메뉴 건너뛰기




Volumn 258, Issue 1-4 SPEC. ISS., 2005, Pages 303-312

Microscale abrasion - Corrosion behaviour of WC-Co hardmetals and HVOF sprayed coatings

Author keywords

Cermet; Synergy; Thermal spraying; Tungsten carbide; Wear

Indexed keywords

ABRASION; COATINGS; COBALT; MICROSTRUCTURE; PARTICLE SIZE ANALYSIS; SINTERING; SPRAYING; WEAR RESISTANCE;

EID: 10644293685     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.wear.2004.04.003     Document Type: Conference Paper
Times cited : (72)

References (33)
  • 1
    • 0016876948 scopus 로고
    • Wear characteristics of metals
    • T.S. Eyre, Wear characteristics of metals, Tribol. Int. 10 (1976) 203-212.
    • (1976) Tribol. Int. , vol.10 , pp. 203-212
    • Eyre, T.S.1
  • 2
    • 0018454697 scopus 로고
    • Abrasion of WC-Co alloys with quartz
    • J. Larsen-Basse, E.T. Koyanagi, Abrasion of WC-Co alloys with quartz, Trans. ASME 101 (1979) 208-211.
    • (1979) Trans. ASME , vol.101 , pp. 208-211
    • Larsen-Basse, J.1    Koyanagi, E.T.2
  • 3
    • 0025004801 scopus 로고
    • Abrasion and erosion of WC-Co with controlled microstructures
    • S.F. Wayne, J.G. Baldoni, S.T. Buljan, Abrasion and erosion of WC-Co with controlled microstructures, Tribol. Trans. 33 (1990) 611-617.
    • (1990) Tribol. Trans. , vol.33 , pp. 611-617
    • Wayne, S.F.1    Baldoni, J.G.2    Buljan, S.T.3
  • 4
    • 0037174653 scopus 로고    scopus 로고
    • 2 coatings using powder produced by self propagating high temperature synthesis: Microstructure and abrasive wear behaviour
    • 2 coatings using powder produced by self propagating high temperature synthesis: microstructure and abrasive wear behaviour, Mater. Sci. Eng. A336 (2002) 88-98.
    • (2002) Mater. Sci. Eng. , vol.A336 , pp. 88-98
    • Horlock, A.J.1    McCartney, D.G.2    Shipway, P.H.3    Wood, J.V.4
  • 5
    • 0034696063 scopus 로고    scopus 로고
    • Influence of coating microstructure on the abrasive wear resistance of WC/Co cermet coatings
    • H. Liao, B. Normand, C. Coddet, Influence of coating microstructure on the abrasive wear resistance of WC/Co cermet coatings, Surf. Coat. Tech. 124 (2000) 235-242.
    • (2000) Surf. Coat. Tech. , vol.124 , pp. 235-242
    • Liao, H.1    Normand, B.2    Coddet, C.3
  • 6
    • 0028992413 scopus 로고
    • Combined erosion and corrosion of thermal sprayed WC and CrC coatings
    • M. Bjordal, E. Bardal, T. Rogne, T.R. Eggen, Combined erosion and corrosion of thermal sprayed WC and CrC coatings, Surf. Coat. Tech. 70 (1995) 215-220.
    • (1995) Surf. Coat. Tech. , vol.70 , pp. 215-220
    • Bjordal, M.1    Bardal, E.2    Rogne, T.3    Eggen, T.R.4
  • 10
    • 0031100324 scopus 로고    scopus 로고
    • Theory and application of a micro-scale abrasive wear test
    • K.L. Rutherford, I.M. Hutchings, Theory and application of a micro-scale abrasive wear test, J. Test. Evaluat. 25 (1997) 250-260.
    • (1997) J. Test. Evaluat. , vol.25 , pp. 250-260
    • Rutherford, K.L.1    Hutchings, I.M.2
  • 12
    • 0030811459 scopus 로고    scopus 로고
    • An empirical ranking of a wide range of WC-Co Grades in terms of their abrasion resistance measured by the ASTM standard B611-85 test
    • D.G.F. O'Quigley, S. Luyckx, M.N. James, An empirical ranking of a wide range of WC-Co Grades in terms of their abrasion resistance measured by the ASTM standard B611-85 test, Int. J. Refract. Metals Hard Mater. 14 (1997) 73-79.
    • (1997) Int. J. Refract. Metals Hard Mater. , vol.14 , pp. 73-79
    • O'Quigley, D.G.F.1    Luyckx, S.2    James, M.N.3
  • 13
    • 0036776723 scopus 로고    scopus 로고
    • The role of lubrication in abrasion of materials in aqueous environments
    • P.H. Shipway, S. Wirojanupatump, The role of lubrication in abrasion of materials in aqueous environments, Tribol. Int. 35 (2002) 661-667.
    • (2002) Tribol. Int. , vol.35 , pp. 661-667
    • Shipway, P.H.1    Wirojanupatump, S.2
