메뉴 건너뛰기




Volumn 35, Issue 3, 2009, Pages 1129-1132

Oxidation behavior of polymer derived SiCO powders

Author keywords

A: Precursors: organic; C: Corrosion; D: SiC; Oxidation mechanism

Indexed keywords

ACTIVATION ENERGY; CERAMIC MATERIALS; CORROSION; GRAVIMETRIC ANALYSIS; POLYSILANES; POWDERS; SILANES; SILICA; SILICON CARBIDE; THERMOGRAVIMETRIC ANALYSIS;

EID: 59349114301     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ceramint.2008.05.006     Document Type: Article
Times cited : (23)

References (24)
  • 1
    • 85047673403 scopus 로고
    • Sialons and related nitrogen ceramics
    • Jack H. Sialons and related nitrogen ceramics. J. Mater. Sci. 11 (1976) 1135-1138
    • (1976) J. Mater. Sci. , vol.11 , pp. 1135-1138
    • Jack, H.1
  • 2
    • 0000819681 scopus 로고    scopus 로고
    • Newtonian viscosity of amorphous silicon carbonitride at high temperature
    • An L., Riedel R., Konetachny C., Kleebe H., and Raj R. Newtonian viscosity of amorphous silicon carbonitride at high temperature. J. Am. Ceram. Soc. 81 (1998) 1349-1352
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 1349-1352
    • An, L.1    Riedel, R.2    Konetachny, C.3    Kleebe, H.4    Raj, R.5
  • 3
    • 0032302150 scopus 로고    scopus 로고
    • Amorphous silicoboron carbonitride ceramics with anomalously high resistance to creep
    • Riedel R., Ruwisch L., An L., and Raj R. Amorphous silicoboron carbonitride ceramics with anomalously high resistance to creep. J. Am. Ceram. Soc. 81 (1998) 3341-3344
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 3341-3344
    • Riedel, R.1    Ruwisch, L.2    An, L.3    Raj, R.4
  • 5
    • 0026626324 scopus 로고
    • Silicon carbonitride derived from an organometallic precursor: influence of the microstructure on the oxidation behavior
    • Bahloul D., Pereira M., and Goursat P. Silicon carbonitride derived from an organometallic precursor: influence of the microstructure on the oxidation behavior. Ceram. Int. 18 (1992) 1-9
    • (1992) Ceram. Int. , vol.18 , pp. 1-9
    • Bahloul, D.1    Pereira, M.2    Goursat, P.3
  • 6
    • 0029637640 scopus 로고
    • A covalent micro/nano composite resistant to high temperature oxidation
    • Riedel R., Kleebe H., Schonfelder H., and Aldinger F. A covalent micro/nano composite resistant to high temperature oxidation. Nature 374 (1995) 526-528
    • (1995) Nature , vol.374 , pp. 526-528
    • Riedel, R.1    Kleebe, H.2    Schonfelder, H.3    Aldinger, F.4
  • 8
    • 33744817596 scopus 로고    scopus 로고
    • Polymer-derived SiAlCN ceramics resist oxidation at 1400 °C
    • Wang Y., Fan Y., Zhang L., Zhang W., and An L. Polymer-derived SiAlCN ceramics resist oxidation at 1400 °C. Scripta Mater. 55 (2006) 295-297
    • (2006) Scripta Mater. , vol.55 , pp. 295-297
    • Wang, Y.1    Fan, Y.2    Zhang, L.3    Zhang, W.4    An, L.5
  • 10
    • 33644786858 scopus 로고    scopus 로고
    • Oxidation/corrosion of polymer-derived SiAlCN ceramics in water vapor
    • Wang Y., Fei W., and An L. Oxidation/corrosion of polymer-derived SiAlCN ceramics in water vapor. J. Am. Ceram. Soc. 89 (2006) 1079-1082
    • (2006) J. Am. Ceram. Soc. , vol.89 , pp. 1079-1082
    • Wang, Y.1    Fei, W.2    An, L.3
  • 11
    • 33747517879 scopus 로고    scopus 로고
    • Silicoaluminum carbonitride ceramic resist to oxidation/corrosion in water vapor
    • Wang Y., Fei W., Fan Y., Zhang L., Zhang W., and An L. Silicoaluminum carbonitride ceramic resist to oxidation/corrosion in water vapor. J. Mater. Res. 21 (2006) 1625-1628
    • (2006) J. Mater. Res. , vol.21 , pp. 1625-1628
