Volumn 27, Issue 2, 2009, Pages 137-151

Ageing of HDPE geomembrane exposed to air, water and leachate at different temperatures

Author keywords

Durability; Geomembranes; Landfills; Liners; Service life; Temperature

Indexed keywords

DURABILITY; FORECASTING; GEOMEMBRANES; GRANULAR MATERIALS; LAND FILL; LANDFILL LININGS; LEACHATE TREATMENT; LEACHING; MECHANICAL PROPERTIES; POLYMER MATRIX COMPOSITES; REFUSE DISPOSAL; SERVICE LIFE; SURFACE CHEMISTRY; WATER ANALYSIS;

EID: 60449093510     PISSN: 02661144     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.geotexmem.2008.09.007     Document Type: Article
Times cited : (179)

References (64)
  • 1
    • 50049085782 scopus 로고    scopus 로고
    • An investigation into the use of blends of two bentonites for geosynthetic clay liners
    • Andrejkovicova S., Rocha F., Janotka I., and Komadel P. An investigation into the use of blends of two bentonites for geosynthetic clay liners. Geotextiles and Geomembranes 26 5 (2008) 236-445
    • (2008) Geotextiles and Geomembranes , vol.26 , Issue.5 , pp. 236-445
    • Andrejkovicova, S.1    Rocha, F.2    Janotka, I.3    Komadel, P.4
  • 2
    • 4344615994 scopus 로고    scopus 로고
    • Standard test method for evaluation of stress crack resistance of polyolefin geomembranes using notched constant tensile load test
    • ASTM D5397
    • ASTM D5397. Standard test method for evaluation of stress crack resistance of polyolefin geomembranes using notched constant tensile load test, Annual Book of ASTM Standards. vol. 04.13.
    • Annual Book of ASTM Standards , vol.4 .13
  • 3
    • 60449093282 scopus 로고    scopus 로고
    • Standard test method for tensile properties of plastics
    • ASTM D638
    • ASTM D638. Standard test method for tensile properties of plastics, Annual Book of Standards, vol. 8.01.
    • Annual Book of Standards, vol , vol.8 .01
  • 4
    • 60449102789 scopus 로고    scopus 로고
    • Terminology Relating to Plastics
    • ASTM D883
    • ASTM D883. Terminology Relating to Plastics, Annual Book of ASTM Standards, vol. 8.01.
    • Annual Book of ASTM Standards, vol , vol.8 .01
  • 5
    • 48249149862 scopus 로고    scopus 로고
    • Standard test method for flow rates of thermoplastics by extrusion plastometer
    • ASTM D1238
    • ASTM D1238. Standard test method for flow rates of thermoplastics by extrusion plastometer, Annual Book of ASTM Standards. vol. 08.01.
    • Annual Book of ASTM Standards , vol.8 .01
  • 6
    • 60449114925 scopus 로고    scopus 로고
    • ASTM D3895. Standard test method for oxidative-induction time of polyolefins by differential scanning calorimetry Annual Book of ASTM Standards. 08.02.
    • ASTM D3895. Standard test method for oxidative-induction time of polyolefins by differential scanning calorimetry Annual Book of ASTM Standards. vol. 08.02.
  • 7
    • 4344615994 scopus 로고    scopus 로고
    • Standard test method for determining tensile properties of nonreinforced polyethylene and nonreinforced flexible polypropylene geomembranes
    • ASTM D6693
    • ASTM D6693. Standard test method for determining tensile properties of nonreinforced polyethylene and nonreinforced flexible polypropylene geomembranes, Annual Book of Standards, vol. 04.13.
    • Annual Book of Standards, vol , vol.4 .13
  • 8
    • 4344615994 scopus 로고    scopus 로고
    • Standard test method for melting and crystallization temperatures by thermal analysis
    • ASTM E794
    • ASTM E794. Standard test method for melting and crystallization temperatures by thermal analysis, Annual Book of ASTM Standards. vol. 14.02.
    • Annual Book of ASTM Standards , vol.14 .02
  • 9
    • 60449095041 scopus 로고    scopus 로고
    • August H., Tatzky-Gerth R., Preuschmann R., Jakob I., 1992. Permeationsverhalten von kombinationsdichtungen bei deponien und altasten gegenüber wassergefährdenden stiffen. Umweltforschungsplan des Bundesministers für Umwelt, Naturshutz und Reaktorsichercheit, F + EVorhaben 102 03 412, Durchgeführt an der Bundesanstalt für Materialforschung und-prüfung (BAM) im Auftrag des Umweltbundesamtes.
