Volumn 30, Issue 8, 2009, Pages 3225-3228

Evaluating the bond strength of opaque material on porcelain fused to metal restorations (PFM) alloys by scratch test method

Author keywords

[No Author keywords available]

Indexed keywords

BOND STRENGTH; CRITICAL FORCE; LAYER THICKNESS; OPAQUE MATERIALS; PORCELAIN-FUSED-TO-METAL RESTORATION; SCRATCH TEST; SCRATCH TEST METHOD; SURFACE PROFILOMETER;

EID: 67349227744     PISSN: 02641275     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.matdes.2008.12.018     Document Type: Article
Times cited : (19)

References (32)
  • 1
    • 33845421930 scopus 로고    scopus 로고
    • Effect of esthetic core shades on the final color of IPS empress all-ceramic crowns
    • Azer S.S., Ayash G.M., Johnston W.M., Khalil M.F., and Rosenstiel S.F. Effect of esthetic core shades on the final color of IPS empress all-ceramic crowns. J Prosthet Dent 96 (2006) 397-401
    • (2006) J Prosthet Dent , vol.96 , pp. 397-401
    • Azer, S.S.1    Ayash, G.M.2    Johnston, W.M.3    Khalil, M.F.4    Rosenstiel, S.F.5
  • 3
    • 0032201224 scopus 로고    scopus 로고
    • Effect of beryllium on the castability and resistance of ceramometal bonds in nickel-chromium alloys
    • Bezzon O.L., de Mattos Mda G., Ribeiro R.F., and Rollo J.M. Effect of beryllium on the castability and resistance of ceramometal bonds in nickel-chromium alloys. J Prosthet Dent 80 (1998) 570-574
    • (1998) J Prosthet Dent , vol.80 , pp. 570-574
    • Bezzon, O.L.1    de Mattos Mda, G.2    Ribeiro, R.F.3    Rollo, J.M.4
  • 5
    • 0014297307 scopus 로고
    • Chemico-physical analysis and mechanical tests of the ceramo-metallic complex
    • Nally J.N. Chemico-physical analysis and mechanical tests of the ceramo-metallic complex. Int Dent J 18 (1968) 309-325
    • (1968) Int Dent J , vol.18 , pp. 309-325
    • Nally, J.N.1
  • 7
    • 0017531563 scopus 로고
    • Bonding mechanism evidence in a ceramic nonprecious alloy system
    • Anusavice K.J., Ringle R.D., and Fairhurst C.W. Bonding mechanism evidence in a ceramic nonprecious alloy system. J Biomed Mater Res 11 (1977) 701-709
    • (1977) J Biomed Mater Res , vol.11 , pp. 701-709
    • Anusavice, K.J.1    Ringle, R.D.2    Fairhurst, C.W.3
  • 8
    • 0017751935 scopus 로고
    • Adherence controlling elements in ceramicmetal systems II. Nonprecious alloys
    • Anusavice K.J., Ringle R.D., and Fairhurst C.W. Adherence controlling elements in ceramicmetal systems II. Nonprecious alloys. J Dent Res 56 (1977) 1053-1061
    • (1977) J Dent Res , vol.56 , pp. 1053-1061
    • Anusavice, K.J.1    Ringle, R.D.2    Fairhurst, C.W.3
  • 9
    • 11144224810 scopus 로고    scopus 로고
    • Shear bond strengths of a ceramic system to alternative metal alloys
    • Melo R.M., Travassos A.C., and Neisser M.P. Shear bond strengths of a ceramic system to alternative metal alloys. J Prosthet Dent 93 (2005) 64-69
    • (2005) J Prosthet Dent , vol.93 , pp. 64-69
    • Melo, R.M.1    Travassos, A.C.2    Neisser, M.P.3
  • 10
    • 37649025800 scopus 로고    scopus 로고
    • Evaluation of the shear bond strength of the union between two Co-Cr alloys and a dental ceramic
    • Pretti M., Hilgert E., Bottino M.A., and Avelar R.P. Evaluation of the shear bond strength of the union between two Co-Cr alloys and a dental ceramic. J Appl Oral Sci 12 (2004) 280-284
    • (2004) J Appl Oral Sci , vol.12 , pp. 280-284
    • Pretti, M.1    Hilgert, E.2    Bottino, M.A.3    Avelar, R.P.4
  • 11
    • 0022807872 scopus 로고
    • Effect of four pretreatment techniques on porcelain-to-metal bond strength
