Volumn 21, Issue 1, 2010, Pages 109-122

Hardness properties and microscopic investigation of crack-crystal interaction in SiO2-MgO-Al2O3-K 2O-B2O3-F glass ceramic system

Author keywords

[No Author keywords available]

Indexed keywords

ABRASION WEAR; ARTIFICIAL SALIVA; CRACK BLUNTING; CRACK DEFLECTIONS; CRYSTAL INTERACTIONS; CRYSTAL MORPHOLOGIES; DAMAGE BEHAVIOR; DAMAGE TOLERANT; DENDRITIC STRUCTURES; ENGINEERING APPLICATIONS; EXPERIMENTAL OBSERVATION; GLASS MATRICES; GLASS-CERAMIC SYSTEMS; HIGH LOAD; INDUCED CRACK; INTERFACIAL AREAS; MACHINING OPERATIONS; MICA CRYSTALS; MICA PLATES; MICRO-INDENTATION TESTS; PLATE-LIKE CRYSTALS; SCRATCH TEST; WORK FOCUS;

EID: 75049085036     PISSN: 09574530     EISSN: None     Source Type: Journal    
DOI: 10.1007/s10856-009-3853-7     Document Type: Article
Times cited : (24)

References (32)
  • 1
    • 0021394315 scopus 로고
    • Development of machinable bioactive glass-ceramics for medical uses
    • 10.1016/0022-3093(86)90377-7 1:CAS:528:DyaL28XitlShurk%3D 1986JNCS.80.34V
    • W Vogel W Höland K Kaumann 1986 Development of machinable bioactive glass-ceramics for medical uses J Non-Cryst Solids 80 34 51 10.1016/0022- 3093(86)90377-7 1:CAS:528:DyaL28XitlShurk%3D 1986JNCS...80...34V
    • (1986) J Non-Cryst Solids , vol.80 , pp. 34-51
    • Vogel, W.1    Höland, W.2    Kaumann, K.3
  • 2
    • 0023843735 scopus 로고
    • High-temperature dielectric properties of ruby mica perpendicular to the cleavage planes
    • 10.1007/BF01174055 1:CAS:528:DyaL1cXktlSrtrw%3D 1988JMatS.23.208C
    • MA Chaudhry AK Jonscher 1988 High-temperature dielectric properties of ruby mica perpendicular to the cleavage planes J Mater Sci 23 208 216 10.1007/BF01174055 1:CAS:528:DyaL1cXktlSrtrw%3D 1988JMatS..23..208C
    • (1988) J Mater Sci , vol.23 , pp. 208-216
    • Chaudhry, M.A.1    Jonscher, A.K.2
  • 3
    • 0000717191 scopus 로고
    • Machineable and phosphate glass ceramics
    • L.L. Hench J. Wilson (eds). World Scientific Singapore
    • Holand W, Vogel W. Machineable and phosphate glass ceramics. In: Hench LL, Wilson J, editors. Introduction to bioceramics. Singapore: World Scientific; 1993. pp. 125-38.
    • (1993) Introduction to Bioceramics , pp. 125-138
    • Holand, W.1    Vogel, W.2
  • 5
    • 0035155929 scopus 로고    scopus 로고
    • +) glasses with different fluorine source
    • DOI 10.1016/S0167-577X(00)00201-9
    • +) glasses with different fluorine sources Mater Lett 47 1 6 10.1016/S0167-577X(00)00201-9 1:CAS:528:DC%2BD3cXoslaqtL8%3D (Pubitemid 32070701)
    • (2001) Materials Letters , vol.47 , Issue.1-2 , pp. 1-6
    • Cheng, K.1    Wan, J.2    Liang, K.3
  • 7
    • 0345770042 scopus 로고    scopus 로고
    • TEM study on the origin of cabbage-shaped mica crystal aggregates in machinable glass-ceramics
    • 10.1016/S1359-6454(99)00317-1 1:CAS:528:DC%2BD3cXjtVWhsw%3D%3D
    • A Gebhardt T Hoche G Carl II Khodos 1999 TEM study on the origin of cabbage-shaped mica crystal aggregates in machinable glass-ceramics Acta Mater 47 17 4427 4434 10.1016/S1359-6454(99)00317-1 1:CAS:528:DC%2BD3cXjtVWhsw%3D%3D
    • (1999) Acta Mater , vol.47 , Issue.17 , pp. 4427-4434
    • Gebhardt, A.1    Hoche, T.2    Carl, G.3    Khodos, I.I.4
  • 8
    • 0042128698 scopus 로고    scopus 로고
    • Influence of microstructure and chemistry on the fracture toughness of dental ceramics
    • 10.1016/S0109-5641(03)00002-2 1:CAS:528:DC%2BD3sXlvFymt7Y%3D 12901984