  • 14
    • 0030785269 scopus 로고    scopus 로고
    • The erosion-corrosion resistance of tungsten-carbide hard metals
    • E.J. Wentzel, C. Allen, The erosion-corrosion resistance of tungsten-carbide hard metals, Int. J. Refract. Metals Hard Mater. 15 (1997) 81-87.
    • (1997) Int. J. Refract. Metals Hard Mater. , vol.15 , pp. 81-87
    • Wentzel, E.J.1    Allen, C.2
  • 15
    • 0029254403 scopus 로고
    • Erosion-corrosion resistance of tungsten carbide hard metals with different binder compositions
    • E.J. Wentzel, C. Alien, Erosion-corrosion resistance of tungsten carbide hard metals with different binder compositions, Wear 181-183 (1995) 63-69.
    • (1995) Wear , vol.181-183 , pp. 63-69
    • Wentzel, E.J.1    Alien, C.2
  • 17
    • 0030733743 scopus 로고    scopus 로고
    • The relationship between electrochemical behaviour and in-service corrosion of WC based cemented carbides
    • A.M. Human, H.E. Exner, The relationship between electrochemical behaviour and in-service corrosion of WC based cemented carbides, Int. J. Refract. Metals Hard Mater. 15 (1997) 65-71.
    • (1997) Int. J. Refract. Metals Hard Mater. , vol.15 , pp. 65-71
    • Human, A.M.1    Exner, H.E.2
  • 18
    • 0345534766 scopus 로고    scopus 로고
    • Corrosion behaviour of cermet coatings in artificial seawater
    • A. Collazo, X.R. Nóvoa, C. Pérez, Corrosion behaviour of cermet coatings in artificial seawater, Electrochim Acta 44 (1999) 4289-4296.
    • (1999) Electrochim Acta , vol.44 , pp. 4289-4296
    • Collazo, A.1    Nóvoa, X.R.2    Pérez, C.3
  • 19
    • 0033490378 scopus 로고    scopus 로고
    • Abrasive wear behaviour of conventional and nanocomposite HVOF-sprayed WC-Co coatings
    • D.A. Stewart, P.H. Shipway, D.G. McCartney, Abrasive wear behaviour of conventional and nanocomposite HVOF-sprayed WC-Co coatings, Wear 225-229 (1999) 789-798.
    • (1999) Wear , vol.225-229 , pp. 789-798
    • Stewart, D.A.1    Shipway, P.H.2    McCartney, D.G.3
  • 20
    • 0035897253 scopus 로고    scopus 로고
    • Wear and corrosion behaviour of thermally sprayed cermet coatings
    • D. Toma, W. Brandl, G. Marginean, Wear and corrosion behaviour of thermally sprayed cermet coatings, Surf. Coatings Tech. 138 (2001) 149-158.
    • (2001) Surf. Coatings Tech. , vol.138 , pp. 149-158
    • Toma, D.1    Brandl, W.2    Marginean, G.3
  • 21
    • 0031182364 scopus 로고    scopus 로고
    • Effect of carbide grain size on the sliding and abrasive wear behaviour of thermally sprayed WC-Co coatings
    • S. Usamani, S. Sampath, D.L. Houck, D. Lee, Effect of carbide grain size on the sliding and abrasive wear behaviour of thermally sprayed WC-Co coatings, Tribol. Trans. 40 (1997) 470-478.
    • (1997) Tribol. Trans. , vol.40 , pp. 470-478
    • Usamani, S.1    Sampath, S.2    Houck, D.L.3    Lee, D.4
  • 22
    • 0043065597 scopus 로고    scopus 로고
    • Sliding wear behaviour of HVOF sprayed WC-Co coatings deposited with both gas-fuelled and liquid-fuelled systems
    • T. Sudaprasert, P.H. Shipway, D.G. McCartney, Sliding wear behaviour of HVOF sprayed WC-Co coatings deposited with both gas-fuelled and liquid-fuelled systems, Wear 255 (2003) 943-949.
    • (2003) Wear , vol.255 , pp. 943-949
    • Sudaprasert, T.1    Shipway, P.H.2    McCartney, D.G.3
  • 23
    • 0001377883 scopus 로고
    • High temperature engineering ceramics in materials science and technology
    • M.N. Swain (Ed.), VCH Publishers Inc., New York, USA
    • K. Komeya, M. Matsui, High temperature engineering ceramics in materials science and technology, in: M.N. Swain (Ed.), Structure and Properties of Ceramics, vol. 11, VCH Publishers Inc., New York, USA, 1994, pp. 517-565.
    • (1994) Structure and Properties of Ceramics , vol.11 , pp. 517-565
    • Komeya, K.1    Matsui, M.2
  • 24
    • 0001036807 scopus 로고    scopus 로고
    • The effects of ball surface condition in the microscale abrasive wear test