    • Daftary F., and Donovan T. Effect of four pretreatment techniques on porcelain-to-metal bond strength. J Prosthet Dent 56 (1986) 535-539
    • (1986) J Prosthet Dent , vol.56 , pp. 535-539
    • Daftary, F.1    Donovan, T.2
  • 12
    • 0023173607 scopus 로고
    • Bonding of dental porcelain to ceramic-metal alloys
    • Uusalo E.K., Lassila V.P., and Yli-Urpo A.U. Bonding of dental porcelain to ceramic-metal alloys. J Prosthet Dent 57 (1987) 26-29
    • (1987) J Prosthet Dent , vol.57 , pp. 26-29
    • Uusalo, E.K.1    Lassila, V.P.2    Yli-Urpo, A.U.3
  • 13
    • 0035292632 scopus 로고    scopus 로고
    • Castability and resistance of ceramometal bonding in Ni-Cr and Ni-Cr-Be alloys
    • Bezzon O.L., Ribeiro R.F., Rollo J.M., and Crosara S. Castability and resistance of ceramometal bonding in Ni-Cr and Ni-Cr-Be alloys. J Prosthet Dent 85 (2001) 299-304
    • (2001) J Prosthet Dent , vol.85 , pp. 299-304
    • Bezzon, O.L.1    Ribeiro, R.F.2    Rollo, J.M.3    Crosara, S.4
  • 14
    • 0017749852 scopus 로고
    • The chemical nature of dental porcelain
    • Lacy A.M. The chemical nature of dental porcelain. Dent Clin North Am 21 (1977) 661-667
    • (1977) Dent Clin North Am , vol.21 , pp. 661-667
    • Lacy, A.M.1
  • 15
    • 0034277695 scopus 로고    scopus 로고
    • Influence of metal finishing on porcelain porosity and beam failure loads at the metal-ceramic interface
    • Hofstede T.M., Ercoli C., Graser G.N., Tallents R.H., Moss M.E., and Zero D.T. Influence of metal finishing on porcelain porosity and beam failure loads at the metal-ceramic interface. J Prosthet Dent 84 (2000) 309-317
    • (2000) J Prosthet Dent , vol.84 , pp. 309-317
    • Hofstede, T.M.1    Ercoli, C.2    Graser, G.N.3    Tallents, R.H.4    Moss, M.E.5    Zero, D.T.6
  • 16
    • 0033087402 scopus 로고    scopus 로고
    • Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain
    • Yilmaz H., and Dincer C. Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain. J Dent 27 (1999) 215-222
    • (1999) J Dent , vol.27 , pp. 215-222
    • Yilmaz, H.1    Dincer, C.2
  • 17
    • 0037364451 scopus 로고    scopus 로고
    • Fracture reasons in ceramicfused-to-metal restorations
    • Ozcan M. Fracture reasons in ceramicfused-to-metal restorations. J Oral Rehabil 30 (2003) 265-269
    • (2003) J Oral Rehabil , vol.30 , pp. 265-269
    • Ozcan, M.1
  • 18
    • 0025103078 scopus 로고
    • Metal ceramic compatibility: a review of the literature
    • Bagby M., Marshall S.J., and Marshall Jr. G.W. Metal ceramic compatibility: a review of the literature. J Prosthet Dent 63 (1990) 21-25
    • (1990) J Prosthet Dent , vol.63 , pp. 21-25
    • Bagby, M.1    Marshall, S.J.2    Marshall Jr., G.W.3
  • 20
    • 0028457320 scopus 로고
    • Adhesion promotion between metadent and a high palladium alloy with a pyrolytically fused porcelain opaque layer
    • Van Putten M.C., and Culbertson B.M. Adhesion promotion between metadent and a high palladium alloy with a pyrolytically fused porcelain opaque layer. J Prosthod 3 (1994) 79-87
    • (1994) J Prosthod , vol.3 , pp. 79-87
    • Van Putten, M.C.1    Culbertson, B.M.2
  • 24
    • 33644848880 scopus 로고    scopus 로고
    • Surface analyses of porcelain fused to metal systems
    • Johnson T., van Noort R., and Stokes C.V. Surface analyses of porcelain fused to metal systems. Dent Mater 22 (2006) 330-337
    • (2006) Dent Mater , vol.22 , pp. 330-337
    • Johnson, T.1    van Noort, R.2    Stokes, C.V.3
  • 25
    • 0017726960 scopus 로고
    • Adherence controlling elements in ceramic-metal systems. I. Precious alloys