    • JB Quinn V Sundar IK Lloyd 2003 Influence of microstructure and chemistry on the fracture toughness of dental ceramics Dent Mater 19 603 611 10.1016/S0109-5641(03)00002-2 1:CAS:528:DC%2BD3sXlvFymt7Y%3D 12901984
    • (2003) Dent Mater , vol.19 , pp. 603-611
    • Quinn, J.B.1    Sundar, V.2    Lloyd, I.K.3
  • 10
    • 0031099529 scopus 로고    scopus 로고
    • Machinability and brittleness of glass-ceramics
    • 10.1016/S0924-0136(96)02275-3
    • AR Boccaccini 1997 Machinability and brittleness of glass-ceramics J Mater Process Technol 65 302 304 10.1016/S0924-0136(96)02275-3
    • (1997) J Mater Process Technol , vol.65 , pp. 302-304
    • Boccaccini, A.R.1
  • 11
    • 0038206761 scopus 로고    scopus 로고
    • Ductile-mode material removal of a mica-glass-ceramic
    • 10.1111/j.1151-2916.2003.tb03418.x 1:CAS:528:DC%2BD3sXksleqtrk%3D
    • XP Ma GX Li L Shen ZH Jin 2003 Ductile-mode material removal of a mica-glass-ceramic J Am Ceram Soc 86 6 1040 1042 10.1111/j.1151-2916.2003. tb03418.x 1:CAS:528:DC%2BD3sXksleqtrk%3D
    • (2003) J Am Ceram Soc , vol.86 , Issue.6 , pp. 1040-1042
    • Ma, X.P.1    Li, G.X.2    Shen, L.3    Jin, Z.H.4
  • 12
    • 0028375917 scopus 로고
    • Making ceramics 'ductile'
    • 10.1126/science.263.5150.1114 1:CAS:528:DyaK2cXit1CktL4%3D 17831623 1994Sci.263.1114L
    • BR Lawn NP Padture H Cai F Guiberteau 1994 Making ceramics 'ductile' Science 263 1114 1116 10.1126/science.263.5150.1114 1:CAS:528:DyaK2cXit1CktL4%3D 17831623 1994Sci...263.1114L
    • (1994) Science , vol.263 , pp. 1114-1116
    • Lawn, B.R.1    Padture, N.P.2    Cai, H.3    Guiberteau, F.4
  • 13
    • 0031147628 scopus 로고    scopus 로고
    • Effect of the aspect ratio of mica crystals and crystallinity on the microhardness and machinability of mica glass-ceramics
    • 10.1016/S0924-0136(96)02817-8
    • DS Baik KS No JS Chun HY Cho 1997 Effect of the aspect ratio of mica crystals and crystallinity on the microhardness and machinability of mica glass-ceramics J Mater Process Technol 67 50 54 10.1016/S0924-0136(96)02817-8
    • (1997) J Mater Process Technol , vol.67 , pp. 50-54
    • Baik, D.S.1    No, K.S.2    Chun, J.S.3    Cho, H.Y.4
  • 14
    • 84979340076 scopus 로고
    • Machinable glass-ceramics based on tetrasilicic mica
    • 10.1111/j.1151-2916.1972.tb11337.x 1:CAS:528:DyaE38XltFOnsLs%3D
    • DG Grossman 1972 Machinable glass-ceramics based on tetrasilicic mica J Am Ceram Soc 55 9 446 449 10.1111/j.1151-2916.1972.tb11337.x 1:CAS:528:DyaE38XltFOnsLs%3D
    • (1972) J Am Ceram Soc , vol.55 , Issue.9 , pp. 446-449
    • Grossman, D.G.1
  • 15
    • 0029254292 scopus 로고
    • Scratching and grinding of a machinable glass-ceramic with weak interfaces and rising T-curve
    • 10.1111/j.1151-2916.1995.tb08831.x 1:CAS:528:DyaK2MXjvVanu78%3D
    • HK Xu S Jahanmir 1995 Scratching and grinding of a machinable glass-ceramic with weak interfaces and rising T-curve J Am Ceram Soc 78 497 500 10.1111/j.1151-2916.1995.tb08831.x 1:CAS:528:DyaK2MXjvVanu78%3D
    • (1995) J Am Ceram Soc , vol.78 , pp. 497-500
    • Xu, H.K.1    Jahanmir, S.2
  • 16
    • 0141539365 scopus 로고    scopus 로고
    • Scratch hardness and chipping of dental ceramics under different environments
    • 10.1016/S0109-5641(03)00018-6 1:CAS:528:DC%2BD3sXnsVals7o%3D 14511729
    • LA Flanders JB Quinn OC Wilson Jr IK Lloyd 2003 Scratch hardness and chipping of dental ceramics under different environments Dent Mater 19 716 724 10.1016/S0109-5641(03)00018-6 1:CAS:528:DC%2BD3sXnsVals7o%3D 14511729
