메뉴 건너뛰기




Volumn 79, Issue 5, 1998, Pages 514-519

Effects of dental laboratory processing variables and in vitro testing medium on the porcelain adherence of high-palladium casting alloys

Author keywords

[No Author keywords available]

Indexed keywords

ALLOY; DENTAL ALLOY; GOLD ALLOY; PALLADIUM; SALIVA SUBSTITUTE; WATER;

EID: 0032065619     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0022-3913(98)70171-4     Document Type: Article
Times cited : (29)

References (44)
  • 2
    • 0344850931 scopus 로고
    • Oxide formation on palladium alloys and its effects on porcelain adherence
    • [Abstract No. 722]
    • Cascone PJ. Oxide formation on palladium alloys and its effects on porcelain adherence. [Abstract No. 722]. J Dent Res 62 (1983) 255
    • (1983) J Dent Res , vol.62 , pp. 255
    • Cascone, PJ.1
  • 3
    • 0021962098 scopus 로고
    • The structure and oxidation of two palladium ceramic fusing alloys
    • Suoninen E., and Herø H. The structure and oxidation of two palladium ceramic fusing alloys. Biomaterials 6 (1985) 133-137
    • (1985) Biomaterials , vol.6 , pp. 133-137
    • Suoninen, E.1    Herø, H.2
  • 4
    • 0022072232 scopus 로고
    • Carbon impurities and properties of some palladium alloys for ceramic veneering
    • Herø H., and Syverud M. Carbon impurities and properties of some palladium alloys for ceramic veneering. Dent Mater 1 (1985) 106-110
    • (1985) Dent Mater , vol.1 , pp. 106-110
    • Herø, H.1    Syverud, M.2
  • 5
    • 0023357125 scopus 로고
    • A new dental Pd-Co alloy for ceramic veneering
    • Syverud M., Kvam K., and Herø H. A new dental Pd-Co alloy for ceramic veneering. Dent Mater 3 (1987) 102-106
    • (1987) Dent Mater , vol.3 , pp. 102-106
    • Syverud, M.1    Kvam, K.2    Herø, H.3
  • 6
    • 0023393033 scopus 로고
    • Gold-based bonding agents between palladium- alloys and ceramic veneer
    • Herø H., and Austrheim E. Gold-based bonding agents between palladium- alloys and ceramic veneer. Dent Mater 3 (1987) 168-175
    • (1987) Dent Mater , vol.3 , pp. 168-175
    • Herø, H.1    Austrheim, E.2
  • 10
    • 0028402743 scopus 로고
    • Bond characteristics of porcelain fused to milled titanium
    • Gilbert J.L., Covey D.A., and Lautenschlager EP. Bond characteristics of porcelain fused to milled titanium. Dent Mater 10 (1994) 134-140
    • (1994) Dent Mater , vol.10 , pp. 134-140
    • Gilbert, J.L.1    Covey, D.A.2    Lautenschlager, EP.3
  • 11
    • 0029181886 scopus 로고
    • Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy
    • Pang I.C., Gilbert J.L., Chai J., and Lautenschlager EP. Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy. J Prosthet Dent 73 (1995) 17-25
    • (1995) J Prosthet Dent , vol.73 , pp. 17-25
    • Pang, I.C.1    Gilbert, J.L.2    Chai, J.3    Lautenschlager, EP.4
  • 12
    • 0030119324 scopus 로고    scopus 로고
    • Castability, opaque masking, and porcelain bonding of 17 porcelain-fused-to-metal alloys
    • O'Connor R.P., Mackert Jr. J.R., Myers M.L., and Parry E.E. Castability, opaque masking, and porcelain bonding of 17 porcelain-fused-to-metal alloys. J Prosthet Dent 75 (1996) 367-374
    • (1996) J Prosthet Dent , vol.75 , pp. 367-374
    • O'Connor, R.P.1    Mackert Jr., J.R.2    Myers, M.L.3    Parry, E.E.4
  • 14
    • 0026150304 scopus 로고
    • New high-palladium casting alloys: 1. Overview and initial studies
    • Carr A.B., and Brantley WA. New high-palladium casting alloys: 1. Overview and initial studies. Int J Prosthodont 4 (1991) 265-275
    • (1991) Int J Prosthodont , vol.4 , pp. 265-275
    • Carr, A.B.1    Brantley, WA.2
  • 17
    • 0023969674 scopus 로고
    • Carbon absorption of palladium-enriched ceramic alloys
    • van der Zel J.M., and Vrijhoef MM. Carbon absorption of palladium-enriched ceramic alloys. J Oral Rehab 15 (1988) 163-166
    • (1988) J Oral Rehab , vol.15 , pp. 163-166
    • van der Zel, J.M.1    Vrijhoef, MM.2
  • 20
    • 0020804570 scopus 로고
    • An x-ray spectrometric technique for measuring porcelain-metal adherence
    • Ringle R.D., Mackert Jr. J.R., and Fairhurst CW. An x-ray spectrometric technique for measuring porcelain-metal adherence. J Dent Res 62 (1983) 933-936
    • (1983) J Dent Res , vol.62 , pp. 933-936
    • Ringle, R.D.1    Mackert Jr., J.R.2    Fairhurst, CW.3
  • 23
    • 84944661914 scopus 로고
    • Rank transformation as a bridge between parametric and nonparametric statistics
    • Conover W.J., and Iman RL. Rank transformation as a bridge between parametric and nonparametric statistics. Am Stat 35 (1981) 124-129
    • (1981) Am Stat , vol.35 , pp. 124-129