    • August H., Tatzky-Gerth R., Preuschmann R., Jakob I., 1992. Permeationsverhalten von kombinationsdichtungen bei deponien und altasten gegenüber wassergefährdenden stiffen. Umweltforschungsplan des Bundesministers für Umwelt, Naturshutz und Reaktorsichercheit, F + EVorhaben 102 03 412, Durchgeführt an der Bundesanstalt für Materialforschung und-prüfung (BAM) im Auftrag des Umweltbundesamtes.
  • 10
    • 39749118634 scopus 로고    scopus 로고
    • Analytical modelling of gas leakage rate through a geosynthetic clay liner-geomembrane composite liner due to a circular defect in the geomembrane
    • Bouazza A., Vangpaisal T., Abuel-Naga H., and Kodikara J. Analytical modelling of gas leakage rate through a geosynthetic clay liner-geomembrane composite liner due to a circular defect in the geomembrane. Geotextiles and Geomembranes 26 2 (2008) 122-129
    • (2008) Geotextiles and Geomembranes , vol.26 , Issue.2 , pp. 122-129
    • Bouazza, A.1    Vangpaisal, T.2    Abuel-Naga, H.3    Kodikara, J.4
  • 11
    • 55749108701 scopus 로고    scopus 로고
    • Gravel contacts and geomembrane strains for a GM/CCL composite liner
    • Brachman R.W.I., and Gudina S. Gravel contacts and geomembrane strains for a GM/CCL composite liner. Geotextiles and Geomembranes 26 6 (2008) 448-459
    • (2008) Geotextiles and Geomembranes , vol.26 , Issue.6 , pp. 448-459
    • Brachman, R.W.I.1    Gudina, S.2
  • 12
    • 55749112161 scopus 로고    scopus 로고
    • Geomembrane strains from coarse gravel and wrinkles in a GM/GCL composite liner
    • Brachman R.W.I., and Gudina S. Geomembrane strains from coarse gravel and wrinkles in a GM/GCL composite liner. Geotextiles and Geomembranes 26 6 (2008) 488-497
    • (2008) Geotextiles and Geomembranes , vol.26 , Issue.6 , pp. 488-497
    • Brachman, R.W.I.1    Gudina, S.2
  • 13
    • 77955611516 scopus 로고    scopus 로고
    • Development of an Apparatus to Simulate the Ageing of Geomembranes Under Chemical Exposure, Elevated Temperatures and Applied Stresses
    • Cancun, Mexico, March. pp
    • Brachman, R.W.I., Rowe, R.K., Arnepalli, D.N., Dickinson, S., Islam, M.Z., Sabir, A., 2008. Development of an Apparatus to Simulate the Ageing of Geomembranes Under Chemical Exposure, Elevated Temperatures and Applied Stresses. In: GeoAmericas 2008, Cancun, Mexico, March. pp. 444-451.