    • (2003) Dent Mater , vol.19 , pp. 716-724
    • Flanders, L.A.1    Quinn, J.B.2    Wilson Jr, O.C.3    Lloyd, I.K.4
  • 17
    • 58549089486 scopus 로고    scopus 로고
    • 3-F glass-ceramic system
    • 10.1007/s10856-008-3536-9 2403532 2008AIPC.1003.61R
    • 3-F glass-ceramic system J Mater Sci: Mater Med 20 1 51 66 10.1007/s10856-008-3536-9 2403532 2008AIPC.1003...61R
    • (2008) J Mater Sci: Mater Med , vol.20 , Issue.1 , pp. 51-66
    • Roy, S.1    Basu, B.2
  • 18
    • 45849097597 scopus 로고    scopus 로고
    • 3-F glass-ceramic system
    • 10.1007/s10856-008-3440-3 1:CAS:528:DC%2BD1cXnsFaqu7s%3D
    • 3-F glass-ceramic system J Mater Sci: Mater Med 19 3123 3133 10.1007/s10856-008-3440-3 1:CAS:528:DC%2BD1cXnsFaqu7s%3D
    • (2008) J Mater Sci: Mater Med , vol.19 , pp. 3123-3133
    • Roy, S.1    Basu, B.2
  • 20
    • 0035055801 scopus 로고    scopus 로고
    • Multilayerd interface in Ti/Macor® machinable glass-ceramic joints
    • DOI 10.1016/S0921-5093(00)01804-9, PII S0921509300018049
    • A Guedes AMP Pinto M Vieira F Viana 2001 Multilayered interface in Ti:Macor® machinable glass-ceramic joints Mater Sci Eng A 301 118 124 10.1016/S0921-5093(00)01804-9 (Pubitemid 32333824)
    • (2001) Materials Science and Engineering A , vol.301 , Issue.2 , pp. 118-124
    • Guedes, A.1    Pinto, A.M.P.2    Vieira, M.3    Viana, F.4
  • 22
    • 0032647808 scopus 로고    scopus 로고
    • Evaluation of the degree of crystallization in glass-ceramics by density measurements
    • 10.1016/S0955-2219(98)00226-X 1:CAS:528:DyaK1MXisVWgtbs%3D
    • A Karamanov M Pelino 1999 Evaluation of the degree of crystallization in glass-ceramics by density measurements J Eur Ceram Soc 19 649 654 10.1016/S0955-2219(98)00226-X 1:CAS:528:DyaK1MXisVWgtbs%3D
    • (1999) J Eur Ceram Soc , vol.19 , pp. 649-654
    • Karamanov, A.1    Pelino, M.2
  • 23
    • 41349116111 scopus 로고    scopus 로고
    • Mechanical and tribological characterization of human tooth
    • 10.1016/j.matchar.2007.06.008 1:CAS:528:DC%2BD1cXkt1OmtL8%3D
    • S Roy B Basu 2008 Mechanical and tribological characterization of human tooth Mater Charact 59 747 756 10.1016/j.matchar.2007.06.008 1:CAS:528:DC%2BD1cXkt1OmtL8%3D
    • (2008) Mater Charact , vol.59 , pp. 747-756
    • Roy, S.1    Basu, B.2
  • 24
    • 0035504690 scopus 로고    scopus 로고
    • Wear behaviour of human teeth in dry and artificial saliva conditions
    • 10.1016/S0043-1648(01)00835-3
    • H Li ZR Zhou 2002 Wear behaviour of human teeth in dry and artificial saliva conditions Wear 249 980 984 10.1016/S0043-1648(01)00835-3
    • (2002) Wear , vol.249 , pp. 980-984
    • Li, H.1    Zhou, Z.R.2
  • 25
    • 0002552683 scopus 로고
    • Crystal growth in glass-forming systems-a review
    • Hench LL, Freiman FW, editors special publication 5. Columbus, OH: American Ceramic Society
    • Uhlmann DR. Crystal growth in glass-forming systems-a review. In: Hench LL, Freiman FW, editors. Advances in nucleation and crystallization in glasses, special publication 5. Columbus, OH: American Ceramic Society; 1971. pp. 91-115.
    • (1971) Advances in Nucleation and Crystallization in Glasses , pp. 91-115
    • Uhlmann, D.R.1
  • 26
    • 0030086772 scopus 로고    scopus 로고
    • Indentation stress-strain curves for quasi-ductile ceramics
    • DOI 10.1016/1359-6454(95)00204-9
