Volumn 44, Issue 5, 2008, Pages 619-629

Influence of operation of Kh52 steel on corrosion processes in a model solution of gas condensate

Author keywords

[No Author keywords available]

Indexed keywords

ANODIC DISSOLUTIONS; CORROSION MECHANISMS; CORROSION PROCESS; CORROSION PRODUCTS; CORROSION PROPERTIES; HIGH CONCENTRATIONS; INITIAL STATE; MODEL SOLUTIONS; SERVICE DEGRADATIONS; SHIELDING ACTIONS; WORKING MEDIUMS;

EID: 67349265619     PISSN: 1068820X     EISSN: None     Source Type: Journal    
DOI: 10.1007/s11003-009-9138-y     Document Type: Article
Times cited : (50)

References (15)
  • 1
    • 49349101502 scopus 로고    scopus 로고
    • Detecting internal corrosion of natural gas transmission pipelines: Field tests of probes and systems for real-time corrosion measurement
    • Lisbon Paper 395
    • B. S. Covino, Jr., S. J. Bullard, S. D. Cramer et al., "Detecting internal corrosion of natural gas transmission pipelines: field tests of probes and systems for real-time corrosion measurement," in: Proc. of the European Corrosion Cong. "Eurocorr 2000", Lisbon (2005), Paper 395.
    • (2005) Proc. of the European Corrosion Cong. "eurocorr 2000"
    • Covino Jr. B., S.1    Bullard, S.J.2    Cramer, S.D.3
  • 2
    • 34250896098 scopus 로고    scopus 로고
    • Assessing mechanical damage in offshore pipelines - Two case studies
    • DOI 10.1016/j.engfailanal.2006.11.074, PII S1350630706002196
    • KA Macdonald A Cosham CR Alexander P Hopkins 2007 Assessing mechanical damage of offshore pipelines-two case studies Eng. Failure Anal. 14 Issue 8 1667 1679 (Pubitemid 46969913)
    • (2007) Engineering Failure Analysis , vol.14 , Issue.SPELL. ISS. , pp. 1667-1679
    • MacDonald, K.A.1    Cosham, A.2    Alexander, C.R.3    Hopkins, P.4
  • 3
    • 33846782781 scopus 로고    scopus 로고
    • Stress corrosion failure of high-pressure gas pipeline
    • DOI 10.1016/j.engfailanal.2006.11.002, PII S1350630706001506
    • F Hasan J Iqbal F Ahmed 2007 Stress corrosion failure of high-pressure pipeline Eng. Failure Anal. 14 Issue 5 801 809 (Pubitemid 46206817)
    • (2007) Engineering Failure Analysis , vol.14 , Issue.5 , pp. 801-809
    • Hasan, F.1    Iqbal, J.2    Ahmed, F.3
  • 4
    • 34247597322 scopus 로고    scopus 로고
    • Best practice for the assessment of defects in pipelines - Corrosion
    • DOI 10.1016/j.engfailanal.2006.11.035, PII S1350630706001622
    • A Cosham P Hopkins KA Macdonald 2007 Best practice for the assessment of defects in pipelines-corrosion Eng. Failure Anal. 14 Issue 7 1245 1265 (Pubitemid 46682013)
    • (2007) Engineering Failure Analysis , vol.14 , Issue.7 , pp. 1245-1265
    • Cosham, A.1    Hopkins, P.2    MacDonald, K.A.3
  • 5
    • 53549100722 scopus 로고    scopus 로고
    • Effect of in-service degradation of trunk gas pipeline steel on its "in-bulk" properties
    • G Gabetta NM Nykyforchyn E Lunarska 2008 Effect of in-service degradation of trunk gas pipeline steel on its "in-bulk" properties Fiz.-Khim. Mekh. Mater. 44 1 88 99
    • (2008) Fiz.-Khim. Mekh. Mater. , vol.44 , Issue.1 , pp. 88-99
    • Gabetta, G.1    Nykyforchyn, N.M.2    Lunarska, E.3
  • 8
    • 0029259718 scopus 로고
    • On corrosion of a pipe steel and main pipelines under different soil-climatic conditions
    • A. F. Marchenko, "On corrosion of a pipe steel and main pipelines under different soil-climatic conditions," Zashch. Met., No. 2, 161-169 (1995).
    • (1995) Zashch. Met. , Issue.2 , pp. 161-169
    • Marchenko, A.F.1
  • 9
    • 0004209522 scopus 로고
    • Newness-Butterworths London
    • L. L. Shrier (editor), Corrosion, Newness-Butterworths, London (1979).
    • (1979) Corrosion
    • Shrier, L.L.1
  • 11
    • 67349217969 scopus 로고    scopus 로고
    • Anodic hydrogenation of iron in carbonate-bicarbonate solution
    • S Hirnyi 2001 Anodic hydrogenation of iron in carbonate-bicarbonate solution Fiz.-Khim. Mekh. Mater. 37 3 103 110
    • (2001) Fiz.-Khim. Mekh. Mater. , vol.37 , Issue.3 , pp. 103-110
    • Hirnyi, S.1
  • 13
    • 0036647160 scopus 로고    scopus 로고
    • Anaerobic corrosion of carbon steel and cast iron in artificial ground waters: Part 1. Electrochemical aspects
    • NR Smart DJ Blackwood L Werme 2002 Anaerobic corrosion of carbon steel and cast iron in artificial ground waters: Part 1. Electrochemical aspects Corrosion 58 7 547 559
    • (2002) Corrosion , vol.58 , Issue.7 , pp. 547-559
    • Smart, N.R.1    Blackwood, D.J.2    Werme, L.3
  • 14
    • 0000312637 scopus 로고    scopus 로고
    • Effect of Solution Composition and Electrochemical Potential on Stress Corrosion Cracking of X-52 Pipeline Steel
    • RB Rebak Z Xia R Safruddin Z Szklarska-Smialowska 1996 Effect of solution composition and electrochemical potential in stress corrosion cracking of Kh-52 pipeline steel Corrosion 52 5 396 405 (Pubitemid 126451528)
    • (1996) Corrosion , vol.52 , Issue.5 , pp. 396-405
    • Rebak, R.B.1    Xia, Z.2    Safruddin, R.3    Szklarska-Smialowska, Z.4
  • 15
    • 32344442141 scopus 로고
    • Corrosion of low-carbon steel in sodium chloride solutions and in fresh water
    • Kaliningrad State University Kaliningrad. in Russian
    • M. E. Volkova, I. V. Gimbitskaya, and Yu. A. Vorotnikov, "Corrosion of low-carbon steel in sodium chloride solutions and in fresh water," in: Corrosion and Protection of Metals [in Russian], Issue 4, Kaliningrad State University, Kaliningrad, (1978), pp. 3-8.
    • (1978) Corrosion and Protection of Metals, Issue 4 , pp. 3-8
    • Volkova, M.E.1    Gimbitskaya, I.V.2    Vorotnikov Yu, A.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.