    • (2008) GeoAmericas 2008 , pp. 444-451
    • Brachman, R.W.I.1    Rowe, R.K.2    Arnepalli, D.N.3    Dickinson, S.4    Islam, M.Z.5    Sabir, A.6
  • 14
    • 0032304697 scopus 로고    scopus 로고
    • Influence of various stabilizer systems on the ageing behavior of PE-ME-I. Hot water ageing compression molding plaques
    • Dörner G., and Lang R.W. Influence of various stabilizer systems on the ageing behavior of PE-ME-I. Hot water ageing compression molding plaques. Polymer Degradation and Stability 62 (1998) 421-430
    • (1998) Polymer Degradation and Stability , vol.62 , pp. 421-430
    • Dörner, G.1    Lang, R.W.2
  • 15
    • 0042274282 scopus 로고
    • Controlling thermal damage in flexible membrane liners
    • Fisher G.E. Controlling thermal damage in flexible membrane liners. Geotechnical Fabrics Report 7 2 (1989) 39-41
    • (1989) Geotechnical Fabrics Report , vol.7 , Issue.2 , pp. 39-41
    • Fisher, G.E.1
  • 16
    • 33947481982 scopus 로고
    • Melting points of linear-chain homologs. The normal paraffin hydrocarbons
    • Flory P.J., and Vrij A. Melting points of linear-chain homologs. The normal paraffin hydrocarbons. Journal of the American Chemical Society 85 (1963) 3548-3553
    • (1963) Journal of the American Chemical Society , vol.85 , pp. 3548-3553
    • Flory, P.J.1    Vrij, A.2
  • 17
    • 34250795185 scopus 로고
    • Batch extraction with reaction: phenolic antioxidant migration from polyolefins to water. 2. Experimental results and discussion
    • Gandek T.P., Hatton T.A., and Reid R.C. Batch extraction with reaction: phenolic antioxidant migration from polyolefins to water. 2. Experimental results and discussion. Industrial and Engineering Chemistry Research 28 (1989) 1036-1045
    • (1989) Industrial and Engineering Chemistry Research , vol.28 , pp. 1036-1045
    • Gandek, T.P.1    Hatton, T.A.2    Reid, R.C.3
  • 20
    • 23844450985 scopus 로고    scopus 로고
    • Effect of acidic mine drainage on the polymer properties of an HDPE geomembrane
    • Gulec S.B., Edil T.B., and Benson C.H. Effect of acidic mine drainage on the polymer properties of an HDPE geomembrane. Geosynthetics International 11 2 (2004) 60-72
    • (2004) Geosynthetics International , vol.11 , Issue.2 , pp. 60-72
    • Gulec, S.B.1    Edil, T.B.2    Benson, C.H.3
  • 21
    • 0037150398 scopus 로고    scopus 로고
    • Loss and transformation products of the aromatic antioxidants in MDPE film under long-term exposure to biotic and abiotic conditions
    • Haider N., and Karlsson S. Loss and transformation products of the aromatic antioxidants in MDPE film under long-term exposure to biotic and abiotic conditions. Journal of Applied Polymer Science 85 (2002) 974-988
    • (2002) Journal of Applied Polymer Science , vol.85 , pp. 974-988
    • Haider, N.1    Karlsson, S.2
  • 23
    • 0002247870 scopus 로고    scopus 로고
    • Antioxidant depletion during thermal oxidation of high density polyethylene geomembrane
    • Industrial Fabrics Association International, St. Paul, MN, USA
    • Hsuan Y.G., and Guan Z. Antioxidant depletion during thermal oxidation of high density polyethylene geomembrane. Proceedings of the Sixth International Conference on Geosynthetics, Atlanta, March (1998), Industrial Fabrics Association International, St. Paul, MN, USA 375-380
    • (1998) Proceedings of the Sixth International Conference on Geosynthetics, Atlanta, March , pp. 375-380
    • Hsuan, Y.G.1    Guan, Z.2
  • 24
    • 0034143566 scopus 로고    scopus 로고
    • Database of field incidents used to establish HDPE Geomembrane stress crack resistance specifications
    • Hsuan Y.G. Database of field incidents used to establish HDPE Geomembrane stress crack resistance specifications. Geotextiles and Geomembranes 18 (2000) 1-22
    • (2000) Geotextiles and Geomembranes , vol.18 , pp. 1-22
    • Hsuan, Y.G.1
  • 26
    • 32044464426 scopus 로고
    • Long term durability of HDPE geomembrane: part i - depletion of antioxidant
    • Hsuan Y.G., and Koerner R.M. Long term durability of HDPE geomembrane: part i - depletion of antioxidant. GRI Report 16 (1995) 35
    • (1995) GRI Report , vol.16 , pp. 35
    • Hsuan, Y.G.1    Koerner, R.M.2
  • 27
    • 0013680049 scopus 로고
    • The single point-notched constant tension load test: a quality control test for assessing stress crack resistance
    • Hsuan Y.G., and Koerner R.M. The single point-notched constant tension load test: a quality control test for assessing stress crack resistance. Geosynthetics International 2 5 (1995) 831-843
    • (1995) Geosynthetics International , vol.2 , Issue.5 , pp. 831-843
    • Hsuan, Y.G.1    Koerner, R.M.2
  • 29
    • 68049114103 scopus 로고    scopus 로고
    • Effect of geomembrane ageing on the diffusion of VOCs through HDPE geomembranes
    • Cancun, Mexico, March. pp
    • Islam, M.Z., Rowe, R.K., 2008a. Effect of geomembrane ageing on the diffusion of VOCs through HDPE geomembranes. In: GeoAmericas 2008, Cancun, Mexico, March. pp. 459-467.