    • Conover, W.J.1    Iman, RL.2
  • 24
    • 0029337408 scopus 로고
    • Mechanical property and microstructural variations for recast low-gold alloy
    • Reisbick M.H., and Brantley WA. Mechanical property and microstructural variations for recast low-gold alloy. Int J Prosthodont 8 (1995) 346-350
    • (1995) Int J Prosthodont , vol.8 , pp. 346-350
    • Reisbick, M.H.1    Brantley, WA.2
  • 27
    • 0022706547 scopus 로고
    • The effect of using recast metal on the bond between porcelain and a gold-palladium alloy
    • Rasmussen S.T., and Doukoudakis AA. The effect of using recast metal on the bond between porcelain and a gold-palladium alloy. J Prosthet Dent 55 (1986) 447-453
    • (1986) J Prosthet Dent , vol.55 , pp. 447-453
    • Rasmussen, S.T.1    Doukoudakis, AA.2
  • 28
  • 29
    • 0023986996 scopus 로고
    • The effect of recasting on the oxidation layer of a palladium-silver porcelain alloy
    • Hong J., Razoog M.E., and Lang BR. The effect of recasting on the oxidation layer of a palladium-silver porcelain alloy. J Prosthet Dent 59 (1988) 420-425
    • (1988) J Prosthet Dent , vol.59 , pp. 420-425
    • Hong, J.1    Razoog, M.E.2    Lang, BR.3
  • 31
    • 0001958444 scopus 로고
    • Role of "adherence oxides" in the development of chemical bonding at the glass-metal interfaces
    • Borom M.P., and Pask J.A. Role of "adherence oxides" in the development of chemical bonding at the glass-metal interfaces. J Am Ceram Soc 49 (1966) 1-6
    • (1966) J Am Ceram Soc , vol.49 , pp. 1-6
    • Borom, M.P.1    Pask, J.A.2
  • 32
    • 0005768970 scopus 로고
    • The theory of bonding for porcelain-to-metal systems
    • Yamade H.N., and Grenoble P.B. (Eds), University of Southern California School of Dentistry, Los Angeles
    • Cascone P.J. The theory of bonding for porcelain-to-metal systems. In: Yamade H.N., and Grenoble P.B. (Eds). Dental porcelain: the state of the art-1977 (1977), University of Southern California School of Dentistry, Los Angeles 109-117
    • (1977) Dental porcelain: the state of the art-1977 , pp. 109-117
    • Cascone, P.J.1
  • 35
    • 0345993999 scopus 로고
    • Fracture toughness of metal-to-ceramic joints as a function of environment
    • Hastings G.W., and Williams D.F. (Eds), John Wiley, New York
    • Elssner G., Barisch W.F., and Pabst R. Fracture toughness of metal-to-ceramic joints as a function of environment. In: Hastings G.W., and Williams D.F. (Eds). Mechanical properties of biomaterials. (1980), John Wiley, New York 265-274
    • (1980) Mechanical properties of biomaterials. , pp. 265-274
    • Elssner, G.1    Barisch, W.F.2    Pabst, R.3
  • 36
    • 0026458869 scopus 로고
    • The effect of corrosive environment on the porcelain-to-metal bond-a fracture mechanics investigation
    • Herrmann M., Rottenegger R., Tinschert J., and Marx R. The effect of corrosive environment on the porcelain-to-metal bond-a fracture mechanics investigation. Dent Mater 8 (1992) 2-6
    • (1992) Dent Mater , vol.8 , pp. 2-6
    • Herrmann, M.1    Rottenegger, R.2    Tinschert, J.3    Marx, R.4
  • 37
    • 0027693235 scopus 로고
    • Fracture toughness of high alumina core dental ceramics: the effect of water and artificial saliva
    • Mante F.K., Brantley W.A., Dhuru V.B., and Ziebert GJ. Fracture toughness of high alumina core dental ceramics: the effect of water and artificial saliva. Int J Prosthodont 6 (1993) 546-552
    • (1993) Int J Prosthodont , vol.6 , pp. 546-552
    • Mante, F.K.1    Brantley, W.A.2    Dhuru, V.B.3    Ziebert, GJ.4
  • 41
    • 0347885513 scopus 로고    scopus 로고
    • Proposed ISO "bond strength" test: residual stress and fracture behavior analysis
    • [Abstract no. 3085.]
    • Kelly J.R., Myers M.L., and DeHoff P.H. Proposed ISO "bond strength" test: residual stress and fracture behavior analysis. [Abstract no. 3085.]. J Dent Res 79 (1997) 399
    • (1997) J Dent Res , vol.79 , pp. 399
    • Kelly, J.R.1    Myers, M.L.2    DeHoff, P.H.3
  • 43
    • 0024710875 scopus 로고
    • Effect of visco-elastic behavior on stress development in a metal-ceramic system
    • DeHoff P.H., and Anusavice KJ. Effect of visco-elastic behavior on stress development in a metal-ceramic system. J Dent Res 68 (1989) 1223-1230
    • (1989) J Dent Res , vol.68 , pp. 1223-1230
    • DeHoff, P.H.1    Anusavice, KJ.2
  • 44
    • 0025378845 scopus 로고
    • Transient and residual stress in a porcelain-metal strip
    • Asaoka K., and Tesk JA. Transient and residual stress in a porcelain-metal strip. J Dent Res 69 (1990) 463-469
    • (1990) J Dent Res , vol.69 , pp. 463-469
    • Asaoka, K.1    Tesk, JA.2