메뉴 건너뛰기




Volumn 68, Issue 15-16, 2008, Pages 3401-3405

Axial fatigue behaviour of polyamide-6 and polyamide-6 nanocomposites at room temperature

Author keywords

A. Nanocomposites; B. Polyamide matrix; C. Fatigue; D. Modulus drop

Indexed keywords

ABS RESINS; DROPS; MACHINE DESIGN; METALLIC MATRIX COMPOSITES; NANOCOMPOSITES; POLYMERS;

EID: 55649093377     PISSN: 02663538     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.compscitech.2008.09.027     Document Type: Article
Times cited : (26)

References (14)
  • 1
    • 0242407166 scopus 로고    scopus 로고
    • Polymer/layered silicate nanocomposites: a review from preparation to processing
    • Ray S.S., and Okamoto M. Polymer/layered silicate nanocomposites: a review from preparation to processing. Prog Polym Sci 28 (2003) 1539-1641
    • (2003) Prog Polym Sci , vol.28 , pp. 1539-1641
    • Ray, S.S.1    Okamoto, M.2
  • 2
    • 21644468633 scopus 로고    scopus 로고
    • Effect of nanoclay reinforcement on tensile and tribo behavior of nylon 6
    • Srinath G., and Gnanamoorthy R. Effect of nanoclay reinforcement on tensile and tribo behavior of nylon 6. J Mater Sci 40 (2005) 2897-2901
    • (2005) J Mater Sci , vol.40 , pp. 2897-2901
    • Srinath, G.1    Gnanamoorthy, R.2
  • 3
    • 0037299802 scopus 로고    scopus 로고
    • Morphology, thermal and mechanical behavior of polyamide 6/layered-silicate nanocomposites
    • Liu T.X., Liu Z.H., Ma K.X., Shen L., Zeng K.Y., and He C.B. Morphology, thermal and mechanical behavior of polyamide 6/layered-silicate nanocomposites. Compos Sci Technol 63 (2003) 331-337
    • (2003) Compos Sci Technol , vol.63 , pp. 331-337
    • Liu, T.X.1    Liu, Z.H.2    Ma, K.X.3    Shen, L.4    Zeng, K.Y.5    He, C.B.6
  • 4
    • 30544438804 scopus 로고    scopus 로고
    • Bulk fatigue damage evolution in polyamide-6 and in a polyamide-6 nanocomposite
    • Bellemare S.C., Bureau M.N., Denault J., and Dickson J.I. Bulk fatigue damage evolution in polyamide-6 and in a polyamide-6 nanocomposite. Polym Compos 26 5 (2005) 636-646
    • (2005) Polym Compos , vol.26 , Issue.5 , pp. 636-646
    • Bellemare, S.C.1    Bureau, M.N.2    Denault, J.3    Dickson, J.I.4
  • 5
    • 0141639750 scopus 로고    scopus 로고
    • Yield and fatigue behavior of polypropylene and polyamide-6 nanocomposites
    • Mallick P.K., and Zhou Y. Yield and fatigue behavior of polypropylene and polyamide-6 nanocomposites. J Mater Sci 38 (2003) 3138-3190
    • (2003) J Mater Sci , vol.38 , pp. 3138-3190
    • Mallick, P.K.1    Zhou, Y.2
  • 6
    • 4444364926 scopus 로고    scopus 로고
    • Fatigue crack initiation and propagation in polyamide-6 and in polyamide-6 nanocomposites
    • Bellemare S.C., Bureau M.N., Denault J., and Dickson J.I. Fatigue crack initiation and propagation in polyamide-6 and in polyamide-6 nanocomposites. Polym Compos 25 4 (2004) 433-441
    • (2004) Polym Compos , vol.25 , Issue.4 , pp. 433-441
    • Bellemare, S.C.1    Bureau, M.N.2    Denault, J.3    Dickson, J.I.4
  • 7
    • 33745966434 scopus 로고    scopus 로고
    • Characterization of the tensile fatigue behavior of RTM-laminates by isocyclic stress-strain diagrams