    • D.N. Allsopp, R.I. Trezona, I.M. Hutchings, The effects of ball surface condition in the microscale abrasive wear test, Tribol. Lett. 5 (1998) 259-264.
    • (1998) Tribol. Lett. , vol.5 , pp. 259-264
    • Allsopp, D.N.1    Trezona, R.I.2    Hutchings, I.M.3
  • 25
    • 17144447125 scopus 로고    scopus 로고
    • Three-body abrasive wear testing of soft materials
    • R.I. Trezona, I.M. Hutchings, Three-body abrasive wear testing of soft materials, Wear 233-235 (1999) 209-221.
    • (1999) Wear , vol.233-235 , pp. 209-221
    • Trezona, R.I.1    Hutchings, I.M.2
  • 26
    • 0033387422 scopus 로고    scopus 로고
    • The role of test conditions on the microabrasive wear behaviour of soda-lime glass
    • P.H. Shipway, The role of test conditions on the microabrasive wear behaviour of soda-lime glass, Wear 233-235 (1999) 191-199.
    • (1999) Wear , vol.233-235 , pp. 191-199
    • Shipway, P.H.1
  • 27
    • 35548950679 scopus 로고
    • Hardness and deformation of cemented tungsten carbide
    • H.C. Lee, J. Gurland, Hardness and deformation of cemented tungsten carbide, Mater. Sci. Eng. 33 (1978) 125-133.
    • (1978) Mater. Sci. Eng. , vol.33 , pp. 125-133
    • Lee, H.C.1    Gurland, J.2
  • 28
    • 0033905225 scopus 로고    scopus 로고
    • Microstructural evolution in thermally sprayed WC-Co coatings: Comparison between nanocomposite and conventional starting powder
    • D.A. Stewart, P.H. Shipway, D.G. McCartney, Microstructural evolution in thermally sprayed WC-Co coatings: Comparison between nanocomposite and conventional starting powder, Acta Mater. 48 (2000) 1596-1604.
    • (2000) Acta Mater. , vol.48 , pp. 1596-1604
    • Stewart, D.A.1    Shipway, P.H.2    McCartney, D.G.3
  • 29
    • 0035482861 scopus 로고    scopus 로고
    • The wear of ultrafine WC-Co hard metals
    • C. Allen, M. Sheen, J. Williams, V.A. Pugsley, The wear of ultrafine WC-Co hard metals, Wear 250 (2001) 604-610.
    • (2001) Wear , vol.250 , pp. 604-610
    • Allen, C.1    Sheen, M.2    Williams, J.3    Pugsley, V.A.4
  • 30
    • 0035482705 scopus 로고    scopus 로고
    • Wear of tungsten carbide-cobalt hardmetals and hot isostatically pressed high speed steels under dry abrasive conditions
    • A.J. Gant, M.G. Gee, Wear of tungsten carbide-cobalt hardmetals and hot isostatically pressed high speed steels under dry abrasive conditions, Wear 251 (2001) 908-915.
    • (2001) Wear , vol.251 , pp. 908-915
    • Gant, A.J.1    Gee, M.G.2
  • 31
    • 0037444641 scopus 로고    scopus 로고
    • Microstructure formation and corrosion behaviour in HVOF-sprayed Inconel 625 coatings
    • D. Zhang, S. J. Harris, D.G. McCartney, Microstructure formation and corrosion behaviour in HVOF-sprayed Inconel 625 coatings, Mater. Sci. Eng. 344 (2003) 45-56.
    • (2003) Mater. Sci. Eng. , vol.344 , pp. 45-56
    • Zhang, D.1    Harris, S.J.2    McCartney, D.G.3
  • 32
    • 0041520643 scopus 로고    scopus 로고
    • Wear and corrosion behaviour of electrodeposited cobalt-tungsten and Cobalt-tungsten-iron alloys
    • H. Capel, P.H. Shipway, S.J. Harris, Wear and corrosion behaviour of electrodeposited cobalt-tungsten and Cobalt-tungsten-iron alloys, Wear 255 (2003) 917-923.
    • (2003) Wear , vol.255 , pp. 917-923
    • Capel, H.1    Shipway, P.H.2    Harris, S.J.3
  • 33
    • 10644255438 scopus 로고    scopus 로고
    • Role of spray system and powder feedstock on the sliding wear behaviour of WC-Co HVOF sprayed coatings
    • E. Lugscheider (Ed.), DVS, Düsseldorf
    • T. Sudaprasert, D.G. McCartney, P.H. Shipway, Role of spray system and powder feedstock on the sliding wear behaviour of WC-Co HVOF sprayed coatings, in: E. Lugscheider (Ed.), Proc. Int. Thermal Spray Conf., DVS, Düsseldorf, 2002.
    • (2002) Proc. Int. Thermal Spray Conf.
    • Sudaprasert, T.1    McCartney, D.G.2    Shipway, P.H.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.