332(02)00258-1 (Pubitemid 34807870)
    • (2002) Applied Surface Science , vol.193 , Issue.1-4 , pp. 167-174
    • Kabasakaloglu, M.1    Kiyak, T.2    Sendil, O.3    Asan, A.4
  • 23
    • 0019571522 scopus 로고
    • Study of the kinetics and mechanism of brass dezincification by radiotracer and electrochemical methods
    • DOI 10.1016/0013-4686(81)80025-4
    • A. P. Pchelnikov, A. D. Sitnikov, I. K. Marshakov, and V. V. Losev, Electrochim. Acta 0013-4686, 26, 591 (1981). 10.1016/0013-4686(81)80025-4 (Pubitemid 11505113)
    • (1981) Electrochimica Acta , vol.26 , Issue.5 , pp. 591-600
    • Pchelnikov, A.P.1    Sitnikov, A.D.2    Marshakov, I.K.3    Losev, V.V.4
  • 25
    • 0001890171 scopus 로고
    • 0013-4651. 10.1149/1.2407450
    • H. W. Pickering, J. Electrochem. Soc. 0013-4651, 117, 8 (1970). 10.1149/1.2407450
    • (1970) J. Electrochem. Soc. , vol.117 , pp. 8
    • Pickering, H.W.1
  • 28
    • 0026241847 scopus 로고
    • 0921-5093. 10.1016/0921-5093(91)90264-N
    • T. Tsuru, Mater. Sci. Eng., A 0921-5093, 146, 1 (1991). 10.1016/0921-5093(91)90264-N
    • (1991) Mater. Sci. Eng., A , vol.146 , pp. 1
    • Tsuru, T.1
  • 31
    • 0032835539 scopus 로고    scopus 로고
    • The quantitative analysis of chromous ions by channel flow double electrode (CFDE) technique
    • DOI 10.1016/S0010-938X(98)00196-6, PII S0010938X98001966
    • B. Vuillemin and R. Oltra, Corros. Sci. 0010-938X, 41, 1419 (1999). 10.1016/S0010-938X(98)00196-6 (Pubitemid 29417177)
    • (1999) Corrosion Science , vol.41 , Issue.7 , pp. 1419-1430
    • Vuillemin, B.1    Oltra, R.2
  • 32
    • 0016559053 scopus 로고
    • 0001-6160. 10.1016/0001-6160(75)90036-X
    • S. Kou and Y. A. Chang, Acta Metall. 0001-6160, 23, 1185 (1975). 10.1016/0001-6160(75)90036-X
    • (1975) Acta Metall. , vol.23 , pp. 1185
    • Kou, S.1    Chang, Y.A.2
  • 35
    • 84951279351 scopus 로고
    • 0044-3328. 10.1007/BF01337937
    • G. Sauerbrey, Z. Phys. 0044-3328, 155, 206 (1959). 10.1007/BF01337937
    • (1959) Z. Phys. , vol.155 , pp. 206
    • Sauerbrey, G.1
  • 36
    • 2342619416 scopus 로고    scopus 로고
    • The Electrochemical Society of Japan, Editor, Maruzen, Tokyo, Japan
    • Denki Kagaku Binran, The Electrochemical Society of Japan, Editor, Maruzen, Tokyo, Japan (2000).
    • (2000) Denki Kagaku Binran
  • 38
    • 0014712141 scopus 로고
    • 0010-938X. 10.1016/S0010-938X(70)80095-6
    • J. A. Bittles and E. L. Littauer, Corros. Sci. 0010-938X, 10, 29 (1970). 10.1016/S0010-938X(70)80095-6
    • (1970) Corros. Sci. , vol.10 , pp. 29
    • Bittles, J.A.1    Littauer, E.L.2
  • 39
    • 0036608826 scopus 로고    scopus 로고
    • The electrochemical dissolution of platinum
    • DOI 10.1016/S0304-386X(02)00044-0, PII S0304386X02000440
    • G. Benke and W. Gnot, Hydrometallurgy 0304-386X, 64, 205 (2002). 10.1016/S0304-386X(02)00044-0 (Pubitemid 34704425)
    • (2002) Hydrometallurgy , vol.64 , Issue.3 , pp. 205-218
    • Benke, G.1    Gnot, W.2
  • 41
    • 34547871135 scopus 로고
    • 0010-938X. 10.1016/0010-938X(64)90022-8
    • J. Mieluch and M. Smialowski, Corros. Sci. 0010-938X, 4, 237 (1964). 10.1016/0010-938X(64)90022-8
    • (1964) Corros. Sci. , vol.4 , pp. 237
    • Mieluch, J.1    Smialowski, M.2
  • 43
    • 0027666834 scopus 로고
    • 0956-7151. 10.1016/0956-7151(93)90147-K
    • A. Tschöpe and R. Birringer, Acta Metall. Mater. 0956-7151, 41, 2791 (1993). 10.1016/0956-7151(93)90147-K
    • (1993) Acta Metall. Mater. , vol.41 , pp. 2791
    • Tschöpe, A.1    Birringer, R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.