Volumn 95, Issue 5, 2010, Pages 709-718

Mechanism of thermal decomposition of poly(ether ether ketone) (PEEK) from a review of decomposition studies

Author keywords

[No Author keywords available]

Indexed keywords

DECOMPOSITION MECHANISM; THERMAL DECOMPOSITIONS;

EID: 77949913236     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymdegradstab.2010.01.024     Document Type: Review
Times cited : (303)

References (29)
  • 1
    • 0142154973 scopus 로고    scopus 로고
    • Comparison of new PEEK seals with traditional helicoflex for ultra high vacuum applications
    • Murari A., and Barzon A. Comparison of new PEEK seals with traditional helicoflex for ultra high vacuum applications. Vacuum 72 3 (2003) 327-334
    • (2003) Vacuum , vol.72 , Issue.3 , pp. 327-334
    • Murari, A.1    Barzon, A.2
  • 2
    • 33748282386 scopus 로고
    • The thermal decomposition kinetics of poly(ether-ether-ketone) (PEEK) and its carbon fibre composite
    • Yao F., Zheng J., Qi M., Wang W., and Qi Z. The thermal decomposition kinetics of poly(ether-ether-ketone) (PEEK) and its carbon fibre composite. Thermochim Acta 183 (1991) 91-97
    • (1991) Thermochim Acta , vol.183 , pp. 91-97
    • Yao, F.1    Zheng, J.2    Qi, M.3    Wang, W.4    Qi, Z.5
  • 3
    • 0037211553 scopus 로고    scopus 로고
    • Poly(ether ether ketone)/poly(aryl ether sulphone) blends: thermal degradation behaviour
    • Nandan B., Kandpal L., and Mathur G.N. Poly(ether ether ketone)/poly(aryl ether sulphone) blends: thermal degradation behaviour. Eur Polymer J 39 1 (2002) 193-198
    • (2002) Eur Polymer J , vol.39 , Issue.1 , pp. 193-198
    • Nandan, B.1    Kandpal, L.2    Mathur, G.N.3
  • 4
    • 0033360713 scopus 로고    scopus 로고
    • Thermal decomposition of technological polymer blends. 1. Poly(aryl ether ether ketone) with a thermotropic liquid crystalline polymer
    • Naffakh M., Ellis G., Gomez M., and Marco C. Thermal decomposition of technological polymer blends. 1. Poly(aryl ether ether ketone) with a thermotropic liquid crystalline polymer. Polymer Degrad Stab 66 3 (1999) 405-413
    • (1999) Polymer Degrad Stab , vol.66 , Issue.3 , pp. 405-413
    • Naffakh, M.1    Ellis, G.2    Gomez, M.3    Marco, C.4
  • 5
    • 0026852856 scopus 로고
    • Generalised composite degradation kinetics for polymeric systems under isothermal and nonisothermal conditions
    • Nam J.D., and Seferis J.C. Generalised composite degradation kinetics for polymeric systems under isothermal and nonisothermal conditions. J Polymer Sci 30 5 (1992) 455-463
    • (1992) J Polymer Sci , vol.30 , Issue.5 , pp. 455-463
    • Nam, J.D.1    Seferis, J.C.2
  • 6
    • 77949914552 scopus 로고
    • Kinetic studies on thermal degradation of poly(aryl ether ether ketone) and sulphonated poly(aryl ether ether ketone) by thermogravimetry
    • Huo R., Luo Y., Liang L., Jin X., and Karasz F.E. Kinetic studies on thermal degradation of poly(aryl ether ether ketone) and sulphonated poly(aryl ether ether ketone) by thermogravimetry. J Functional Polymers 4 (1990) 426-433
    • (1990) J Functional Polymers , vol.4 , pp. 426-433
    • Huo, R.1    Luo, Y.2    Liang, L.3    Jin, X.4    Karasz, F.E.5
  • 7
    • 0009686039 scopus 로고
    • The kinetics of the oxidative degradation of poly(aryl-ether-ether-ketone) (PEEK)
    • Day M., Cooney J.D., and Wiles D.M. The kinetics of the oxidative degradation of poly(aryl-ether-ether-ketone) (PEEK). Thermochim Acta 147 1 (1989) 189-197
    • (1989) Thermochim Acta , vol.147 , Issue.1 , pp. 189-197
    • Day, M.1    Cooney, J.D.2    Wiles, D.M.3
  • 8
    • 0024701121 scopus 로고
