1
-
-
0010331876
-
Production technology for nanocrystalline WC-Co powders
-
Wu B L, Shao G Q, Duan X L, et al. Production technology for nanocrystalline WC-Co powders[J]. Materials Review, 2000, 14(7): 55-58.
-
(2000)
Materials Review
, vol.14
, Issue.7
, pp. 55-58
-
-
Wu, B.L.1
Shao, G.Q.2
Duan, X.L.3
-
2
-
-
58149213264
-
Sintering characteristics of nanophase WC-Co composite powders
-
Zhang L, Huang B Y, Wu E X. Sintering characteristics of nanophase WC-Co composite powders[J]. Cemented Carbide, 2001, 18(2): 65-68.
-
(2001)
Cemented Carbide
, vol.18
, Issue.2
, pp. 65-68
-
-
Zhang, L.1
Huang, B.Y.2
Wu, E.X.3
-
3
-
-
0010331746
-
Development of WC materials with ultrafine grain size
-
Shao G Q, Wu B L, Wei M K, et al. Development of WC materials with ultrafine grain size[J]. Journal of Wuhan University of Technology, 1999, 21(6): 18-20.
-
(1999)
Journal of Wuhan University of Technology
, vol.21
, Issue.6
, pp. 18-20
-
-
Shao, G.Q.1
Wu, B.L.2
Wei, M.K.3
-
4
-
-
20544448000
-
Progress in nanostructured tungsten carbides
-
Zhang F L, Zhu M, Wang C Y. Progress in nanostructured tungsten carbides[J]. Chinese Journal of Rare Metals, 2002, 26(1): 54-58.
-
(2002)
Chinese Journal of Rare Metals
, vol.26
, Issue.1
, pp. 54-58
-
-
Zhang, F.L.1
Zhu, M.2
Wang, C.Y.3
-
5
-
-
58149266981
-
Production technology for nanophase WC-Co powders
-
Wang Z T, Chen H H. Production technology for nanophase WC-Co powders[J]. Yunnan Metallurgy, 2005, 34: 37-40.
-
(2005)
Yunnan Metallurgy
, vol.34
, pp. 37-40
-
-
Wang, Z.T.1
Chen, H.H.2
-
6
-
-
0032869666
-
Grooving wear of single-crystal tungsten carbide
-
Engpvist H, Ederyd S, Axen N, et al. Grooving wear of single-crystal tungsten carbide[J]. Wear, 1999, 230(2): 165-174.
-
(1999)
Wear
, vol.230
, Issue.2
, pp. 165-174
-
-
Engpvist, H.1
Ederyd, S.2
Axen, N.3
-
7
-
-
10644293685
-
Microscale abrasion-corrosion behaviour of WC-Co hardmetals and HVOF sprayed coatings
-
Shipway P H, Howell L. Microscale abrasion-corrosion behaviour of WC-Co hardmetals and HVOF sprayed coatings[J]. Wear, 2005, 258: 303-312.
-
(2005)
Wear
, vol.258
, pp. 303-312
-
-
Shipway, P.H.1
Howell, L.2
-
8
-
-
3042814429
-
Friction and wear behavior of cemented carbides
-
Pirso J, Letunovits S, Viljus M. Friction and wear behavior of cemented carbides[J]. Wear, 2004, 257: 257-265.
-
(2004)
Wear
, vol.257
, pp. 257-265
-
-
Pirso, J.1
Letunovits, S.2
Viljus, M.3
-
9
-
-
0037312047
-
Experimental study on the precision grinding of nanostructured ceramic coatings
-
Deng Z H, Zhang B, Sun Z Y. Experimental study on the precision grinding of nanostructured ceramic coatings[J]. Diamond and Abrasives Engineering, 2003, 1: 12-17.