    • (2008) GeoAmericas , pp. 459-467
    • Islam, M.Z.1    Rowe, R.K.2
  • 30
    • 60449103245 scopus 로고    scopus 로고
    • Permeation of BTEX through unaged and aged HDPE geomembranes
    • Queen's University
    • Islam, M.Z., Rowe, R.K., 2008b. Permeation of BTEX through unaged and aged HDPE geomembranes. Queen's University Research report.
    • (2008) Research report
    • Islam, M.Z.1    Rowe, R.K.2
  • 31
    • 30944445580 scopus 로고    scopus 로고
    • Long term temperature monitoring of geomembranes at dry and wet landfills
    • Koerner G.R., and Koerner R.M. Long term temperature monitoring of geomembranes at dry and wet landfills. Geotextiles and Geomembranes 24 1 (2006) 72-77
    • (2006) Geotextiles and Geomembranes , vol.24 , Issue.1 , pp. 72-77
    • Koerner, G.R.1    Koerner, R.M.2
  • 32
    • 0037052525 scopus 로고    scopus 로고
    • The measurement of the crystallinity of polymers by DSC
    • Kong Y., and Hay J.N. The measurement of the crystallinity of polymers by DSC. Polymer 43 (2002) 3873-3878
    • (2002) Polymer , vol.43 , pp. 3873-3878
    • Kong, Y.1    Hay, J.N.2
  • 33
    • 0000826506 scopus 로고
    • Physical loss of stabilizers from polymers
    • Scott G. (Ed), Applied Science Publishers Ltd, London Chapter 5
    • Luston J. Physical loss of stabilizers from polymers. In: Scott G. (Ed). Development in Polymer Stabilization-2 (1986), Applied Science Publishers Ltd, London 185-240 Chapter 5
    • (1986) Development in Polymer Stabilization-2 , pp. 185-240
    • Luston, J.1
  • 34
    • 60449094503 scopus 로고    scopus 로고
    • MoE, 1998. Landfill standards: a guideline on the regulatory and approval requirements for the new or expanding landfilling sites, Ontario Ministry of the Environment, Ontario Regulation 232/98, Queen's Printer for Ontario, Toronto.
    • MoE, 1998. Landfill standards: a guideline on the regulatory and approval requirements for the new or expanding landfilling sites, Ontario Ministry of the Environment, Ontario Regulation 232/98, Queen's Printer for Ontario, Toronto.
  • 36
    • 0037210457 scopus 로고    scopus 로고
    • Oxidative resistance of high-density polyethylene geomembranes
    • Müller W., and Jakob I. Oxidative resistance of high-density polyethylene geomembranes. Polymer Degradation and Stability 79 (2003) 161-172
    • (2003) Polymer Degradation and Stability , vol.79 , pp. 161-172
    • Müller, W.1    Jakob, I.2
  • 39
    • 0009766711 scopus 로고
    • Photo-induced degradation of polymers
    • Hamid A.H., Amin M.B., and Maadah A.G. (Eds), Marcel Dekker Inc., New York
    • Osawa Z. Photo-induced degradation of polymers. In: Hamid A.H., Amin M.B., and Maadah A.G. (Eds). Handbook of Polymer Degradation (1992), Marcel Dekker Inc., New York 169-217
    • (1992) Handbook of Polymer Degradation , pp. 169-217
    • Osawa, Z.1
  • 40
    • 2142857694 scopus 로고
    • Catalytic action of metal salts in autoxidation and polymerization (x) - the effect of various methyl stearates on the thermal oxidation of 2,6,10,14-tetramethylpentadecane
    • Osawa Z., and Ishizuka T. Catalytic action of metal salts in autoxidation and polymerization (x) - the effect of various methyl stearates on the thermal oxidation of 2,6,10,14-tetramethylpentadecane. Journal of Applied Polymer Science 17 (1973) 2897-2907