    • The thermal stability of poly(aryl ether ether ketone) as assessed by thermogravimetry
    • Day M., Cooney J.D., and Wiles D.M. The thermal stability of poly(aryl ether ether ketone) as assessed by thermogravimetry. J Appl Polymer Sci 38 2 (1989) 323-337
    • (1989) J Appl Polymer Sci , vol.38 , Issue.2 , pp. 323-337
    • Day, M.1    Cooney, J.D.2    Wiles, D.M.3
  • 9
    • 33745174670 scopus 로고    scopus 로고
    • Study on the kinetics and mechanism of thermal degradation of PEEK by temperature programmed decomposition
    • He J., Duan X., and Wang Z.-X. Study on the kinetics and mechanism of thermal degradation of PEEK by temperature programmed decomposition. Acta Chim Sin 55 12 (1997) 1152-1157
    • (1997) Acta Chim Sin , vol.55 , Issue.12 , pp. 1152-1157
    • He, J.1    Duan, X.2    Wang, Z.-X.3
  • 10
    • 0027549653 scopus 로고
    • Fourier transform infrared spectroscopic study of thermal degradation in poly(ether ether ketone) - carbon composites
    • Cole K.C., and Casella I.G. Fourier transform infrared spectroscopic study of thermal degradation in poly(ether ether ketone) - carbon composites. Polymer 34 4 (1993) 740-745
    • (1993) Polymer , vol.34 , Issue.4 , pp. 740-745
    • Cole, K.C.1    Casella, I.G.2
  • 11
    • 1442300308 scopus 로고
    • Fourier transform infrared spectroscopic study of thermal degradation in films of poly(ether ether ketone)
    • Cole K.C., and Casella I.G. Fourier transform infrared spectroscopic study of thermal degradation in films of poly(ether ether ketone). Thermochim Acta 211 (1992) 209-228
    • (1992) Thermochim Acta , vol.211 , pp. 209-228
    • Cole, K.C.1    Casella, I.G.2
  • 12
    • 0346308524 scopus 로고    scopus 로고
    • Stable polymeric materials for non-linear optics: a review based on azobenzene systems
    • Yesodha S.K., Pillai C.K.S., and Tsutsuni N. Stable polymeric materials for non-linear optics: a review based on azobenzene systems. Prog Polymer Sci 29 1 (2004) 45-74
    • (2004) Prog Polymer Sci , vol.29 , Issue.1 , pp. 45-74
    • Yesodha, S.K.1    Pillai, C.K.S.2    Tsutsuni, N.3
  • 13
    • 0004289922 scopus 로고    scopus 로고
    • Stevens M.P. (Ed), Oxford University Press, New York
    • In: Stevens M.P. (Ed). Polymer chemistry: an introduction (1999), Oxford University Press, New York
    • (1999) Polymer chemistry: an introduction
  • 15
    • 0036589632 scopus 로고    scopus 로고
    • Molar group contributions to the heat of combustion
    • Walters R.N. Molar group contributions to the heat of combustion. Fire Mater 26 (2002) 131-145
    • (2002) Fire Mater , vol.26 , pp. 131-145
    • Walters, R.N.1
  • 16
    • 77949914837 scopus 로고    scopus 로고
    • Determination of kinetic parameters for thermal decomposition of combustible solids using microscale combustion calorimetry
    • Presented at, Gaithersburg, MD, April 29
    • Safronava N, Stoliarov SI, Lyon RE. Determination of kinetic parameters for thermal decomposition of combustible solids using microscale combustion calorimetry. Presented at NIST/BFRL Annual Conference, Gaithersburg, MD, April 29 2009
    • (2009) NIST/BFRL Annual Conference
    • Safronava, N.1    Stoliarov, S.I.2    Lyon, R.E.3
  • 18
    • 34249290251 scopus 로고    scopus 로고
    • US Department of Transport, Washington, DC Report Number: DOT/FAA/AR-04/11
    • Zhang H. Fire-safe polymers and polymer composites (2004), US Department of Transport, Washington, DC Report Number: DOT/FAA/AR-04/11
    • (2004) Fire-safe polymers and polymer composites
    • Zhang, H.1
  • 20
    • 0345034788 scopus 로고    scopus 로고
    • Mechanism and kinetic modelling of PEEK pyrolysis by TG/MS