-
(2003)
Diamond and Abrasives Engineering
, vol.1
, pp. 12-17
-
-
Deng, Z.H.1
Zhang, B.2
Sun, Z.Y.3
-
10
-
-
0018105794
-
Influence of work material on grinding forces
-
Werner G. Influence of work material on grinding forces[J]. Annals of the CIRP, 1978, 27: 243-248.
-
(1978)
Annals of the CIRP
, vol.27
, pp. 243-248
-
-
Werner, G.1
-
12
-
-
0004059140
-
Grinding technology: Theory and applications of machining with abrasives
-
New York: Society of Manufacturing Engineers
-
Malkin S. Grinding Technology: Theory and Applications of Machining with Abrasives[R]. New York: Society of Manufacturing Engineers, 1996.
-
(1996)
-
-
Malkin, S.1
-
14
-
-
0030212751
-
Analysis and simulation of the grinding process(Part II): Mechanics of grinding
-
Chen X, Rowe W B. Analysis and simulation of the grinding process(Part II): Mechanics of grinding[J]. International Journal of Machine Tools and Manufacture, 1996, 36(8): 883-896.
-
(1996)
International Journal of Machine Tools and Manufacture
, vol.36
, Issue.8
, pp. 883-896
-
-
Chen, X.1
Rowe, W.B.2
-
15
-
-
0029233416
-
Subsurface evaluation of ground ceramics
-
Zhang B, Howes T D. Subsurface evaluation of ground ceramics[J]. Annals of the CIRP, 1995, 44: 44-49.
-
(1995)
Annals of the CIRP
, vol.44
, pp. 44-49
-
-
Zhang, B.1
Howes, T.D.2
-
16
-
-
0027962274
-
Effect of grit depth of cut on strength of ground ceramics
-
Mayer J E Jr, Fang G P. Effect of grit depth of cut on strength of ground ceramics[J]. Annals of the CIRP, 1994, 43: 309-312.
-
(1994)
Annals of the CIRP
, vol.43
, pp. 309-312
-
-
Mayer, Jr.J.E.1
Fang, G.P.2
-
17
-
-
0003749418
-
-
2nd ed. London: Cambridge University Press
-
Lawn B R. Fracture of Brittle Solids[M]. 2nd ed. London: Cambridge University Press, 1993.
-
(1993)
Fracture of Brittle Solids
-
-
Lawn, B.R.1
-
18
-
-
0017555307
-
A model for crack initiation in elastic/plastic: Indentation fields
-
Lawn B R, Evans A G. A model for crack initiation in elastic/plastic: Indentation fields[J]. Journal of Material Science, 1977, 12(11): 2195-2199.
-
(1977)
Journal of Material Science
, vol.12
, Issue.11
, pp. 2195-2199
-
-
Lawn, B.R.1
Evans, A.G.2
-
19
-
-
84979434138
-
Hardness, toughness, and brittleness: An indentation analysis
-
Lawn B R, Marshall D B. Hardness, toughness, and brittleness: An indentation analysis[J]. Journal of American Ceramic Social, 1979, 62: 347-350.
-
(1979)
Journal of American Ceramic Social
, vol.62
, pp. 347-350
-
-
Lawn, B.R.1
Marshall, D.B.2
-
20
-
-
3142586814
-
Research on the grinding force when machining nanostructured WC/12Co coating
-
Cao J P, Deng Z H, Liu J, et al. Research on the grinding force when machining nanostructured WC/12Co coating[J]. Diamond and Abrasives Engineering, 2004, 2: 5-9.
-
(2004)
Diamond and Abrasives Engineering
, vol.2
, pp. 5-9
-
-
Cao, J.P.1
Deng, Z.H.2
Liu, J.3
-
21
-
-
0035280281
-
Grinding of WC-Co hardmetals
-
Hegeman J B J W, De Hosson J Th M. Grinding of WC-Co hardmetals[J]. Wear, 2001, 248: 187-196.
-
(2001)
Wear
, vol.248
, pp. 187-196
-
-
Hegeman, J.B.J.W.1
de Hosson, J.Th.M.2
|