    • ACF Cripps BR Lawn 1996 Indentation stress-strain curves for 'quasi-ductile' ceramics Acta Mater 44 2 519 527 10.1016/1359-6454(95)00204-9 (Pubitemid 126341875)
    • (1996) Acta Materialia , vol.44 , Issue.2 , pp. 519-527
    • Fischer-Cripps, A.C.1    Lawn, B.R.2
  • 27
    • 0031598699 scopus 로고    scopus 로고
    • Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics
    • PII S010956419800013X
    • IM Peterson S Wuttiphan BR Lawn K Chyung 1998 Role of microstructure on contact damage and strength degradation of micaceous glass-ceramic Dent Mater 14 1 80 89 10.1016/S0109-5641(98)00013-X 1:STN:280:DyaK1M7jvVWjsA%3D%3D 9972155 (Pubitemid 128419492)
    • (1998) Dental Materials , vol.14 , Issue.1 , pp. 80-89
    • Peterson, I.M.1    Wuttiphan, S.2    Lawn, B.R.3    Chyung, K.4
  • 28
    • 0001058582 scopus 로고
    • Machinable mica-based glass-ceramic
    • 10.1007/BF00543933 1:CAS:528:DyaK38XhtFWkurk%3D 1992JMatS.27.429S
    • V Saraswati S Raoot 1992 Machinable mica-based glass-ceramic J Mater Sci 27 429 432 10.1007/BF00543933 1:CAS:528:DyaK38XhtFWkurk%3D 1992JMatS..27..429S
    • (1992) J Mater Sci , vol.27 , pp. 429-432
    • Saraswati, V.1    Raoot, S.2
  • 29
    • 0037401545 scopus 로고    scopus 로고
    • The influence of lithia content on the properties of fluorphlogopite glass-ceramics. II. Microstructure hardness and machinability
    • 10.1016/S0022-3093(02)01959-2 1:CAS:528:DC%2BD3sXisFeru78%3D 2003JNCS.319.13H
    • J Henry RG Hill 2003 The influence of lithia content on the properties of fluorphlogopite glass-ceramics. II. Microstructure hardness and machinability J Non-Cryst Solids 319 13 30 10.1016/S0022-3093(02)01959-2 1:CAS:528: DC%2BD3sXisFeru78%3D 2003JNCS..319...13H
    • (2003) J Non-Cryst Solids , vol.319 , pp. 13-30
    • Henry, J.1    Hill, R.G.2
  • 30
    • 0035586827 scopus 로고    scopus 로고
    • Crystallization process and some properties of calcium mica-apatite glass-ceramics
    • DOI 10.1016/S0022-3093(01)00909-7, PII S0022309301009097
    • S Taruta K Mukoyama SS Suzuki K Kitajima N Takusagawa 2001 Crystallization process and some properties of calcium mica-apatite glass-ceramics J Non-Cryst Solids 296 201 211 10.1016/S0022-3093(01)00909-7 1:CAS:528:DC%2BD3MXptlCrtL0%3D 2001JNCS..296..201T (Pubitemid 33149477)
    • (2001) Journal of Non-Crystalline Solids , vol.296 , Issue.3 , pp. 201-211
    • Taruta, S.1    Mukoyama, K.2    Suzuki, S.S.3    Kitajima, K.4    Takusagawa, N.5
  • 31
    • 0032139481 scopus 로고    scopus 로고
    • Machinable ceramics containing rare-earth phosphates
    • 1:CAS:528:DyaK1cXlsVKns74%3D
    • JB Davis DB Marshall RM Housley PED Morgan 1998 Machinable ceramics containing rare-earth phosphates J Am Ceram Soc 81 2169 2175 1:CAS:528:DyaK1cXlsVKns74%3D
    • (1998) J Am Ceram Soc , vol.81 , pp. 2169-2175
    • Davis, J.B.1    Marshall, D.B.2    Housley, R.M.3    Morgan, P.E.D.4
  • 32
    • 0036063526 scopus 로고    scopus 로고
    • Study of some thermal and mechanical properties of magnesium aluminium silicate glass-ceramic
    • Goswami M, Sarkar A, Mirza T, Shrikhande VK, Sangeeta, Gurumurthy KR, et al. Study of some thermal and mechanical properties of magnesium aluminium silicate glass-ceramic. Ceram Int. 2002;28:585-92.
    • (2002) Ceram Int. , vol.28 , pp. 585-592
    • Goswami, M.1    Sarkar, A.2    Mirza, T.3    Shrikhande, V.K.4    Sangeeta5    Gurumurthy, K.R.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.