Volumn 39, Issue 3-4, 1997, Pages 309-318

Effect of volume fraction of carbon fibers on wear behavior of Al/Al2O3/C hybrid metal matrix composites

Author keywords

[No Author keywords available]

Indexed keywords

FIBER; FILM; PROCESS DEVELOPMENT;

EID: 0031279014     PISSN: 02638223     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0263-8223(97)00124-4     Document Type: Article
Times cited : (63)

References (26)
  • 3
    • 0042281971 scopus 로고
    • Microstructural studies of d-alumina fiber reinforced aluminum and Al alloys
    • Bengtson, S., Li, C. H. & Warren, R., Microstructural studies of d-alumina fiber reinforced aluminum and Al alloys. Proceedings ICCM - VIII, 1989, 3, pp. 607-12.
    • (1989) Proceedings ICCM - VIII , vol.3 , pp. 607-612
    • Bengtson, S.1    Li, C.H.2    Warren, R.3
  • 4
    • 0024613048 scopus 로고
    • Microwave processing of ceramic materials
    • Sutton, W. H., Microwave processing of ceramic materials. Ceramic Bulletin 1989, 68, (2), 376-386.
    • (1989) Ceramic Bulletin , vol.68 , Issue.2 , pp. 376-386
    • Sutton, W.H.1
  • 6
    • 0017012093 scopus 로고
    • Progress in the development of graphite-aluminum composites using liquid infiltration technology
    • Amateau, M. F., Progress in the development of graphite-aluminum composites using liquid infiltration technology. J. Comp. Mat. 1976, 10, 279-296.
    • (1976) J. Comp. Mat. , vol.10 , pp. 279-296
    • Amateau, M.F.1
  • 7
    • 0024734070 scopus 로고
    • Microstructure and wear of cast (Al-Si alloy)-graphite composites
    • Das, S. and Prasad, S. V., Microstructure and wear of cast (Al-Si alloy)-graphite composites. Wear 1989, 133, 173-187.
    • (1989) Wear , vol.133 , pp. 173-187
    • Das, S.1    Prasad, S.V.2
  • 8
    • 0022113457 scopus 로고
    • Strength and interfacial reaction of high modulus carbon fiber reinforced aluminum matrix
    • Towata, S., Yamada, S. and Ohwaki, S., Strength and interfacial reaction of high modulus carbon fiber reinforced aluminum matrix. Transactions of the Japan Institute of Methods 1985, 26, (8), 563-570.
    • (1985) Transactions of the Japan Institute of Methods , vol.26 , Issue.8 , pp. 563-570
    • Towata, S.1    Yamada, S.2    Ohwaki, S.3
  • 12
    • 0038586665 scopus 로고
    • Mechanical properties of squeeze cast zinc-aluminum composites
    • Dionne, S., Lo, S. H. J. and Carpenter, G. J. C,. Mechanical properties of squeeze cast zinc-aluminum composites. ICCM9 1993, 1, 195-202.
    • (1993) ICCM9 , vol.1 , pp. 195-202
    • Dionne, S.1    Lo, S.H.J.2    Carpenter, G.J.C.3
  • 13
    • 0027187426 scopus 로고
    • 3/Al alloy composites and their effects on mechanical properties
    • 3/Al alloy composites and their effects on mechanical properties. Composites Science and Technology 1993, 46, 245-252.
    • (1993) Composites Science and Technology , vol.46 , pp. 245-252
    • Liu, X.C.1    Bathias, C.2
  • 14
    • 0023401555 scopus 로고
    • The effect of matrix properties on reinforcement in short alumina fibre-aluminum MMC's
    • Friend, C. M., The effect of matrix properties on reinforcement in short alumina fibre-aluminum MMC's. J. of Material Science 1987, 22, 3005-3010.
    • (1987) J. of Material Science , vol.22 , pp. 3005-3010
    • Friend, C.M.1
  • 15
    • 0042678778 scopus 로고
    • Performance characteristics of metal ceramic composites made by the squeeze casting process
    • Suresh, K. V. and John, L. D., Performance characteristics of metal ceramic composites made by the squeeze casting process. Ceram. Eng. Sci. Proc. 1888, 9, 579-596.
    • (1888) Ceram. Eng. Sci. Proc. , vol.9 , pp. 579-596
    • Suresh, K.V.1    John, L.D.2
  • 17
    • 0026905367 scopus 로고
    • Wear behavior of hybrid metal matrix composite materials
    • Park, H. C., Wear behavior of hybrid metal matrix composite materials. Scripta Metallurgical et Materialia 1993, 27, 465-470.
    • (1993) Scripta Metallurgical et Materialia , vol.27 , pp. 465-470
    • Park, H.C.1
  • 18
    • 33645133683 scopus 로고
    • Wear behavior of aluminium matrix composite materials
    • Lee, C. S., Kim, Y. H., Han, K. S. and Lim, T., Wear behavior of aluminium matrix composite materials. J. of Materials Science 1992, 27, 793-800.
    • (1992) J. of Materials Science , vol.27 , pp. 793-800
    • Lee, C.S.1    Kim, Y.H.2    Han, K.S.3    Lim, T.4
  • 19
    • 0002884895 scopus 로고
    • Friction behavior of ceramic fiber-reinforced aluminum metal-matrix composites against a 440C steel counterface
    • Prasad, S. V. and Mecklenburg, K. R., Friction behavior of ceramic fiber-reinforced aluminum metal-matrix composites against a 440C steel counterface. Wear 1993, 162-164, 47-56.
    • (1993) Wear , vol.162-164 , pp. 47-56
    • Prasad, S.V.1    Mecklenburg, K.R.2
  • 21
    • 0026223444 scopus 로고
    • Tribology of aluminum metal-matrix composites: Lubrication by graphite
    • Prasad, S. V. and McConnell, B. D., Tribology of aluminum metal-matrix composites: lubrication by graphite. Wear 1991, 149, 241-253.
    • (1991) Wear , vol.149 , pp. 241-253
    • Prasad, S.V.1    McConnell, B.D.2
  • 22
    • 0026154906 scopus 로고
    • Tribology of Al-Si alloy composites: Triboinduced graphite films and the silicon morphology
    • Das, S., Prasad, S. V. and Ramachandran, T. R., Tribology of Al-Si alloy composites: triboinduced graphite films and the silicon morphology. Materials Science and Engineering 1993, A138, 123-132.
    • (1993) Materials Science and Engineering , vol.A138 , pp. 123-132
    • Das, S.1    Prasad, S.V.2    Ramachandran, T.R.3
  • 24
    • 0042678779 scopus 로고    scopus 로고
    • Data Sheet from Japanese Industrial Standards (JIS) H 5303
    • Data Sheet from Japanese Industrial Standards (JIS) H 5303
  • 25
    • 0043179727 scopus 로고    scopus 로고
    • Data Sheet from ICI Co.
    • Data Sheet from ICI Co.
  • 26
    • 0042177584 scopus 로고    scopus 로고
    • Data Sheet from Kureha Co.
    • Data Sheet from Kureha Co.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.