    • Perng L.H., Tsai C.J., and Ling Y.C. Mechanism and kinetic modelling of PEEK pyrolysis by TG/MS. Polymer 40 (1999) 7321-7329
    • (1999) Polymer , vol.40 , pp. 7321-7329
    • Perng, L.H.1    Tsai, C.J.2    Ling, Y.C.3
  • 21
    • 0023451034 scopus 로고
    • Thermal decomposition of poly(aryl ether ketones)
    • Hay J.N., and Kemmish D.J. Thermal decomposition of poly(aryl ether ketones). Polymer 28 (1987) 2047-2051
    • (1987) Polymer , vol.28 , pp. 2047-2051
    • Hay, J.N.1    Kemmish, D.J.2
  • 22
    • 0031453347 scopus 로고    scopus 로고
    • A study of thermal degradation of poly(aryl-ether-ether-ketone) using stepwise pyrolysis/gas chromatography/mass spectrometry
    • Tsai C.J., Perng L.H., and Ling Y.C. A study of thermal degradation of poly(aryl-ether-ether-ketone) using stepwise pyrolysis/gas chromatography/mass spectrometry. Rapid Commun Mass Spectrom 11 (1997) 1987-1995
    • (1997) Rapid Commun Mass Spectrom , vol.11 , pp. 1987-1995
    • Tsai, C.J.1    Perng, L.H.2    Ling, Y.C.3
  • 24
    • 0019027112 scopus 로고
    • Estimation of the rate of heat release by means of oxygen consumption measurements
    • Huggett C. Estimation of the rate of heat release by means of oxygen consumption measurements. Fire Mater 4 2 (1980) 61-65
    • (1980) Fire Mater , vol.4 , Issue.2 , pp. 61-65
    • Huggett, C.1
  • 25
    • 34547526017 scopus 로고    scopus 로고
    • Application of cone calorimetry to the development of materials with improved fire performance
    • Schartel B., and Hull T.R. Application of cone calorimetry to the development of materials with improved fire performance. Fire Mater 31 (2007) 327-354
    • (2007) Fire Mater , vol.31 , pp. 327-354
    • Schartel, B.1    Hull, T.R.2
  • 26
    • 34648840525 scopus 로고    scopus 로고
    • Effect of multiple shear histories on rheological behaviour and devolatilisation of poly (ether ether ketone)
    • Cincinnati, OH: SPE;
    • Galloway J, Hoffamn R, Bhatt S. Effect of multiple shear histories on rheological behaviour and devolatilisation of poly (ether ether ketone). ANTEC Conference Proceedings, 5. Cincinnati, OH: SPE; 2007, p. 3031-3035.
    • (2007) ANTEC Conference Proceedings , vol.5 , pp. 3031-3035
    • Galloway, J.1    Hoffamn, R.2    Bhatt, S.3
  • 27
    • 0037211553 scopus 로고    scopus 로고
    • Poly(ether ether ketone)/poly(aryl ether sulphone) blends: thermal degradation behaviour
    • Nandan B., Kandpal L.D., and Mathur G.N. Poly(ether ether ketone)/poly(aryl ether sulphone) blends: thermal degradation behaviour. Euro Polymer J 39 (2003) 193-198
    • (2003) Euro Polymer J , vol.39 , pp. 193-198
    • Nandan, B.1    Kandpal, L.D.2    Mathur, G.N.3
  • 28
    • 0000352440 scopus 로고
    • The thermal degradation of poly(aryl ether ether ketone) (PEEK) as monitored by pyrolysis-GC/MS and TG/MS
    • Day M., Cooney J., and Wiles D.M. The thermal degradation of poly(aryl ether ether ketone) (PEEK) as monitored by pyrolysis-GC/MS and TG/MS. J Anal Appl Pyrol 18 (1990) 163-173
    • (1990) J Anal Appl Pyrol , vol.18 , pp. 163-173
    • Day, M.1    Cooney, J.2    Wiles, D.M.3
  • 29
    • 0025701252 scopus 로고
    • Thermal degradation of poly(aryl-ether-ether-ketone): experimental evaluation of crosslinking reactions
    • Day M., Sally D., and Wiles D.M. Thermal degradation of poly(aryl-ether-ether-ketone): experimental evaluation of crosslinking reactions. J Appl Polymer Sci 40 (1990) 1615-1620
    • (1990) J Appl Polymer Sci , vol.40 , pp. 1615-1620
    • Day, M.1    Sally, D.2    Wiles, D.M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.