    • (1973) Journal of Applied Polymer Science , vol.17 , pp. 2897-2907
    • Osawa, Z.1    Ishizuka, T.2
  • 41
    • 0012255785 scopus 로고
    • The effects of transition metal compounds on the thermal oxidative degradation of polypropylene in solution
    • American Chemical Society, Washington, D.C. 2897-2907
    • Osawa Z., and Saito T. The effects of transition metal compounds on the thermal oxidative degradation of polypropylene in solution. Stabilisation and Degradation of Polymers. Advances in Chemistry, Series 169 (1978), American Chemical Society, Washington, D.C. 2897-2907
    • (1978) Stabilisation and Degradation of Polymers. Advances in Chemistry, Series 169
    • Osawa, Z.1    Saito, T.2
  • 43
    • 0002849992 scopus 로고
    • Stress cracking of polyethylene geomembrane seams: field experience
    • Koerner R.M. (Ed), Elsevier Science Publishers Ltd, London, England
    • Peggs I.D., and Carlson D.S. Stress cracking of polyethylene geomembrane seams: field experience. In: Koerner R.M. (Ed). Durability and Aging of Geosynthetics (1989), Elsevier Science Publishers Ltd, London, England 195-211
    • (1989) Durability and Aging of Geosynthetics , pp. 195-211
    • Peggs, I.D.1    Carlson, D.S.2
  • 46
    • 32144443341 scopus 로고    scopus 로고
    • Long-term performance of contaminant barrier systems
    • Rowe R.K. Long-term performance of contaminant barrier systems. Geotechnique 55 9 (2005) 631-678
    • (2005) Geotechnique , vol.55 , Issue.9 , pp. 631-678
    • Rowe, R.K.1
  • 47
    • 60449101656 scopus 로고    scopus 로고
    • Ageing and long-term performance of geomembrane liners
    • Cancun, Mexico, March. pp
    • Rowe, R.K., Rimal, S., 2008a. Ageing and long-term performance of geomembrane liners. In: GeoAmericas 2008, Cancun, Mexico, March. pp. 425-434.
    • (2008) GeoAmericas , pp. 425-434
    • Rowe, R.K.1    Rimal, S.2
  • 50
    • 44249103533 scopus 로고    scopus 로고
    • Leachate chemical composition effects on OIT depletion in an HDPE geomembranes
    • Rowe R.K., Islam M.Z., and Hsuan Y.G. Leachate chemical composition effects on OIT depletion in an HDPE geomembranes. Geosynthetics International 15 2 (2008) 136-157
    • (2008) Geosynthetics International , vol.15 , Issue.2 , pp. 136-157
    • Rowe, R.K.1    Islam, M.Z.2    Hsuan, Y.G.3
  • 52
    • 39849099278 scopus 로고    scopus 로고
    • Numerical modelling of advective flow through composite liners in case of two interacting adjacent square defects in the geomembrane
    • Saidi F., Touze-Foltz N., and Goblet P. Numerical modelling of advective flow through composite liners in case of two interacting adjacent square defects in the geomembrane. Geotextiles and Geomembranes 26 2 (2008) 196-204
    • (2008) Geotextiles and Geomembranes , vol.26 , Issue.2 , pp. 196-204
    • Saidi, F.1    Touze-Foltz, N.2    Goblet, P.3
  • 53
    • 0003788948 scopus 로고    scopus 로고
    • Ph.D. thesis, Department of Civil and Environmental Engineering. The University of Western Ontario, Ontario, Canada, 400pp
    • Sangam, H.P., 2001. Performance of HDPE geomembrane liners in landfill applications. Ph.D. thesis, Department of Civil and Environmental Engineering. The University of Western Ontario, Ontario, Canada, 400pp.