    • Anusavice K.J., Horner J.A., and Fairhurst C.W. Adherence controlling elements in ceramic-metal systems. I. Precious alloys. J Dent Res 56 (1977) 1045-1052
    • (1977) J Dent Res , vol.56 , pp. 1045-1052
    • Anusavice, K.J.1    Horner, J.A.2    Fairhurst, C.W.3
  • 26
    • 27844436626 scopus 로고    scopus 로고
    • An ASTM standart for quantitative scratch adhesion testing of thin, hard ceramic coatings
    • Gonczy S.T., and Randall N. An ASTM standart for quantitative scratch adhesion testing of thin, hard ceramic coatings. Int J Appl Ceram Technol 2 (2005) 422-428
    • (2005) Int J Appl Ceram Technol , vol.2 , pp. 422-428
    • Gonczy, S.T.1    Randall, N.2
  • 27
    • 33646410093 scopus 로고    scopus 로고
    • Effect of the microstructure of Si3N4 on the adhesion strength of TiN film on Si3N4
    • Kim Y.G., Tatami J., Komeya K., and Kim D.K. Effect of the microstructure of Si3N4 on the adhesion strength of TiN film on Si3N4. Thin Solid Films 510 (2006) 222-228
    • (2006) Thin Solid Films , vol.510 , pp. 222-228
    • Kim, Y.G.1    Tatami, J.2    Komeya, K.3    Kim, D.K.4
  • 28
    • 31344479876 scopus 로고    scopus 로고
    • Comparison of bond strength of a pressed ceramic fused to metal versus feldspathic porcelain fused to metal
    • Schweitze D.M., Goldstein G.R., Ricci J.L., Silva N.R.F.A., and Hittelman E.L. Comparison of bond strength of a pressed ceramic fused to metal versus feldspathic porcelain fused to metal. J Prosthod 14 (2005) 239-247
    • (2005) J Prosthod , vol.14 , pp. 239-247
    • Schweitze, D.M.1    Goldstein, G.R.2    Ricci, J.L.3    Silva, N.R.F.A.4    Hittelman, E.L.5
  • 29
    • 0035227549 scopus 로고    scopus 로고
    • Effect of soldering on metal-porcelain bond strength in repaired porcelain fused-to-metal castings
    • Galindo D.F., Ercoli C., Graser N.G., Tallents R.H., and Moss M.E. Effect of soldering on metal-porcelain bond strength in repaired porcelain fused-to-metal castings. J Prosthet Dent 85 (2001) 88-94
    • (2001) J Prosthet Dent , vol.85 , pp. 88-94
    • Galindo, D.F.1    Ercoli, C.2    Graser, N.G.3    Tallents, R.H.4    Moss, M.E.5
  • 30
    • 0035220559 scopus 로고    scopus 로고
    • Evolution of dental ceramics in the twentieth century
    • McLean J.W. Evolution of dental ceramics in the twentieth century. J Prosthet Dent 85 (2001) 61-66
    • (2001) J Prosthet Dent , vol.85 , pp. 61-66
    • McLean, J.W.1
  • 31
    • 14844341823 scopus 로고    scopus 로고
    • Effect of chemical composition of Ni-Cr dental casting alloys on the bonding characterization between porcelain and metal
    • Huang H.H., Lin M.C., Lee T.H., Yang H.W., Chen F.L., Wu S.C., and Hsu C.C. Effect of chemical composition of Ni-Cr dental casting alloys on the bonding characterization between porcelain and metal. J Oral Rehabil 32 (2005) 206-212
    • (2005) J Oral Rehabil , vol.32 , pp. 206-212
    • Huang, H.H.1    Lin, M.C.2    Lee, T.H.3    Yang, H.W.4    Chen, F.L.5    Wu, S.C.6    Hsu, C.C.7
  • 32
    • 0032065619 scopus 로고    scopus 로고
    • Effects of dental laboratory processing variables and in vitro testing medium on the porcelain adherence of high-palladium casting alloys
    • Papazoglou E., Brantley W.A., Johnston W.M., and Carr A.B. Effects of dental laboratory processing variables and in vitro testing medium on the porcelain adherence of high-palladium casting alloys. J Prosthet Dent 79 (1998) 514-519
    • (1998) J Prosthet Dent , vol.79 , pp. 514-519
    • Papazoglou, E.1    Brantley, W.A.2    Johnston, W.M.3    Carr, A.B.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.