    • Wang, Y.1    Fei, W.2    Fan, Y.3    Zhang, L.4    Zhang, W.5    An, L.6
  • 12
    • 0027282886 scopus 로고
    • Corrosion of silicon-based ceramics in combustion environments
    • Jacobson N. Corrosion of silicon-based ceramics in combustion environments. J. Am. Ceram. Soc. 76 (1993) 3-20
    • (1993) J. Am. Ceram. Soc. , vol.76 , pp. 3-20
    • Jacobson, N.1
  • 13
    • 0026102267 scopus 로고
    • Oxygen tracer diffusion in vitreous silica
    • Kalen J., Boyce R., and Cawley J. Oxygen tracer diffusion in vitreous silica. J. Am. Ceram. Soc. 74 (1991) 203-209
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 203-209
    • Kalen, J.1    Boyce, R.2    Cawley, J.3
  • 15
    • 0021481862 scopus 로고
    • Isotope labeling studies of the oxidation of silicon at 1000 °C and 1300 °C
    • Costello J., and Tressler R. Isotope labeling studies of the oxidation of silicon at 1000 °C and 1300 °C. J. Electrochem. Soc. 131 (1984) 1944-1947
    • (1984) J. Electrochem. Soc. , vol.131 , pp. 1944-1947
    • Costello, J.1    Tressler, R.2
  • 16
    • 0023401674 scopus 로고
    • Oxygen-18 tracer study of the passive thermal oxidation of silicon
    • Cawley J., Halloran J., and Cooper A. Oxygen-18 tracer study of the passive thermal oxidation of silicon. Oxid. Met. 28 (1987) 1-16
    • (1987) Oxid. Met. , vol.28 , pp. 1-16
    • Cawley, J.1    Halloran, J.2    Cooper, A.3
  • 17
    • 0035526631 scopus 로고    scopus 로고
    • Oxygen transport in silica at high temperatures: implications of oxidation kinetics
    • Ramberg C., and Worrell W. Oxygen transport in silica at high temperatures: implications of oxidation kinetics. J. Am. Ceram. Soc. 84 (2001) 2607-2616
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 2607-2616
    • Ramberg, C.1    Worrell, W.2
  • 18
    • 84987344259 scopus 로고
    • Oxidation of silicon carbide crystals and ceramics. I. In dry oxygen
    • Costello J., and Tressler R. Oxidation of silicon carbide crystals and ceramics. I. In dry oxygen. J. Am. Ceram. Soc. 69 (1986) 674-681
    • (1986) J. Am. Ceram. Soc. , vol.69 , pp. 674-681
    • Costello, J.1    Tressler, R.2
  • 20
    • 43249117093 scopus 로고    scopus 로고
    • Polymer-ceramic conversion of liquid polycarbosilane for SiC-based ceramics
    • Li H., Zhang L., Cheng L., Wang Y., Yu Z., Huang M., Tu H., and Xia H. Polymer-ceramic conversion of liquid polycarbosilane for SiC-based ceramics. J. Mater. Sci. 43 (2008) 2806-2811
    • (2008) J. Mater. Sci. , vol.43 , pp. 2806-2811
    • Li, H.1    Zhang, L.2    Cheng, L.3    Wang, Y.4    Yu, Z.5    Huang, M.6    Tu, H.7    Xia, H.8
  • 21
    • 0035437640 scopus 로고    scopus 로고
    • Oxidation kinetics of an amorphous silicon carbonitride ceramic
    • Raj R., An L., Shah S., Riedel R., Fasel C., and Kleebe H. Oxidation kinetics of an amorphous silicon carbonitride ceramic. J. Am. Ceram. Soc. 84 (2001) 1803-1810
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 1803-1810
    • Raj, R.1    An, L.2    Shah, S.3    Riedel, R.4    Fasel, C.5    Kleebe, H.6
  • 22
    • 0346294509 scopus 로고
    • Oxidation mechanism of porous silicon nitride
    • Porz F., and Thummler F. Oxidation mechanism of porous silicon nitride. J. Mater. Sci. 19 (1984) 1283-1295
    • (1984) J. Mater. Sci. , vol.19 , pp. 1283-1295
    • Porz, F.1    Thummler, F.2
  • 23
    • 0023329856 scopus 로고
    • Calculations of parabolic rate constants
    • Pierragi B. Calculations of parabolic rate constants. Oxid. Met. 27 (1987) 177-185
    • (1987) Oxid. Met. , vol.27 , pp. 177-185
    • Pierragi, B.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.