    • (2001) Performance of HDPE geomembrane liners in landfill applications
    • Sangam, H.P.1
  • 54
    • 0036027004 scopus 로고    scopus 로고
    • Effects of exposure conditions on the depletion of antioxidants from high-density polyethylene (HDPE) geomembranes
    • Sangam H.P., and Rowe R.K. Effects of exposure conditions on the depletion of antioxidants from high-density polyethylene (HDPE) geomembranes. Canadian Geotechnical Journal 39 (2002) 1221-1230
    • (2002) Canadian Geotechnical Journal , vol.39 , pp. 1221-1230
    • Sangam, H.P.1    Rowe, R.K.2
  • 56
    • 37549065324 scopus 로고    scopus 로고
    • Characterization and identification of plastics
    • Kutz M. (Ed), John Wiley and Sons, New York
    • Shah V. Characterization and identification of plastics. In: Kutz M. (Ed). Handbook of Materials Selection (2002), John Wiley and Sons, New York 591-614
    • (2002) Handbook of Materials Selection , pp. 591-614
    • Shah, V.1
  • 57
    • 0022679250 scopus 로고
    • Melt flow index: more than just a quality control rheological parameter. Part I
    • Shenoy A.V., and Saini D.R. Melt flow index: more than just a quality control rheological parameter. Part I. Advances in Polymer Technology 6 1 (1986) 1-58
    • (1986) Advances in Polymer Technology , vol.6 , Issue.1 , pp. 1-58
    • Shenoy, A.V.1    Saini, D.R.2
  • 58
    • 84989029849 scopus 로고
    • Modeling of antioxidant loss from polyolefins in hot-water applications. I: model and application to medium density polyethylene pipes
    • Smith G.D., Karlsson K., and Gedde U.W. Modeling of antioxidant loss from polyolefins in hot-water applications. I: model and application to medium density polyethylene pipes. Polymer Engineering and Science 32 10 (1992) 658-667
    • (1992) Polymer Engineering and Science , vol.32 , Issue.10 , pp. 658-667
    • Smith, G.D.1    Karlsson, K.2    Gedde, U.W.3
  • 60
    • 34548462201 scopus 로고    scopus 로고
    • Quantifying geomembrane wrinkles using aerial photography and digital image processing
    • Take W.A., Chappel M.J., Brachman R.W.I., and Rowe R.K. Quantifying geomembrane wrinkles using aerial photography and digital image processing. Geosynthetics International 14 4 (2007) 219-227
    • (2007) Geosynthetics International , vol.14 , Issue.4 , pp. 219-227
    • Take, W.A.1    Chappel, M.J.2    Brachman, R.W.I.3    Rowe, R.K.4
  • 61
    • 0028497922 scopus 로고
    • Degradation of unstabilized medium-density polyethylene pipes in hot-water applications
    • Viebke J., Elble E., Ifwarson M., and Gedde U.W. Degradation of unstabilized medium-density polyethylene pipes in hot-water applications. Polymer Engineering and Science 34 17 (1994) 1354-1361
    • (1994) Polymer Engineering and Science , vol.34 , Issue.17 , pp. 1354-1361
    • Viebke, J.1    Elble, E.2    Ifwarson, M.3    Gedde, U.W.4
  • 62
    • 36649007008 scopus 로고    scopus 로고
    • The influence of bentonites extrusion on shear strength of GCL/geomembrane interface
    • Vukelić A., Szavits-Nossan A., and Kvasnička P. The influence of bentonites extrusion on shear strength of GCL/geomembrane interface. Geotextiles and Geomembranes 26 1 (2008) 82-90
    • (2008) Geotextiles and Geomembranes , vol.26 , Issue.1 , pp. 82-90
    • Vukelić, A.1    Szavits-Nossan, A.2    Kvasnička, P.3
  • 63
    • 0141516493 scopus 로고
    • Evaluation of the Life expectancy of polypropylene geotextiles used in bottom protection structures around the Ooster Schelde storm surge barrier: a case study
    • Proceedings of the fourth International Conference on Geotextiles The Hague, Netherlands
    • Wisse J.D.M., Broos C.J.M., and Boels W.H. Evaluation of the Life expectancy of polypropylene geotextiles used in bottom protection structures around the Ooster Schelde storm surge barrier: a case study. Proceedings of the fourth International Conference on Geotextiles. Geomembranes and Related Products vol. 2 (1990) 697-702 The Hague, Netherlands
    • (1990) Geomembranes and Related Products , vol.2 , pp. 697-702
    • Wisse, J.D.M.1    Broos, C.J.M.2    Boels, W.H.3
  • 64
    • 60449105068 scopus 로고
    • The durability and aging of geogrids
    • Koerner R.M. (Ed), Elsevier, New York
    • Wrigley N.E. The durability and aging of geogrids. In: Koerner R.M. (Ed). Durability and Aging of Geosynthetics (1989), Elsevier, New York 110-134
    • (1989) Durability and Aging of Geosynthetics , pp. 110-134
    • Wrigley, N.E.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.