    • Pinter G., Ladstatter E., Billinger W., and Lang R.W. Characterization of the tensile fatigue behavior of RTM-laminates by isocyclic stress-strain diagrams. Int J Fatigue 28 (2006) 1277-1283
    • (2006) Int J Fatigue , vol.28 , pp. 1277-1283
    • Pinter, G.1    Ladstatter, E.2    Billinger, W.3    Lang, R.W.4
  • 8
    • 1942456670 scopus 로고    scopus 로고
    • Creep resistant polymeric nanocomposites
    • Zhang Z., Yang J.-L., and Friedrich K. Creep resistant polymeric nanocomposites. Polymer 45 (2004) 3481-3485
    • (2004) Polymer , vol.45 , pp. 3481-3485
    • Zhang, Z.1    Yang, J.-L.2    Friedrich, K.3
  • 9
    • 23044438542 scopus 로고    scopus 로고
    • Experimental study on thermal and mechanical behavior of polypropylene, talc/polypropylene and polypropylene/clay nanocomposites
    • Zhou Y., Rangari V., Mahfuz H., Jeelani S., and Mallick P.K. Experimental study on thermal and mechanical behavior of polypropylene, talc/polypropylene and polypropylene/clay nanocomposites. Mater Sci Eng A 402 (2005) 109-117
    • (2005) Mater Sci Eng A , vol.402 , pp. 109-117
    • Zhou, Y.1    Rangari, V.2    Mahfuz, H.3    Jeelani, S.4    Mallick, P.K.5
  • 10
    • 33846947117 scopus 로고    scopus 로고
    • Mechanics of polymer-clay nanocomposites
    • Rao Y., and Pochan J.M. Mechanics of polymer-clay nanocomposites. Macromolecules 40 (2007) 290-296
    • (2007) Macromolecules , vol.40 , pp. 290-296
    • Rao, Y.1    Pochan, J.M.2
  • 11
    • 8644292555 scopus 로고    scopus 로고
    • The coupled thermal and mechanical influence on a glassy thermoplastic polyamide: nylon 6,6 under vibro-creep
    • Liu Z.Y., Beniwal S., Jenkins C.H.M., and Winter R.M. The coupled thermal and mechanical influence on a glassy thermoplastic polyamide: nylon 6,6 under vibro-creep. Mech Time-Dependent Mater 8 (2004) 235-253
    • (2004) Mech Time-Dependent Mater , vol.8 , pp. 235-253
    • Liu, Z.Y.1    Beniwal, S.2    Jenkins, C.H.M.3    Winter, R.M.4
  • 12
    • 0015972395 scopus 로고
    • Cyclic stress fatigue and thermal softening failure of a thermoplastic
    • Crawford R.J., and Benham P.P. Cyclic stress fatigue and thermal softening failure of a thermoplastic. J Mater Sci 9 (1974) 18-28
    • (1974) J Mater Sci , vol.9 , pp. 18-28
    • Crawford, R.J.1    Benham, P.P.2
  • 13
    • 0037474758 scopus 로고    scopus 로고
    • Hysteretic heating of modified polymethylmethacrylate
    • Rittel D., Eliash N., and Halary J.L. Hysteretic heating of modified polymethylmethacrylate. Polymer 44 (2003) 2817-2822
    • (2003) Polymer , vol.44 , pp. 2817-2822
    • Rittel, D.1    Eliash, N.2    Halary, J.L.3
  • 14
    • 0242500882 scopus 로고    scopus 로고
    • Effect of sample thickness on the mechanical properties of injection-molded polyamide-6 and polyamide-6 clay nanocomposites
    • Paola U.-A., Mehler C., Puskas J.E., and Altstädt V. Effect of sample thickness on the mechanical properties of injection-molded polyamide-6 and polyamide-6 clay nanocomposites. Polymer 44 (2003) 2441-2446
    • (2003) Polymer , vol.44 , pp. 2441-2446
    • Paola, U.-A.1    Mehler, C.2    Puskas, J.E.3    Altstädt, V.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.