메뉴 건너뛰기




Volumn 256, Issue 5, 2009, Pages 1419-1425

Surface evaluation of cardiac angiographic catheters after simulated use and reprocessing

Author keywords

Cardiovascular; Catheter reuse; Diagnostic techniques; Molecular structure; Reprocessing cycle; Surface characterization

Indexed keywords

DEGRADATION; FOURIER TRANSFORM INFRARED SPECTROSCOPY; HYDROGEN BONDS; MOLECULAR STRUCTURE; PHOTODEGRADATION; SCANNING ELECTRON MICROSCOPY; SURFACE ROUGHNESS; TENSILE TESTING;

EID: 70849120079     PISSN: 01694332     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.apsusc.2009.08.102     Document Type: Article
Times cited : (8)

References (20)
  • 4
    • 33646497641 scopus 로고    scopus 로고
    • The effect of sterilization on a poly (dimetilsiloxane)/poly (hexamethylene oxide) mixed macrodiol-based polyurethane elastomer
    • Simmons A., Hyvarinen J., and Poole-Warren L. The effect of sterilization on a poly (dimetilsiloxane)/poly (hexamethylene oxide) mixed macrodiol-based polyurethane elastomer. Biomaterials 27 (2006) 4484-4497
    • (2006) Biomaterials , vol.27 , pp. 4484-4497
    • Simmons, A.1    Hyvarinen, J.2    Poole-Warren, L.3
  • 6
    • 0035897271 scopus 로고    scopus 로고
    • Hydrogen plasma treatment of poly(ethylene terephthalate) surfaces
    • Borucki V.S., Achete A.C., and Jacó W. Hydrogen plasma treatment of poly(ethylene terephthalate) surfaces. Surf. Coat. Technol. 138 (2001) 256-263
    • (2001) Surf. Coat. Technol. , vol.138 , pp. 256-263
    • Borucki, V.S.1    Achete, A.C.2    Jacó, W.3
  • 7
    • 36549067693 scopus 로고    scopus 로고
    • Photooxidation and stabilization of silanised poly(ether-urethane) hybrid systems
    • Recondo A., Berridi-Fernándes M.J., and Irusta L. Photooxidation and stabilization of silanised poly(ether-urethane) hybrid systems. Polym. Degrad. Stab. 92 (2007) 2173-2180
    • (2007) Polym. Degrad. Stab. , vol.92 , pp. 2173-2180
    • Recondo, A.1    Berridi-Fernándes, M.J.2    Irusta, L.3
  • 8
    • 4644372560 scopus 로고    scopus 로고
    • Evaluation and qualification of reprocessing modification in single-use devices in interventional cardiology
    • Tessarolo F., Ferrari P., Silva B., Motta A., Migliaresi C., and Zennaro L. Evaluation and qualification of reprocessing modification in single-use devices in interventional cardiology. Appl. Surf. Sci. 238 (2004) 341-346
    • (2004) Appl. Surf. Sci. , vol.238 , pp. 341-346
    • Tessarolo, F.1    Ferrari, P.2    Silva, B.3    Motta, A.4    Migliaresi, C.5    Zennaro, L.6
  • 9
    • 70849085544 scopus 로고    scopus 로고
    • Curr. Biofilms on central catheters: is eradication is possible?
    • Donlan R.M. Curr. Biofilms on central catheters: is eradication is possible?. Top. Microbiol. Immunol. 322 (2008) 161-163
    • (2008) Top. Microbiol. Immunol. , vol.322 , pp. 161-163
    • Donlan, R.M.1
  • 10
    • 33750034623 scopus 로고    scopus 로고
    • Efficiency in endotoxin removal by a reprocessing protocol for electrophysiology catheters based on hydrogen peroxide plasma sterilization
    • Tessarolo F., Caola I., Nollo G., Antolini R., Guarrera G.M., and Caciagli P. Efficiency in endotoxin removal by a reprocessing protocol for electrophysiology catheters based on hydrogen peroxide plasma sterilization. Int. J. Hyg. Environ. Health. 209 (2006) 557-565
    • (2006) Int. J. Hyg. Environ. Health. , vol.209 , pp. 557-565
    • Tessarolo, F.1    Caola, I.2    Nollo, G.3    Antolini, R.4    Guarrera, G.M.5    Caciagli, P.6
  • 12
    • 70849091903 scopus 로고    scopus 로고
    • 10555-1:2003, sterile, single-use intravascular catheters
    • European Committee for Standardization CEN, Brussels, Belgium
    • BS/EN/ISO, ISO 10555-1:2003, sterile, single-use intravascular catheters. Part 1. General requirements, European Committee for Standardization (CEN), Brussels, Belgium, 2003, pp. 1-10.
