1
-
-
5544277047
-
The tribological characteristics of A356.2Al. alloy/Gr composites
-
Yang J.B., Lin C.B., Wang T.C., and Chu H.Y. The tribological characteristics of A356.2Al. alloy/Gr composites. Wear 257 (2004) 941-952
-
(2004)
Wear
, vol.257
, pp. 941-952
-
-
Yang, J.B.1
Lin, C.B.2
Wang, T.C.3
Chu, H.Y.4
-
2
-
-
0038278422
-
Graphite flake carbon composites with a 'sinterable' microbed matrix
-
Mirhabibi A., Rand B., Baghshahi S., and Agha B.Z. Graphite flake carbon composites with a 'sinterable' microbed matrix. Carbon 41 (2003) 1593-1603
-
(2003)
Carbon
, vol.41
, pp. 1593-1603
-
-
Mirhabibi, A.1
Rand, B.2
Baghshahi, S.3
Agha, B.Z.4
-
3
-
-
0036680515
-
Tribological behavior of aluminium/SiC/nickel-coated graphite hybrid composites
-
Ted Guo M.L., and Tsao Chi.-Y.A. Tribological behavior of aluminium/SiC/nickel-coated graphite hybrid composites. Mater. Sci. Eng. A 333 (2002) 134-145
-
(2002)
Mater. Sci. Eng. A
, vol.333
, pp. 134-145
-
-
Ted Guo, M.L.1
Tsao, Chi.-Y.A.2
-
4
-
-
1542288263
-
3 and/or carbon short fibre reinforced Al-12Si alloy composites
-
3 and/or carbon short fibre reinforced Al-12Si alloy composites. Wear 256 (2004) 275-285
-
(2004)
Wear
, vol.256
, pp. 275-285
-
-
Liu, Y.-H.1
Jun, D.2
Yu, S.-R.3
Wang, W.4
-
5
-
-
6344270098
-
Strength and fracture toughness of interpenetrating graphite/aluminium composites produced by the indirect squeeze casting process
-
Etter T., Kuebler J., Frey T., Schulz P., Loffler J.F., and Uggowitzer P.J. Strength and fracture toughness of interpenetrating graphite/aluminium composites produced by the indirect squeeze casting process. Mater. Sci. Eng. A 386 (2004) 61-67
-
(2004)
Mater. Sci. Eng. A
, vol.386
, pp. 61-67
-
-
Etter, T.1
Kuebler, J.2
Frey, T.3
Schulz, P.4
Loffler, J.F.5
Uggowitzer, P.J.6
-
6
-
-
0033639789
-
Tribological behavior of self-lubricating aluminium/Sic/graphite hybrid composites. synthesized by the semi-solid powder-desification method
-
Ted Guo M.L., and Tsao C.-Y.A. Tribological behavior of self-lubricating aluminium/Sic/graphite hybrid composites. synthesized by the semi-solid powder-desification method. Compos. Sci. Technol. 60 (1999) 65-74
-
(1999)
Compos. Sci. Technol.
, vol.60
, pp. 65-74
-
-
Ted Guo, M.L.1
Tsao, C.-Y.A.2
-
7
-
-
4344637029
-
Wear performance of 2014 Al. Alloy reinforced with continuous carbon fibres manufactured by gas pressure infiltration
-
Daoud A. Wear performance of 2014 Al. Alloy reinforced with continuous carbon fibres manufactured by gas pressure infiltration. Mater. Lett. 58 (2004) 3206-3213
-
(2004)
Mater. Lett.
, vol.58
, pp. 3206-3213
-
-
Daoud, A.1
-
8
-
-
0031279014
-
3/C hybrid metal matrix composites
-
3/C hybrid metal matrix composites. Compos. Struct. 39 (1997) 309-318
-
(1997)
Compos. Struct.
, vol.39
, pp. 309-318
-
-
Song, J.I.1
Han, K.S.2
-
9
-
-
5644276477
-
3 and carbon short fibers reinforced Al-Si12 alloy hybrid composites
-
3 and carbon short fibers reinforced Al-Si12 alloy hybrid composites. Wear 257 (2004) 930-940
-
(2004)
Wear
, vol.257
, pp. 930-940
-
-
Jun, D.1
Liu, Y.-H.2
Yu, S.-R.3
Li, W.-F.4
-
10
-
-
1842686713
-
3/Al and Saffil/Sic/Al hydrid metal matrix composites
-
3/Al and Saffil/Sic/Al hydrid metal matrix composites. Wear 256 (2004) 705-713
-
(2004)
Wear
, vol.256
, pp. 705-713
-
-
Fu, H.-H.1
Han, K.-S.2
Song, J.-I.3
-
11
-
-
0033300445
-
Wear-resistance mechanism of an Al-12Si alloy reinforced with aluminosilicate short fibers
-
Cao G.H., Wu S.Q., Liu J.M., and Liu Z.g. Wear-resistance mechanism of an Al-12Si alloy reinforced with aluminosilicate short fibers. Tribology 32 (1999) 721-724
-
(1999)
Tribology
, vol.32
, pp. 721-724
-
-
Cao, G.H.1
Wu, S.Q.2
Liu, J.M.3
Liu, Z.g.4
-
13
-
-
0031251708
-
Friction and wear characteristics of Al-Cu/C composites synthesised using partial liquid phase casting process
-
Lim S.C., Gupta M., and Ng W.B. Friction and wear characteristics of Al-Cu/C composites synthesised using partial liquid phase casting process. Mater. Des. 18 (1997) 161-166
-
(1997)
Mater. Des.
, vol.18
, pp. 161-166
-
-
Lim, S.C.1
Gupta, M.2
Ng, W.B.3
-
14
-
-
0345392703
-
Influence of carbon fibre content on the processing and tribological properties of silico nitride/carbon fibre composites
-
Hyuga H., Mark J.I., Hirao K., and Yamauchi Y. Influence of carbon fibre content on the processing and tribological properties of silico nitride/carbon fibre composites. J. Eur. Ceram. Soc. 24 (2004) 877-885
-
(2004)
J. Eur. Ceram. Soc.
, vol.24
, pp. 877-885
-
-
Hyuga, H.1
Mark, J.I.2
Hirao, K.3
Yamauchi, Y.4
-
15
-
-
0034295248
-
Technology and mechanical properties of ceramic preforms for composite materials
-
Naplocha K., Janus A., Kaczmar J., and Samsonowicz Z. Technology and mechanical properties of ceramic preforms for composite materials. J. Mater. Process. Technol. 106 1-3 (2000) 119-122
-
(2000)
J. Mater. Process. Technol.
, vol.106
, Issue.1-3
, pp. 119-122
-
-
Naplocha, K.1
Janus, A.2
Kaczmar, J.3
Samsonowicz, Z.4
-
16
-
-
0942278704
-
Thermoexfoliated graphite as support for production of metal-graphite nanocomposites
-
Vovchenko L., Matzui L., Zakharenko M., Babich M., and Brusilovetz A. Thermoexfoliated graphite as support for production of metal-graphite nanocomposites. J. Phys. Chem. Solids 65 (2004) 171-175
-
(2004)
J. Phys. Chem. Solids
, vol.65
, pp. 171-175
-
-
Vovchenko, L.1
Matzui, L.2
Zakharenko, M.3
Babich, M.4
Brusilovetz, A.5
-
17
-
-
0039763788
-
On the role of brittle interfacial phases on the mechanical properties of carbon fibre reinforced Al-based matrix composites
-
Vidal-Setif M.H., Lancin M., Marhic C., Valle R., Raviart J.L., Daux J.C., and Robinovitch M. On the role of brittle interfacial phases on the mechanical properties of carbon fibre reinforced Al-based matrix composites. Mater. Sci. Eng. A 272 (1999) 321-333
-
(1999)
Mater. Sci. Eng. A
, vol.272
, pp. 321-333
-
-
Vidal-Setif, M.H.1
Lancin, M.2
Marhic, C.3
Valle, R.4
Raviart, J.L.5
Daux, J.C.6
Robinovitch, M.7
-
19
-
-
0032640067
-
Eustathopoulos, the role of Van der Waals interactions on wetting and adhesion in metal/carbon systems
-
Dezellus N. Eustathopoulos, the role of Van der Waals interactions on wetting and adhesion in metal/carbon systems. Scripta Mater. 40 11 (1999) 1283-1288
-
(1999)
Scripta Mater.
, vol.40
, Issue.11
, pp. 1283-1288
-
-
Dezellus, N.1
-
20
-
-
0029454203
-
Mechanical properties of cast ZA-27/graphite particulate composites
-
Seah K.H.W. Mechanical properties of cast ZA-27/graphite particulate composites. Mater. Des. 16 (1995) 272-275
-
(1995)
Mater. Des.
, vol.16
, pp. 272-275
-
-
Seah, K.H.W.1
-
21
-
-
0032648930
-
The incorporation of ceramic particles in molten aluminium and the relationship to contact angle data
-
Kennedy A.R., and Karantzalis A.E. The incorporation of ceramic particles in molten aluminium and the relationship to contact angle data. Mater. Sci. Eng. A 264 (1998) 122-129
-
(1998)
Mater. Sci. Eng. A
, vol.264
, pp. 122-129
-
-
Kennedy, A.R.1
Karantzalis, A.E.2
-
22
-
-
3042796969
-
Effect of the reinforcement volume fraction on the dry sliding wear behaviour of Al-10Si/SiCp composites produced by vacuum infiltration technique
-
Gul F., and Acilar M. Effect of the reinforcement volume fraction on the dry sliding wear behaviour of Al-10Si/SiCp composites produced by vacuum infiltration technique. Compos. Sci. Technol. 64 (2004) 1959-1970
-
(2004)
Compos. Sci. Technol.
, vol.64
, pp. 1959-1970
-
-
Gul, F.1
Acilar, M.2
|