    • (2003) General requirements , Issue.PART 1 , pp. 1-10
    • BS, E.N.1    ISO, I.S.O.2
  • 13
    • 34547484927 scopus 로고    scopus 로고
    • Infrared microspectroscopic study of the thermo-oxidative degradation of hydroxyl-terminated polybutadiene/isophorone diisocyanate polyurethane rubber
    • Nagle D.J., Celina M., Rintoul L., and Fredericks P.M. Infrared microspectroscopic study of the thermo-oxidative degradation of hydroxyl-terminated polybutadiene/isophorone diisocyanate polyurethane rubber. Polym. Degrad. Stab. 92 (2007) 1446-1454
    • (2007) Polym. Degrad. Stab. , vol.92 , pp. 1446-1454
    • Nagle, D.J.1    Celina, M.2    Rintoul, L.3    Fredericks, P.M.4
  • 14
    • 33646337166 scopus 로고    scopus 로고
    • Degradation of pré-aged polymers exposed to simulated recycling: properties and thermal stability
    • Luziriaga S., kovárová J., and Fortelný I. Degradation of pré-aged polymers exposed to simulated recycling: properties and thermal stability. Polym. Degrad. Stab. 91 (2006) 1226-1232
    • (2006) Polym. Degrad. Stab. , vol.91 , pp. 1226-1232
    • Luziriaga, S.1    kovárová, J.2    Fortelný, I.3
  • 15
    • 54449084984 scopus 로고    scopus 로고
    • Synthesis and properties of poly (urethane-imide) interpenetrating network, membranes
    • Tsai M.H., Huang S.L., Liu S.J., Chen C.J., Chen J.P., and Chen S.H. Synthesis and properties of poly (urethane-imide) interpenetrating network, membranes. Desalination 233 (2008) 191-200
    • (2008) Desalination , vol.233 , pp. 191-200
    • Tsai, M.H.1    Huang, S.L.2    Liu, S.J.3    Chen, C.J.4    Chen, J.P.5    Chen, S.H.6
  • 16
    • 47649126380 scopus 로고    scopus 로고
    • Synthesis, characterization and biodegradation studies of poly(ester urethane)s
    • Umare S.S., and Chandure A.S. Synthesis, characterization and biodegradation studies of poly(ester urethane)s. Chem. Eng. J. 142 (2008) 65-77
    • (2008) Chem. Eng. J. , vol.142 , pp. 65-77
    • Umare, S.S.1    Chandure, A.S.2
  • 17
    • 0034579061 scopus 로고    scopus 로고
    • Plasma-based sterilization: effect on surface and bulk properties and hydrolytic stability of reprocessed polyurethane electrophysiology catheters
    • Lerouge S., Guignot C., Tabrizian M., Ferrier D., Yagoubi N., and Yahia L. Plasma-based sterilization: effect on surface and bulk properties and hydrolytic stability of reprocessed polyurethane electrophysiology catheters. J. Biomed. Mater. Res. 52 (2000) 774-782
    • (2000) J. Biomed. Mater. Res. , vol.52 , pp. 774-782
    • Lerouge, S.1    Guignot, C.2    Tabrizian, M.3    Ferrier, D.4    Yagoubi, N.5    Yahia, L.6
  • 18
    • 57449107787 scopus 로고    scopus 로고
    • Hydrolytic degradation and functional stability of a segmented shape memory poly(ester urethane)
    • Pretsch T., Jakob I., and Muler W. Hydrolytic degradation and functional stability of a segmented shape memory poly(ester urethane). Polym. Degrad. Stab. 94 (2009) 61-73
    • (2009) Polym. Degrad. Stab. , vol.94 , pp. 61-73
    • Pretsch, T.1    Jakob, I.2    Muler, W.3
  • 19
    • 40249100138 scopus 로고    scopus 로고
    • Mechanistic implications of plastic degradation
    • Singh B., and Sharma N. Mechanistic implications of plastic degradation. Polym. Degrad. Stab. 93 (2008) 561-584
    • (2008) Polym. Degrad. Stab. , vol.93 , pp. 561-584
    • Singh, B.1    Sharma, N.2
  • 20
    • 54349113045 scopus 로고    scopus 로고
    • Thermo-oxidative behavior of high-temperature PMR-15 resin and composites
    • Tandon G.P., Pochiraju K.V., and Schoeppner G.A. Thermo-oxidative behavior of high-temperature PMR-15 resin and composites. Mater. Sci. Eng. 498 (2008) 150-161
    • (2008) Mater. Sci. Eng. , vol.498 , pp. 150-161
    • Tandon, G.P.1    Pochiraju, K.V.2    Schoeppner, G.A.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.